CN1230586C - 纳米级羽毛绒粉末及其加工方法和应用 - Google Patents

纳米级羽毛绒粉末及其加工方法和应用 Download PDF

Info

Publication number
CN1230586C
CN1230586C CN 03106564 CN03106564A CN1230586C CN 1230586 C CN1230586 C CN 1230586C CN 03106564 CN03106564 CN 03106564 CN 03106564 A CN03106564 A CN 03106564A CN 1230586 C CN1230586 C CN 1230586C
Authority
CN
China
Prior art keywords
feather down
powder
feather
nanoscale
care
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 03106564
Other languages
English (en)
Other versions
CN1439768A (zh
Inventor
张立文
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shunde Foshan star Feather Trading Co., Ltd.
Original Assignee
SHENYU TEXTILE CO Ltd FOSHAN
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SHENYU TEXTILE CO Ltd FOSHAN filed Critical SHENYU TEXTILE CO Ltd FOSHAN
Priority to CN 03106564 priority Critical patent/CN1230586C/zh
Publication of CN1439768A publication Critical patent/CN1439768A/zh
Application granted granted Critical
Publication of CN1230586C publication Critical patent/CN1230586C/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本发明属一种纳米级羽毛绒粉末及其加工方法和应用,其特点是采用水洗鸭、鹅、鸟禽类羽毛绒,经过筛选、剪切粉碎、酒精混合、浸泡、甩干、微波振荡、速冷、低温粉碎、过筛加工而成,其颗粒至少有一维处于1-200nm之间。该工艺在80℃以下进行加工,原子结构和分子量不变,保持了天然羽毛绒的化学成分和物理特性,该粉末细腻,比表面积增大,分子活性大,与人体亲和性更强,更易于皮肤吸收,防病治病保健效果更好。该粉沫与水、酒精或油可制成膏或糊状保健组合物,可加入常规护肤护发保健品、沐浴露、化工日用品及外用药中;还可加入溶液性化学纤维原料粉中制成溶液纺丝液、经喷丝加工可制成羽毛绒复合纤维,还可作为功能性保健食品和饲料添加剂。

Description

纳米级羽毛绒粉末及其加工方法和应用
所属领域
本发明涉及羽毛绒粉及其加工方法,是一种利用羽毛绒加工成纳米级羽毛绒粉末及其加工方法和应用。
背景技术
羽毛绒是禽类皮肤的衍生物,属于天然蛋白质材料,含有十七种氨基酸和脂肪、钙、磷、硅酸、硫、氯等多种元素,对人体有极好的亲和性,并对多种疾病有很好的医疗保健功效。如,《别录》中记载:“鹅毛性凉、解毒、消肿、吸湿敛疮,主治臃肿疮毒、风癣疥癞、湿疹湿疮、噎膈、惊痫;”《华佗神医秘传》中记载:“农家浇类十此,为烈日蒸晒,人跣足其上,受其热毒、足趾肿痛似遗非遗、以鸭羽煎汤和皂巩洗之”、还有《本草纲目》等很多历史资料中都记载有鸭、鹅羽毛绒对人体的医疗保健作用。但是近百年来,天然鸭、鹅羽毛绒在医疗保健方面应用早已被人们淡忘,目前对这一天然资源利用主要是作为填充物制作羽绒服和寝具,并形成了羽绒轻工业,而大部分粗羽毛的羽毛绒在加工过程中产生的大量飞丝粉无法利用被废弃,造成羽毛绒资源使用单一,没有物尽其用。
发明内容
本发明的目的是提供一种纳米级羽毛绒粉末及其加工方法和应用,以解决现有鸭、鹅羽毛绒资源使用单一,没有物尽其用的问题。
本发明的目的是这样实现的:将现有鸭、鹅羽毛绒加工成纳米级超细羽毛绒粉末,其粒度至少有一维处于1-200nm之间。
纳米级羽毛绒粉末加工方法主要包括以下工艺步骤:羽毛绒筛选、剪切粉碎、酒精混合、浸泡、甩干、微波振荡、速冷、低温粉碎、过筛工序。微波振荡采用微波机,振荡频率在800MHZ-300GHZ之间,温度为40-60℃,在10℃以下速冷,低温粉碎采用-30--40℃环境下机械粉碎,过1200-1300目筛。
酒精混合:酒精浓度为80%以上,按重量比羽毛绒粗粉∶酒精=1∶5-15。
本发明与现有技术相比具有以下优点:(1)该羽毛绒粉末在80℃以下加工而成,羽毛绒不会被水解,其原子结构和分子量不变,保持了其天然的化学成分和物理特性;(2)该粉末粒度细小在1-200nm之间,其体表面积大,晶界处的原子数比率高,表面分子活性大,与人体亲和性更强,更易皮肤吸收,防病治病保健效果更好;(3)用途广:鸭、鹅羽毛绒羽枝、羽杆可分别粉碎,可分别或混合应用,如用鸭或鹅羽毛绒纳米级粉末与水、酒精、奶或油制成膏或糊状护肤、护发保健品、沐浴露、化工日用品及外用药品,还可将羽毛绒粉末加入溶液性化学纤维原料粉中,利用现有工艺制成纺丝液、喷丝加工,可制成羽毛绒复合纤维,也可作为功能性保健食品和饲料添加剂。
具体实施方式
实施例一:纳米级羽毛绒粉末的加工工艺
工艺流程:羽毛绒筛选-剪切粉碎-酒精混合-浸泡-甩干-微波振荡-速冷-低温粉碎-过筛。
工序说明
1、羽毛绒过筛:采用水洗鸭、鹅、鸟禽类羽毛绒或羽毛绒在加工过程中产生的飞丝粉为原料。
2、剪切粉碎:采用现有剪切粉碎技术将羽毛绒粉碎成1mm以下的粗粉,根据用途需要也可采用气流分选技术将羽毛绒的羽枝、羽杆或羽根分离开分别进行以下工艺加工。
3、酒精混合:在常温下,按重量比羽毛绒粗粉∶酒精=1∶5-15混合搅拌,使其均匀分散止。
4、浸泡:浸泡时间为20-40分钟,使羽毛绒粗粉进一步脱脂、灭菌。
5、甩干:将浸泡液放入离心甩干机内甩干,得到含酒精溶液50-70%的纯净羽毛绒粗粉。
6、微波振荡:将甩干的羽毛绒粗粉放入微波机内进行微波振荡,振荡频率为800MHZ-300GHZ,温度控制在60-80℃,通过振荡,使组合物的分子间高速磨擦,使羽毛绒粗粉内部结构松动、断裂、内部水分被置换蒸发,化学键长度和方向发生变化,待羽毛绒粗粉含水量降到2-5%时止。
7、速冷:将振荡好的羽毛绒粗粉置于10℃以下低温环境下速冷。
8、低温粉碎:采用现有技术,在-30--40℃条件下机械粉碎。
9、过筛:将低温粉碎的羽毛绒粉过1200-1300目筛,筛下即为1-200nm的羽毛绒粉末,筛上的再重新粉碎。
该羽毛绒粉末性能:(1)保持了原羽毛绒的原子结构和分子量,原天然羽毛绒的化学成分和物理特性不变;(2)粉末粒度小在1-200nm之间,比表面积增大,提高了分子活性和与人体的亲和性,更易于皮肤吸收,易于与液态或固体粉料混合均匀。
实施例二:例一所述的鸭、鹅羽毛绒羽枝、羽杆或羽根粉末分别或混合与油、酒精、水、姜汁或奶,制成组合物。油是指鸭、鹅、蛇、芝麻或蓖麻天然动植物油;姜汁是用鲜姜轧成的汁;组合物指具有灭菌、消毒、促进皮肤细胞活性和新陈代谢功能的护肤、护发、保健品。按重量比羽毛绒粉末占组合物的1-80%。
实施例三:例一所述的鸭或鹅羽毛绒粉末加入常规护肤、护发品、沐浴露、口红、粉底箱、化妆品及皂类内,加入量为总重量的1-60%;即可增强分子活性和对人体的亲和性,更易于皮肤吸收,从而可增强护肤、护发、灭菌的保健效果。
实施例四:例一所述的鸭或鹅羽毛绒羽枝、羽杆或羽根粉末分别或混合加入外用药品中,可提高和增加外用药的疗效。外用药是指:药水、药膏、药液或膏药。
实施例五:例一所述的羽毛绒粉末按总重量的5-60%加入溶液性化学纤维的固体原料粉内,再利用现有工艺制万溶液纺丝液,羽毛绒粉末可均匀分散混合在纺丝液内,经喷丝工艺加工可制成羽毛绒复合纤维。化学纤维是指腈纶、维纶、氯纶、粘胶纤维。
实施例六:例一所述的羽毛绒粉末可作为功能性保健食品和饲料添加剂。

Claims (8)

1、一种纳米级羽毛绒粉末,其特征在于:羽毛绒粉末颗粒至少有一维处于1-200nm之间。
2、根据权利要求1所述的纳米级羽毛绒粉末,其特征在于:羽毛绒采用水洗鸭、鹅、鸟禽类羽毛绒或羽毛绒在加工过程中产生的飞丝粉为原料。
3、如权利要求1所述的纳米级羽毛绒粉末的加工方法,其特征在于包括以下工艺步骤:羽毛绒筛选、剪切粉碎、酒精混合、浸泡、甩干、微波振荡、速冷、低温粉碎、过筛工序;微波振荡采用微波机,振荡频率为800MHZ-300GHZ,温度控制在60-80℃,在10℃以下速冷,-30--40℃环境下机械粉碎,过1200-1300目筛。
4、根据权利要求3所述的纳米级羽毛绒粉末的加工方法,其特征在于:酒精混合,酒精浓度80%以上,按重量比,羽毛绒粗粉末∶酒精=1∶5-15。
5、如权利要求1所述的纳米级羽毛绒粉末的应用,其特征在于:该羽毛绒羽枝、羽杆或羽根粉沫分别或混合与油、酒精、水姜汁或奶制成组合物,油指鸭、鹅、蛇、芝和蓖麻天然动植物油;按重量比羽毛绒粉末占组合物的1-80%。
6、根据权利要求1所述的纳米级羽毛绒粉末的应用,其特征在于:羽毛绒粉末加入常规护肤、护发品沐浴露、口红、粉底霜、化妆品及皂类内,加入量为总重量的1-60%。
7、根据权利要求1所述的纳米级羽毛绒粉沫的应用,其特征在于:羽毛绒羽枝、羽杆或羽根的粉末可分别或混合加入外用药品中,外用药是指药水、药液、药膏或膏药。
8、如权利要求1所述的纳米级羽毛绒粉末的应用,其特征在于:羽毛绒粉末可按总重量的5-60%加入溶液性化学纤维的原料粉内,再利用现有工艺制成溶液纺丝液、经喷丝工艺加工,可制成羽毛绒复合纤维;化学纤维是指:腈纶、维纶、氯纶、粘胶纤维。
CN 03106564 2003-03-03 2003-03-03 纳米级羽毛绒粉末及其加工方法和应用 Expired - Fee Related CN1230586C (zh)