CN201306126Y - 防偏磨油管接缝衬环 - Google Patents
防偏磨油管接缝衬环 Download PDFInfo
- Publication number
- CN201306126Y CN201306126Y CNU2008202251409U CN200820225140U CN201306126Y CN 201306126 Y CN201306126 Y CN 201306126Y CN U2008202251409 U CNU2008202251409 U CN U2008202251409U CN 200820225140 U CN200820225140 U CN 200820225140U CN 201306126 Y CN201306126 Y CN 201306126Y
- Authority
- CN
- China
- Prior art keywords
- tubing
- oil pipe
- sucker rod
- eccentric
- oil
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了一种石油工业采油井使用的防偏磨油管接缝衬环,用于有杆泵采油井的油管接缝中,降低抽油杆接箍与油管的磨损。防偏磨油管接缝衬环是筒体,两端内圆设有倒角。本实用新型在两根油管的连接处加入衬环,大大缩小了油管间隙,防止油管柱和抽油杆柱的磨损。可使抽油杆柱在上下冲程中平稳通过,避免了抽油杆接箍卡碰油管。既保护了油管丝扣,又保护了抽油杆接箍,大大减少偏磨躺井,延长油井生产周期,提高了抽油杆柱和油管柱的使用寿命。
Description
技术领域
本实用新型涉及石油工业的井下采油辅助装置,特别是防偏磨油管接缝衬环,在有杆泵采油井的油管接缝中充填衬环,降低抽油杆接箍与油管的磨损。
背景技术
目前油田进入高含水开发阶段,井筒状况和产出液性质发生了很大变化,有杆泵系统工作环境逐步恶化,加剧了杆管偏磨程度,抽油杆断脱、油管漏失现象频繁发生。通过对偏磨井的现场作业跟踪分析发现,油井偏磨有以下特点:一是绝大部分偏磨井是油管丝扣处偏磨迹象最为明显,据现场跟踪井统计有86%的油井油管丝扣磨穿;二是偏磨井抽油杆偏磨迹象最集中的部位是抽油杆接箍,只有极少数抽油杆出现本体偏磨严重的现象。
目前在用的防偏磨技术主要有抗磨副、抽油杆扶正器、抗磨管杆等技术,抗磨副和抽油杆扶正器延长的周期短,增大了悬点载荷,增加了过流阻力,使用后仍存在抗磨副接箍和抽油杆接箍偏磨现象;抗磨管杆价格昂贵,影响了其大规模的推广使用。
常规抽油杆柱是用抽油杆接箍将各根抽油杆连接起来,抽油杆接箍的直径比抽油杆粗,抽油杆在油管内往复运动时接箍和油管相互接触引起磨损,尤其是接箍往复运动经过两根油管接缝处。由于油管是依靠锥管扣来连接并实现密封的,连接螺纹有一定的紧密距,因此在油管本体与油管接箍连接时,油管本体端面不能够接触在一起,而是存在一定的间隙,根据实际测量,大约在17-25mm不等。当受到侧向力的影响时,抽油杆接箍与油管本体端面产生交错碰撞,在抽油杆上下径向拉力的作用下,加剧抽油杆接箍与油管端面丝扣连接处的磨损。从现场偏磨井发现,油管的丝扣连接部位大都比油管本体磨损严重。同时,油管接缝的存在也使配套的防偏磨扶正器的磨损加剧,降低了防偏磨装置的使用寿命。
发明内容
本实用新型的目的是提供防偏磨油管接缝衬环,缩小油管接缝,克服抽油杆接箍在往复运动时,在油管连接间隙处产生的交错碰撞,保护抽油杆接箍和油管丝扣。
为达上述目的,本实用新型采用的技术方案是:防偏磨油管接缝衬环是筒体,两端内圆设有倒角,将衬环安装在两根油管的接缝处。
本实用新型的明显效果是:在两根油管的连接处加入衬环,大大缩小了油管间隙,防止油管柱和抽油杆柱的磨损。可使抽油杆柱在上下冲程中平稳通过,避免了抽油杆接箍卡碰油管。既保护了油管丝扣,又保护了抽油杆接箍,大大减少偏磨躺井,延长油井生产周期,提高了抽油杆柱和油管柱的使用寿命。本实用新型与现有的防偏磨工具和装置相比,结构简单、成本低廉,大大降低了生产成本。施工更是方便,只需在下入油管时,将本衬环放入油管接箍中的两油管接缝处即可,大大降低了生产施工成本。
附图说明
图1是本实用新型的安装使用示意图。
图2是本实用新型的结构示意图。
具体实施方式
下面结合附图和实施例对本实用新型做进一步的说明,参见图1,在油管接缝处加入衬环3。参见图2,防偏磨油管接缝衬环3是筒体,两端内圆设有倒角,便于抽油杆接箍顺利通过。衬环3的内径与油管1和4的内径相等或者是小于油管1和4的内径0.5毫米—1.5毫米之间的任意一种尺寸,最好是比油管1和4的内径略小。衬环3的内径略小于油管1和4的内径,使抽油杆接箍往复通过时,保护油管1和4不被磨损,只要定期更换衬环3即可,延长油管管柱的使用寿命。衬环3的外径与油管接箍2的内径相符或者是略小0.5毫米—1毫米,只要能放入油管接箍2中就行。衬环3的高度是小于油管接缝4—6毫米之间的任意一种尺寸,衬环3的高度以油管1和4拧紧后与两个油管端面的间隙最小为宜。
在下入油管柱的施工中,将衬环3从油管4带油管接箍2的一端放进去,再拧上另一根油管1。这样在两根油管1和4的连接处就形成一个过渡,抽油杆接箍从中经过时,就可避免卡碰油管1和4,既保护了油管1和4的丝扣,又保护了抽油杆接箍。
Claims (4)
1、防偏磨油管接缝衬环,其特征是衬环(3)是筒体,两端内圆设有倒角。
2、根据权利要求1所述的防偏磨油管接缝衬环,其特征是衬环(3)的内径与油管(1)和(4)的内径相等或者是小于油管(1)和(4)的内径0.5毫米—1.5毫米之间的任意一种尺寸。
3、根据权利要求1所述的防偏磨油管接缝衬环,其特征是衬环(3)的外径与油管接箍(2)的内径相符。
4、根据权利要求1所述的防偏磨油管接缝衬环,其特征是衬环(3)的高度是小于油管接缝4—6毫米之间的任意一种尺寸。