CN202076027U - 有机高分子材料薄膜及玻璃布补强云母带绕包线 - Google Patents
有机高分子材料薄膜及玻璃布补强云母带绕包线 Download PDFInfo
- Publication number
- CN202076027U CN202076027U CN2011201141348U CN201120114134U CN202076027U CN 202076027 U CN202076027 U CN 202076027U CN 2011201141348 U CN2011201141348 U CN 2011201141348U CN 201120114134 U CN201120114134 U CN 201120114134U CN 202076027 U CN202076027 U CN 202076027U
- Authority
- CN
- China
- Prior art keywords
- glass cloth
- layer
- wire
- insulating barrier
- mica tape
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Abstract
本实用新型提供一种有机高分子材料薄膜及玻璃布补强云母带绕包线,涉及电机附件技术领域,其包括导体,以及导体表面绕包的绝缘层,绝缘层分为第一绝缘层和第二绝缘层,第一绝缘层由内到外为云母带层,玻璃布补强层,两层连接为一整体,云母带层内侧靠近第二绝缘层,玻璃布补强层外侧为绕包线最外层;第二绝缘层由内向外依次为有机高分子材料薄膜层,云母带层,玻璃布补强层,三层依次连接为一整体。本实用新型主要用于地铁变压器上的绕组线,有益效果在于能减少线圈浸漆后气泡产生,并缩短绝缘漆固化时间,使其稳定性更好。
Description
技术领域
本实用新型涉及电机附件技术领域,具体涉及一种有机高分子材料薄膜及玻璃布补强云母带绕包线。
背景技术
1、现有云母线绕包电磁线产品大致分为两类:一类为玻璃丝包双面薄膜补强云母带绕包线,该类产品具有绝缘层机械强度大、有效绝缘层厚度小,浸漆后气隙较多等特点;另一类为单面聚酯薄膜绕包线,该类产品的特点是绝缘层机械强度小、有效绝缘厚度大,浸漆后气隙少。
2、绕制成的线圈在嵌入定子槽隙后进行VPI技术浸漆,绝缘漆渗入绝缘层内的速度较慢,绝缘漆固化的时间长、稳定性差。
发明内容
为解决上述缺陷,本实用新型提供一种有机高分子材料薄膜及玻璃布补强云母带绕包线,减少线圈浸漆后气泡的产生,并缩短绝缘漆固化时间,使其稳定性更好。
本实用新型解决上述缺陷的技术方案包括:一种有机高分子材料薄膜及玻璃布补强云母带绕包线,包括导体,以及导体表面绕包的绝缘层,绝缘层分为第一绝缘层和第二绝缘层,第一绝缘层由内到外为云母带层,玻璃布补强层,两层连接为一整体,云母带层内侧靠近第二绝缘层,玻璃布补强层外侧为绕包线最外层;第二绝缘层由内向外依次为有机高分子材料薄膜层,云母带层,玻璃布补强层,三层依次连接为一整体,有机高分子材料薄膜层里侧靠近导体。
进一步来说,上述的一种有机高分子材料薄膜及玻璃布补强云母带绕包线,其有机高分子材料薄膜层为聚酯薄膜层。
又进一步来说,上述的一种有机高分子材料薄膜及玻璃布补强云母带绕包线,其第一绝缘层与第二绝缘层内部各层之间添加有胶粘剂。
更一进步,上述的一种有机高分子材料薄膜及玻璃布补强云母带绕包线,所述导体为裸铜扁线、裸铜圆线、裸铝扁线、裸铝圆线、裸铜包铝扁线、裸铜包铝圆线中的一种。
本实用新型主要用于地铁变压器上的绕组线,相比现有技术,其有益效果在于绝缘层的玻璃布补强层一侧朝向外面,可有效提高绝缘层的机械强度,有利于绕组线加工成型,后期绕制线圈在嵌入定子槽后进行VPI技术浸漆过程中,绝缘漆尽快地渗入绝缘层内,排除气隙,使绝缘漆固化的时间大大缩短,稳定性增强。
附图说明
图1是本实用新型结构示意图;
图2是图1第二绝缘层结构示意图;
图3是图1第一绝缘层结构示意图。
具体实施方式
实施例1:
如附图1所示,一种有机高分子材料薄膜及玻璃布补强云母带绕包线,其导体3为裸铜扁线,所述导体3外表面重叠绕包有绝缘层,所述绝缘层分为第一绝缘层1和第二绝缘层2。如附图2所示,所述第一绝缘层1为含有玻璃布补强的粉云母带,云母带由内而外第一层为云母带层1-2,第二层为玻璃布补强层1-1,这两层之间添加有胶粘剂,使各层之间紧密连接成为一个整体,云母带层1-2朝内侧靠近第二绝缘层,玻璃布补强层1-1外侧为绕包线最外层。如附图2所示,所述第二绝缘层2是含有聚酯薄膜及玻璃布补强的粉云母带,云母带由内而外的结构为第一层为有机高分子薄膜层2-3,第二层为云母带层2-2,第三层为玻璃布补强层2-1,本实施例中有机高分子薄膜层2-3为聚酯薄膜层,这三层之间添加有胶粘剂连接为一个整体,聚酯薄膜层里侧靠近导体3,玻璃布补强层2-1一侧朝外。
实施例2:
导体3为裸铜圆线,所述导体3外表面绝缘层为对缝绕包,第二绝缘层2是含有聚酰亚胺薄膜及玻璃布补强的粉云母带,云母带由内而外的结构为第一层有机高分子薄膜层2-3为聚酰亚胺薄膜层,第二层为云母带层2-2,第三层为玻璃布补强层2-1,这三层依次利用胶粘剂连接为一个整体,聚酰亚胺薄膜层里侧靠近导体,玻璃布补强层2-1一侧朝外,其余均与实施例1一致。
实施例3:
仅将导体3换为裸铝扁线,所述导体3外表面绝缘层为间隙绕包,其余均与实施例1一致。
实施例4:
仅将导体3换为裸铝圆线,所述导体3外表面绕包有绝缘层,其第一绝缘层为重叠绕包,第二绝缘层为对缝绕包,其余均与实施例1一致。
实施例5:
仅将导体3换为裸铜包铝扁线,所述导体3外表面绕包有绝缘层,其第一绝缘层为重叠绕包,第二绝缘层为间隙绕包,其余均与实施例1一致。
实施例6:
仅将导体3换为裸铜包铝圆线,所述导体3外表面绕包有绝缘层,其第一绝缘层为对缝绕包,第二绝缘层为间隙绕包,其余均与实施例1一致。
Claims (4)
1.一种有机高分子材料薄膜及玻璃布补强云母带绕包线,包括导体,以及导体表面绕包的绝缘层,其特征在于:绝缘层分为第一绝缘层和第二绝缘层,第一绝缘层由内到外为云母带层,玻璃布补强层,两层连接为一整体,云母带层内侧靠近第二绝缘层,玻璃布补强层外侧为绕包线最外层;第二绝缘层由内向外依次为有机高分子材料薄膜层,云母带层,玻璃布补强层,三层依次连接为一整体,有机高分子材料薄膜层里侧靠近导体。
2.根据权利要求1所述的有机高分子材料薄膜及玻璃布补强云母带绕包线,其特征在于:所述有机高分子材料薄膜层为聚酯薄膜层。
3.根据权利要求1所述的有机高分子材料薄膜及玻璃布补强云母带绕包线,其特征在于:所述第一绝缘层与第二绝缘层内部各层之间添加有胶粘剂。
4.根据权利要求1所述的有机高分子材料薄膜及玻璃布补强云母带绕包线,其特征在于:所述导体为裸铜扁线、裸铜圆线、裸铝扁线、裸铝圆线、裸铜包铝扁线、裸铜包铝圆线中的一种。