CN201288150Y - 一种制造黑刚玉用的水套接包 - Google Patents

一种制造黑刚玉用的水套接包 Download PDF

Info

Publication number
CN201288150Y
CN201288150Y CNU200820220415XU CN200820220415U CN201288150Y CN 201288150 Y CN201288150 Y CN 201288150Y CN U200820220415X U CNU200820220415X U CN U200820220415XU CN 200820220415 U CN200820220415 U CN 200820220415U CN 201288150 Y CN201288150 Y CN 201288150Y
Authority
CN
China
Prior art keywords
wall
water
black corundum
water jacket
drum
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CNU200820220415XU
Other languages
English (en)
Inventor
王建勋
杜怀玉
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ZHENGZHOU YEDA WEAR RESISTANT MATIEIAL CO Ltd
Original Assignee
ZHENGZHOU YEDA WEAR RESISTANT MATIEIAL CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ZHENGZHOU YEDA WEAR RESISTANT MATIEIAL CO Ltd filed Critical ZHENGZHOU YEDA WEAR RESISTANT MATIEIAL CO Ltd
Priority to CNU200820220415XU priority Critical patent/CN201288150Y/zh
Application granted granted Critical
Publication of CN201288150Y publication Critical patent/CN201288150Y/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型提供了一种以水为冷却剂的制造黑刚玉用的水套接包。包括包壁和由炭砖组成的包底,包壁由内壁和外壁组成,在外壁和内壁之间有空隙,在外壁下部设有至少1个进水口,外壁上部设有4~10个出水口。直接用水快速冷却,从而减少了气孔的生成,使黑刚玉更质密,提高了黑刚玉的柔韧性;省去了涂石墨粉的工序,耐火层使用时间长,降低了成本,减少了工人的劳动强度;黑刚玉比包壁钢板收缩系数大,收缩后直接形成空隙,容易翻倒。

Description

一种制造黑刚玉用的水套接包
技术领域
本实用新型涉及一种黑刚玉冶炼中使用的接包。
背景技术
黑刚玉,又名低铝刚玉,是一种新型抛光材料。以三水型和一水型铝樊土为原料经电弧高温冶炼冷却加工而成。黑刚玉磨料基本粒集中,切削力强,任性大,刚柔相济,耐磨性好,工效高。主要用于不锈钢,金属制品,光学玻璃,竹木制品的抛光和喷砂,又是制造树脂砂轮,切割片,砂布的新颖磨料。同行业中使用的接包是借鉴棕刚玉接包,接包内壁及底部是一层炭砖,炭砖上部和接包壁是用耐火材料浇注而成。使用时,每次还要用石墨粉活成泥在包壁上涂一层,便于在熔液凝结后翻倒时容易脱落,其中存在以下问题:由于炭砖和耐火材料都有保温隔热作用,造成导入包内的溶液不能及时冷却,从而产生大量气孔,导致部分黑刚玉不质密,降低了黑刚玉的柔韧性;虽然每次都涂上石墨粉,但在翻倒时还是容易破坏耐火层,接包用不了多久就需要重新浇注耐火层,增加了成本;每次涂石墨粉增加了工人的劳动强度;当包内倒入少量硅铁溶液时,还会造成翻倒困难。
实用新型内容
本实用新型的目的是提供一种以水为冷却剂的制造黑刚玉用的水套接包。
为了达到上述目的本实用新型采用以下技术方案:包括包壁和由炭砖组成的包底,包壁由内壁和外壁组成,在外壁和内壁之间有空隙,在外壁下部设有至少1个进水口,外壁上部设有4~10个出水口。
所述内壁为耐火材料层。
所述外壁为钢板。
进水口为1个,出水口为8个。
直接用水快速冷却,从而减少了气孔的生成,使黑刚玉更质密,提高了黑刚玉的柔韧性;省去了涂石墨粉的工序,耐火层使用时间长,降低了成本,减少了工人的劳动强度;黑刚玉比包壁钢板收缩系数大,收缩后直接形成空隙,容易翻倒。
附图说明
附图为本实用新型制造黑刚玉用的水套接包的结构示意图。
具体实施方式
由附图所示,制造黑刚玉用的水套接包,包括包壁1和由炭砖7组成的底部6,包壁由内壁2和外壁3组成,在外壁和内壁之间形成有空隙,在外壁下部设有1个进水口5,也可以设置2个或者更多进水口,外壁上部设有8个出水口4,也可以设置4个,6个,10个出水口。内壁为耐火材料层,外壁为钢板。使用时,直接用水快速冷却,从而减少了气孔的生成,使黑刚玉更质密,提高了黑刚玉的柔韧性;省去了涂石墨粉的工序,耐火层使用时间长,降低了成本,减少了工人的劳动强度;黑刚玉比包壁钢板收缩系数大,收缩后直接形成空隙,容易翻倒。

Claims (4)

1、一种制造黑刚玉用的水套接包,包括包壁(1)和由炭砖(7)组成的包底(6),其特征是:包壁由内壁(2)和外壁(3)组成,在外壁和内壁之间有空隙,在外壁下部设有至少1个进水口(5),外壁上部设有4~10个出水口(4)。
2、根据权利要求1所述一种制造黑刚玉用的水套接包,其特征是:所述内壁为耐火材料层。
3、根据权利要求2所述一种制造黑刚玉用的水套接包,其特征是:所述外壁为钢板。
4、根据权利要求3所述一种制造黑刚玉用的水套接包,其特征是:进水口为1个,出水口为8个。
CNU200820220415XU 2008-10-27 2008-10-27 一种制造黑刚玉用的水套接包 Expired - Fee Related CN201288150Y (zh)