CN1407074A - 抗粘扣石油油套管螺纹密封脂 - Google Patents
抗粘扣石油油套管螺纹密封脂 Download PDFInfo
- Publication number
- CN1407074A CN1407074A CN 01108735 CN01108735A CN1407074A CN 1407074 A CN1407074 A CN 1407074A CN 01108735 CN01108735 CN 01108735 CN 01108735 A CN01108735 A CN 01108735A CN 1407074 A CN1407074 A CN 1407074A
- Authority
- CN
- China
- Prior art keywords
- powder
- oil
- seizure
- sealing grease
- accounts
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
石油油套管是石油开采的主要消耗管材,由于螺纹粘扣每年造成损失很大,本发明提供一种抗粘扣石油油套管螺纹密封脂,它由占密封脂组合物重量35-39%的00#复合锂基脂和61-65%的固体粉料组成,其中00#复合锂基脂由占自身重量7.55%的12-羟基硬脂酸,1.55%癸二酸,0.91%硼酸,2.55%氢氧化锂,添加78.44%的基础油N-100(或减3B)、经皂化并辅加9%的添加剂经调合均质工艺而制得,固体粉料由占组合物重量18-21%的α-Al2O3,20-25%的鳞片石墨粉,5-10%的湿法云母粉,5-10%的聚四氟乙烯超细粉,3-5%氟化稀土粉,5-8%鳞片状金光铜粉组成。具有润滑性好、防锈防腐蚀性高、抗粘扣等优点,适于石油天然气井钻探使用。
Description
技术领域:
本发明涉及一种石油油套管螺纹密封脂。
背景技术:
石油套管油管是石油开采的主要消耗管材,全世界的石油钻采行业,每年消耗石油套管油管达数百万吨之多,仅我国每年也要消耗百万吨。石油套管油管每根间的连接都是靠管端螺纹,连接时端部螺纹都要涂上石油油套管螺纹密封脂,以确保油套管连接的密封性和连接强度。我国厂家生产的油套管,在端部螺纹连接时经常出现粘扣而无法使用,每年由于这种螺纹粘扣所造成的直接经济损失都在仟万元以上,已成为生产厂家的技术难题。造成油套管螺纹粘扣的原因是多方面的,而研制出抗粘扣石油油套管螺纹密封脂,是解决这一技术难题的重要途径。
发明内容:
本发明目的在于:解决石油油套管螺纹连接的粘扣问题,为用户提供一种能有效防止石油油套管螺纹粘扣的抗粘扣螺纹密封脂。抗粘扣石油油套管螺纹密封脂组合物,特征是由占密封脂组合物重量35-39%的00#复合锂基脂和61-65%的固体粉料组成,其中00#复合锂基脂则由占自身重量7.55%的12-羟基硬脂酸,1.55%的癸二酸,0.91%的硼酸,2.55%的氢氧化锂,添加78.44%的基础油N-100(或减3B),经皂化并辅加9%的添加剂经调合、均质工艺而得;固体粉料则由占组合物重量18-21%的α-Al2O3,20-25%的鳞片石墨粉,5-10%的湿法云母粉,5-10%的聚四氟乙烯超细粉,3-5%的氟化稀土粉,5-8%的鳞片状金光铜粉组成。附加技术特是:(1)添加剂可用0.65%二丁基二硫化氨基甲酸锑,2.15%油溶性石油磺酸钡,6%二壬基萘磺酸钡,0.2%苯并三氮唑等。(2)鳞片石墨粉、湿法云母粉、氟化稀土粉为325目以上的细粉,聚四氟乙烯粉为1000目以上的超细粉。
本发明的制备工艺由制备00#复合锂基脂载体,及将制备成的该基脂与上述固体粉料按所述比例混合、搅拌均匀,然后在胶体磨中将其磨匀而成。
本发明的优点是:(1)防粘扣性能高,其烧结负荷PD值在800kg以上;其上卸扣性能达到APIRP5C5要求。(2)防锈防腐蚀性能高(3)具有高密封性,达到APIRP5C5要求(4)摩擦系数稳定(5)在-6.9℃-150℃温度区间具有良好的润滑性
具体实施方式:
抗粘扣石油油套管螺纹密封脂,由占重量43%的00#复合锂基脂和57%的固体粉料组合而成;其中:00#复合锂基脂由占自身重量7.55%的12-羟基硬脂酸,1.55%的癸二酸,0.91%的硼酸,2.55%的氢氧化锂,添加78.44%的基础油N-100(或减3B),经皂化并辅加9%的添加剂调合均质而成,其中:添加剂有:0.65%的二丁基二硫化氨基甲酸锑,2.15%的油溶性石油磺酸钡,6%的二壬基萘磺酸钡,0.20%的苯并三氮唑;固体粉料由占组合物重量18%的α-Al2O3,23%的325目以上鳞片石墨粉,5%1000目以上聚四氟乙烯超细粉,3%的325目以上氟化稀土粉,3%的325目以上鳞片金光铜粉,5%的铅粉组成;制备方法是:先将所用比例12-羟基硬脂酸,癸二酸,硼酸、氢氧化锂及三分之二用量的基础油N-100(或减3B)混合进行皂化,再添加所述组份及比例的添加剂和余下的三分之一用量的基础油进行调合,之后经剪切器均质出料而成00#复合锂基脂,然后再将该基脂与所述组份及比例的固体粉料,在锥形搅拌釜中搅拌混合,最后在胶体磨中磨匀出料包装成产品。经测量:其主要技术指标如下:相对摩擦系数为1.0(用GB3142-82标准方法测得)工作锥入度(25℃,150g):0.1mm,350-380滴点℃ 不低于138腐蚀(45#钢片,100℃,24小时) 合格钢网分油(100℃,24小时)%(V/V) 不大于10水沥滤(65℃,2小时)% 不大于5.0逸气量(65℃,120小时)mL 不大于20PD值 ≥800kg
Claims (3)
1、一种抗粘扣石油油套管螺纹密封脂组合物,其特征在于:由占该密封脂组合物重量35-39%的00#复合锂基脂和61-65%的固体粉料组成,其中00#复合锂基脂则由占自身重量7.55%的12-羟基硬脂酸,1.55%的癸二酸,0.91%的硼酸,2.55%的氢氧化锂,添加78.44%的基础油N-100(或减3B),经皂化并辅加9%的添加剂经调合、均质工艺而制得,其固体粉料由占该密封脂重量18-21%的a-Al2O3,20-25%的鳞片石墨粉,5-10%的湿法云母粉,5-10%的聚四氟乙烯超细粉,3-5%的氟化稀土粉,5-8%的鳞片状金光铜粉组成。
2、按照权利要求1所述的抗粘扣石油油套管螺纹密封脂组合物,其特征在于:在制备00#复合锂基脂中,皂化并辅加9%的添加剂可以由0.65%二丁基二硫代氨基甲酸锑,2.15%的油溶性后油磺酸钡,2%的苯并三氮唑,6%二壬基萘磺酸钡组成。
3、按照权利要求1所述的抗粘扣石油油套管螺纹密封脂组合物,其特征在于:在密封脂组合物中固体粉料中:鳞片石墨粉、湿法云母粉、氟化稀土粉为325目以上的细粉,聚四氟乙烯粉为1000目以上超细粉。