- Publication number
- CN1309794C CN1309794C CNB2005100207313A CN200510020731A CN1309794C CN 1309794 C CN1309794 C CN 1309794C CN B2005100207313 A CNB2005100207313 A CN B2005100207313A CN 200510020731 A CN200510020731 A CN 200510020731A CN 1309794 C CN1309794 C CN 1309794C
- Authority
- CN
- China
- Prior art keywords
- oil
- weight
- parts
- component
- ethanol
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
The present invention relates to a protective agent for shinning leather and stone, which is prepared from the raw materials of 2 to 12 parts by weight of beeswax, 2 to 31.5 parts by weight of mineral wax, 0 to 79.5 parts by weight of paraffin wax, 2 to 6 parts by weight of stearic acid, 2 to 12 parts by weight of rosin, 8 to 24 parts by weight of shellac wine liquid with the ratio of 1: 8, 2 to 4 parts by weight of silicon oil, 10.8 to 60 parts by weight of boiled tung oil, 60 to 150 parts by weight of turpentine, 0 to 3.5 parts by weight of pine oil, 87 to 170 parts by weight of white oil, 0 to 132 parts by weight of engine oil of 10<#>, 25 to 262 parts by weight of ethanol, 5.71 to 11.3 parts by weight of polyoxyethylene castor oil, 6 to 15 parts by weight of essence, 0 to 10 parts by weight of oil colour and 1 to 2 parts by weight of dibutyl ester.
Description
Technical field:
The present invention and leather, stone surface auxiliary agent are relevant, and be especially relevant with surperficial optical brightener, protective material.
Background technology:
Existing leather agent such as glossy dose, surface slip agent, hand feeling agent, clean-out system, brightening agent is many is made price height, function singleness by imported raw material such as carnauba wax.Existing stone material brightening protecting agent is also because raw materials cost height and price is more expensive, and home-made uses price to be 5-8 unit/m
2, the price of using of import is 15-30 unit/m
2
Summary of the invention:
The object of the invention provides a kind of raw material and is easy to get, and is with low cost, the leather of diverse in function, stone material brightening protective agent.
The present invention is achieved in that
Leather of the present invention, stone material brightening protective agent, it is to be made by the raw material of following weight parts:
Beeswax 2-12
Ceresine 2-31.5
Paraffin 0-79.5
Stearic acid 2-6
Rosin 2-12
1: 8 shellac alcohol liquid 8-24
Silicone oil 2-4
Boiled wood oil 10.8-60
Turps 60-150
Pine tar 0-3.5
White oil 87-170
10
#Machine oil 0-132
Ethanol 25-262
Polyoxyethylenated castor oil 5.71-11.3
Essence 6-15
Oil-soluble colourant 0-10
Dibutyl phthalate 1-2.
Above-mentioned raw materials is mixed as follows:
(1) beeswax, ceresine, paraffin, stearic acid, rosin Hybrid Heating are dissolved after, add polyoxyethylenated castor oil again and make it emulsification, after the cooling, add turps, pine tar is made the A component;
(2) with white oil, 10
#Machine oil, boiled wood oil, 1: 8 shellac alcohol liquid, mix the B component;
(3) ethanol is added in the silicone oil, add essence again and make the C component;
(4) with A, B, the addition of C component, mix, stir.
The ethanol that adds in the step (3) be most of, the ethanol with remainder adds in the oil-soluble colourant in addition, gets the D component, in step (4) with A, B, C, the addition of D component, mix, stir.
Raw material of the present invention is easy to get, and is with low cost, and diverse in function is embrocated the slight dirt that can remove on it with it on leather, stone material, timber floor, plywood, prevents that goods are aging, increases product gloss, and can appropriate waterproof.Raw materials cost of the present invention<8 yuan/kg.Per kilogram can be embrocated stone surface 15-20m
2, raw materials cost only is 0.4-0.54 unit/m
2If price is by 30 yuan/kg, every square metre of expense of embrocating is a 1.5-2 unit, is lower than the 5-8 unit/m of homemade wax brightening protecting agent
215-30 unit/m with the import like product
2
Embodiment:
Select synthetic ceresine for use, its fusing point is 60-80 ℃, as one of major ingredient of brightening agent, ceresine also can with paraffin compatibility, the coarse-grain situation when changing wax crystal.Select beeswax for use, 62~58 ℃ of fusing points are as the brightening agent raw material.Paraffin can be Chinese wax or yellow wax, and 48~66 ℃ of fusing points are as the brightening agent raw material.Stearic acid, 70~71 ℃ of fusing points, select for use industrial goods one, two, three all can, as the emulsification promotor of brightening agent and paraffin.Rosin is selected industrial I and II product for use, plays saponification emulsification promotion and enhanced shine, and shellac has another name called lac, makes lustering agent.Boiled wood oil squeezes oil by the seeds of a tung oil tree and gets through boiling, and is siccative oil, plays promoter effect.White oil claims Liquid Paraffin again, and through underpressure distillation, the lubricating oil distillate that obtains medium viscosity forms through refining again, selects industrial goods 7-18 white oil for use, plays glossy and glossiness-giving effect by black petroleum products.10
#Machine oil is made rust cleaning decontamination, lustering agent.Turps, select industrial goods for use, make solvent.Pine tar through extraction and fractionation or through a class essential oil of steam distillation gained, is made solvent, sanitas by the stem of pine tree, branch, leaf.Silicone oil claims silicone oil again, selects the industrial goods of mooring in the viscosity 350-800 for use, makes luminous brightening agent, water-resisting agent.Ethanol is made solvent and quick dry agent.Polyoxyethylenated castor oil, nonionogenic tenside is made emulsifying agent oily, Wax.Essence is selected oily cosmetics essence for use.Oil-soluble colourant are prepared coloured product and are used.Dibutyl phthalate is made softening agent.
Embodiment 1:
The present invention is made by following weight part raw material:
Beeswax 2
Ceresine 2
Paraffin 6
Rosin 5
Stearic acid 2
Silicone oil 2
Boiled wood oil 10.8
Turps 115
1: 8 shellac liquid 8
White oil 106.5
The polyoxyethylene castor
Sesame oil 5.71
Dibutyl phthalate 1
Ethanol 25
Essence 6
Wherein 1: 8 shellac liquid is shellac: ethanol=1: 8
Preparation method of the present invention is as follows:
(1) ethanol is added in the silicone oil, mix thoroughly, diluted for use,
(2) rosin, Wax and stearic acid are added in the emulsification pot, be warming up to about 90 ℃, be cooled to after the fusing about 50 ℃, add oily substance, emulsifying agent and 1: 8 shellac liquid, stir, make wax and oily emulsification.
Embodiment 2:
Beeswax 12
Ceresine 24
Rosin 12
Stearic acid 4
Silicone oil 3
Boiled wood oil 60
Turps 150
Pine tar 3.5
White oil 170
10
#Machine oil 132
1: 8 shellac liquid 8
Dibutyl phthalate 2
Ethanol 150
Polyoxyethylenated castor oil 11.3
Essence 11.
This routine preparation method is identical with embodiment 1.
Embodiment 3:
The present invention is made by the raw material of following weight parts:
Beeswax 8
Ceresine 12
Rosin 10
Stearic acid 6
1: 8 shellac liquid 24
Silicone oil 4
Boiled wood oil 12
Turps 60
White oil 87
10
#Machine oil 15
Dibutyl phthalate 2
Ethanol 92
Polyoxyethylenated castor oil 9.3
Essence 11.
Preparation method of the present invention is identical with embodiment 1.
Embodiment 4:
The present invention is made by the raw material of following weight parts:
Beeswax 2
Ceresine 31.5
Paraffin 78.5
Rosin 2
Stearic acid 6
Silicone oil 3
Boiled wood oil 23.5
Turps 119
White oil 119
1: 8 shellac liquid 12
Dibutyl phthalate 1
Ethanol 262
Polyoxyethylenated castor oil 9.7
Essence 15
Oil-soluble colourant 10.
Preparation method of the present invention is identical with embodiment 1.
With the present invention in the urban district, Chengdu and the how tame leatherware beauty point in Shuangliu County on probation, homogeneous response " the glossiness height is embrocated effective ".Oppose than test with commercially available four tame reputable brand shoe polish with the present invention, test-results is as follows: (surveying instrument: SS-82 type photoelectric glossmeter)
Table 1:
The present invention | The commercially available prod | |||||||
Embodiment 1 | Embodiment 2 | Embodiment 3 | Embodiment 4 | Brand 1 | Brand 2 | Brand 3 | Brand 4 | |
Base plate (90) | 92.4 | 96.6 | 98.4 | 92.4 | 81.8 | 79.6 | 75.6 | |
Base plate 112 | 101.3 | 90.5 | 90.2 | 87.3 | 82.6 |
With embodiments of the invention 2, the product of embodiment 3 is to 8 kinds of stone materials, 2 kinds of ceramic tiles, and laminated flooring, plywood is embrocated, and all obtains satisfied effect, sees the following form:
Former degree product number | Embodiment 2 products | Embodiment 3 products | |||
The actual measurement number of degrees | The increase and decrease number of degrees | The actual measurement number of degrees | The increase and decrease number of degrees | ||
Two # red (Xinjiang) stone material | 78° | 74.68° | -3.3° | 83.38° | +5.38° |
Shandong hemp stone material | 63° | 64° | +1° | 75.2° | +12.2° |
Rong Jinghong (Sichuan) stone material | 69° | 74.43° | +5.43° | 79.6° | +10.6° |
White marble (Sichuan) stone material | 60° | 60° | / | 78° | +18° |
Jinan green grass or young crops (Shandong) stone material | 65.5° | 78° | +12.5° | 73° | +7.5° |
ROSA PORRINO (import) stone material | 60° | 83.6° | +23.6° | 83.86° | +23.86° |
Dark Green (import) stone material | 66° | 78° | +12° | 88.9° | +22.9° |
White ceramic tile | 81° | 77.63° | -3.38° | 97.2° | +16.2° |
Purple frost flower ceramic tile | 54° | 64.2° | +10.2° | 75.7° | +21.7° |
Laminated flooring | 7° | 38.6° | +31.6° | 53.2° | +46.2° |
Plywood | 110.6° | 104.6° | -6° | 109.8° | -0.8° |
Surveying instrument: SS-80 type photoelectric glossmeter
Measure the date: on March 18th, 2005
7 stone material kinds are described, after wiping with product of the present invention, except that indivedual kind glossiness slightly descend, glossiness all increases by 1 °-23.6 ° after the obliterating of overwhelming majority kind, average increasing by 7.32 °, promptly is indivedual kinds that glossiness has been fallen, and embrocates still than beautiful attractive in appearance before embrocating.
Claims (2)
1, leather, stone material brightening protective agent, it is to be made by the raw material of following weight parts:
Beeswax 2-12
Ceresine 2-31.5
Paraffin 0-79.5
Stearic acid 2-6
Rosin 2-12
1: 8 shellac alcohol liquid 8-24
Silicone oil 2-4
Boiled wood oil 10.8-60
Turps 60-150
Pine tar 0-3.5
White oil 87-170
10
#Machine oil 0-132
Ethanol 25-262
Polyoxyethylenated castor oil 5.71-11.3
Essence 6-15
Oil-soluble colourant 0-10
Dibutyl phthalate 1-2.
Above-mentioned raw materials is mixed as follows:
(1) beeswax, ceresine, paraffin, stearic acid, rosin Hybrid Heating are dissolved after, add polyoxyethylenated castor oil again and make it emulsification, after the cooling, add turps, pine tar is made the A component;
(2) with white oil, 10
#Machine oil, boiled wood oil, 1: 8 shellac alcohol liquid, mix the B component;
(3) ethanol is added in the silicone oil, add essence again and make the C component;
(4) with A, B, the addition of C component, mix, stir.
2, leather according to claim 1, stone material brightening protective agent; the ethanol that it is characterized in that adding in the step (3) is for most of; in addition the ethanol with remainder adds in the oil-soluble colourant, the D component, in step (4) with A, B, C, the addition of D component, mix, stir.