CN1405026A - Imitation of ancient stone - Google Patents
Imitation of ancient stone Download PDFInfo
- Publication number
- CN1405026A CN1405026A CN 01127724 CN01127724A CN1405026A CN 1405026 A CN1405026 A CN 1405026A CN 01127724 CN01127724 CN 01127724 CN 01127724 A CN01127724 A CN 01127724A CN 1405026 A CN1405026 A CN 1405026A
- Authority
- CN
- China
- Prior art keywords
- stone
- sand blasting
- knock
- flushing
- brush
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The present invention relates to an imitation old stone. It is made up by using stone material and adopting the processes of burning, knocking, sand blasting and corrosion.
Description
The present invention relates to stone material, building stones are made into antique stone, with burn, knock, sandblast, corrosion be made.
Present most of building stones, stone material all cut into sheet material with square stock, through becoming a useful person behind the bubble light.
Because manufacturing process is simple, brightness is big, radiation is big, smooth surface, does not have shortcomings such as anti-skidding, sound-absorbing, radiation are little, not environmental protection, and the market demand is saturated substantially.
Task of the present invention provides a kind of and saves time, efficiently, little, anti-skidding, the sound-absorbing of radiation, antique stone that the environmental protection cost is low.Because this is made through high temperature and burns, can destroy the molecular structure of radiation element, reduce radiation, explosion takes place, produce concave-convex sense.Because this is made through excessive erosion, makes sour impermeable surface, produce chemical reaction, the corrosion stone surface.Because it is concavo-convex that this makes the grain of rice shape that adopts sandblast technology, sand to wash stone surface under the effect of external force, washes away smoothly.
With grouan material through cutting, burn, knock, the burn into sandblast is made.
Different preparation methods is applicable to that hardness is different, and the stone material that material is different, the making of stone are also answered the demand in market and changed.
Be described in further detail below in conjunction with the drawings and specific embodiments:
Fig. 1 is first kind of preparation method of the present invention
Fig. 2 is second kind of preparation method of the present invention
Fig. 3 is the third preparation method of the present invention
Figure one described antique stone comprises three processes:
First process is that (1) is cut into dish formula Jie machine.(2) second processes are that (2) are produced the high temperature focus with the even torch firing of 2500 ℃ high temperature acetylene-oxygen, and one has slight rich blow-out to become (3) until the sheet material vindication.The 3rd process is with (3) blasting treatment, until the slightly smooth one-tenth in surface (4) with sand-blasting machine.
Antique stone shown in the figure two is made and is made to divide three processes:
First process is cutting, is that (1) is cut into thin (2) with Jie's machine.Second process is to use the wedge angle iron hammer gently with stone surface knock uneven (3) with (2).The 3rd process with sand-blasting machine with (3).Blasting treatment is carried out on the surface, until surface slightly smooth (4).
Antique stone shown in the figure three is made and is made to divide three processes:
First process is that (1) is cut into (2) with Jie's machine.Second process is (2) to be carried out blasting treatment with sand-blasting machine become (3).The 3rd process is (3) to be positioned over copper acid carry out immersion corrosion, and there is rib shape face (4) on the surface about about ten minutes.
Antique stone is compared superior part with general stone:
1, antique stone is processed through the torch firing of 2,500 degree high temperature, destroys the molecular structure of radioactive element in the rock, Radiation is dropped to minimum.
2, antique stone is through the copper acid attack, reaches the centuries wind and rain baptism of exposing to the weather, the effect of rain drop erosion.
3, antique stone makes, sound-absorbing anti-skidding, moistureproof with coarse energy in the surface smoothing through the impact of sandblasting.
Actual practical:
Anything is returned to back-to-the ancients ideology again through initial stage, mid-term, peak period, and especially American-European experts pursue anti-Piao especially and return very, reply the rooting psychology of the Nature, the process flow of antique stone, and manufacture craft all satisfies above-mentioned people's psychology.
" antique stone " applied widely is widely used, and can be used for repairs profession, decoration technology, and collection is viewed and admired, and has good hand touch, and moistureproof anti-skidding, reflectance is little, and radiation is few, environmental protection, characteristics such as practical.
Claims (2)
1, stone material, building stones through baked wheaten cake, knock, sandblast, corrosion are made antique stone.
The one, granite plates is spent high temperature torch firing sheet materials until there being small explosive sound to end with 2,500.Just finish with the flushing of wind folder sand blasting brush then.
The 2nd, knock slabstone, stone surface with the wedge angle hammer, make the surface tiny uneven hollow occur, just finish with the flushing of wind folder sand blasting sand blasting brush then.
The 3rd, marble surface with the flushing of wind folder sand blasting brush, is just finished with copper acid attack surface then.
One, two, three, plant preparation method, be applicable to that hardness is different, the stone material that material is different, the making of stone.
2,, it is characterized in that burning, knock, sandblast, corrosion are made antique stone according to the requirement of right 1.