CN1634789A - Energy-saving sintering brick - Google Patents
Energy-saving sintering brick Download PDFInfo
- Publication number
- CN1634789A CN1634789A CNA2003101097398A CN200310109739A CN1634789A CN 1634789 A CN1634789 A CN 1634789A CN A2003101097398 A CNA2003101097398 A CN A2003101097398A CN 200310109739 A CN200310109739 A CN 200310109739A CN 1634789 A CN1634789 A CN 1634789A
- Authority
- CN
- China
- Prior art keywords
- energy
- coal ash
- saving
- clay
- raw material
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
Disclosed is an energy-saving clinker brick, characterized in that, it is made by the raw materials of clay or oil shale land, waste coal ash and additives. In comparision with the prior art, the invention has the advantages of 40% energy saving, 20 to 30 labels improvement of compression strength and transverse strength, reinforced industrial waste slag processing capacity, wide raw material source, scientific formula and wide applicable aspects.
Description
Technical field:
The present invention relates to building brick, particularly a kind of energy-saving clinker brick that additive is arranged.
Background technology:
At present, the production of vitrified brick is except that minority enterprise adds some cinders, all do not use additive, though the appearance of non-fuel autoignition sintered brick is arranged, its feature is to add an amount of waste coal ash and ignition dope, make this brick in sintering process without fuel, thereby reduced cost, its solubility promoter mainly is that potassium felspar sand is made raw material, but use potassium felspar sand to make raw material and can not select optimum formula for use according to various places adobe material difference because raw material is single, and because potassium felspar sand at China's skewness, will cause raw material in short supply in some place.
Summary of the invention:
The purpose of this invention is to provide a kind of energy-saving clinker brick, make it utilize the waste coal ash more and vitrified brick obtains energy-conservation effect.
Technical scheme of the present invention is: with clay or shale ore, waste coal ash is raw material, is 100% to calculate by each component concentration summation, and the per-cent of each component concentration is:
Clay or shale ore 60-70%
Waste coal ash 30-40%
Additive 0.1-0.2%
The present invention compared with prior art advantage is: but save energy 40%, and ultimate compression strength, folding strength all improve 20-30 label; The useless scoriaceous ability of enhancement process industry; Raw material sources are extensive, and scientific formulation is widely applicable.
Embodiment 1
Each component concentration per-cent is:
Clay or shale ore 60%
Waste coal ash 40%
Additive is NaCL 0.05%, BaSO
40.05%
Embodiment 2
Clay or shale ore 70%
Waste coal ash 30%
Additive is NaCL 0.04%, BaSO
40.06%.
Claims (1)
1, a kind of energy-saving clinker brick is characterized in that: with clay or shale ore, waste coal ash is raw material, is 100% to calculate by each component concentration summation, and the per-cent of each component concentration is:
Clay or shale ore 60-70%
Waste coal ash 30-40%
Additive 0.1-0.2%.