CN1724439A - Energy-saving environment protecting waste brick - Google Patents
Energy-saving environment protecting waste brick Download PDFInfo
- Publication number
- CN1724439A CN1724439A CNA2005100438746A CN200510043874A CN1724439A CN 1724439 A CN1724439 A CN 1724439A CN A2005100438746 A CNA2005100438746 A CN A2005100438746A CN 200510043874 A CN200510043874 A CN 200510043874A CN 1724439 A CN1724439 A CN 1724439A
- Authority
- CN
- China
- Prior art keywords
- energy
- brick
- saving environment
- environment protecting
- grain slag
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
An energy-saving grain slag brick is prepared proportionally from the grain slag generated by smelting iron, cement, cobbles, coal ash and gypsum powder through proportional mixing, adding water, stirring and shaping in non-calcining brack maker. Its advantages are no need of calcining, high compression strength and high thermal insulation effect.
Description
(1) technical field:
The present invention relates to building brick.
(2) background technology:
At present, clay brick, heat insulation effect difference short because of waste soil and coal resource, life-span just progressively withdraws from the building materials market.The substitute is with industrial residues such as coal ash is the brick that raw material is made, and this brick is mixed with lime more, and indexs such as it is freeze proof, drying shrinkage are difficult to reach, and ultimate compression strength is low, and heat insulating effect is poor.
(3) summary of the invention:
The present invention is directed to the deficiencies in the prior art, provide that a kind of crushing resistance is strong, the energy-saving environment protecting waste brick of high insulating effect.
This energy-saving environment protecting waste brick comprises the component of following weight proportion: grain slag 40--60%, cement 10--15%, stone 10--25%, coal ash 5--10%, terra alba 1--3%.
A kind of waste material that produces when grain slag is for ironmaking in the said components plays insulation effect; Cement, stone can be gained in strength, and improve compressive property; Coal ash plays adhesive effect; Terra alba plays the rapid solidification effect.Each component is prepared mixing in proportion, after the adding suitable quantity of water stirs, sends into baking-free brick-making machine and shapes.
The present invention is by having the not component preparation of same-action, and direct forming need not be fired energy-conserving and environment-protective.The compressive strength rate clay brick can improve 10-20%, and good effect of heat insulation is difficult for suction, long service life.
(4) embodiment:
Embodiment 1:
Each component is pressed following weight proportion: grain slag 53%, 325# cement 15%, stone 24%, coal ash 7%, terra alba 1%.Each component is prepared mixing in proportion, adds at normal temperatures and pressures after suitable quantity of water stirs, and sends into baking-free brick-making machine and shapes.The ultimate compression strength that makes brick is 9Kg/cm
2
Embodiment 2:
Each component is pressed following weight proportion: grain slag 60%, 325# cement 10%, stone 23%, coal ash 5%, terra alba 2%.Each component is prepared mixing in proportion, adds at normal temperatures and pressures after suitable quantity of water stirs, and sends into baking-free brick-making machine and shapes.The ultimate compression strength that makes brick is 7.5Kg/cm
2
Claims (1)
1. energy-saving environment protecting waste brick, it is characterized in that: this grain slag brick comprises the component of following weight proportion: grain slag 40--60%, cement 10--15%, stone 10--25%, coal ash 5--10%, terra alba 1--3%.