CN201153139Y - 蓄电池生产用抽酸装置 - Google Patents
蓄电池生产用抽酸装置 Download PDFInfo
- Publication number
- CN201153139Y CN201153139Y CNU2008200830873U CN200820083087U CN201153139Y CN 201153139 Y CN201153139 Y CN 201153139Y CN U2008200830873 U CNU2008200830873 U CN U2008200830873U CN 200820083087 U CN200820083087 U CN 200820083087U CN 201153139 Y CN201153139 Y CN 201153139Y
- Authority
- CN
- China
- Prior art keywords
- acid
- sour
- cylinder
- main
- buffering
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了一种蓄电池生产用抽酸装置,包括依次串联的真空泵、缓冲酸缸、主酸缸,所述缓冲酸缸和主酸缸的底部均设置有出酸阀,主酸缸的顶部连接有抽酸管,抽酸管的另一端固定有抽酸孔座。本实用新型通过抽酸孔座与待抽酸电池的注液孔相连,通过真空泵将缓冲酸缸和主酸缸内部的空气抽出后,依靠内外压差将酸快速抽出,抽出的酸液首先进入主酸缸,然后通过缓冲酸缸,可将抽酸过程中的酸雾、酸滴减压集中收集在缓冲酸缸中,定期进行清理,保证了在整个抽酸作业过程中不产生酸雾、无酸滴外泄,优化了生产环境,做到了清洁生产,保护了环境,保证了员工的安全健康。并保证了蓄电池的产品性能。
Description
【技术领域】
本实用新型涉及蓄电池生产制造领域,尤其涉及生产过程中对蓄电池内的电解液进行去除的抽酸装置。
【技术背景】
密封铅酸蓄电池为荷电出厂的免维护贫液电池。在充电生产过程中蓄电池为有利于电化学反应,内部是富液状态,过程中后期为了去除内部多余的电解液,要对蓄电池恒压抽酸,使电池内部满足一定的贫液状态,如抽酸过程未达到工艺控制要求,蓄电池内部将残存流动电解液,使用时会影响内部氧循环,增加酸雾的析出量,严重时导致出现蓄电池漏液问题。
目前,抽酸装置采用单缸装置,蓄电池由于在恒压抽酸过程中酸液温度在40℃以上,夏天更在50℃以上,单缸抽酸造成的酸雾、酸滴因没有足够的冷却时间及冷却载体,直接产生挥发,产生一定量的酸雾,产生的酸雾一是对车间生产现场环境和操作工人身体健康产生不良影响,二是腐蚀车间现场设备及工器具的金属部件,容易将有害金属杂质带入蓄电池中,造成蓄电池的自放电加大,影响性能。
【发明内容】
本实用新型的目的就是为了解决现有技术中存在的问题,提出一种蓄电池生产用抽酸装置,能够优化生产环境,提高产品性能。
为实现上述目的,本实用新型专利提出了一种蓄电池生产用抽酸装置,包括依次串联的真空泵、缓冲酸缸、主酸缸,所述缓冲酸缸和主酸缸的底部均设置有出酸阀,主酸缸的顶部连接有抽酸管,抽酸管的另一端固定有抽酸孔座。
作为优选,所述抽酸孔座上设置有均匀排列的6个抽酸孔。
作为优选,所述真空泵与缓冲酸缸之间、缓冲酸缸与主酸缸之间均采用连接管连接。
作为优选,所述缓冲酸缸、主酸缸上与连接管的连接处设置有橡胶底座。
作为优选,所述真空泵采用550W的真空泵。
本实用新型专利的有益效果:本实用新型通过抽酸孔座与待抽酸电池的注液孔相连,通过真空泵将缓冲酸缸和主酸缸内部的空气抽出后,依靠内外压差将酸快速抽出,抽出的酸液首先进入主酸缸,然后通过缓冲酸缸,可将抽酸过程中的酸雾、酸滴减压集中收集在缓冲酸缸中,定期进行清理,保证了在整个抽酸作业过程中不产生酸雾、无酸滴外泄,优化了生产环境,做到了清洁生产,保护了环境,保证了员工的安全健康。并且保证了车间设备上金属部件的清洁,避免有害金属杂质带入蓄电池内,保证了蓄电池的产品性能。
【附图说明】
图1是本实用新型蓄电池生产用抽酸装置的结构示意图。
【具体实施方式】
参阅图1,蓄电池生产用抽酸装置,包括依次串联的真空泵1、缓冲酸缸2、主酸缸3,所述缓冲酸缸2和主酸缸3的底部均设置有出酸阀4,主酸缸3的顶部连接有抽酸管5,抽酸管5的另一端固定有抽酸孔座6。所述抽酸孔座6上设置有均匀排列的6个抽酸孔7。抽酸孔7的数量和位置要求与待抽酸电池上的注液孔对应即可,可根据需要适当调整。所述真空泵1与缓冲酸缸2之间、缓冲酸缸2与主酸缸3之间均采用连接管8连接。所述缓冲酸缸2、主酸缸3上与连接管8的连接处设置有橡胶底座9。采用橡胶底座9可提高连接性能,放置泄露。所述真空泵1采用550W的真空泵,根据需要测算,采用550W的真空泵为最佳选择。上述真空泵1、缓冲酸缸2、主酸缸3可整体放置在专用工具车上,使用时只要将工具车移动就能够实现该装置整体移动。
上述实施例是对本实用新型的说明,不是对本实用新型的限定,任何对本实用新型简单变换后的方案均属于本实用新型的保护范围。
Claims (5)
1.蓄电池生产用抽酸装置,其特征在于:包括依次串联的真空泵(1)、缓冲酸缸(2)、主酸缸(3),所述缓冲酸缸(2)和主酸缸(3)的底部均设置有出酸阀(4),主酸缸(3)的顶部连接有抽酸管(5),抽酸管(5)的另一端固定有抽酸孔座(6)。
2.如权利要求1所述的蓄电池生产用抽酸装置,其特征在于:所述抽酸孔座(6)上设置有均匀排列的6个抽酸孔(7)。
3.如权利要求1所述的蓄电池生产用抽酸装置,其特征在于:所述真空泵(1)与缓冲酸缸(2)之间、缓冲酸缸(2)与主酸缸(3)之间均采用连接管(8)连接。
4.如权利要求3所述的蓄电池生产用抽酸装置,其特征在于:所述缓冲酸缸(2)、主酸缸(3)上与连接管(8)的连接处设置有橡胶底座(9)。
5.如权利要求1所述的蓄电池生产用抽酸装置,其特征在于:所述真空泵(1)采用550W的真空泵。