CN201370439Y - 铝合金压铸锅 - Google Patents

铝合金压铸锅 Download PDF

Info

Publication number
CN201370439Y
CN201370439Y CN200920112418U CN200920112418U CN201370439Y CN 201370439 Y CN201370439 Y CN 201370439Y CN 200920112418 U CN200920112418 U CN 200920112418U CN 200920112418 U CN200920112418 U CN 200920112418U CN 201370439 Y CN201370439 Y CN 201370439Y
Authority
CN
China
Prior art keywords
iron plate
aluminum alloy
pot body
convex ribs
aluminium alloy
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN200920112418U
Other languages
English (en)
Inventor
周赛方
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN200920112418U priority Critical patent/CN201370439Y/zh
Application granted granted Critical
Publication of CN201370439Y publication Critical patent/CN201370439Y/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

一种铝合金压铸锅,它包括有一铝合金压铸而成的锅体,在该锅体的底部覆制有至少一块圆形铁板;所述的圆形铁板的相接面上制有多条相连或断连的圆弧形凹槽,而在锅体的底部压制有与所述圆弧形凹槽相对应的圆弧形凸筋,且该圆弧形凸筋嵌接在圆弧形凹槽中并压接成一体;所述的圆弧形凹槽和对应的圆弧形凸筋可以用发散状、即由圆心向外缘扩散的凹槽和对应的凸筋代替;它具有结构简单,使用方便,成本低,节能,适用范围广等特点。

Description

铝合金压铸锅
技术领域
本实用新型涉及的是一种能在电磁炉上使用的压铸锅,尤其是一种导热性能好的铝合金压铸锅,属于日常生活用品。
背景技术
通常人们使用的锅是用铝合金材料通过压铸制造而成的,这是因为铝合金压铸锅制造方便,成本低,重量轻,使用时加热快,节能。但铝合金压铸锅的使用缺陷是:不能使用在电磁炉上,因为铝合金材料不导磁。所以,在电磁炉上使用的锅通常是铁锅,但我们知道,铁锅的重量要比铝合金重,制作工艺复杂,成本高,热传导性能比铝合金差。
发明内容
本实用新型的目的在于克服现有技术存在的不足,而提供一种能在电磁炉上使用的铝合金压铸锅。它包括有一铝合金压铸而成的锅体,在该锅体的底部覆制有至少一块覆底铁板。
所述的覆底铁板为圆形铁板,在该圆形铁板的相接面上制有多条相连或断连的圆弧形凹槽,而在锅体的底部压制有与所述圆弧形凹槽相对应的圆弧形凸筋,且该圆弧形凸筋嵌接在圆弧形凹槽中并压接成一体。
所述的圆形铁板的相接面上也可以制有多条发散状、即由圆心向外缘扩散的凹槽,而在锅体的底部压制有与所述凹槽相对应的凸筋,且该凸筋嵌接在凹槽中并压接成一体。
本实用新型属于对现有技术的一种改良,它通过在铝合金锅的锅体底部覆制铁板,将原铝合金不导磁而无法使用在电磁炉上的缺陷得以克服,从而使其具有结构简单,使用方便,成本低,节能,适用范围广等特点。
附图说明
图1是本实用新型的结构示意图。
图2是图1中I部的局部放大图。
图3是本实用新型的锅体底部正面视图。
图4是本实用新型另一实施例的锅体底部正面视图。
具体实施方式
下面将结合附图对本实用新型作详细的介绍:附图1所示,本实用新型包括有一铝合金压铸而成的锅体1,在该锅体1的底部覆制有至少一块覆底铁板2,附图中所示的覆底铁板2为圆形铁板;本实用新型在其它实施例中的覆底铁板2也可以是方形铁板或是其它形状的铁板构成,或是由多块相同或不同形状铁板构成。
结合附图2、3所示,在圆形铁板2的相接面上制有多条相连或断连的圆弧形凹槽3,而在锅体1的底部压制有与所述圆弧形凹槽3相对应的圆弧形凸筋4,且该圆弧形凸筋4嵌接在圆弧形凹槽3中并压接成一体;本实用新型在其它实施例中,所述的圆弧形凹槽3和对应的圆弧形凸筋4可以用发散状、即由圆心向外缘扩散的凹槽和对应的凸筋代替,见附图4所示。
本实用新型是在铝合金压铸锅的锅体底部预先压铸出如附图1所示的圆弧形凸筋4,此凸筋可以根据锅底部的大小设置多条,或如附图3所示的多个圆环圈状,中间设置多个断连,或设置如盘状蚊香的螺旋状。此圆弧形凸筋4的顶部如附图2所示,在凸筋的中间部位有一个凹弧5,当对应的圆形铁板2,也称之为覆底板放入锅体的底部后,圆形铁板上的相应形状的圆弧形凹槽3与所述圆形铁板2上的圆弧形凸筋4相互套住,然后放入大吨位的压机中一体压出,经过压制后,其锅体上凹弧两侧突起的部分由于受到外力的作用,材料发生位移并被压平,这样圆形铁板2便永久地与锅体连接成一体。

Claims (3)

1、一种铝合金压铸锅,它包括有一铝合金压铸而成的锅体,其特征在于在该锅体(1)的底部覆制有至少一块圆形铁板(2)。
2、根据权利要求1所述的铝合金压铸锅,其特征在于所述的圆形铁板(2)的相接面上制有多条相连或断连的圆弧形凹槽(3),而在锅体(1)的底部压制有与所述圆弧形凹槽(3)相对应的圆弧形凸筋(4),且该圆弧形凸筋(4)嵌接在圆弧形凹槽(3)中并压接成一体。
3、根据权利要求1所述的铝合金压铸锅,其特征在于所述的圆形铁板(2)的相接面上制有多条发散状、即由圆心向外缘扩散的凹槽(3),而在锅体(1)的底部压制有与所述凹槽(3)相对应的凸筋(4),且该凸筋(4)嵌接在凹槽(3)中并压接成一体。
CN200920112418U 2009-01-08 2009-01-08 铝合金压铸锅 Expired - Fee Related CN201370439Y (zh)