CN1346752A - 金属蚀刻装饰条及其制造方法 - Google Patents

金属蚀刻装饰条及其制造方法 Download PDF

Info

Publication number
CN1346752A
CN1346752A CN 01125660 CN01125660A CN1346752A CN 1346752 A CN1346752 A CN 1346752A CN 01125660 CN01125660 CN 01125660 CN 01125660 A CN01125660 A CN 01125660A CN 1346752 A CN1346752 A CN 1346752A
Authority
CN
China
Prior art keywords
metal
laths
metal bar
manufacture method
imaging
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 01125660
Other languages
English (en)
Inventor
徐勇
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 01125660 priority Critical patent/CN1346752A/zh
Publication of CN1346752A publication Critical patent/CN1346752A/zh
Pending legal-status Critical Current

Abstract

一种涉及装饰材料的金属蚀刻装饰条及其制造方法,其制造过程是,首先设计装饰图案并制成版,再在金属板条的表面上感光成像,经化学腐蚀一定深度后,不再腐蚀,清洗、烘干、上色、打磨,再经模具冲压成高低不同的弯曲度或弧度,最后涂防腐层,制得金属蚀刻装饰条。它可以代替木制装饰条或石膏装饰条,可制作相框、门、窗的边框,衣柜边框及用于室内装饰。具有不变形,不变色,图案有凹凸的立体感之优点。

Description

金属蚀刻装饰条及其制造方法
                      技术领域
本发明涉及装饰材料,其金属装饰条应用于相框、衣柜、门、窗及室内装饰等。
                      背景技术
目前国内所使用的装饰条为木制装饰条,因木材紧缺,使用较少,并受气候干湿的影响,易干裂或湿涨变形,另一种为石膏装饰条,由于受潮湿气候影响,表面易出现霉点,影响美观,此外,也有少量金属装饰条,但无凹凸图案,不美观。为此,本发明提供一种具有凹凸立体感的装饰图案或美术画,并呈高低不同弯曲度或弧度的金属装饰条。
                      发明内容
本发明的装饰条之金属板条(1)表面具有化学腐蚀后成为凹凸立体感的装饰图案或一幅乃至几幅美术画,并经模具冲压成高低不同弯曲度或弧度。该金属装饰板条可以由一块整板条制成,也可以由两块或多块金属板条(2)、(3)经蚀刻装饰图案或美术画后,再经冲压成为不同弯曲度或弧度,然后组合成连续或断续的呈现不同弯曲度或弧度的金属装饰条。
本发明的金属蚀刻装饰条的制造过程是,首先根据不同用户的要求及使用场合设计装饰图案或一幅和多幅美术画,然后进行制版,再在金属板条的表面上进行感光成像,烘干后进行化学腐蚀,待腐蚀到一定深度后,不再腐蚀,清洗掉腐蚀液,烘干,然后根据要求或使用场合的环境,选择不同的颜色进行上色,上色后对金属板条表面进行打磨,这样,未被腐蚀的表面经打磨后露出金属的本色,腐蚀后凹下去的部分留下了颜色,从而衬托出未被腐蚀部分的金属图案或画面,以增加美感,下一步由模具进行冲压成高低不同的弯曲度或弧度,进一步增强图案或画面的立体感,最后涂防腐层,完成金属蚀刻装饰条的制造。
在进行化学腐蚀过程中,可以腐蚀到一定深度后不再腐蚀,也可以腐蚀到金属板条穿透为止。
上述在金属板条表面上感光成像,可以采用丝网印刷成像,或用电脑雕刻机刻不干胶纸漏版成像,也可以采用在金属板条表面涂蜡后,对蜡进行雕刻成像,或采用在金属板条表面贴不干胶纸后,雕刻不干胶纸成像。
随着科技的进步,现已有电脑控制雕刻机出现,因此,有关制版、感光成像、化学腐蚀等工序可以简化,只需将设计好的装饰图案或美术画,输入电脑控制雕刻机后,由电脑控制自动完成机械雕刻,但成批生产效率较低。
金属板条表面被腐蚀后凹下去的部分上色,也可以在模具冲压后,涂防腐层前上色,或涂防腐层后进行上色。也可以不上色,仅为金属的本色。
采用本发明的金属蚀刻装饰条,可以制成相框、衣柜边框、门、窗边框以及用于室内装饰等,总之,可以代替木制装饰条和石膏装饰条,使用本产品后,不受气候干湿等的变化影响而引起变形及变色的问题,具有稳定和图案有立体感的优点。
                     附图说明
图1为金属蚀刻装饰条的主视图。
图2为图1的俯视图。
图3为金属蚀刻装饰条两条断续组合的主视图。
图4为图3的俯视图。
                     具体实施方式
本发明将结合附图作进一步描述,首先选择0.5mm厚的铜板,下料,使其成为一定宽度的板条,按设计好的装饰图案,制成版,在铜板条表面上成像,再进行化学腐蚀,图1中黑色部分为被腐蚀部分,待腐蚀到一定深度后,不再腐蚀,清洗掉腐蚀液,烘干,涂上选好的颜色,然后打磨,使未腐蚀表面露出铜的本色,再在事先制作的具有不同高低弯曲度或弧度的模具内冲压、成型。最后涂上防腐层,即完成金属蚀刻装饰条的制造,贴防护纸,入库待用。

Claims (7)

1.一种涉及装饰材料的金属蚀刻装饰条及其制造方法,其特征在于装饰条之金属板条(1)表面有凹凸的装饰图案或美术画,并呈高低不同的弯曲度或弧度。
2.根据权利要求1所述的金属蚀刻装饰条及其制造方法,其特征在于所说的装饰条之金属板条可以是一整条,也可以是两块或多块金属板条(2)、(3)组合成连续或断续的高低不同的弯曲度或弧度。
3.根据权利要求1所述的金属蚀刻装饰条及其制造方法,其制造方法的特征在于,首先设计装饰图案或美术画,然后制版,再在金属板条表面上感光成像,烘干后进行化学腐蚀,待腐蚀到一定深度后,清洗、烘干、上色、打磨未腐蚀的表面,再经模具冲压成高低不同的弯曲度或弧度,最后涂防腐层。
4.根据权利要求3所述的金属蚀刻装饰条及其制造方法,其特征在于所说的腐蚀一定深度,也可以将金属板条腐蚀穿透。
5.根据权利要求3所述的金属蚀刻装饰条及其制造方法,其特征在于所说的感光成像,可以采用丝网印刷成像,或采用电脑雕刻机刻不干胶纸漏版成像,也可以采用金属板条表面涂蜡后,蜡刻成像,或采用金属板条表面贴不干胶纸后,雕刻不干胶纸成像。
6.根据权利要求3所述的金属蚀刻装饰条及其制造方法,其特征在于所说的制版,感光成像,化学腐蚀,也可以将设计的装饰图案或美术画输入电脑雕刻机,由电脑控制机械刻制而成。
7.根据权利要求3所述的金属蚀刻装饰条及其制造方法,其特征在于所说的上色,也可以在模具冲压后,涂防腐层前上色,或在涂防腐层后上色。也可以不上色,仅为金属本色。
CN 01125660 2001-08-27 2001-08-27 金属蚀刻装饰条及其制造方法 Pending CN1346752A (zh)