CN201620103U - 没有抽真空玻璃管的平板轧凸真空玻璃 - Google Patents

没有抽真空玻璃管的平板轧凸真空玻璃 Download PDF

Info

Publication number
CN201620103U
CN201620103U CN200920252932XU CN200920252932U CN201620103U CN 201620103 U CN201620103 U CN 201620103U CN 200920252932X U CN200920252932X U CN 200920252932XU CN 200920252932 U CN200920252932 U CN 200920252932U CN 201620103 U CN201620103 U CN 201620103U
Authority
CN
China
Prior art keywords
glass
convex
rolling convex
vacuum
flat
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN200920252932XU
Other languages
English (en)
Inventor
欧阳宝武
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN200920252932XU priority Critical patent/CN201620103U/zh
Application granted granted Critical
Publication of CN201620103U publication Critical patent/CN201620103U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型公开了一种太阳能热水器及门窗上用的没有抽真空玻璃管的平板轧凸真空玻璃,包括一面是平面,另一面具有均布均高下大上小的锥凸点(1a),其四周里边有和锥凸点(1a)一样高的、具有1毫米左右宽的、下宽上窄的封闭边(1b),封闭边(1b)上有1条以上的、外大内小的锥形通气孔(1c);四周外边也是封闭边(1b)的外边,有数毫米以上宽度、其深度是锥凸点(1a)高度两倍以上的玻璃粉膏沟(1d);把平板轧凸玻璃(1)有轧凸面(1e)的一面向里盖在和其膨胀系数相同、大小相等的平板玻璃(2)任一平面上四周对齐并在玻璃粉膏沟(1d)全部涂抹填满低熔点玻璃粉膏(4);然后在真空加热炉(6)里通电加热烘烤的同时用真空泵(7)抽真空。本实用新型生产工艺简单,成品率高,成本低,易推广。

Description

没有抽真空玻璃管的平板轧凸真空玻璃
技术领域  本实用新型涉及一种太阳能热水器及门窗上用的没有抽真空玻璃管的平板轧凸真空玻璃。
背景技术  国家专利局授权的专利“96208977x”“022002073”和“200720159455.3”以及“2007101158830”都有加热熔焊上抽空玻璃管再抽真空后,加热熔封抽真空玻璃管,加工工艺复杂,成品率低。
发明内容  本实用新型的目的是:提供一种生产工艺简单,成品率高的、没有抽真空玻璃管的平板轧凸真空玻璃。本实用新型的技术方案是:用一根平轧辊和一根特殊设计制造的轧凸轧辊滚压轧制成的一面是平面,另一面是轧凸面(1e)的平板轧凸玻璃(1)上具有均布均高、下大上小的锥凸点(1a);其四周里边有和锥凸点(1a)一样高的、具有1毫米左右宽的、下宽上窄的封闭边(1b),封闭边(1b)上有1条以上的、外大内小的锥形通气孔(1c);四周外边也是封闭边(1b)的外边,有数毫米以上宽度、其深度是锥凸点(1a)高度两倍以上的玻璃粉膏沟(1d);把平板轧凸玻璃(1)有轧凸面(1e)的一面向里盖在和其膨胀系数相同、大小相等的平板玻璃(2)任一平面上四周对齐;在一条以上锥形通气孔(1c)上放入锥度相同的锥形针(3),使锥形针(3)的针尖(3a)伸进轧凸面(1e)里,锥形针(3)的针把(3b)露出玻璃粉膏沟(1d);把和平板轧凸玻璃(1)膨胀系数相同的低熔点玻璃粉兑水调成低熔点玻璃粉膏(4);一条以上的锥形通气孔(1c)不涂抹低熔点玻璃粉膏(4),玻璃粉膏沟(1d)全部涂抹填满低熔点玻璃粉膏(4),涂抹好的低熔点玻璃粉膏(4)干固后,轻轻转动一下锥形针(3)的针把(3b)后再拔出锥形针(3);把涂抹好的下面是平板玻璃(2)、上面是平板轧凸玻璃(1)一起正体放进真空加热炉(6)里,关上门封闭好后,通电加热烘烤慢慢升温的同时,用真空泵(7)抽真空加热炉(6)的真空,升温到低熔点玻璃粉膏(4)的熔点以上保温后,断电停止加热,降温到低熔点玻璃粉膏(4)的熔点以下数百度后再停止真空泵(7)抽真空,降温至退火下限温度后,开门从真空加热炉(6)里取出没有抽真空玻璃管的平板轧凸真空玻璃(5)。
本实用新型的有益效果:生产工艺简单,成品率高、成本低、易推广。
附图说明  图1是本实用新型的结构示意图;图2是加工本实用新型的设备示意图;图3是本实用新型安装在太阳能热水器上的结构示意图。
图中零体序号如下所示:平板轧凸玻璃(1),锥凸点(1a),封闭边(1b),锥形通气孔(1c),玻璃粉膏沟(1d),轧凸面(1e);平板玻璃(2);锥形针(3),针尖(3a),针把(3b);低熔点玻璃粉膏(4);没有抽真空玻璃管的平板轧凸真空玻璃(5);真空加热热炉(6);真空泵(7);太阳能热水器(8);太阳能热水器外壳及支架(9);热水器保温层(10);貯热桶(11);貯热桶保温层(12);热交换器盘管(13);自来水连接阀(14);三通阀(15);淋浴器(16);自来水管(17);上管总成(18);下管总成(19);传热介质水(20)。
具体实施方式:本实用新型如图1.2所示实施例中,把平板轧凸玻璃(1)有轧凸面(1e)的一面向里盖在和其膨胀系数相同、大小相等的平板玻璃(2)任意一面上四周对齐后,在一条以上锥形通气孔(1c)上放入锥度相同的锥形针(3),使针尖(3a)伸进轧凸面(1e)里,把和平板轧凸玻璃(1)膨胀系数相同的低熔点玻璃粉兑水调成低熔点玻璃粉膏(4);把低熔点玻璃粉膏(4)涂抹填满玻璃粉膏沟(1d),低熔点玻璃粉膏(4)干固后,轻轻拧动一下锥形针(3)的针把(3b),然后再慢慢把锥形针(3)拔出后,使锥形通气孔(1c)无阻塞可通气;把下面是平板玻璃(2)上面是平板轧凸玻璃(1)并涂抹好低熔点玻璃粉膏(4)一起正体放进真空加热炉(6)里关上门封闭好后,一边通电加热烘烤慢慢升温的同时,用真空泵(7)抽真空加热炉(6)的真空,升温到350℃时保温半小时继续抽真空,此时一条以上锥形通气孔(1c)依然无阻塞可通气;然后再升温到低熔点玻璃粉膏(4)的熔点以上50℃左右保温半小时,这时低熔点玻璃粉膏(4)已全部熔化,在重力的作用下自然把锥形通气孔(1c)熔焊封闭好;此时断电停止加热烘烤而继续抽真空,当降温到低熔点玻璃粉膏(4)的熔点以下200℃左右,可停止真空泵(7)抽真空,降温到退火下限温度后,打开真空加热炉(6)的进气阀慢慢进气到常压后,打开真空加热炉(6)的门,取出没有抽真空玻璃管的平板轧凸真空玻璃(5)
本实用新型如图1.2.3所示实施例中,把本实用新型安装在太阳能热水器(8)上后,可提高太阳能热水器的集热性能降低热损。

Claims (2)

1.一种没有抽真空玻璃管的平板轧凸真空玻璃,包括平板轧凸玻璃、平板玻璃、锥形针、低熔点玻璃粉膏,真空加热炉通电加热烘烤,真空泵抽真空。其特征是:一面是平面,另一面是轧凸面(1e)的平板轧凸玻璃(1)上具有均布均高、下大上小的锥凸点(1a),其四周里边有和锥凸点(1a)一样高的、具有1毫米左右宽的、下宽上窄的封闭边(1b),封闭边(1b)上有1条以上的、外大内小的锥形通气孔(1c),把平板轧凸玻璃(1)有轧凸面(1e)的一面向里盖在和其膨胀系数相同、大小相等的平板玻璃(2)任一平面上四周对齐。
2.根据权利要求1所述的没有抽真空玻璃管的平板轧凸真空玻璃,其特征是:平板轧凸玻璃(1)的轧凸面(1e)四周外边也是封闭边(1b)的外边,有数毫米以上宽度、其深度是锥凸点(1a)高度两倍以上的玻璃粉膏沟(1d)。
CN200920252932XU 2009-11-13 2009-11-13 没有抽真空玻璃管的平板轧凸真空玻璃 Expired - Fee Related CN201620103U (zh)