CN201367390Y - 双头线玻璃热弯生产模 - Google Patents
双头线玻璃热弯生产模 Download PDFInfo
- Publication number
- CN201367390Y CN201367390Y CNU200920041531XU CN200920041531U CN201367390Y CN 201367390 Y CN201367390 Y CN 201367390Y CN U200920041531X U CNU200920041531X U CN U200920041531XU CN 200920041531 U CN200920041531 U CN 200920041531U CN 201367390 Y CN201367390 Y CN 201367390Y
- Authority
- CN
- China
- Prior art keywords
- base
- shaping frame
- forming frame
- shaping
- frame
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型是关于一种平板玻璃加工用的模具领域,特别是关于一种弯曲玻璃板的模具。其具有底座,底座上具有第二成型框,第二成型框具有用于玻璃板成型的与玻璃板外围边缘相吻合的弯曲表面,底座上设置有高于第二成型框的第一成型框,底座上设置有一可活动的定位装置,第一成型框和第二成型框通过该定位装置与底座连接,定位装置由固定设置在底座的支轴、设置在支轴端部沿支轴转动的支撑托、设置在支撑托端部的拉杆组成,第一成型框通过第一支撑脚和支撑托连接,第二成型框通过第二支撑脚和支撑托连接。本实用新型的有益效果是两次成型防止了因弯曲前后尺寸变化引起的模具痕迹宽而重的现象,改善了外观质量。
Description
技术领域
本实用新型是关于一种平板玻璃加工用的模具领域,特别是关于一种弯曲玻璃板的模具。
背景技术
现有用于夹层玻璃弯曲成型的模具大多只有一个侧翼,其结构包括有底座及成型环,成型环分为定成型环和动成型环,定成型环固定在底座上,动成型环固定在带有重锤的侧翼上,动成型环与定成型环通过绞链铰接在一起。成型的玻璃一般成类矩形状,类矩形模具的长边中部为定成型环,而两端为动成型环,大玻璃在烘弯成型时中部由定成型环成型,而两端玻璃在烘软后,在重锤重力的配合下,侧翼带动动成型环绕铰接点逐渐向上将玻璃不断弯曲成型。这种结构的模具在生产大弧度、大球面烘弯玻璃过程中一次弯曲成型,会造成玻璃局部变形太大,生产出来的玻璃不够设计要求,导致成本增加。
发明目的
本实用新型针对上述技术的生产出的玻璃不够要求的缺点提供一种能两次弯曲成型的双头线玻璃热弯生产模。
实现本实用新型的技术方案如下:
双头线玻璃热弯生产模,其具有底座,底座上具有第二成型框,第二成型框具有用于玻璃板成型的与玻璃板外围边缘相吻合的弯曲表面,底座上设置有高于第二成型框的第一成型框,底座上设置有一可活动的定位装置,第一成型框和第二成型框通过该定位装置与底座连接,定位装置由固定设置在底座的支轴、设置在支轴端部沿支轴转动的支撑托、设置在支撑托端部的拉杆组成,第一成型框通过第一支撑脚和支撑托连接,第二成型框通过第二支撑脚和支撑托连接。
所述第二成型框上设置有调整装置,该调整装置由固定设置在第二成型框上的平衡杆、设置在平衡杆上的调整锤和设置在平衡杆端部的调整螺栓组成。
所述的第一成型框和底座之间设置有保护装置,该保护装置由保护托和保护架组成,保护托卡合在保护架内。
所述的第一成型框有两条长边和两条短边组成。
本实用新型设计有第一成型框和第二成型框,可以进行两次玻璃成型弯曲,其优点在于增加了第一成型框,对玻璃板进行两次弯曲成型,当采用短边第二成型框的玻璃板弯曲模具时,对于因玻璃板短边方向的急剧变化而产生的角部反向球面的问题起到了良好的改善效果,防止了因弯曲前后尺寸变化引起的模具痕迹宽而重的现象,改善了外观质量,避免了因传统模具一次自重成型而使玻璃板局部变形量太大造成荷叶边。
附图说明
图1为本实用新型的结构示意图;
图2为图1的A-A向剖视图;
图中,1、底座,2、第二成型框,3、第一成型框,4、支轴,5、支撑托,6、拉杆,7、第一支撑脚,8、第二支撑脚,9、平衡杆,10、调整锤,11、调整螺栓,12、保护托,13、保护架,14、长边,15、短边。
具体实施方式
如图1、图2所示,双头线玻璃热弯生产模,其具有底座1,底座1上具有第二成型框2,第二成型框2具有用于玻璃板成型的与玻璃板外围边缘相吻合的弯曲表面,底座上设置有高于第二成型框2的第一成型框3,底座1上设置有一可活动的定位装置,第一成型框3和第二成型框2通过该定位装置与底座1连接,定位装置由固定设置在底座1的支轴4、设置在支轴4端部沿支轴4转动的支撑托5、设置在支撑托5端部的拉杆6组成,第一成型框3通过第一支撑脚7和支撑托5连接,第二成型框2通过第二支撑脚8和支撑托5连接,第二成型框2上设置有调整装置,该调整装置由固定设置在第二成型框上的平衡杆9、设置在平衡杆9上的调整锤10和设置在平衡杆9端部的调整螺栓11组成,第一成型框3和底座1之间设置有保护装置,该保护装置由保护托12和保护架13组成,保护托12卡合在保护架13内,第一成型框3有两条长边14和两条短边15组成。
Claims (4)
1、双头线玻璃热弯生产模,其具有底座,底座上具有第二成型框,第二成型框具有用于玻璃板成型的与玻璃板外围边缘相吻合的弯曲表面,其特征在于:底座上设置有高于第二成型框的第一成型框,底座上设置有一可活动的定位装置,第一成型框和第二成型框通过该定位装置与底座连接,定位装置由固定设置在底座的支轴、设置在支轴端部沿支轴转动的支撑托、设置在支撑托端部的拉杆组成,第一成型框通过第一支撑脚和支撑托连接,第二成型框通过第二支撑脚和支撑托连接。
2、根据权利要求1所述的双头线玻璃热弯生产模,其特征在于:所述第二成型框上设置有调整装置,该调整装置由固定设置在第二成型框上的平衡杆、设置在平衡杆上的调整锤和设置在平衡杆端部的调整螺栓组成。
3、根据权利要求1所述的双头线玻璃热弯生产模,其特征在于:所述的第一成型框和底座之间设置有保护装置,该保护装置由保护托和保护架组成,保护托卡合在保护架内。
4、根据权利要求1所述的双头线玻璃热弯生产模,其特征在于:所述的第一成型框有两条长边和两条短边组成。