CN202293489U - Composite facing material - Google Patents
Composite facing material Download PDFInfo
- Publication number
- CN202293489U CN202293489U CN2011203589715U CN201120358971U CN202293489U CN 202293489 U CN202293489 U CN 202293489U CN 2011203589715 U CN2011203589715 U CN 2011203589715U CN 201120358971 U CN201120358971 U CN 201120358971U CN 202293489 U CN202293489 U CN 202293489U
- Authority
- CN
- China
- Prior art keywords
- layer
- plastic film
- facing material
- paper bearing
- finishing material
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Abstract
The utility model relates to a composite facing material, which comprises a kraft paper bearing layer. A main plastic film layer, an aluminum foil layer, an auxiliary plastic film layer, a paper layer, a veneer layer and a coating layer are sequentially piled on the kraft paper bearing layer. Therefore, unexpected folding of lagging can be effectively avoided, whole attachment and gluing effects are better simultaneously, more importantly the aluminum foil layer has good inflaming retarding effect, and safety performance of products is promoted accordingly. In addition, the composite facing material removes a fussy brush coating process during decoration using, using is simple and convenient, and the composite facing material can be applicable to decoration of various panel furniture.
Description
Technical field
The utility model relates to a kind of lagging ornament materials, relates in particular to a kind of compound finishing material.
Background technology
Use wooden skin in the interior decoration industry through regular meeting, in work progress, directly wooden skin is attached to the surface of all kinds of furniture; Brush paint then, the shortcoming of this site operation brush paint is: paint is prone to reveal the exact details, bubbles, influences attractive in appearance, and; The site operation cycle is long, and construction is inconvenient, and labour intensity is big; Use cost is high, and paint also can pollute metope and ground.This wooden skin does not have fire prevention, moisture-proof function simultaneously; In addition, existing wooden micromicro still can not bend to curl; More can not be used to coat the knuckle more than 90 ° or 90 °; Be that it can not carry out 90 ° of bendings that reach greater than 90 °, influence the scope of application of wooden skin, this also is the bottleneck difficult problem of wooden skin in decoration industry uses.
The utility model content
The purpose of the utility model is exactly the problems referred to above that exist in the prior art in order to solve, and a kind of compound finishing material is provided.
The purpose of the utility model realizes through following technical scheme:
Compound finishing material includes the brown paper bearing bed, wherein: stacked gradually main plastic film layers, aluminium foil layer, secondary plastic film layers, ply of paper, wooden cortex, application layer on the described brown paper bearing bed.
Further, above-mentioned compound finishing material, wherein: described brown paper bearing bed, main plastic film layers, aluminium foil layer, secondary plastic film layers, ply of paper, wooden cortex are distributed with adhesive linkage between the interval of each layer.
Further, above-mentioned compound finishing material, wherein: depended on protective film on the described application layer.
Again further, above-mentioned compound finishing material, wherein: be distributed with the oiliness mucigel under the described brown paper bearing bed, described oiliness mucigel is attached with release liners outward.
The advantage of the utility model technical scheme is mainly reflected in: can prevent effectively that unexpected fold from appearring in lagging, simultaneously whole to depend on stickiness better.What is more important, aluminium foil layer have flame retardant effect preferably, have promoted the safety of products performance.In addition, the utility model has been removed loaded down with trivial details brush coating process from when decorate using, use simple and easy, applicable to the decoration of various sheet material furniture.
Description of drawings
The purpose of the utility model, advantage and characteristics will illustrate through the non-limitative illustration of following preferred embodiment and explain.These embodiment only are the prominent examples of using the utility model technical scheme, and all technical schemes of taking to be equal to replacement or equivalent transformation and forming all drop within the scope of the utility model requirement protection.In the middle of these accompanying drawings,
Fig. 1 is the organigram of compound finishing material.
The specific embodiment
Compound finishing material as shown in Figure 1; Include brown paper bearing bed 8, its unusual part is: stacked gradually main plastic film layers 7, aluminium foil layer 6, secondary plastic film layers 5, ply of paper 4, wooden cortex 3, application layer 2 on the brown paper bearing bed 8 that the utility model adopted.Thus, rely on the existence of aluminium foil layer 6, can prevent effectively that unexpected fold from appearring in lagging, simultaneously whole to depend on stickiness better, can be applicable to the decoration of various sheet material furniture.
With regard to the utility model one preferred implementation; Consider between each layer and can effectively be connected tight; Make the whole thickness of lagging to reduce; At brown paper bearing bed 8, main plastic film layers 7, aluminium foil layer 6, secondary plastic film layers 5, ply of paper 4, wooden cortex 3, be distributed with adhesive linkage between the interval of each layer.Like this, it is identical to guarantee that in actual manufacture process each laminating closes.
Further, for the back in operating period between application layer 2 is carried out proper protection, the prevention cut, on described application layer 2, depended on protective film 1.
Again further, consider that can be convenient to the workmen fits, and can remove loaded down with trivial details brush coating process from simultaneously.Be distributed with oiliness mucigel 98 times at the brown paper bearing bed, the described oiliness mucigel 9 outer release liners 10 that are attached with.
In conjunction with the actual manufacturing situation of the utility model, wooden cortex 3 is formed through operation manufacturings such as screening, bag cage, bleaching, dyeing, dehydration and oven dry by wooden skin.Wooden skin after the dyeing is thought and acted in one and the same way, and stands polishing and handles, and shows the wooden decorative pattern of wooden skin more especially, can remove the special-shaped defective in the wooden skin, flaw.
Can find out through above-mentioned character express, adopt the utility model after, can prevent effectively that unexpected fold from appearring in lagging, it is whole simultaneously that to depend on stickiness better.What is more important, aluminium foil layer have flame retardant effect preferably, have promoted the safety of products performance.In addition, the utility model has been removed loaded down with trivial details brush coating process from when decorate using, use simple and easy, applicable to the decoration of various sheet material furniture.
Claims (4)
1. compound finishing material includes the brown paper bearing bed, it is characterized in that: stacked gradually main plastic film layers, aluminium foil layer, secondary plastic film layers, ply of paper, wooden cortex, application layer on the described brown paper bearing bed.
2. compound finishing material according to claim 1 is characterized in that: described brown paper bearing bed, main plastic film layers, aluminium foil layer, secondary plastic film layers, ply of paper, wooden cortex are distributed with adhesive linkage between the interval of each layer.
3. compound finishing material according to claim 1 is characterized in that: depended on protective film on the described application layer.
4. compound finishing material according to claim 1 is characterized in that: be distributed with the oiliness mucigel under the described brown paper bearing bed, described oiliness mucigel is attached with release liners outward.