CN200991751Y - 大方坯连铸用四孔浸入式水口 - Google Patents

大方坯连铸用四孔浸入式水口 Download PDF

Info

Publication number
CN200991751Y
CN200991751Y CN 200620168678 CN200620168678U CN200991751Y CN 200991751 Y CN200991751 Y CN 200991751Y CN 200620168678 CN200620168678 CN 200620168678 CN 200620168678 U CN200620168678 U CN 200620168678U CN 200991751 Y CN200991751 Y CN 200991751Y
Authority
CN
China
Prior art keywords
hole
main body
water gap
holes
mouth
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 200620168678
Other languages
English (en)
Inventor
马成
张晓军
宁东
贾宏明
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Angang Steel Co Ltd
Original Assignee
Angang Steel Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Angang Steel Co Ltd filed Critical Angang Steel Co Ltd
Priority to CN 200620168678 priority Critical patent/CN200991751Y/zh
Application granted granted Critical
Publication of CN200991751Y publication Critical patent/CN200991751Y/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型涉及一种用于连铸结晶器的大方坯四孔浸入式水口,它是由水口主体、凸台、中心圆形孔、镶嵌层和四个倾斜通孔组成。特征是镶嵌层设在水口主体下端工作层面,其材质比主体优良,四个倾斜通孔在水口主体最下端绕圆周均匀分布,其孔形为两头带圆弧的长形孔、倾斜度相对水口中心圆孔内壁向下倾斜30±3度。它的使用寿命长成本又低,能使结晶器中的钢液液面活跃又相对地稳定、没有死区,能保证钢液混合均匀、温度均匀、冲刷力不集中、不影响结晶器的使用寿命、不卷渣、钢中夹杂物上浮比较彻底、浇注出的钢坯质量好。

Description

大方坯连铸用四孔浸入式水口
技术领域
本实用新型涉及一种炼钢连铸用浸入式水口,尤其是一种用于连铸结晶器的大方坯四孔浸入式水口。
背景技术
炼钢工业中,连铸结晶器用浸入式水口是起到保护和控制钢流的作用,现有技术中大方坯连铸用浸入式水口一般均采用直筒式或两孔式的。直筒式浸入式水口从水口喷出的钢液流股向下冲击力最大、最集中,使结晶器中的钢水液面不活跃,易形成死区,增加了铸坯卷渣概率;由于钢流流股向下冲击深度也最大,造成钢水中的夹杂物不易上浮,影响钢坯的质量。两孔式浸入式水口一般是设在水口下端两侧,从水口喷出的钢流流股也比较集中、流速大,对坯壳冲刷力也很大,影响了坯壳均匀地形成;由于钢流流股向下冲击深度也很大,造成钢水中的夹杂物也不易上浮,影响钢坯的质量。另外在水口不设孔的两侧,会使结晶器中的钢水液面不活跃,易形成死区,增加了铸坯卷渣概率。
发明内容
鉴于存在的上述问题,本实用新型的目的是研制一种在大方坯浇注过程中,能使结晶器中的钢液液面活跃又相对地稳定、没有死区,能保证钢液混合均匀、温度均匀、冲刷力不集中、结晶器寿命长、钢中夹杂物上浮比较彻底、钢坯质量好的浸入式水口。
为了实现本实用新型的目的,采取的技术措施是发明一种大方坯连铸用四孔浸入式水口,水口主体1是带有中心圆形孔3、上端带有凸台2、下端带孔的圆柱体,其特征在于:1)水口主体1下端外围孔上面三分之一段处内外镶有镶嵌层4,,2)水口主体1最下端绕圆周设有均匀分布的四个倾斜通孔5。
所述的四个倾斜通孔5,其特征在于两面孔形为两头带圆弧的长形孔。
所述的四个倾斜通孔5,其特征在于孔的倾斜度相对水口中心圆孔3内壁向下倾斜30±3度。
所述的镶嵌层4,其特征在于它的材质要比水口主体1的材质优良。
本实用新型是在大方坯浇注过程中使用的四孔浸入式水口,使用寿命长成本又低,能使结晶器中的钢液液面活跃又相对地稳定、没有死区,能保证钢液混合均匀、温度均匀、冲刷力不集中、不影响结晶器的使用寿命、不卷渣、钢中夹杂物上浮比较彻底、浇注出的钢坯质量好。
附图说明
图1为大方坯连铸用四孔浸入式水口的整体结构示意图。
图2为大方坯连铸用四孔浸入式水口A-A截面剖视图。
图3为大方坯连铸用四孔浸入式水口中四个倾斜通孔5两面的B向视图。
如图1、2、3所示,大方坯连铸用四孔浸入式水口是由水口主体1、凸台2、中心圆形孔3、镶嵌层4和四个倾斜通孔5组成的。水口主体1是圆柱形的,水口中心由上至下开有圆孔3,制造方便;其上端设有凸台2,使其坐在中间盛钢桶的座砖上;在水口的最下端设有均匀分布的四个倾斜通孔5,其两面孔形为两头带圆弧的长形孔,其孔的倾斜度相对水口中心圆孔3内壁向下倾斜30±3度,倾斜的角度不能过大,否则会使钢液向下的流速过大,影响结晶器底部钢水夹杂物的上浮,倾斜的角度也不能过小,否则会使钢液向上的流速过大,会使钢水液面波动过大,易造成卷渣(保护渣),四个向下倾斜30±3度、两面孔形为两头带圆弧的长形孔可以使钢水在浇注过程中,使结晶器中钢液液面活跃又相对地稳定、没有死区,钢液混合均匀、温度均匀、对结晶器壁冲刷力缓慢、钢中夹杂物上浮比较彻底,保证了浇注钢坯质量;中心圆形孔3从水口凸台2上面一直开到水口底部;在水口的工作面层,就是在水口主体1最下端四个倾斜通孔5的上面三分之一段处内外镶有镶嵌层4,此镶嵌层4的材质要优于水口主体1的材质,这种复合式水口砖既可提高其使用寿命,又可降低成本。
具体实施方式
下面结合附图和实施例介绍本实用新型详细的技术内容和使用效果:如图1、2、3所示,水口主体1选择铝碳质耐火材料、镶嵌层4选择锆质耐火材料制造浸入式水口:水口主体1为圆柱体,上端设有凸台2、中心开有从上到下的圆孔3、下端绕圆周均匀设有四个倾斜通孔5,其两面孔形为两头带圆弧的长形孔,相对中心圆孔3内壁向下倾斜30±3度角。
将10个四孔浸入式水口和3个两孔浸入式水口在大方坯连铸机上进行比较试验,其结果如下:试验钢种为SWRH72A和SWRH82A,每次试验均于LF炉处理后,在中间包里和第一块铸坯、第三块铸坯上取金相夹杂试样,对试样的夹杂物组成、夹杂颗粒大小、夹杂粒度分级、夹杂平面百分含量进行检验分析。分析表明,四孔浸入式水口要比两孔浸入式水口的去除夹杂能力提高22.21%。

Claims (3)

1.一种大方坯连铸用四孔浸入式水口,水口主体(1)是带有中心圆形孔(3)、上端带有凸台(2)、下端带孔的圆柱体,其特征在于:
1)水口主体(1)下端外围孔上面三分之一段处内外镶有镶嵌层(4),
2)水口主体(1)最下端绕圆周设有均匀分布的四个倾斜通孔(5)。
2.根据权利要求1所述的大方坯连铸用四孔浸入式水口,其特征在于四个倾斜通孔(5)的两面孔形为两头带圆弧的长形孔。
3.根据权利要求1或2所述的大方坯连铸用四孔浸入式水口,其特征在于四个倾斜通孔(5)的倾斜度相对水口中心圆孔(3)内壁向下倾斜30±3度。
CN 200620168678 2006-12-28 2006-12-28 大方坯连铸用四孔浸入式水口 Expired - Fee Related CN200991751Y (zh)