CN201462226U - 混凝土内壁淬火硬化管 - Google Patents

混凝土内壁淬火硬化管 Download PDF

Info

Publication number
CN201462226U
CN201462226U CN2009200978822U CN200920097882U CN201462226U CN 201462226 U CN201462226 U CN 201462226U CN 2009200978822 U CN2009200978822 U CN 2009200978822U CN 200920097882 U CN200920097882 U CN 200920097882U CN 201462226 U CN201462226 U CN 201462226U
Authority
CN
China
Prior art keywords
pipe
wall
quench
hardened layer
hardened
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2009200978822U
Other languages
English (en)
Inventor
张文岐
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN2009200978822U priority Critical patent/CN201462226U/zh
Application granted granted Critical
Publication of CN201462226U publication Critical patent/CN201462226U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型公开了一种混凝土内壁淬火硬化管,其包括有:管体(1),其特征在于:在管体(1)内壁附着一层淬火硬化层(2)。淬火硬化层(2)厚度为管壁总厚度的三分之一到二分之一。本实用新型由于在管体内壁附着一层淬火硬化层,该硬化层是在原来管件的基础上经过高频机感应圈对其加热、喷淋冷却液,利用淬火原理实现表层硬化,该硬化层与其外部的未硬化层结合紧密,并且不增加原来管件的重量,保障混凝土管的垂直度和良好的使用效果。

Description

混凝土内壁淬火硬化管
所属技术领域
本实用新型属于一种钢管,具体地是一种内壁硬化钢管。
背景技术
目前,输送混凝土的钢管因内壁接触硬质介质,这就要求其内壁硬化具有耐磨性。在现有技术中,混凝土钢管的内壁增强耐磨性的方法主要是在管壁上焊接钢筋。其存在的不足是:增加了管子的重量,造成管子垂直度下沉过快,影响使用效果。
发明内容
本实用新型之目的,在于克服现有技术上述之不足,提供一种改进的混凝土内壁硬化管,其结构简单,不增加重量,使用效果好。
为达到上述之目的,本实用新型采取以下的技术方案:本实用新型包括有:管体,其特征在于:在管体内壁附着一层淬火硬化层。
本实用新型采取上述技术方案,具有以下的有益效果:本实用新型由于在管体内壁附着一层淬火硬化层,该硬化层是在原来管件的基础上经过高频机感应圈对其加热、喷淋冷却液,利用淬火原理实现表层硬化,该硬化层与其外部的未硬化层结合紧密,浑然一体。并且,并不增加原来管件的重量,保障混凝土管的垂直度和良好的使用效果。
附图说明
下面结合附图和实施例对本实用新型进行详细说明:
图1为本实用新型结构简图。
图中标记:1-管体、2-淬火硬化层。
具体实施方式
由图1所示,本实用新型包括有:管体1、淬火硬化层2,淬火硬化层2附着在管体1内壁。
本实用新型根据需要,可将淬火硬化层(2)厚度设置为管壁总厚度的三分之一到二分之一。

Claims (2)

1.一种混凝土内壁淬火硬化管,其包括有:管体(1),其特征在于:在管体(1)内壁附着一层淬火硬化层(2)。
2.根据权利要求1所述的一种混凝土内壁淬火硬化管,其特征在于:淬火硬化层(2)厚度为管壁总厚度的三分之一到二分之一。
CN2009200978822U 2009-07-22 2009-07-22 混凝土内壁淬火硬化管 Expired - Fee Related CN201462226U (zh)