CN1931492A - Machining process of side gap in cold and hot metal cutting circular saw blade - Google Patents

Machining process of side gap in cold and hot metal cutting circular saw blade Download PDF

Info

Publication number
CN1931492A
CN1931492A CN 200610048375 CN200610048375A CN1931492A CN 1931492 A CN1931492 A CN 1931492A CN 200610048375 CN200610048375 CN 200610048375 CN 200610048375 A CN200610048375 A CN 200610048375A CN 1931492 A CN1931492 A CN 1931492A
Authority
CN
China
Prior art keywords
saw blade
processing
cold
grinding machine
grinding
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN 200610048375
Other languages
Chinese (zh)
Other versions
CN100404182C (en
Inventor
郭继富
褚建坤
方宪民
万红侠
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
TANGSHAN METALLURGICAL SAW BLADE CO Ltd
Original Assignee
TANGSHAN METALLURGICAL SAW BLADE CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by TANGSHAN METALLURGICAL SAW BLADE CO Ltd filed Critical TANGSHAN METALLURGICAL SAW BLADE CO Ltd
Priority to CNB2006100483750A priority Critical patent/CN100404182C/en
Publication of CN1931492A publication Critical patent/CN1931492A/en
Application granted granted Critical
Publication of CN100404182C publication Critical patent/CN100404182C/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The present invention relates to metallurgical saw blade machining, and is especially the machining process of side gap of circular saw blade for cold and hot metal cutting. The machining process in a symmetrical grinding machine includes the following steps: 1. preparing flattened plate saw blade; 2. turning or milling the parallel notches on two sides simultaneously; 3. grinding with end faces of grinding wheels; 4. grinding the inclined side gaps to finish the side gap machining; 5. re-flattening the saw blade; and 6. balance detection and treatment. The symmetrical machining process of the present invention has less deformation and high production efficiency.

Description

Machining process of side gap in cold and hot metal cutting circular saw blade
Technical field:
The present invention relates to the metallurgical saw processing method, specifically a kind of machining process of side gap in cold and hot metal cutting circular saw blade.
Background technology:
Cold and hot metal cutting circular saw blade is a Metallurgical Enterprise steel parting tool commonly used.The blade bodies structure generally is divided into the structure that slab construction and side have groove, and the former handling ease is most widely used, latter's processed complex, but can save energy consumption.At home, cold and hot metal cutting circular saw blade is based on slab construction, few sheet body structure that adopts two-sided sideshake, even adopt also be take single face respectively the mode of turning carry out sideshake processing, because saw blade local pyrexia in turning process is higher, be very easy to cause the saw blade distortion and be difficult to smoothing, saw blade thermal deformation simultaneously makes the turning degree of depth inequality of saw blade later on, to the very big harmful effect of balance quality generation of saw blade.Therefore, bilateral crack cold and hot metal cutting circular saw blade production application at home up to the present still belongs to blank.
Summary of the invention:
The object of the invention provides a kind of bilateral machining process of side gap in cold and hot metal cutting circular saw blade of machining simultaneously that adopts, to solve original single face problem of serious, the balance quality difference of the saw blade distortion that exists of turning processing sideshake method respectively.
The technical scheme that realizes the foregoing invention purpose is:
A kind of cold and hot metal cutting circular saw blade processing method, it adopts the processing of grinding machine bed, and its step is as follows:
A, the good dull and stereotyped saw blade of preparation smoothing;
B, process the bilateral parallel groove simultaneously on to the grinding machine bed, processing mode is turning, milling;
C, fluted with abrasive wheel end face grinding simultaneously on to the grinding machine bed improves its roughness;
D, adjust the bistrique angle on to the grinding machine bed, grind the double-sided bevel sideshake of saw blade simultaneously, thereby finish the processing of compound sideshake;
E, smooth the saw blade flatness again, Circular Run-out Tolerance reaches the saw blade standard-required;
F, saw blade is carried out balance detection and processing, reach technological requirement.
The difference of the present invention and existing method is: at first adopt the method for bilateral machining to process the bilateral parallel groove to saw blade, to enhance productivity, reduce the sheet body deformability, adopt bilateral to mill then, grinding bilateral parallel groove, improve the uniformity of saw blade thickness, improve surface quality, improve the balance quality of saw blade.
In process, saw blade vertically is held on a rotary power unit, rotating speed is stepless adjustable, move arbitrarily position, the left and right sides, and the location, places a cover machining cell respectively in the both sides of saw blade, cutter or emery wheel can rotate arbitrarily, and can be to saw blade feed or withdrawing, for easy to process, the main-shaft axis of machining cell can about, left and right adjusting.
Description of drawings:
Fig. 1 is of the present invention to grinding machine bed structure schematic diagram for being used for.
The specific embodiment:
Below in conjunction with drawings and Examples in detail the present invention is described in detail.
A kind of cold and hot metal cutting circular saw blade processing method, it adopts the processing of grinding machine bed, and its step is as follows:
A, prepare the qualified dull and stereotyped saw blade 2 of smoothing, it is installed between the chuck 3 and fastening, driven by saw blade whirligig 1, speed is stepless adjustable.
B, processing bilateral parallel groove, processing mode is turning, milling.In this cutting process, machining cell () 4 and machining cell (two) 5 is installed respectively by lathe tool or milling cutter 6 is processed, the cutter rotary speed is stepless adjustable, and can be along the axis direction advance and retreat to finish the processing of bilateral parallel groove;
C, grinding are fluted, to improve its roughness.In this grinding process, machining cell () 4 and machining cell (two) 5 are installed emery wheel 6 respectively, and be fluted with the abrasive wheel end face grinding.
D, processing double-sided bevel sideshake carry out compound sideshake processing.In this operation, adjust the bistrique angle is angle of emery wheel 6 cards inclination, finishes inclined-plane processing along axis advance and retreat cutter.
E, smooth operation again.Again smooth flatness, the Circular Run-out Tolerance value of saw blade 2, make saw blade 2 flatnesses≤0.3mm, Circular Run-out Tolerance value≤1.5mm.
F, balance detection and treatment process.The saw blade 2 minimum amount of unbalances that allow reach as following table numerical value.
The saw blade diameter φ1000mm~ φ1500mm >φ1500mm~φ 1800mm >φ1800mm~φ 2000mm >φ2000mm~φ 2500mm
Allow maximum amount of unbalance (gcm) 1600 2400 4000 5500
Present embodiment adapts to saw blade diameter D=φ 1000mm~φ 2500mm, saw blade thickness T=5mm~15m, the one-sided sideshake degree of depth (T-T 1)/2=0.5mm~0.75mm, one-sided sideshake gradient 1: 400~1: 800, sideshake width t≤550mm.
Processing for convenience, the axis of above-mentioned each machining cell can about, about etc. direction regulate.

Claims (1)

1, a kind of cold and hot metal cutting circular saw blade processing method, it adopts the processing of grinding machine bed, and its step is as follows:
A, the good dull and stereotyped saw blade of preparation smoothing;
B, process the bilateral parallel groove simultaneously on to the grinding machine bed, processing mode is turning, milling;
C, fluted with abrasive wheel end face grinding simultaneously on to the grinding machine bed improves its roughness;
D, adjust the bistrique angle on to the grinding machine bed, grind the double-sided bevel sideshake of saw blade simultaneously, thereby finish the processing of compound sideshake;
E, smooth the saw blade flatness again, Circular Run-out Tolerance reaches the saw blade standard-required;
F, saw blade is carried out balance detection and processing, reach technological requirement.
CNB2006100483750A 2006-09-29 2006-09-29 Machining process of side gap in cold and hot metal cutting circular saw blade Expired - Fee Related CN100404182C (en)