CN1923942A - 一种自动补胎液 - Google Patents

一种自动补胎液 Download PDF

Info

Publication number
CN1923942A
CN1923942A CN 200610140768 CN200610140768A CN1923942A CN 1923942 A CN1923942 A CN 1923942A CN 200610140768 CN200610140768 CN 200610140768 CN 200610140768 A CN200610140768 A CN 200610140768A CN 1923942 A CN1923942 A CN 1923942A
Authority
CN
China
Prior art keywords
liquid
tire
parts
mending
tyre
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 200610140768
Other languages
English (en)
Inventor
赵良松
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shen Lvyuan
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 200610140768 priority Critical patent/CN1923942A/zh
Publication of CN1923942A publication Critical patent/CN1923942A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种自动补胎液,所述补胎液为由下列重量份配比的原料制备而成的一种罐装液:天然橡胶2.5-4.0份;氨水48.0-54.0份;蒸馏水48.0-54.0份;稳定剂0.5-1.5份;推进剂0.15-0.20份。本发明根据动态密封原理研制生产,通过与汽车轮胎匹配的喷嘴,充入到轮胎中,立即在破洞处聚合,结胶将破洞纵向堵住,其余液体气化后膨胀,使补胎充气一次完成,高效方便,特别适用于所有无内胎的高级轿车。高效奇特,自动补胎充气,是真空轮胎的伴侣。

Description

一种自动补胎液
技术领域
本发明涉及一种自动补胎液。
背景技术
轮胎的橡胶中的微细孔以及无内胎轮胎与轮辋的接触不严都会造成慢泄气。车辆在行驶中,轮胎会被路面上的钉子或尖硬物质扎破,造成急性泄气。长距离高速行驶,特别是在炎热的夏季,在灼热的路面上行驶,也会使轮胎内局部聚集越来越高的温度,以至最后会发生爆胎。以上这些情况,轻者使车辆抛锚,重者会发生翻车或控车,甚至发生车毁人亡的重大事故。这种事故,在世界范围内都是屡见不鲜的。因此,自有充气轮胎以来,人们就不断地致力于研究轮胎的补胎技术,特别是如何在轮胎内灌注某种预防轮胎慢泄气和填补轮胎孔洞的产品。最早出现的这类产品是本世纪二三十年代在美国的军用车辆的轮胎中灌注的自动补胎液。在六十年代,美国的阿波罗登月车轮胎内也灌注了补胎液。一代接一代的补胎液相继问世,不断地改进和提高。但以往的各种产品都存在着一定的缺陷。如有的是充气灌补胎液,其成份只能使泄气的轮胎暂时充气,行使到最近的修理站为止。有的轮胎补胎液会在胎内干枯或遇寒冷天气结冰,非但失去补漏效果,反而会损害轮胎的内壁。有的补胎液用各种天然纤维或石棉纤维和化学物品,这些纤维会在轮胎内逐渐结团,失去补胎效果,且会磨损轮胎内壁,还会使车辆在行驶时颤动。还有一种产品,是用再生橡胶颗粒在甲苯中膨胀后作为填补轮胎孔洞的基料。这种补股液有一定的长处,但被橡胶颗粒吸收的甲苯在胎中散发出气体,会使轮胎的橡胶变脆,容易开裂,况且甲苯是危险品,在工作场地稍有不甚就会发生爆炸。
发明内容
本发明需要解决的技术问题就在于克服现有技术的缺陷,提供一种自动补胎液。
为解决上述问题,本发明采用如下技术方案:
本发明一种自动补胎液,所述补胎液为由下列重量份配比的原料制备而成的一种罐装液:天然橡胶2.5-4.0份;氨水48.0-54.0份;蒸馏水48.0-54.0份;稳定剂0.5-1.5份;推进剂0.15-0.20份。
优选的,本发明所述补胎液制备原料的重量份配比为:天然橡胶3份;氨水50份;蒸馏水50份;稳定剂1份;推进剂0.15份。
本发明所述推进剂为氟利昂负12。
本发明补胎液补胎不用扒胎,3秒即可补好,一次加入可长期使用,车辆在行驶中一旦胎被扎破,不用停车自动补好,彻底改变了传统的手工补胎的方法。补胎能力强,能够填补小至微细孔和大至6mm的孔洞。对各类车辆的充气橡胶轮胎,不论有无内胎均同样适用。注入轮胎后,长期保持液态,至一40℃不冻结,至100℃不分解;对轮胎和金属轮钢不腐蚀并能防锈;产品本身不燃烧,且无毒和不污染。市场潜力极大。
本发明根据动态密封原理研制生产,通过与汽车轮胎匹配的喷嘴,充入到轮胎中,立即在破洞处聚合,结胶将破洞纵向堵住,其余液体气化后膨胀,使补胎充气一次完成,高效方便,特别适用于所有无内胎的高级轿车。高效奇特,自动补胎充气,是真空轮胎的伴侣。
本发明的使用方法:
1、使用前摇匀;
2、打开罐上保险盖,在轮胎气门嘴上按顺时针方向拧紧铁筒喷嘴;
3、按下顶部开关按钮,即可注入补胎液自行补胎充气;
4、注气后立即将车慢速行驶3~5公里,使注入的补胎剂均匀在整个轮胎内层面。
5、补漏充气后应立即开动行驶,以防补胎液凝聚;
6、充气时尽量避免吸入本产品气体或与皮肤长时间触,勿使儿童接近。
具体实施方式
实施例1
将天然橡胶2.5份;氨水54.0份;蒸馏水48.0份;稳定剂1.5份;推进剂0.15份混合均匀,进行密封罐装即得本发明所述补胎液。
实施例2
将天然橡胶3份;氨水50份;蒸馏水50份;稳定剂1份;推进剂0.15份混合均匀,进行密封罐装即得本发明所述补胎液。
实施例3
将天然橡胶4.0份;氨水48.0份;蒸馏水54.0份;稳定剂0.5份;推进剂0.20份混合均匀,进行密封罐装即得本发明所述补胎液。
实施例1-3所述推进剂为氟利昂负12。
本发明不局限于上述最佳实施方式,任何人在本发明的启示下得出的其他任何与本发明相同或相近似的产品,均落在本发明的保护范围之内。

Claims (3)

1、一种自动补胎液,其特征在于:所述补胎液为由下列重量份配比的原料制备而成的一种罐装液:天然橡胶2.5-4.0份;氨水48.0-54.0份;蒸馏水48.0-54.0份;稳定剂0.5-1.5份;推进剂0.15-0.20份。
2、如权利要求1所述的自动补胎液,其特征在于:所述补胎液制备原料的重量份配比为:天然橡胶3份;氨水50份;蒸馏水50份;稳定剂1份;推进剂0.15份。
3、如权利要求1或2所述的自动补胎液,其特征在于:所述推进剂为氟利昂负12。
CN 200610140768 2006-10-10 2006-10-10 一种自动补胎液 Pending CN1923942A (zh)