A kind of flexible circuit board that prevents that golden finger from fractureing
[technical field]
The utility model relates to a kind of flexible circuit board (Flexible Printed Circuit is called for short FPC), relates in particular to a kind of flexible circuit board that prevents that golden finger from fractureing.
[background technology]
Along with the fast development of mobile communication, the popularity rate of mobile phone is more and more higher, and mobile phone has become out and out multimedia information dissemination carrier, for more prompt people's work and life providing and information service easily.Current people have had higher requirement to the combination property of mobile phone, and simultaneously, keen competition in the industry makes liquid crystal display module (Liquid Crystal Module is called for short LCM) technology become better and approaching perfection day by day.In order to prolong the useful life of product, improve cost performance, and the liquid crystal display module is as an important component part of mobile phone, optimize its structural design and not only saved cost but also behave efficiently beyond doubt.And flexible circuit board is one of modal assembly in the liquid crystal display module, and the quality of its design directly influences the product yield of entire module.
Now, flexible circuit board manually is welded on the mainboard by two-sided pad, become a kind of maturation, utilization process comparatively widely.And face the trend of the slim design of current mobile phone, many companies often become the pad design of flexible circuit board the form of single-face hollowed-out, the flexible circuit board of single-face hollowed-out as shown in Figure 1 and Figure 2: comprise double-deck district 1, the single-face hollowed-out district is pad position 2 (as seen), the part 3 (invisible) that the single-face hollowed-out district is pushed down by the flexible circuit board epiphragma.On the one hand, single-face hollowed-out district thickness is 10Z (10Z=0.035mm), and the thickness of common two-sided pad is about 0.10mm, as shown in Figure 3, Figure 4, adopts the connected mode of single-face hollowed-out just thin a lot of than general two-sided pad connected mode like this; On the other hand, owing to adopt the mode of opening, in the single-face hollowed-out district is that place, pad position opens the mouth that waits width up and down, like this, when flexible circuit board bends, Copper Foil shear surface up and down overlaps, be easy to just produce the obvious stress concentration problem like this at A point place, double-deck simultaneously district thickness is 0.12mm to 0.20mm, and vacancy section thickness is 0.035mm, and both differ an order of magnitude, cause the pad fracture of A point place easily, make to connect open circuit, give to produce to operate on the line and bring great inconvenience, have a strong impact on the production yield.
[summary of the invention]
Technical problem underlying to be solved in the utility model is to overcome the deficiencies in the prior art, from the angle of structural design, provides a kind of flexible circuit board that prevents that golden finger from fractureing, and improves the buckling strength of golden finger pad.
A kind of flexible circuit board that prevents that golden finger from fractureing comprises the golden finger pad, and described golden finger pad is the structure of two sides opening, and wherein, the both sides of a described opening all extend to form reinforced sheet to the epiphragma direction respectively with respect to the both sides of another side opening.
Above-mentioned prevent the flexible circuit board that golden finger fractures, wherein, identical length is all extended to form reinforced sheet to the epiphragma direction respectively with respect to the both sides of another side opening in the both sides of a described opening.
Above-mentioned prevent the flexible circuit board that golden finger fractures, wherein, it is 0.30mm to 0.50mm that identical length range is all extended to the epiphragma direction respectively with respect to the both sides of another side opening in the both sides of a described opening.
The beneficial effects of the utility model and advantage are as follows:
Owing to adopt the structure of two-sided staggered opening, effectively avoided the problem that described stress is concentrated, prevented the phenomenon that golden finger is fractureed, adopt the design of single-face hollowed-out simultaneously, therefore also reduced the integral thickness of flexible circuit board.
Feature of the present utility model and advantage will be elaborated in conjunction with the accompanying drawings by embodiment.
[description of drawings]
Fig. 1 is the flexible circuitry plate structure vertical view of existing single-face hollowed-out.
Fig. 2 is the flexible circuitry plate structure right view of existing single-face hollowed-out.
Fig. 3 is the flexible circuitry plate structure vertical view of existing two-sided pad.
Fig. 4 is the flexible circuitry plate structure right view of existing two-sided pad.
Fig. 5 is the flexible circuitry plate structure left view of the two-sided staggered opening of the utility model.
Fig. 6 is the flexible circuit board upper and lower opening magnitude relationship structural representation of Fig. 5.
[embodiment]
Present embodiment is preferred specific embodiment, as illustrated in Figures 5 and 6.
A kind of flexible circuit board that prevents that golden finger from fractureing comprises double-deck district 1, and the single-face hollowed-out district is golden finger pad position 2 (as seen), the part 3 (invisible) that the single-face hollowed-out district is pushed down by the flexible circuit board epiphragma.As shown in Figure 5, the FPC pad is that the epiphragma 7 that is attached on the Copper Foil 6 is opened a gap the part that its Copper Foil is exposed.Therefore, to be golden finger pad position 2 by epiphragma 7 up and down window vacancy section obtains.Wherein said golden finger pad position 2 is the structure of two sides opening, be respectively upper shed 4 and under shed 5, the width of upper shed 4 is designed to (L) mm (for ease of explanation, here be defined as L), the width of under shed 5 is designed to (L+0.60) mm, monolaterally have more 0.30mm, make the upper and lower opening certain distance that staggers, form the structure of staggered opening than upper shed 4.
When adopting upper and lower opening to stagger, the shear surface that A, B place form staggers mutually, upper shed simultaneously is more following little, when bending, also play a supporting role, so just significantly reduced stress and concentrated, increased the bending strength of golden finger pad, verified through production test, can effectively prevent fractureing of golden finger pad, and when helping producing anchor clamps repeatedly test and reprocess.
Be to be the test of example (volume production 600K) with BYD FPC674C-V0 model below, test data such as following table:
Method for designing |
Bent number of times |
Do not adopt the staggered mode of windowing |
2 times |
Adopt the staggered mode of windowing |
6 times |
Certain further improvement of the utility model, the width that also can be designed under shed 5 is (L) mm, and the width of upper shed 4 is the structure of (L+0.60) mm, and the effect that it produced is the same with effect.
Above content be in conjunction with concrete preferred implementation to further describing that the utility model is done, can not assert that concrete enforcement of the present utility model is confined to these explanations.For the utility model person of an ordinary skill in the technical field; under the prerequisite that does not break away from the utility model design; can also make some simple deduction or replace, all should be considered as belonging to the scope of patent protection that the utility model is determined by claims of being submitted to.