CN202209483U - 内衬钢板的混凝土管 - Google Patents
内衬钢板的混凝土管 Download PDFInfo
- Publication number
- CN202209483U CN202209483U CN2011203348742U CN201120334874U CN202209483U CN 202209483 U CN202209483 U CN 202209483U CN 2011203348742 U CN2011203348742 U CN 2011203348742U CN 201120334874 U CN201120334874 U CN 201120334874U CN 202209483 U CN202209483 U CN 202209483U
- Authority
- CN
- China
- Prior art keywords
- pipe
- steel plate
- concrete
- construction
- concrete pipe
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
一种内衬钢板的混凝土管,在钢筋混凝土管外壁的内壁上装有内衬钢板。这种管道将钢筋混凝土排水管和钢管进行了结合,这种管道既可以采用沟槽式施工又可以采用顶进施工,而且工作压力可以根据调整内衬钢板的厚度或者调整混凝土的配筋量来实现,因此可满足既需要高工压又需要顶进施工的工况要求。另外由于钢板置于混凝土管的内壁,混凝土会很好的保护钢管大大提高了管道的使用寿命。
Description
技术领域:
本实用新型属于一种混凝土管,特别涉及一种内衬钢板的混凝土管。
背景技术:
目前国内给排水管道主要有预应力混凝土管、预应力钢筒混凝土管、钢筋混凝土排水管、玻璃钢管和钢管等几种。每一种管道都有存在自身的不足。
1、预应力混凝土管:承压范围为0.2-2Mpa、施工采用沟槽式施工方法,管道的制造成本低、设备成本较高。
2、预应力钢筒混凝土管:承压范围为0.2-2Mpa、采用沟槽式施工方法、管道的制造成本较高、设备成本高。
3、钢筋混凝土排水管:承压范围最高为0.2Mpa、采用沟槽式施工或顶进式施工方法、管道的制造成本低、设备成本低。
4、玻璃钢管:承压范围为0.2-2Mpa、采用沟槽式施工方法、管道的制造成本高、设备成本较高。
5、钢管:承压范围依照板厚确定、采用沟槽式施工或顶进式施工方法、管道的制造成本高、设备成本低。
由此看出,预应力混凝土管、预应力钢筒混凝土管虽然承受内水压力的性能比较优越,但是施工方法受到了限制,在管道安装的过程中势必会产生工程变更、拆迁或者改线的难题;钢筋混凝土排水管虽然可以采用沟槽施工和顶进施工,但是其抗内水压的能力比较低最高0.2MPa;玻璃钢管由于其抗外压荷载的能力比较低,加之制造成本和设备成本都比较高,目前国内给排水市场所占的份额很小;对于钢管不管是在抗水压能力,还是施工方法以及生产成本方面都可以和其他管道媲美,但是在顶进施工过程中由于管子外壁要与土壤摩擦,防腐涂层很容易破损,这样一来管道的使用寿命将会大幅度的降低。
发明内容:
本实用新型的目的就在于克服上述现有技术中存在的不足,而提供一种内衬钢板的混凝土管,这种管道将钢筋混凝土排水管和钢管进行了结合,这种管道既可以采用沟槽式施工又可以采用顶进施工,而且工作压力可以根据调整内衬钢板的厚度或者调整混凝土的配筋量来实现,因此可满足既需要高工压又需要顶进施工的工况要求。另外由于钢板置于混凝土管的内壁,混凝土会很好的保护钢管大大提高了管道的使用寿命。
如上构思,本实用新型的技术方案是:一种内衬钢板的混凝土管,包括钢筋混凝土管,其特征在于:在钢筋混凝土管外壁的内壁上装有内衬钢板。
本实用新型具有如下的优点和积极效果:
1、这种管子既具有钢筋混凝土管外压承载力高、制造成本低、施工方式灵活的优点,同时还具备钢板的内压承载力高、接头密封性能好以的特点,可以说时将钢筋混凝土管和压力钢板的完美组合。
2、这种管子弥补了压力钢板在顶进施工过程中对防腐涂层的破坏,整个钢板全部用钢筋混凝土进行了保护,延长了管道的使用寿命,整个管道的设计使用寿命统一可达到50年。
附图说明:
图1是本实用新型采用沟槽式施工时的剖面示意图。
图2是本实用新型采用顶进施工时使用钢承口管的剖面示意图。
具体实施方式:
如图1所示:一种内衬钢板的混凝土管,在钢筋混凝土管外壁1的内壁上装有内衬钢板2。沟槽式施工采用本实用新型时,将多节管道的内衬钢板进行焊接,焊接完毕后从砂浆封口3向焊缝4处注入砂浆,这样保证了焊缝的密闭性。
如图2所示:一种内衬钢板的混凝土管,在钢筋混凝土管外壁1的内壁上装有内衬钢板2。顶进施工采用本实用新型时,将多节管道的承口5与插口6接头相接后用橡胶密封圈7密封,同时将管道内的内衬钢板进行焊接,焊接完毕后形成焊缝8。本实用新型弥补了压力钢板在顶进施工过程中对防腐涂层的破坏,是整个钢板全部用钢筋混凝土进行了保护,从而延长了管道的使用寿命。一般来讲,钢筋混凝土的设计使用寿命为50年,钢管的设计使用寿命为25年(主要依据钢管防腐涂层的质量以及防腐涂料的使用寿命而定),而将这种管子进行组合即达到了管道高工压的要求,又使使整个管道的设计使用寿命统一达到了50年。
Claims (1)
1.一种内衬钢板的混凝土管,包括钢筋混凝土管,其特征在于:在钢筋混凝土管外壁的内壁上装有内衬钢板。