Prior art keywords
iron
runner
blast furnace
tap drain
slag
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
CN2010205101059U
Other languages
English (en)
Inventor
石会营
王战民
许远超
张三华
曹喜营
张晔
王守业
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Sinosteel Luoyang Institute of Refractories Research Co Ltd
Original Assignee
Sinosteel Luoyang Institute of Refractories Research Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Sinosteel Luoyang Institute of Refractories Research Co Ltd filed Critical Sinosteel Luoyang Institute of Refractories Research Co Ltd
Priority to CN2010205101059U priority Critical patent/CN201801532U/zh
Application granted granted Critical
Publication of CN201801532U publication Critical patent/CN201801532U/zh
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Links

Images

Abstract

本实用新型属于炼铁行业单出铁口高炉出铁沟主沟技术,提出一种单出铁口高炉储铁式出铁沟主沟,依次设置有:使铁渣通过流出的渣沟(2),对铁渣起阻挡作用、使渣铁分离的撇渣器过梁(3),在高炉修风时放出残留在出铁沟内铁水的残铁口(4);所述高炉出铁沟主沟的沟底为一由前至后逐渐向下倾斜的斜面,所述向下倾斜的斜面其前端距高炉出铁口1.5米-2.5米,后端位于撇渣器后端出铁口,由此保证铁水顺利的从出铁沟主沟流出;撇渣器后端出铁口主沟沟底低于支沟沟底0.8米-1.2米,在出铁沟主沟内构成用以储存一定量铁水的凹槽。

Description

一种单出铁口高炉储铁式出铁沟主沟
技术领域
本实用新型属于炼铁行业单出铁口高炉出铁沟技术,主要涉及一种单出铁口高炉储铁式出铁沟主沟。
背景技术
目前,我国尚有大量容积为1000m3以下的单出铁口高炉,出铁沟主沟性能的好坏直接影响到高炉的正常生产。过去出铁沟主沟一般采用非储铁式,这种结构的出铁沟主沟在使用过程中铁水对沟底和沟帮的冲刷都比较严重,出铁沟主沟使用寿命短,维修频率比较高,由于是单出铁口高炉,必然会耽误出铁时间,从而严重影响了的高炉正常炼铁生产,降低了高炉的利用系数,这样不仅降低了生产效率,而且浪费了大量人力、物力。为了提高出铁沟主沟寿命和出铁效率,降低吨铁耐材消耗,应该逐渐地将这些小高炉的原非储铁式出铁沟主沟改造为储铁式出铁沟主沟。储铁式出铁沟主沟在出铁期间和出铁间隔时间,出铁沟主沟内始终充满铁水,这样出铁沟主沟工作衬就会处在温度相对恒定的环境当中,避免了出铁沟主沟浇注料的急冷急热,延长了出铁沟主沟的使用寿命;另外,由于出铁沟主沟内始终存有大量铁水,在一定程度上减少了从高炉铁口冲出铁水对出铁沟主沟的冲击,也能在很大程度上延长出铁沟主沟的使用寿命;一般改造完的储铁式出铁沟主沟一次通铁量在10~15万吨,且性能稳定。
发明内容
本实用新型的目的是提供一种单出铁口高炉储铁式出铁沟主沟,使其使用寿命延长、降低吨铁生产成本。
本实用新型实现其发明目的采取的技术方案是:一种单出铁口高炉储铁式出铁沟主沟,出铁沟主沟为从高炉出铁口到撇渣器后端出铁口部分,从高炉出铁口流出的铁水通过出铁沟主沟进入支沟;从高炉出铁口到撇渣器后端出铁口依次设置有:使铁渣通过流出的渣沟,对铁渣起阻挡作用、使渣铁分离的撇渣器过梁,在高炉修风时放出残留在出铁沟内铁水的残铁口;高炉出铁沟主沟的沟底为一由前至后逐渐向下倾斜的斜面,所述向下倾斜的斜面其前端距高炉出铁口1.5米-2.5米,后端位于撇渣器后端出铁口,由此保证铁水顺利的从出铁沟主沟流出;撇渣器后端出铁口主沟沟底低于支沟沟底0.8米-1.2米,在出铁沟主沟内构成用以储存一定量铁水的凹槽,使出铁沟主沟在高炉出铁时能储存一定量的铁水。
本实用新型的优点在于,高炉出铁沟主沟内始终存有一定量的铁水,这样能保证出铁沟主沟用耐火材料处在温度相对恒定的环境中,减少了出铁沟主沟用耐火材料使用过程中的急冷急热,同时也减少了出铁沟主沟用耐火材料在空气中的氧化,有利于出铁沟主沟寿命的提高出铁沟的寿命;另外,出铁沟主沟存有一定的铁水后,当铁水从高炉出铁口流出时,减少了铁水对出铁沟主沟用耐火材料的冲击,在很大程度上延长了出铁沟主沟的使用寿命。而且,极大的改善了高炉炉前工人的作业环境,减少了粉尘以及有害物质的排放,降低了炉前工人的劳动强度。
附图说明
图1为本实用新型的结构示意图。
图中:1、高炉出铁口,2、渣沟,3、撇渣器过梁,4、残铁口,5、支沟。
具体实施方式
结合附图给出的实施例对本实用新型的结构加以进一步说明:
如图1所示,一种单出铁口高炉储铁式出铁沟主沟,所述的出铁沟主沟为从高炉出铁口到撇渣器后端出铁口部分,从高炉出铁口1到撇渣器后端出铁口依次设置有:渣沟2,撇渣器过梁3,残铁口4;高炉出铁沟主沟的沟底为一由前至后逐渐向下倾斜的斜面,所述向下倾斜的斜面其前端距高炉出铁口1.5米-2.5米,后端位于撇渣器后端出铁口,由此保证铁水顺利的从出铁沟主沟流出;撇渣器后端出铁口的主沟沟底低于支沟沟底0.8米-1.2米,在出铁沟主沟内构成用以储存一定量铁水的凹槽,使出铁沟主沟在高炉出铁时能储存一定量的铁水。当铁水充满出铁沟主沟时,撇渣器过梁3起到挡渣的作用,铁水从出铁沟主沟流向支沟5,而铁渣则通过渣沟2流出,实现了渣铁分离的效果;当高炉修风时,残留在出铁沟主沟的铁水由残铁口4放出,以便于修补施工的进行。

Claims (1)

1.一种单出铁口高炉储铁式出铁沟主沟,所述的出铁沟主沟为高炉出铁口到撇渣器后端出铁口部分,从高炉出铁口到撇渣器后端出铁口依次设置有:使铁渣通过流出的渣沟(2),对铁渣起阻挡作用、使渣铁分离的撇渣器过梁(3),在高炉修风时放出残留在出铁沟内铁水的残铁口(4);其特征在于:所述高炉出铁沟主沟的沟底为一由前至后逐渐向下倾斜的斜面,所述向下倾斜的斜面其前端距高炉出铁口1.5米-2.5米,后端位于撇渣器后端出铁口;撇渣器后端出铁口的主沟沟底低于支沟沟底0.8米-1.2米,在出铁沟主沟内构成用以储存一定量铁水的凹槽。
CN2010205101059U 2010-08-24 2010-08-24 一种单出铁口高炉储铁式出铁沟主沟 Expired - Lifetime CN201801532U (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN2010205101059U CN201801532U (zh) 2010-08-24 2010-08-24 一种单出铁口高炉储铁式出铁沟主沟

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN2010205101059U CN201801532U (zh) 2010-08-24 2010-08-24 一种单出铁口高炉储铁式出铁沟主沟

Publications (1)

Publication Number Publication Date
CN201801532U true CN201801532U (zh) 2011-04-20

Family

ID=43871047

Family Applications (1)

Application Number Title Priority Date Filing Date
CN2010205101059U Expired - Lifetime CN201801532U (zh) 2010-08-24 2010-08-24 一种单出铁口高炉储铁式出铁沟主沟

Country Status (1)

Country Link
CN (1) CN201801532U (zh)

Cited By (7)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN102618678A (zh) * 2012-03-28 2012-08-01 攀钢集团西昌钢钒有限公司 高炉渣铁分离装置、渣铁分离方法和高炉下渣铁回收方法
CN103849702A (zh) * 2012-11-30 2014-06-11 中冶建筑研究总院有限公司 一种高炉出铁沟
CN103924016A (zh) * 2014-04-18 2014-07-16 攀钢集团成都钢钒有限公司 一种更换高炉渣口大套的方法
CN104858411A (zh) * 2015-04-07 2015-08-26 巩义市华伟耐火材料厂 一种熔渣、铁、铅混合物三分离撇渣器及其分离方法
CN106086265A (zh) * 2016-08-08 2016-11-09 长兴煤山新型炉料有限公司 一种耐火高炉出铁用撇渣器
CN108339971A (zh) * 2018-04-18 2018-07-31 宜兴市龙宸炉料有限公司 一种组合型储铁式沟撇渣器
CN111944939A (zh) * 2020-08-13 2020-11-17 广东韶钢松山股份有限公司 主沟残铁含渣量控制及排放主沟残铁工艺

Cited By (11)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN102618678A (zh) * 2012-03-28 2012-08-01 攀钢集团西昌钢钒有限公司 高炉渣铁分离装置、渣铁分离方法和高炉下渣铁回收方法
CN102618678B (zh) * 2012-03-28 2014-11-26 攀钢集团西昌钢钒有限公司 高炉渣铁分离装置、渣铁分离方法和高炉下渣铁回收方法
CN103849702A (zh) * 2012-11-30 2014-06-11 中冶建筑研究总院有限公司 一种高炉出铁沟
CN103849702B (zh) * 2012-11-30 2015-12-23 中冶建筑研究总院有限公司 一种高炉出铁沟
CN103924016A (zh) * 2014-04-18 2014-07-16 攀钢集团成都钢钒有限公司 一种更换高炉渣口大套的方法
CN103924016B (zh) * 2014-04-18 2015-10-14 攀钢集团成都钢钒有限公司 一种更换高炉渣口大套的方法
CN104858411A (zh) * 2015-04-07 2015-08-26 巩义市华伟耐火材料厂 一种熔渣、铁、铅混合物三分离撇渣器及其分离方法
CN104858411B (zh) * 2015-04-07 2017-01-04 巩义市华伟耐火材料厂 一种熔渣、铁、铅混合物三分离撇渣器及其分离方法
CN106086265A (zh) * 2016-08-08 2016-11-09 长兴煤山新型炉料有限公司 一种耐火高炉出铁用撇渣器
CN108339971A (zh) * 2018-04-18 2018-07-31 宜兴市龙宸炉料有限公司 一种组合型储铁式沟撇渣器
CN111944939A (zh) * 2020-08-13 2020-11-17 广东韶钢松山股份有限公司 主沟残铁含渣量控制及排放主沟残铁工艺

Similar Documents

Publication Publication Date Title
CN201801532U (zh) 一种单出铁口高炉储铁式出铁沟主沟
CN104293993B (zh) 高Zn负荷原料高炉冶炼的控制方法
CN201514113U (zh) 有色金属双室氧气侧吹炉
CN201713555U (zh) 杂铜再生浇铸阳极板连续生产组合式精炼炉
CN201330258Y (zh) 撇渣器
CN201778041U (zh) 一种主铁沟结构
CN208008841U (zh) 一种侵蚀引导型弧形炉底炉缸
CN201983617U (zh) 一种铸焊机熔铅炉改进结构
CN201581094U (zh) 一种双撇渣器主沟
CN201325999Y (zh) 还原炉出渣口装置
CN101979942A (zh) 一步炼铅鼓风炉
CN205205165U (zh) 一种长寿命的高炉出铁沟
CN211866588U (zh) 一种包底呈阶梯状的钢包
CN202099306U (zh) 高炉无料钟布料溜槽
CN203269958U (zh) 一种高炉出铁沟
CN2887885Y (zh) 转炉炼钢用全均质挡渣球
CN107338361A (zh) 节能型保温前床及其使用方法
CN201553747U (zh) 一种钒钛高炉渣金属铁回收装置
CN105033235A (zh) 一种冶炼钢包
CN202885551U (zh) 冶金炉虹吸放渣装置
CN202382562U (zh) 组合式熔铝炉
CN202452839U (zh) 一种冶金炉炉渣虹吸排放装置
CN206447915U (zh) 节能型保温前床
CN201648431U (zh) 一种带有排渣槽的新型侧兑铁槽
CN201255568Y (zh) 立式钒矿焙烧炉

Legal Events

Date Code Title Description
C14 Grant of patent or utility model
GR01 Patent grant
CX01 Expiry of patent term

Granted publication date: 20110420