Prior art keywords
crest
shunting net
net
shunting
tin
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
CN2009200546087U
Other languages
Chinese (zh)
Inventor
刘飞
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
DONGGUAN ANDA AUTOMATIC EQUIPMENT Co Ltd
Original Assignee
DONGGUAN ANDA AUTOMATIC EQUIPMENT Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by DONGGUAN ANDA AUTOMATIC EQUIPMENT Co Ltd filed Critical DONGGUAN ANDA AUTOMATIC EQUIPMENT Co Ltd
Priority to CN2009200546087U priority Critical patent/CN201423483Y/en
Application granted granted Critical
Publication of CN201423483Y publication Critical patent/CN201423483Y/en
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Links

Images

Landscapes

  • Molten Solder (AREA)

Abstract

The utility model relates to the crest welder technical field, in particular to a tin bath shunting net structure improvement of a crest welder. Two crest tin bathes are arranged on the crest welder,a shunting net is arranged inside the two crest bathes, two nozzles are installed at the upper end of the shunting net, a crest width adjusting plate is arranged at the upper side of the shunting net,an adjusting screw stem is arranged on the adjusting plate to adjust the crest widths of the two nozzles, and a filtering net pressure plate is provided with the crest welder and compresses the shunting net. The shunting net takes the cuboid shape as a whole, the two long side faces of the cuboid shunting net are vertically provided with flat plates and the upper top face of the cuboid shunting net is horizontally provided with a net plate, and a plurality of net plates are slanted between the flat plates at the two long faces. A plurality of separation plates are vertically fixed on the netplate at the upper top face of the cuboid shunting net, and a second net plate is fixed at the upper ends of the separation plates. By adding the shunting net into the two crest tin bathes of the full-automatic crest welder, the tin wave ejected from the two nozzles at different crest widths is continuous, even, stable and perfect, and tin oxidation amount is reduced, thereby meeting the welding requirement of various PCB boards.

Description

The molten tin bath shunting net structural improvement of crest welder
Technical field
The utility model relates to the crest welder technical field of automatic welding, refers in particular to a kind of molten tin bath shunting net structural improvement of crest welder here.
Background technology
Wave-soldering is the liquid solder with fusion, by with the effect of pump, form the solder wave of given shape at the solder bath liquid level, plug-in mounting the pcb board of components and parts put with conveyer chain on, pass solder wave and realize the process of solder joint welding through a certain specific angle and certain immersion depth.
The surface of crest face is all covered by one deck oxide skin, it is along nearly all keeping static on the whole length direction of solder wave, in the wave soldering process, PCB touches the surface, forward position of tin ripple, oxide skin is broken, the tin ripple of PCB front is not pushed to with having the chap pleat and advances, this illustrates that whole oxide skin and PCB move the moulding of crest welder solder joint with same speed: when holding in face of PCB enters crest, substrate and pin are heated, and before not leaving the crest face, whole PCB is immersed in the scolder, promptly by scolder institute bridging, but in the moment of leaving the crest tail end, a spot of scolder sticks on the pad owing to the effect of wetting power, and owing to capillary reason, can occur with the lead-in wire is that the center is contracted to minimum state, and the wetting power between scolder and the pad is greater than the cohesive force of the scolder between two pads at this moment.Therefore can form fullly, the solder joint of rounding leaves the excess solder of crest afterbody, because gravity falls back to Xi Guozhong, prevents the generation of bridging.
At present, the meeting existence of crest welder crest nozzle tin ripple ejection on the market is continuous evenly, not steady, will cause the bad or local tin sticky of pcb board tin sticky of welding bad like this, will cause the pcb board failure welding rate of welding to increase, and increases manufacturing cost.
The utility model content
The purpose of this utility model is, provides a kind of and can make the more steadily uniform molten tin bath shunting net structural improvement of tin ripple.
The molten tin bath shunting net structural improvement of the crest welder that the utility model provides, crest welder is provided with two crest molten tin baths, shunting net is arranged in the two crest grooves, two nozzles are installed in the shunting net upper end, be provided with the crest width adjustment plates at the shunting net upside, width adjustment plates is provided with the crest width that adjusting screw(rod) is regulated two nozzles, and shunting net is installed under the nozzle insied width adjustable plate, one head rest width adjustment plates is pushed down, and the other end is provided with pressing plate at nozzle fixed edge place.
Described shunting net integral body is cuboid, and two long side surfaces of the shunting net of cuboid are perpendicular to be provided with dull and stereotyped and last end face is put down and is provided with web plate, a plurality of web plates of oblique fire between two long side surface flat boards.
Vertically be fixed with a plurality of dividing plates on the web plate of the last end face of the shunting net of described rectangular cylindricality, be fixed with second web plate in the dividing plate upper end.
The beneficial effects of the utility model are: by set up shunting net in two crest molten tin baths of full-automatic crest welder, can make of the tin ripple continuous uniform and stable perfection of two nozzles in different crest width ejections, reduce the tin amount of oxidation, can satisfy the welding requirements of various pcb boards, can realize the purpose of Fast Installation and dismounting on the other hand, maintenance convenient for cleaning.
Description of drawings:
Fig. 1 is a scheme of installation of the present utility model
Fig. 2 is a three-dimensional structure diagram of the present utility model
Fig. 3 is another visual angle three-dimensional structure diagram of the present utility model
Fig. 4 is a dismounting schematic diagram of the present utility model
The specific embodiment:
Only be the utility model preferred embodiment below, do not limit protection domain of the present utility model with this.
See Fig. 1 and shown in Figure 3, the molten tin bath shunting net structural improvement of the crest welder that the utility model provides, crest welder 10 is provided with two crest molten tin baths 1, shunting net 4 is arranged in the two crest grooves 1, two nozzles 2 are installed in shunting net 4 upper ends, be provided with crest width adjustment plates 3 at shunting net 4 upsides, adjustable plate 3 is provided with the crest width that adjusting screw(rod) 6 is regulated two nozzles 2, and filter screen pressing plate 5 is installed crest welder nozzle 2 fixed edges and compressed shunting net 4.On two crest molten tin baths 1, also be provided with tin liquor pump 7, tin liquor flows to distinguished and admirable net 4 and two nozzles 2 by tin liquor pump 7 by mobilization dynamic, the direction of arrow is represented the tin liquor flow direction among the figure, and tin liquor is that tin liquor is mobile more even, more steady by shunting net 4 shunting current stabilization effects.
See Fig. 2 and shown in Figure 3, described shunting net 4 integral body are cuboid, the flat web plate 42 that is provided with of perpendicular flat board of establishing 41 of two long side surfaces of the shunting net 4 of cuboid and last end face, and web plate 42 mainly is the impulsive force of buffering tin liquor.At dull and stereotyped 41 a plurality of oblique web plates 43 of oblique fire of two long side surfaces, tiltedly the number of web plate is advisable with 3-8, and tiltedly web plate 42 is the flows that are used for controlling tin liquor, the flow unanimity of tin liquor before and after ensureing.Can change tin liquor pressure and flow velocity because of transferring wide or transferring when narrow, this structure can keep the tin liquor flow evenly in whole zone, does not have the poor of height size.
Vertically be fixed with a plurality of dividing plates 44 on the web plate 42 of the last end face of the shunting net 4 of cuboid, these dividing plates 44 can guarantee to a great extent that the tin ripple of different tin wave band ejection is more even.Be fixed with second web plate, 45, the second web plates 45 in dividing plate 44 upper ends and make that the tin liquor of gushing is more steady.Whole shunting net 4 is provided with multiple web plate, makes the tin liquor of passing through web plate flow continuously all directions uniform and stable.Adopt polylith dividing plate and web plate to connect, web plate 45 is close to width adjustment plates 3, and dividing plate 44 is used for guiding, and string is moving about when preventing the tin liquor upper punch causes the tin ripple not steady, and that guarantees that web plate 45 and width adjustment plates 3 do not contact with regionally just has a generation of tin ripple.
See shown in Figure 4ly, when needs clean shunting net, be transferred to the crest width adjustment plates 3 of two nozzles 2 the wideest, the filter screen pressing plate 5 of dismantling, whole shunting net can take out from molten tin bath 1, the whole nozzle 2 of need not dismantling during cleaning shunting net 4, thereby make cleaning, safeguard to become convenient.

Claims (3)

1. the molten tin bath shunting net structural improvement of crest welder, it is characterized in that, crest welder is provided with two crest molten tin baths, shunting net is arranged in the two crest grooves, and two nozzles are installed in the shunting net upper end, are provided with the crest width adjustment plates at the shunting net upside, width adjustment plates is provided with the crest width that adjusting screw(rod) is regulated two nozzles, shunting net is installed under the nozzle insied width adjustable plate, and a head rest width adjustment plates is pushed down, and the other end is provided with pressing plate at nozzle fixed edge place.
2. molten tin bath shunting net structural improvement according to claim 1, it is characterized in that: described shunting net integral body is cuboid, two long side surfaces of the shunting net of cuboid are perpendicular to be provided with dull and stereotyped and last end face is put down and is provided with web plate, a plurality of web plates of oblique fire between two long side surface flat boards.
3. molten tin bath shunting net structural improvement according to claim 1 is characterized in that: vertically be fixed with a plurality of dividing plates on the web plate of the last end face of the shunting net of described rectangular cylindricality, be fixed with second web plate in the dividing plate upper end.
CN2009200546087U 2009-04-15 2009-04-15 Tin bath shunting net structure improvement of crest welder Expired - Lifetime CN201423483Y (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN2009200546087U CN201423483Y (en) 2009-04-15 2009-04-15 Tin bath shunting net structure improvement of crest welder

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN2009200546087U CN201423483Y (en) 2009-04-15 2009-04-15 Tin bath shunting net structure improvement of crest welder

Publications (1)

Publication Number Publication Date
CN201423483Y true CN201423483Y (en) 2010-03-17

Family

ID=42022918

Family Applications (1)

Application Number Title Priority Date Filing Date
CN2009200546087U Expired - Lifetime CN201423483Y (en) 2009-04-15 2009-04-15 Tin bath shunting net structure improvement of crest welder

Country Status (1)

Country Link
CN (1) CN201423483Y (en)

Cited By (6)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN104339063A (en) * 2013-07-23 2015-02-11 深圳市堃琦鑫华股份有限公司 Jet-flow brazier
CN106925857A (en) * 2017-03-28 2017-07-07 深圳市联合超越电子设备有限公司 Exempt from the flat ripple spout structure of maintenance
CN107363369A (en) * 2017-08-31 2017-11-21 阜阳扬宇充电设备有限公司 A kind of power template manufactures special tin stove nozzle arrangements
CN109226927A (en) * 2018-11-16 2019-01-18 伟创力电子技术(苏州)有限公司 Nozzle for wide wave crest tin soldering pot
CN114473108A (en) * 2022-03-23 2022-05-13 美的集团股份有限公司 Wave soldering device
CN115090989A (en) * 2022-07-25 2022-09-23 江苏丰源电子科技有限公司 Electronic component lead welding machine

Cited By (9)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN104339063A (en) * 2013-07-23 2015-02-11 深圳市堃琦鑫华股份有限公司 Jet-flow brazier
CN104339063B (en) * 2013-07-23 2016-06-29 深圳市堃琦鑫华股份有限公司 A kind of jet flow weldering brazier
CN106925857A (en) * 2017-03-28 2017-07-07 深圳市联合超越电子设备有限公司 Exempt from the flat ripple spout structure of maintenance
CN106925857B (en) * 2017-03-28 2022-08-09 东莞市新超越智能科技有限公司 Maintenance-free flat wave nozzle structure
CN107363369A (en) * 2017-08-31 2017-11-21 阜阳扬宇充电设备有限公司 A kind of power template manufactures special tin stove nozzle arrangements
CN109226927A (en) * 2018-11-16 2019-01-18 伟创力电子技术(苏州)有限公司 Nozzle for wide wave crest tin soldering pot
CN114473108A (en) * 2022-03-23 2022-05-13 美的集团股份有限公司 Wave soldering device
CN114473108B (en) * 2022-03-23 2023-07-25 美的集团股份有限公司 Wave soldering apparatus
CN115090989A (en) * 2022-07-25 2022-09-23 江苏丰源电子科技有限公司 Electronic component lead welding machine

Similar Documents

Publication Publication Date Title
CN201423483Y (en) Tin bath shunting net structure improvement of crest welder
CN102581409A (en) Jet welding method and jet welding groove
CN103269820B (en) For fusion welding being delivered to the welding tip of the downside of printed circuit board (PCB) and reducing the method for contracting tin incidence of welding tip
CN201913344U (en) Jet-flow welding groove
CN203209812U (en) Spraying type dual wave soldering unit
CN201319701Y (en) Tinning steel mesh
CN202799421U (en) Improved structure of steel mesh and scraper sheet for thickening solder paste of part of PCB pad
JP4473566B2 (en) Jet soldering equipment
CN103002668B (en) Terminal surface mounting method based on circuit board
CN203390351U (en) Wave soldering device
CN202516743U (en) Coating device for soldering flux
CN203045098U (en) Automatic welding device
CN104084661A (en) Nozzle of selective wave soldering equipment
CN104754880A (en) Jet-flow welding method
CN101600305B (en) Wave crest tin soldering machine, wave crest nozzle thereof and tin furnace
CN104349604A (en) Fixed plugboard for printed circuit board
CN201201096Y (en) Plate importing apparatus of reflow machine
CN203537675U (en) Fixed plugboard for printed circuit board
CN208033872U (en) A kind of transport structure of wave-soldering furnace
CN201328216Y (en) Circuit board structure
CN209110354U (en) A kind of Wave-soldering device
CN201312442Y (en) Boss lateral tin-spilling kettle spout
CN208113060U (en) It can prevent the circuit board of PAD short circuit
CN201559005U (en) Flow guiding plate
CN201115040Y (en) Double open kettle mouth on long side of tin overflow mouth

Legal Events

Date Code Title Description
C14 Grant of patent or utility model
GR01 Patent grant
CX01 Expiry of patent term
CX01 Expiry of patent term

Granted publication date: 20100317

DD01 Delivery of document by public notice
DD01 Delivery of document by public notice

Addressee: Dongguan Anda Automatic Equipment Co., Ltd.

Document name: Notification of Expiration of Patent Right Duration