CN1772693A - 一种自流平水泥及其生产工艺 - Google Patents

一种自流平水泥及其生产工艺 Download PDF

Info

Publication number
CN1772693A
CN1772693A CN 200510061004 CN200510061004A CN1772693A CN 1772693 A CN1772693 A CN 1772693A CN 200510061004 CN200510061004 CN 200510061004 CN 200510061004 A CN200510061004 A CN 200510061004A CN 1772693 A CN1772693 A CN 1772693A
Authority
CN
China
Prior art keywords
self
cement
leveling
leveling cement
crossed
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN 200510061004
Other languages
English (en)
Other versions
CN1318345C (zh
Inventor
李凌伟
马国中
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CNB2005100610041A priority Critical patent/CN1318345C/zh
Publication of CN1772693A publication Critical patent/CN1772693A/zh
Application granted granted Critical
Publication of CN1318345C publication Critical patent/CN1318345C/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种自流平水泥及其生产工艺,按重量百分比包括下列组分:铝酸盐水泥5-20%、普通硅酸盐水泥20-26%、石英砂32-50%、重碱15-25%、甲基纤维素0.5-2%、胶粉2.5-5%、无水柠檬酸0.1-0.5%、消石灰1.6-2.5%、石膏粉0.5-1.5%、干粉消泡剂0.5-1.5%,其特征在于还包括干酪素0.8-8%、碳酸锂0.03-0.07%。生产工艺依次是:筛选;配料;送料;搅拌;检验;包装入库。本发明在配方中增加了干酪素及碳酸锂,使产品的抗折、抗压强度、自流平性能及稳定性大大提高。该技术可应用在自流平水泥的生产上。

Description

一种自流平水泥及其生产工艺
                            技术领域
本发明涉及建筑材料,更具体地说涉及一种自流平水泥及其生产工艺。
                            背景技术
随着国民经济的快速发展和人民生活水平的不断提高,对人们生活的环境也提出了更高的要求,一些医院、体育馆、博物馆等高档建筑的地坪采用弹性地材,这类材料足感舒适、颜色丰富漂亮,还可任意的裁剪拼花等,深受消费者的喜爱,而这些材料的铺设对地面的找平提出了更高的要求。近年来,先后研制和生产出自流平水泥或自流平砂浆,而所用的粘结剂主要是胶粉,所用的原料中含有不稳定的柠檬酸分子,这对自流平水泥的粘结强度、自流平性能和质量稳定性都还够不理想。
                            发明内容
本发明克服了现有技术中的不足,提供一种自流平水泥及其生产工艺。
本发明所述的一种自流平水泥,按重量百分比包括下列组分:铝酸盐水泥5-20%、普通硅酸盐水泥20-26%、石英砂32-50%、重碱15-25%、甲基纤维素0.5-2%、胶粉2.5-5%、无水柠檬酸0.1-0.5%、消石灰1.6-2.5%、石膏粉0.5-1.5%、干粉消泡剂0.5-1.5%,其特征在于还包括干酪素0.8-8%、碳酸锂0.03-0.07%。
一种自流平水泥的生产工艺依次是:筛选:将大颗粒的原料通过筛子去除;配料:根据上述配方配料;送料:将各原料输送到搅拌机;搅拌:通过搅拌机将原料搅拌均匀;检验:检查混合料的物理和化学性能;包装入库:将合格的自流平水泥装袋或装罐后入库。
按照上述方法制造的一种自流平水泥,在配方中增加了干酪素和碳酸锂,克服了原料中含有的不稳定柠檬酸分子的影响,使产品的抗折、抗压强度、自流平性能及稳定性大大提高。
                         具体实施方式
下面结合实施例对本发明作进一步的描述。
本发明所述的一种自流平水泥,按重量百分比包括下列组分:铝酸盐水泥5-20%、普通硅酸盐水泥20-26%、石英砂32-50%、重碱15-25%、甲基纤维素0.5-2%、胶粉2.5-5%、无水柠檬酸0.1-0.5%、消石灰1.6-2.5%、石膏粉0.5-1.5%、干粉消泡剂0.5-1.5%、干酪素0.8-8%、碳酸锂0.03-0.07%。
材料名称   实施例1各组分的量Kg   实施例2各组分的量Kg   实施例3各组分的量Kg   实施例4各组分的量Kg   实施例5各组分的量Kg
  铝酸盐水泥   5   6   5   10   20
  普通硅酸盐水泥   20   26   21   22   23
  石英砂   35   36.83   50   35   32
  重碱   25   18   15   17.54   16
  甲基纤维素   2   0.5   1.37   0.8   0.6
  胶粉   5   2.5   4   3   3.5
  无水柠檬酸   0.5   0.1   0.2   0.3   0.4
  消石灰   2.5   2   1.6   1.8   1.7
  石膏粉   1   1.5   0.5   0.7   0.8
  干酪素   3   5   0.8   8   1.26
  干粉消泡剂   0.95   1.5   0.5   0.8   0.7
  碳酸锂   0.05   0.07   0.03   0.06   0.04
以上各实施例一种自流平水泥的生产工艺依次是:筛选:将大颗粒的原料通过筛子去除;配料:根据上述配方配料;送料:将各原料输送到搅拌机;搅拌:通过搅拌机将原料搅拌均匀;检验:检查混合料的物理和化学性能;包装入库:将合格的自流平水泥装袋或装罐后入库。
所述的筛选是指:石英砂过70-140目筛、重碱过300-350目筛、碳酸锂过300-350目筛、无水柠檬酸过60-80目筛。

Claims (3)

1、一种自流平水泥,按重量百分比包括下列组分:铝酸盐水泥5-20%、普通硅酸盐水泥20-26%、石英砂32-50%、重碱15-25%、甲基纤维素0.5-2%、胶粉2.5-5%、无水柠檬酸0.1-0.5%、消石灰1.6-2.5%、石膏粉0.5-1.5%、干粉消泡剂0.5-1.5%,其特征在于还包括干酪素0.8-8%、碳酸锂0.03-0.07%。
2、根据权利要求1所述的一种自流平水泥的生产工艺其特征在于依次是:筛选:将大颗粒的原料通过筛子去除;配料:根据上述配方配料;送料:将各原料输送到搅拌机;搅拌:通过搅拌机将原料搅拌均匀;检验:检查混合料的物理和化学性能;包装入库:将合格的自流平水泥装袋或装罐后入库。
3、根据权利要求2所述的一种自流平水泥的生产工艺,其特征在于所述的筛选是指:石英砂过70-140目筛、重碱过300-350目筛、碳酸锂过300-350目筛、无水柠檬酸过60-80目筛。
CNB2005100610041A 2005-10-09 2005-10-09 一种自流平水泥及其生产工艺 Expired - Fee Related CN1318345C (zh)