CN201376088Y - 一种连铸中间包 - Google Patents

一种连铸中间包 Download PDF

Info

Publication number
CN201376088Y
CN201376088Y CN 200920146346 CN200920146346U CN201376088Y CN 201376088 Y CN201376088 Y CN 201376088Y CN 200920146346 CN200920146346 CN 200920146346 CN 200920146346 U CN200920146346 U CN 200920146346U CN 201376088 Y CN201376088 Y CN 201376088Y
Authority
CN
China
Prior art keywords
tundish
liquid steel
crystallizer
casting blank
continuous casting
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 200920146346
Other languages
English (en)
Inventor
赵福生
韩冬
白守全
刘海平
姜彩艳
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Chengde Jianlong Special Steel Co Ltd
Original Assignee
Chengde Jianlong Special Steel Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Chengde Jianlong Special Steel Co Ltd filed Critical Chengde Jianlong Special Steel Co Ltd
Priority to CN 200920146346 priority Critical patent/CN201376088Y/zh
Application granted granted Critical
Publication of CN201376088Y publication Critical patent/CN201376088Y/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型公开了一种连铸中间包,包括中间包,中间包底部设有出液口,出液口高出中间包底部,当钢液从流入管进入中间包后,改变流动方向后从钢液流出口进入结晶器,使钢液中的非金属夹杂物由于钢液改变流动方向而被滞留在中间包中,使流入结晶器的非金属夹杂物减少,从而使铸坯内非金属夹杂物减少,确保了铸坯质量,解决了现有中间包无法控制钢液中的非金属夹杂物,使流入结晶器的非金属夹杂物过多,造成铸坯内非金属夹杂物增多,铸坯裂纹倾向加剧,影响铸坯质量的问题。

Description

一种连铸中间包
技术领域:
本实用新型涉及一种冶炼生产设施,特变是涉及一种连铸中间包。
背景技术:
在钢铁工业技术发展过程中,连铸已成为现代化钢铁企业炼钢生产的主要方式。目前连续铸钢技术已为全世界各产钢国普遍采用,不少发达国家连续铸钢的比例已达90%以上,不少炼钢厂已实现全连铸。由于连铸取代了模铸和初轧工序,替代了开坯工序,使企业的钢材产品向专业化方向发展;在发展连续铸钢过程中,不断提高连铸坯的质量是一个重要课题。目前,钢铁企业炼钢生产中所用连铸中间包的结构比较简单,只是一个内砌耐火材料的容器,钢液流入管置入中间包接近中间包底部,中间包底部设有钢液流出口通向结晶器,当钢液从流入管进入中间包后,直接从钢液流出口进入结晶器,该种结构的中间包无法控制钢液中的非金属夹杂物,使流入结晶器的非金属夹杂物过多,造成铸坯内非金属夹杂物增多,铸坯裂纹倾向加剧,影响铸坯质量,特别是对高碳高合金钢的危害更为明显,由此給企业造成的经济损失是非常大的。
发明内容:
本实用新型的目的是针对现有技术的不足,提供一种连铸中间包,可有效控制钢液中的非金属夹杂物过多的流入结晶器,减少铸坯内非金属夹杂物,提高铸坯质量,本实用新型所要解决的技术问题是合理设置中间包出液口的位置,改变流入中间包钢液的流动方向,以有效阻止非金属夹杂物过多的流入结晶器,本实用新型所采取的技术方案如下,本实用新型包括中间包,中间包底部设有出液口,其特征在于增加出液口的高度,使出液口高出中间包底部300~400。
本实用新型的作用过程如下,当钢液从流入管进入中间包后,改变流动方向后从钢液流出口进入结晶器,使钢液中的非金属夹杂物由于钢液改变流动方向而被滞留在中间包中,使流入结晶器的非金属夹杂物减少,从而使铸坯内非金属夹杂物减少,确保了铸坯质量。
与现有技术相比,本实用新型可有效控制钢液中的非金属夹杂物过多的流入结晶器,减少铸坯内非金属夹杂物,提高铸坯质量,大大降低经济损失。
附图说明:
附图1是本实用新型结构示意图
具体实施方式:
如图1所示,本实用新型包括中间包1,中间包底部设有出液口5,出液口高出中间包底部300~400mm,钢液2从流入管3进入中间包后,改变流动方向后从出液口5进入结晶器6,使钢液中的非金属夹杂物4由于钢液改变流动方向而被滞留在中间包中。

Claims (1)

1、一种连铸中间包,包括中间包,中间包底部设有出液口,其特征在于增加出液口的高度,使出液口高出中间包底部300~400mm。
CN 200920146346 2009-03-17 2009-03-17 一种连铸中间包 Expired - Fee Related CN201376088Y (zh)