CN201146215Y - 省去锌底的锌锰干电池 - Google Patents

省去锌底的锌锰干电池 Download PDF

Info

Publication number
CN201146215Y
CN201146215Y CN200820001575.5U CN200820001575U CN201146215Y CN 201146215 Y CN201146215 Y CN 201146215Y CN 200820001575 U CN200820001575 U CN 200820001575U CN 201146215 Y CN201146215 Y CN 201146215Y
Authority
CN
China
Prior art keywords
zinc
tube
dry cell
zinc tube
manganese dioxide
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN200820001575.5U
Other languages
English (en)
Inventor
陈新义
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
GUANGZHOU XINKEDA NEW POWER BATTERY CO Ltd
Original Assignee
GUANGZHOU XINKEDA NEW POWER BATTERY CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by GUANGZHOU XINKEDA NEW POWER BATTERY CO Ltd filed Critical GUANGZHOU XINKEDA NEW POWER BATTERY CO Ltd
Priority to CN200820001575.5U priority Critical patent/CN201146215Y/zh
Application granted granted Critical
Publication of CN201146215Y publication Critical patent/CN201146215Y/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型公开了一种省去锌底的锌锰干电池,主要由锌筒、电芯、炭棒和塑料组合帽组成,电芯与锌筒之间有隔离层,锌筒的筒内底部放有涂塑料膜的盆形纸底,锌筒的底面装有铁底,电芯与塑料组合帽之间有空气室,锌筒去掉其底部并镶入一个金属底。该锌锰干电池的主要特点是能够节约大量的锌材,降低干电池的成本。

Description

省去锌底的锌锰干电池
技术领域
本实用新型涉及电化学领域的锌锰干电池。
背景技术
现在的锌锰干电池是由正极活性物质、负极活性物质、炭棒及其它电池零部件组成,锌筒做为负极活性物质,中间装有以锰粉为主的混合粉做成的电芯,也就是正极活性物质,电芯中间插有炭棒,炭棒上端带上铜帽,锌筒底下端有铁底,锌筒和电芯之间有糊式或纸板式隔离层,锌筒的底部放有绝缘材料做成的底片或盆底,锌筒的上端有封口层、沥青或塑料塞做成的封口层,防止正极活性物质与负极活性物质在反应过程中产生的混合气体与液体漏出,同时也防止膨胀。这种锌锰干电池的主要缺点是用锌量和成本太高,国家轻工部多次提出要解决锌锰干电池用锌量高的问题,因锌锰干电池的负极是用锌筒做成的,所以它即是电池的负极参加电化学反应,又是电池本身的容器,这样就浪费了大量的锌。根据电化学的理论计算,负极活性物质和正极活性物质的电化学反应是1∶10,也就是锌用1份,锰粉混合粉用10份,这样在电池参加电化学反应后,电池放完电,锌筒的大部分没有参加电化学反应,三分之二的锌白白浪费,这一严重的问题,亟待进行改进。
实用新型内容
针对现有技术存在的不足,本实用新型旨在提供一种能够节约用锌的锌锰干电池,其用锌量基本上接近电化学反应过程中的理论值。
本实用新型采用的技术方案是:
一种省去锌底的锌锰干电池,包括锌筒、电芯、炭棒和塑料组合帽,电芯与锌筒之间有隔离层,锌筒的筒内底部放有涂塑料膜的盆形纸底,锌筒的底面装有铁底,电芯与塑料组合帽之间有空气室,所述锌筒去掉其底部并镶入一个金属底。
所述金属底呈盆形,与锌筒过盈配合。
所述金属底由马口铁制成。
所述锌筒外边套设一个底部涂有万能胶的塑料筒。
本实用新型按电化学反应计算用锌量,然后做成不带底的锌筒与金属底过盈配合的电池筒,外边再套上一个下部涂有万能胶的塑筒,这样就形成一个完美的电池容器和负极,锌锰干电池在电化学反应过程中,底部不参加反应。该电池筒将原来常规电池锌筒又是容器又是负极的综合作用分开,变成容器和负极的专一作用,能够节约锌锰干电池的用锌量,降低电池成本,提高防漏性能,特别有利于纸板电池在工艺生产过程中使人难以解决的正极上端与负极锌筒相接触部分的污染问题。
附图说明
图1为本实用新型的剖视示意图。
具体实施方式
下面结合附图对本实用新型作进一步详细的描述。
附图标记说明如下:
1-锌筒                2-电芯
3-炭棒                4-塑料组合帽
5-隔离层              6-纸底
7-铁底                8-金属底
9-塑料筒
如图1所示,该锌锰干电池主要由锌筒1、电芯2、炭棒3和塑料组合帽4组成,电芯2与锌筒1之间有隔离层5,锌筒1的筒内底部放有涂塑料膜的盆形纸底6,锌筒的底面装有铁底7,电芯2与塑料组合帽4之间有空气室,防止气胀与漏液,按电化学反应计算用锌量,将锌筒1去掉锌底,镶入一个由马口铁做成的盆形金属底8,这样做成的锌锰干电池容器,既可在电池反应过程中起到负极活性物质作用,又能起到单一的容器作用,为了防止电池在反应过程中气胀和漏液,锌筒1的下端与金属底8的口部过盈配合,然后再套上在底部涂有万能胶的塑料筒9,这样就可以达到防漏的作用。
本实用新型不局限于上述最佳实施方式,任何人在本发明的启示下都可得出其他各种形式的产品。但不论在其形状或结构上作任何变化,凡是与本实用新型相同或相近似的技术方案,均在其保护范围之内。

Claims (4)

1、一种省去锌底的锌锰干电池,包括锌筒、电芯、炭棒和塑料组合帽,电芯与锌筒之间有隔离层,锌筒的筒内底部放有涂塑料膜的盆形纸底,锌筒的底面装有铁底,电芯与塑料组合帽之间有空气室,其特征在于,所述锌筒去掉其底部并镶入一个金属底。
2、根据权利要求1所述的省去锌底的锌锰干电池,其特征在于,所述金属底呈盆形,与锌筒过盈配合。
3、根据权利要求1所述的省去锌底的锌锰干电池,其特征在于,所述金属底由马口铁制成。
4、根据权利要求1所述的省去锌底的锌锰干电池,其特征在于,所述锌筒外边套设一个底部涂有万能胶的塑料筒。
CN200820001575.5U 2008-01-31 2008-01-31 省去锌底的锌锰干电池 Expired - Fee Related CN201146215Y (zh)