CN201314007Y - 一种新型耐用造纸成形网 - Google Patents

一种新型耐用造纸成形网 Download PDF

Info

Publication number
CN201314007Y
CN201314007Y CNU2008202307989U CN200820230798U CN201314007Y CN 201314007 Y CN201314007 Y CN 201314007Y CN U2008202307989 U CNU2008202307989 U CN U2008202307989U CN 200820230798 U CN200820230798 U CN 200820230798U CN 201314007 Y CN201314007 Y CN 201314007Y
Authority
CN
China
Prior art keywords
parallel
spacer screen
net
fabric
wefts
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CNU2008202307989U
Other languages
English (en)
Inventor
董华伟
王友保
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Henan Huafeng Polyester Wire Mesh Science & Technology Co., Ltd.
Original Assignee
董华伟
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 董华伟 filed Critical 董华伟
Priority to CNU2008202307989U priority Critical patent/CN201314007Y/zh
Application granted granted Critical
Publication of CN201314007Y publication Critical patent/CN201314007Y/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型公开了一种新型耐用造纸成形网,由经线和纬线交错编织而成面网和底网,面网采用八综斜纹编织结构,底网采用十六综破缎纹编织结构,所述的纬线包括面网纬线和底网纬线,其特征在于:每厘米长度的成形网排列经线33根,每厘米长度的成形网排列纬线33根;底网纬线采用双锁紧纹理结构,底网纬线在一个编织循环内的浮长为14/16,本实用新型使用寿命长,尤其适于抄造90克/平方米以上包装纸。

Description

一种新型耐用造纸成形网
技术领域
本实用新型涉及造纸技术领域,尤其是涉及一种新型耐用造纸成形网。
背景技术
在造纸行业广泛采用成形网,成形网的成形、脱水、细小纤维留着率、使用寿命等性能指标对造纸质量、成本有着显著性的影响。常规抄造90克/平方米以上包装纸用的成形网,其经向密度为36根/公分;面网纬线为八棕斜纹编织结构,纬线一粗(线径为0.25~0.28mm的聚酯线)一细(线径为0.17mm的聚酯线)相间排列;底网采用16棕破缎纹编织结构,其纬线为等径纬线,即线径为0.45mm的聚酯线和线径为0.45mm的尼龙线相间排列;纬向密度最高可达到35根/公分,并且底网纬线采用单锁紧纹理结构,这样的网型结构稳定、透气度与纤维留着率中等,成形脱水也良好。但是上述的网型结构的造纸成形网的耐磨性较差,因此寿命较短,一般寿命为十天左右。
实用新型内容
有鉴于此,本实用新型的目的在于克服现有技术的缺陷,提供一种新型耐用造纸成形网,提高抄造90克/平方米以上包装纸用的成形网使用寿命。
为达到上述目的,本实用新型采用以下技术方案:
本实用新型的造纸成形网,由经线和纬线交错编织而成面网和底网,面网采用八综斜纹编织结构,底网采用十六综破缎纹编织结构,所述的纬线包括面网纬线和底网纬线,每厘米长度的成形网排列经线33根,每厘米长度的成形网排列纬线33根;底网纬线采用双锁紧纹理结构,底网纬线在一个编织循环内的浮长为14/16。
进一步,所述面网纬线由粗面网纬线和细面网纬线组成,粗面网纬线和细面网纬线相隔排列,粗面网纬线的直径为0.30毫米,细面网纬线的直径为0.22毫米。
进一步,所述底网纬线由尼龙底网纬线和聚酯底网纬线组成,尼龙底网纬线和聚酯底网纬线相隔排列,尼龙底网纬线直径为0.58毫米,聚酯底网纬线直径为0.55毫米。
本实用新型的有益效果是:
本实用新型主要减少了经线密度和纬线密度的同时增加了线径,并且底网纬线处采用双锁紧纹理结构,其浮长线也从现有的12/16上升为14/16,这样成形网的横向挺度得到加强,能够抵抗纸机真空箱的真空抽吸,同时磨面底纬磨损体积得到提高,网的寿命得到明显提高。
本实用新型的其他优点、目标和特征在某种程度上将在随后的说明书中进行阐述,并且在某种程度上,基于对下文的考察研究对本领域技术人员而言将是显而易见的,或者可以从本实用新型的实践中得到教导。
附图说明
附图为本实用新型的造纸成形网片段沿机器方向的剖面示意图。
具体实施方式
下面结合附图和实施例对本实用新型作进一步描述。
如附图所示,本实用新型的造纸成形网,由经线3和纬线交错编织而成面网和底网,面网采用八综斜纹编织结构,底网采用十六综破缎纹编织结构。图中所示的成形网位于上方的为面网,位于下方的为底网。每厘米长度的成形网排列经线33根,每厘米长度的成形网排列纬线33根,底网纬线由现有的单锁紧纹理结构改为双锁紧纹理结构,底网纬线的浮长线增加至14/16,即底网纬线在一个编织循环内的浮长为14/16。所述的纬线包括面网纬线和底网纬线,所述面网纬线由粗面网纬线2和细面网纬线1组成,粗面网纬线2采用直径为0.30毫米聚酯线,细面网纬线1采用直径为0.22毫米聚酯线;粗面网纬线2和细面网纬线1间隔排列。所述底网纬线由尼龙底网纬线5和聚酯底网纬线4,尼龙底网纬线5和聚酯底网纬线4线间隔排列,尼龙底网纬线5直径为0.58毫米,聚酯底网纬线4直径为0.55毫米。本实施例中经线3均采用直径为0.20毫米聚酯线。
本实施例的成形网在使用时具有以下效果:
1)、减少了经线密度和纬线密度的同时增加了线径,并且底网纬线处采用双锁紧纹理结构,其浮长线也从现有的12/16上升为14/16,这样成形网的横向挺度得到加强,能够抵抗纸机真空箱的真空抽吸,同时磨面底纬磨损体积得到提高,增加成形网的透气度、抗拉强度,因而成形网的寿命得到明显提高,有传统成形网的10天左右提升至30天左右。
2)、尼龙丝的强度、耐磨性比聚酯丝好,从而增强了成形网的抗磨性,提高成形网的使用寿命。使用成形网抗拉强度有较大增加,完全能够适应高速纸机的运行。
3)、另外,本实施例成形网的滤水性能也明显提高,因此网部清洗效果显著提高,适合利用废纸回收制成的再生浆广泛用于包装纸,相比传统的网不容易堵塞网孔。
最后说明的是,以上实施例仅用以说明本实用新型的技术方案而非限制,本领域普通技术人员对本实用新型的技术方案所做的其他修改或者等同替换,只要不脱离本实用新型技术方案的精神和范围,均应涵盖在本实用新型的权利要求范围当中。

Claims (3)

1.一种新型耐用造纸成形网,由经线和纬线交错编织而成面网和底网,面网采用八综斜纹编织结构,底网采用十六综破缎纹编织结构,所述的纬线包括面网纬线和底网纬线,其特征在于:每厘米长度的成形网排列经线33根,每厘米长度的成形网排列纬线33根;底网纬线采用双锁紧纹理结构,底网纬线在一个编织循环内的浮长为14/16。
2.根据权利要求1所述的新型耐用造纸成形网,其特征在于:所述面网纬线由粗面网纬线和细面网纬线组成,粗面网纬线和细面网纬线相隔排列,粗面网纬线的直径为0.30毫米,细面网纬线的直径为0.22毫米。
3.根据权利要求2所述的新型耐用造纸成形网,其特征在于:所述底网纬线由尼龙底网纬线和聚酯底网纬线组成,尼龙底网纬线和聚酯底网纬线相隔排列,尼龙底网纬线直径为0.58毫米,聚酯底网纬线直径为0.55毫米。
CNU2008202307989U 2008-12-15 2008-12-15 一种新型耐用造纸成形网 Expired - Fee Related CN201314007Y (zh)