CN200940680Y - 高弹多层阻水密封圈 - Google Patents

高弹多层阻水密封圈 Download PDF

Info

Publication number
CN200940680Y
CN200940680Y CN 200620109481 CN200620109481U CN200940680Y CN 200940680 Y CN200940680 Y CN 200940680Y CN 200620109481 CN200620109481 CN 200620109481 CN 200620109481 U CN200620109481 U CN 200620109481U CN 200940680 Y CN200940680 Y CN 200940680Y
Authority
CN
China
Prior art keywords
seal ring
utility
model
elastic multilayer
sealing
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 200620109481
Other languages
English (en)
Inventor
罗建华
黄安云
刘建
彭文正
涂宇
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SENPU PIPES CO Ltd GUIZHOU
Original Assignee
SENPU PIPES CO Ltd GUIZHOU
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SENPU PIPES CO Ltd GUIZHOU filed Critical SENPU PIPES CO Ltd GUIZHOU
Priority to CN 200620109481 priority Critical patent/CN200940680Y/zh
Application granted granted Critical
Publication of CN200940680Y publication Critical patent/CN200940680Y/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型公开了一种高弹多层阻水密封圈,其特征在于:密封圈圈壁(1)横截面呈锯齿形,齿数为4~8齿(2),齿深e为密封圈厚度的1/2~3/4,齿尖夹角α为30°~60°。具有结构合理、加工成型容易、使用简单快捷、阻水效果好、能实现良好密封的特点。

Description

高弹多层阻水密封圈
技术领域
本法实用新型属于化学建材领域,具体来说涉及一种密封圈。
背景技术
现有的非金属管材,大多采用承插的连接方式,其优点在于方便、快捷,但同时也存在着连接处漏水密封效果不好的问题,如:埋地式高电力电缆用氯化聚氯乙烯(PVC-C)套管,连接处由于没有良好的密封易将水、油渗入套管,会损坏电缆,酿成质量事故。为解决这一问题,目前普遍采用两种办法:第一、专用胶水密封法。胶水密封法主要采用胶水对管材连接处进行密封。这种方法也起到一定的效果,但是,当连接处的间隙较大,其密封效果就很难保证;另外,胶水长期处于潮湿的环境中,容易老化从而影响密封;第二、密封圈密封法。这种方法就是在管材连接处套一橡胶圈,利用橡胶的弹性对其进行密封。橡胶耐腐蚀,不易老化,比起胶水密封更方便,更可靠。但目前市场上针对这一类的密封圈结构大多比较简单,弹性不够、阻水面积小,因而密封效果不理想。
实用新型内容
本实用新型的目的在于克服上述缺点而提供的一种结构合理、加工成型容易、使用简单快捷、阻水效果好、能实现良好密封的高弹多层阻水密封圈。
本实用新型的目的及解决其主要技术问题是采用以下技术方案来实现的:本实用新型的高弹多层阻水密封圈,其密封圈圈壁横截面呈锯齿形,齿数为4~8齿,齿深为密封圈厚度的1/2~3/4,齿尖夹角30°~60°。
上述的高弹多层阻水密封圈,密封圈外径D=C×(101~103)%,其中C为扩口内径,比扩口略大的密封圈外径有利于管材密封
上述密封圈,密封圈内径d在外径D确定的情况下按下式取值:
(D-d)/2=(C-A)/2×(105~120)%
其中:A为管材外径。
本实用新型与现有技术相比,由以上技术方案可知,是综合考虑了密封效果和加工成型问题,来确定的密封圈圈壁结构、密封圈齿数、齿深及齿尖夹角,比扩口略大的密封圈外径有利于管材密封,根据密封国内径取值综合考虑了密封圈外径、扩口内径、管材外径以及橡胶的软弱性,来实现最佳的密封效果。因而本实用新型结构合理、加工成型容易、性能可靠;使用简单、方便、快捷。
本实用新型的具体实施方式由以下实施例及其附图详细给出。
附图说明
图1为本实用新型的结构示意图;
图2为本实用新型的使用状态图。
图中标记:
1、圈壁,2、齿,3、密封圈,4、管材A,5、管材B;
D、密封圈外径,C、扩口内径,d、密封圈内径,A、管材外径,e齿深,α、齿尖夹角。
具体实施方式
以下结合附图及较佳实施例,对依据本实用新型提出的高弹多层阻水密封圈的具体实施方式、结构、特征及其功效,详细说明如后。
参见图1-2,高弹多层阻水密封圈,考虑到密封效果和成型问题,密封圈圈壁1横截面呈锯齿形,齿数为4~8齿2,齿深e为密封圈厚度的1/2~3/4,齿尖夹角α为30°~60°。
密封圈外径D按下式取值:D=C×(101~103)%,其中C为扩口内径,比扩口略大的密封圈外径有利于管材密封。
密封圈内径d在外径D确定的情况下按下式取值:
(D-d)/2=(C-A)/2×(105~120)%
其中:A为管材外径。
根据橡胶的软弱性选择取值,软弱性越好,密封圈内径d值可取大;反之亦然。
使用时,先将密封圈3套入管材A4的承插扩口内,然后将管材B5的一端插入即可,可见此密封圈使用极其简单,方便、快捷。
以上所述,仅是本实用新型的较佳实施例而已,并非对本实用新型作任何形式上的限制,任何未脱离本实用新型的技术方案内容,依据本实用新型的技术实质对以上实施例所作的任何简单修改、等同变化与修饰,均仍属于本实用新型技术方案的范围内。

Claims (3)

1、一种高弹多层阻水密封圈,其特征在于:密封圈圈壁(1)横截面呈锯齿形,齿数为4~8齿(2)。
2、如权利要求1所述的高弹多层阻水密封圈,其特征在于:齿深e为密封圈厚度的1/2~3/4,齿尖夹角α为30°~60°。
3、如权利要求1或2所述的高弹多层阻水密封圈,其特征在于:
密封圈外径D按下式取值
D=C×(101~103)%
其中:C为扩口内径;
密封圈内径d按下式取值
(D-d)/2=(C-A)/2×(105~120)%
其中:A为管材外径。
CN 200620109481 2006-06-29 2006-06-29 高弹多层阻水密封圈 Expired - Fee Related CN200940680Y (zh)