Prior art keywords
aluminium alloy
upsetting
casing
alloy forging
pier
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2011202600223U
Other languages
English (en)
Inventor
胡昌胜
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
YANTAI HUIZHONG AUTOMOTIVE CHASSIS SYSTEMS CO., LTD.
Original Assignee
Shanghai Huizhong Automotive Manufacturing Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shanghai Huizhong Automotive Manufacturing Co Ltd filed Critical Shanghai Huizhong Automotive Manufacturing Co Ltd
Priority to CN2011202600223U priority Critical patent/CN202199709U/zh
Application granted granted Critical
Publication of CN202199709U publication Critical patent/CN202199709U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Links

Images

Landscapes

  • Shaping Metal By Deep-Drawing, Or The Like (AREA)

Abstract

本实用新型的目的在于提供一种铝合金锻造墩粗制坯套管,以减少或消除铝合金材料膨胀后与墩粗套管之间挤压产生的铝合金材料上的锐角。该铝合金锻造墩粗制坯套管,其特征在于,在开口端的内侧有不同半径的圆角。

Description

铝合金锻造墩粗制坯套管
技术领域
本实用新型涉及套管。
背景技术
现有的铝合金墩粗制坯方式:如图1所示,采用铝合金圆柱棒料12a加以上下两个墩粗套管11的形式在压力机台面上加压,使之局部变粗形成合适的毛坯形状12b,再进行锻压成型。该种形式区别于传统的楔横轧、弯曲、压扁等制坯工艺,具有工艺简单、速度快的优势。使用中发现该种制坯形式存在以下缺点:
1、由于铝合金材料12a膨胀后与墩粗套管11之间挤压(在倒角110、111处,倒角110、111在相对两侧,圆角特征相同),在材料表面形成明显的锐角环121,该锐角如不进行打磨直接锻打,极易造成锻造缺陷。
2、该制坯形式墩粗后材料在中部区域会出现均匀分布的凸肚形状122,该形状部分材料是锻造过程中易于锻造成型的,但由于锐角环121的形成,多余的材料会在锻造过程中形成较深的锻造折叠,严重影响铝合金锻件质量。
实用新型内容
本实用新型的目的在于提供一种铝合金锻造墩粗制坯套管,以减少或消除铝合金材料膨胀后与墩粗套管之间挤压产生的铝合金材料上的锐角。
铝合金锻造墩粗制坯套管,其特点是,在开口端的内侧有不同半径的圆角。
本实用新型对传统制坯套管圆角部分进行改进,使用不同的R值(半径值)使材料流动产生不均匀现象,在圆柱型材料中间部分可产生单边凸肚,制成单边凸肚毛坯,大的R角有效减小了凸肚部分挤压锐角的程度。利用传统制坯形式的优点,能够有效满足锻造过程中对材料分配的要求。且大量减少锻造缺陷,实际使用中至少减少锻造缺陷50%以上。
附图说明
图1是已有的铝合金锻造墩粗制坯套管的工作原理图。
图2是本实用新型的一实施例的铝合金锻造墩粗制坯套管的工作原理图。
具体实施方式
如图2所示,铝合金锻造墩粗制坯套管21的开口端的内侧的两相对边有不同半径的圆角210、211,圆角211的半径大于圆角210的半径,这样就使材料流动产生不均匀现象,材料流动主要朝圆角半径大的侧边,在圆柱型材料毛坯形状22b中间部分产生单边凸肚222,大的圆角有效减小了凸肚222部分挤压锐角的程度。

Claims (1)

1.铝合金锻造墩粗制坯套管,其特征在于,在开口端的内侧有不同半径的圆角。
CN2011202600223U 2011-07-21 2011-07-21 铝合金锻造墩粗制坯套管 Expired - Fee Related CN202199709U (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN2011202600223U CN202199709U (zh) 2011-07-21 2011-07-21 铝合金锻造墩粗制坯套管

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN2011202600223U CN202199709U (zh) 2011-07-21 2011-07-21 铝合金锻造墩粗制坯套管

Publications (1)

Publication Number Publication Date
CN202199709U true CN202199709U (zh) 2012-04-25

Family

ID=45963847

Family Applications (1)

Application Number Title Priority Date Filing Date
CN2011202600223U Expired - Fee Related CN202199709U (zh) 2011-07-21 2011-07-21 铝合金锻造墩粗制坯套管

Country Status (1)

Country Link
CN (1) CN202199709U (zh)

Similar Documents

Publication Publication Date Title
CN101780507B (zh) 深方筒形金属外壳的制造方法
CN203991724U (zh) 铝合金棒材生产模具
CN102039361A (zh) 一种汽车突缘叉的复合挤锻压成型方法
CN104947587A (zh) 一种u型肋及其制造方法
CN103846331A (zh) 大型薄壁复杂特征板材双向加压充液成形方法
CN103949544B (zh) 一种冲压件侧壁卷曲回弹控制冲压装置
CN100493821C (zh) 一种铁路货车用钩尾框的制造方法
CN2126120U (zh) 三通管接头轴压成型装置
CN104826919A (zh) 一种用于铝合金锻件的冲孔方法及冲子结构
CN202199709U (zh) 铝合金锻造墩粗制坯套管
CN202045311U (zh) 铁路货车制动拉杆的长棒料连续墩粗装置
CN103447770A (zh) 制造管卡的方法、管卡与管道
CN105344906A (zh) 矩形锻件的径锻机的锻打工艺
CN105414432A (zh) 一种矩形锻件的径锻机
CN102172627A (zh) 一种复合绝缘子金具螺旋孔型斜轧轧辊孔型的设计方法
CN104028685B (zh) 一种l型截面大锻件制坯方法
CN201736734U (zh) 15°dc无内胎对称式型钢轮辋车轮
CN205009912U (zh) 一种采用不等厚板制成的底盘扭转梁
CN106042816A (zh) 一种多焊道的高强度不等壁厚汽车扭转梁及其成形工艺
CN208728607U (zh) 汽车前轴第二道次辊锻模
CN105215635A (zh) 一种冷加工无缝铝合金轮毂的制备方法
CN202900960U (zh) 螺母板
CN113020528B (zh) 一种基于板锻造技术的板材移动成形方法及模具
CN204365851U (zh) 拉拔缠绕式小弯曲半径弯管模具
CN204724691U (zh) 一种带头部冲孔的异型螺栓脱料组合冲模模具

Legal Events

Date Code Title Description
C14 Grant of patent or utility model
GR01 Patent grant
ASS Succession or assignment of patent right

Owner name: YANTAI HUIZHONG AUTOMOTIVE CHASSIS SYSTEM CO., LTD

Effective date: 20121130

C41 Transfer of patent application or patent right or utility model
TR01 Transfer of patent right

Effective date of registration: 20121130

Address after: 200122 No. 1493 South Pudong Road, Shanghai, Shanghai, Pudong New Area

Patentee after: Shanghai Huizhong Automotive Manufacturing Co., Ltd.

Patentee after: YANTAI HUIZHONG AUTOMOTIVE CHASSIS SYSTEMS CO., LTD.

Address before: 200122 No. 1493 South Pudong Road, Shanghai, Shanghai, Pudong New Area

Patentee before: Shanghai Huizhong Automotive Manufacturing Co., Ltd.

CF01 Termination of patent right due to non-payment of annual fee
CF01 Termination of patent right due to non-payment of annual fee

Granted publication date: 20120425

Termination date: 20190721