CN201749958U - 具有材料保护性能的接地体 - Google Patents
具有材料保护性能的接地体 Download PDFInfo
- Publication number
- CN201749958U CN201749958U CN2010205101523U CN201020510152U CN201749958U CN 201749958 U CN201749958 U CN 201749958U CN 2010205101523 U CN2010205101523 U CN 2010205101523U CN 201020510152 U CN201020510152 U CN 201020510152U CN 201749958 U CN201749958 U CN 201749958U
- Authority
- CN
- China
- Prior art keywords
- copper core
- zinc layer
- grounding
- protection performance
- zinc
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了一种具有材料保护性能的接地体,包括有铜芯(2)和沿铜芯长度方向包覆在铜芯外周的锌层(1),其中铜芯(2)的直径为6mm-30mm,包覆在铜芯外的锌层(1)厚度在1mm以上,外层锌层材料通过加热压覆方式与内层铜芯紧密贴合。通过铜芯直径和锌层厚度的合理配合,较粗的铜芯保证了接地体的机械强度和载流量,较厚的锌层对铜芯有很好的保护,有效预防接地体的腐蚀,大大延长了接地材料的寿命,同时对设备和管道起到阴极保护作用。接地和阴极保护合二为一,大大减少施工量和资金投入,且比接地与阴极保护单独做更科学和节约成本,使用年限长。
Description
技术领域
本实用新型涉及一种接地体,具体涉及一种具有材料保护性能的接地体。
背景技术
现有技术中的接地体,一般采用在钢芯表面热镀锌层或者电镀锌层的形式,锌层的厚度较薄,一般为3μm-100μm,使用寿命较短,保护层很快被腐蚀掉,遭受雷电事故的概率增加,安全可靠性较差,同时也造成较大的经济损失。同时,由于钢芯8/20US等典型高频雷电波的冲击下,呈现高阻抗的特性,泄流能力及热稳定性较差。
例如公告号为CN2850012Y的中国实用新型公开了一种锌包钢接地极,该接地极就是包括有钢芯和沿钢芯长度方向在钢芯外包覆的锌,钢芯的直径为8mm-25mm,在钢芯外包覆的锌层厚度在1mm以上,外层锌材料通过加热压覆方式与内层钢芯结合在一起。该实用新型的接地极,由于还是采用在钢芯表面热镀芯层,虽然具有一定的机械强度和载流能力,但如果运用在高要求的场所,其泄流能力及热稳定性还是差强人意。
实用新型内容
本实用新型克服了现有技术的不足,提供一种具有材料保护性能的接地体,该接地体具有较高的载流泄流能力,还可以大幅度提高接地极自身的防腐问题,同时可以对设备和管道的阴极起到保护作用。
为解决上述的技术问题,本实用新型采用以下技术方案:
一种具有材料保护性能的接地体,包括有铜芯和沿铜芯长度方向包覆在铜芯外周的锌层,其中铜芯的直径为6mm-30mm,包覆在铜芯外的锌层厚度在1mm以上,外层锌层通过加热压覆方式与内层铜芯紧密贴合。
所述的铜芯的直径为8mm-25mm,包覆的锌层厚度在3mm以上。
所述的铜芯的形状为圆柱形或扁矩形。
与现有技术相比,本实用新型的有益效果是:通过加热升温将纯锌压覆到铜芯上,使铜芯和锌层完整结合,形成一种复合结构,二者结合紧密不易脱开,可以使锌层较厚,并且由该种复合结构形成的金属铜和锌的连接关系结合度良好、接触电阻低。本实用新型还通过铜芯直径和锌层厚度的合理配合,较粗的铜芯保证了接地体的机械强度和载流量,较厚的锌层对铜芯有很好的保护,有效预防接地体的腐蚀,大大延长了接地材料的寿命,同时对设备和管道起到阴极保护作用。接地和阴极保护合二为一,大大减少施工量和资金投入,且比接地与阴极保护单独做更科学和节约成本,使用年限长。
附图说明
图1为本实用新型结构示意图。
具体实施方式
下面结合附图对本实用新型作进一步阐述。
实施例1:
如图1所示,一种具有材料保护性能的接地体,包括有铜芯2和沿铜芯长度方向包覆在铜芯外周的锌层1,其中铜芯2的直径为6mm,包覆在铜芯2外的锌层1厚度为1.5mm,外层锌层通过加热压覆方式与内层铜芯紧密贴合。铜芯的形状为圆柱形。
实施例2
一种具有材料保护性能的接地体,包括有铜芯2和沿铜芯长度方向包覆在铜芯外周的锌层1,其中铜芯2的直径为8mm,包覆在铜芯外的锌层1厚度为3mm,外层锌层通过加热压覆方式与内层铜芯紧密贴合。铜芯2的形状为圆柱形或矩形。
实施例3
一种具有材料保护性能的接地体,包括有铜芯2和沿铜芯长度方向包覆在铜芯外周的锌层1,其中铜芯2的直径为25mm,包覆在铜芯外的锌层厚度2.5mm,外层锌层通过加热压覆方式与内层铜芯紧密贴合。铜芯2的形状为圆柱形或矩形。
实施例4
一种具有材料保护性能的接地体,包括有铜芯2和沿铜芯长度方向包覆在铜芯外周的锌层1,其中铜芯2的直径为30mm,包覆在铜芯2外的锌层1厚度为4mm,外层锌层通过加热压覆方式与内层铜芯紧密贴合。铜芯2的形状为圆柱形。
下面简要介绍一下本实用新型的制作方法:
将船型锌加热至500℃±50℃,待船型锭熔融后,注入注型模具内,铸成柱形锌锭,将锌锭切割成段,然后将铜芯2放入液压机内固定,将挤压模具在300℃±40℃的炉内强热,同时将柱形锭在另一炉内强热(200℃-260℃),待温度稳定后将模具放入液压机内,将预热好的锌锭放入模具压覆到铜芯2上,压覆完成后进行矫直,并根据要求尺寸切割。
Claims (3)
1.一种具有材料保护性能的接地体,其特征在于:包括有铜芯(2)和沿铜芯(2)长度方向包覆在铜芯外周的锌层(1),其中铜芯(2)的直径为6mm-30mm,包覆在铜芯外的锌层(1)厚度在1mm以上,外层锌层(1)通过加热压覆方式与内层铜芯(2)紧密贴合。
2.根据权利要求1所述的具有材料保护性能的接地体,其特征在于:所述的铜芯(2)的直径为8mm-25mm,包覆的锌层(1)厚度在3mm以上。
3.根据权利要求1或2所述的具有材料保护性能的接地体,其特征在于:所述的铜芯(2)的形状为圆柱形或矩形。