CN1202335C - Manufacturing method of luminous staircase - Google Patents

Manufacturing method of luminous staircase Download PDF

Info

Publication number
CN1202335C
CN1202335C CN 03128237 CN03128237A CN1202335C CN 1202335 C CN1202335 C CN 1202335C CN 03128237 CN03128237 CN 03128237 CN 03128237 A CN03128237 A CN 03128237A CN 1202335 C CN1202335 C CN 1202335C
Authority
CN
China
Prior art keywords
self
staircase
luminous
stair
luminescent material
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 03128237
Other languages
Chinese (zh)
Other versions
CN1478974A (en
Inventor
蒙瑞基
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 03128237 priority Critical patent/CN1202335C/en
Publication of CN1478974A publication Critical patent/CN1478974A/en
Application granted granted Critical
Publication of CN1202335C publication Critical patent/CN1202335C/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

The present invention relates to a manufacturing method of a luminous staircase and is characterized in that self-luminescent material is mixed with other supplementary material to be painted on the surface of the staircase or carry out moulding forming; luminous paint can be painted on an existing staircase; a self-luminescent plastic staircase, a ceramics staircase, an artificial jade staircase, parts of the self-luminescent plastic staircase, the ceramics staircase, the artificial jade and the artificial jade staircase, etc. can be made via the luminous paint. People can go upstairs and downstairs safely under the condition of no light and electricity via the luminous staircase which has an obviously decorative effect.

Description

The preparation method of noctilucence stair
Technical field
The present invention relates to a kind of preparation method of noctilucence stair.
Background technology
Self-luminescent material is a kind of novel energy-saving luminous material, this material behind natural light (comprising visible lights such as daylight and light) irradiation certain hour, but place the dark place or in all self-luminous at night.Because need not the energy, reliable operation, environmental, made things convenient for people's live and work, thereby obtain application more and more widely.The field of using most manyly surely belongs to self-luminescent material and makes various nameplates, as security warning, road sign, direction indication, square mark etc.State according to relevant report: in the September 11 attacks of the U.S., two high buildings are after being hit power failure, the various Warning Marks that dependence is made by self-luminescent material are in the high building that the people flees from high building within a short period of time smoothly surplus 10,000 in the dark, have avoided more casualties; At this, self-luminescent material is performed meritorious deeds never to be obliterated.
China is that minority can be produced one of country of self-luminescent material in the world.Use " non radioactive environmental protection energy-saving luminous material " of rare earth material production by Qingda Huayan Sci. ﹠ Tech. Dev. Co., Ltd., Beijing, detect through relevant department, confirm as nontoxic, harmless, "dead" material, do not burn, do not explode toxic heavy metal element or chemicals such as not phosphorous, lead." the bright Self-luminous Fire Safety Sign in road " series of products that MingFa optical Science Co., Ltd., DaLian Road produces have also become known brand at home and abroad.Their production is used and all is perfectly safe three-waste free pollution, security compliance environmental requirement; Do not need power supply or other energy when using these self-luminescent materials, radiation of visible light can be in the dark luminous 12 hours after 10 minutes, makes full use of lamp; But the light-accumulated luminous process Infinite Cyclic of its extinction, can reach more than 30 years luminous application life, is a generation " green light source ".
Because the excellent specific property of self-luminescent material has obtained people and has generally approved, and because production technology constantly improves and the manufacturing cost of raising, self-luminescent material is more and more lower, add and use self-luminescent material to also have tangible decorative effect, make its scope of application more and more wideer, application is also more and more.
Summary of the invention
The technical problem to be solved in the present invention is that self-luminescent material is used on the stair that making can be luminous, makes the people in the dark also can safe ready ground stair activity.
The preparation method of noctilucence stair of the present invention solves the problems of the technologies described above with following technical scheme: be coated in stair surface or mould injection forming after adopting self-luminescent material and other auxiliary material to be mixed.
1, use luminous paint spraying stair:
The prescription of preparation self-luminous paint is: (weight %, as follows)
Acrylic resin 73~83
Self-luminescent material 15~25
Mill base 2~2.5
Preparation method:
The above-mentioned raw materials mixing is made self-luminous paint back stair are carried out the surface spraying.
2, the making of self luminous plastic stair:
Prescription:
PVC 73~83
Alkane naphthenic acid cobalt 1.5~2.5
Self-luminescent material 15~25
Preparation method:
To add alkane naphthenic acid cobalt, self-luminescent material after the PVC fusion, fully stir evenly the back casting.
3, the making of self-luminescent ceramic stair:
Prescription:
Ceramic glaze 75~85
Self-luminescent material 15~25
Preparation method:
With self-luminescent material and the abundant mixing of ceramic glaze, the gained glaze is coated in reburn on the potter's clay base again and makes ceramic product.
4, self-luminous artificial jade stair:
Prescription:
Aluminium hydroxide 50~67
Unsaturated polyester resin 25~35
Self-luminescent material 7~13
Different cobalt green 1~3
Preparation method:
With casting behind the abundant stirring and evenly mixing of above-mentioned raw materials.
Make the positions such as handrail, railing, ladder of self-luminous stair of method of the present invention, people can be under the unglazed situation of not having an electricity safe stair activity, improve the safety guarantee coefficient, can increase brightness, the color and attractive in appearance on stair surface night.Method of the present invention can be used to make brand-new noctilucence stair, also can be used for transforming the stair made from conventional method, comprises that luminous effect is very remarkable with the stair of material such as wood, iron and steel, natural stone, man-made stone, plastics, pottery.
The specific embodiment
The present invention makes the method for noctilucence stair, can use multiple self-luminescent material, (address: No. 10, Huoju Road, Qixianling, High-Tech. Park, Dalian City) the self-luminescent material resultant effect of (hereinafter to be referred as " the Dalian road is bright ") production is best but grind " non radioactive environmental protection energy-saving luminous material " and the MingFa optical Science Co., Ltd., DaLian Road that development in science and technology Co., Ltd (address: Tsing-Hua University is with No. 409, square mansion Building A) (hereinafter to be referred as " Beijing Hua Yan ") produces with the clear big China in Beijing.
Embodiment 1:
2 kilograms of 80 kilograms of acrylic resins, mill base are inserted add 18 kilograms of the self-luminescent materials that production is ground by Beijing China after stirring a little in the agitator again, fully leave standstill behind the stirring and evenly mixing and can use in 30 minutes.This painting is brushed or is sprayed on the wooden stair that made, and stair have promptly been realized the self-luminous at night.
Embodiment 2:
PVC adds 2.5 kilograms of alkane naphthenic acid cobalts for 78 kilograms after 130 ℃ of following fusions, 19.5 kilograms of the self-luminescent materials that adding Dalian road open-birth is produced after fully mixing, fully being about to compound behind the stirring and evenly mixing pours in the stair railing mould of having smeared release agent, treat complete curing and demolding, sanding and polishing promptly gets the luminous plastics stair railing.
Embodiment 3:
20 kilograms of abundant backs of mixing of self-luminescent material of 80 kilograms of ceramic glazes and Beijing Hua Yan are stand-by.
Potter's clay is after technology is made into the blank of balustrade routinely, under the not absolutely dry as yet state in blank surface, smear above-mentioned ceramic glaze on the blank surface, treat that blank is dried to and go into stove when requiring humidity and under 900~1000 ℃, carry out roasting, burn till product and after arrangement, be the noctilucence balustrade.
Embodiment 4:
With 30 kilograms of unsaturated polyester resins, 58 kilograms in aluminium hydroxide, 10 kilograms of the self-luminescent materials of Beijing Hua Yan, different cobalt green are inserted for 2 kilograms and are put into the staircase step mould of having smeared release agent after agitator fully stirs, the demoulding behind the curing molding is carried out post processing again and is got the staircase step finished product.

Claims (3)

1. the preparation method of noctilucence stair, the raw material that it is characterized in that used self-luminous paint forms and percentage by weight is:
Acrylic resin 73~83
Self-luminescent material 15~25
Mill base 2~2.5
The above-mentioned raw materials mixing is made self-luminous paint back stair are carried out the surface spraying.
2. the preparation method of sharp luminous plastics stair is characterized in that used raw material is formed and percentage by weight is:
PVC 73~83
Alkane naphthenic acid cobalt 1.5~2.5
Self-luminescent material 15~25
With adding alkane naphthenic acid cobalt and self-luminescent material after the PVC fusion, fully stir the back casting.
3. the preparation method of sharp Noctilucent ceramics stair is characterized in that used raw material is formed and percentage by weight is:
Ceramic glaze 75~85
Self-luminescent material 15~25
Behind self-luminescent material and the abundant mixing of ceramic glaze, the gained glaze is coated in reburn on the potter's clay base again and makes ceramic product.
CN 03128237 2003-06-24 2003-06-24 Manufacturing method of luminous staircase Expired - Fee Related CN1202335C (en)