CN119856233A - 玻璃凝固用团块 - Google Patents
玻璃凝固用团块 Download PDFInfo
- Publication number
- CN119856233A CN119856233A CN202380065581.4A CN202380065581A CN119856233A CN 119856233 A CN119856233 A CN 119856233A CN 202380065581 A CN202380065581 A CN 202380065581A CN 119856233 A CN119856233 A CN 119856233A
- Authority
- CN
- China
- Prior art keywords
- glass
- radioactive waste
- less
- agglomerate
- vitrification
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Classifications
-
- G—PHYSICS
- G21—NUCLEAR PHYSICS; NUCLEAR ENGINEERING
- G21F—PROTECTION AGAINST X-RADIATION, GAMMA RADIATION, CORPUSCULAR RADIATION OR PARTICLE BOMBARDMENT; TREATING RADIOACTIVELY CONTAMINATED MATERIAL; DECONTAMINATION ARRANGEMENTS THEREFOR
- G21F9/00—Treating radioactively contaminated material; Decontamination arrangements therefor
- G21F9/04—Treating liquids
- G21F9/06—Processing
- G21F9/16—Processing by fixation in stable solid media
-
- G—PHYSICS
- G21—NUCLEAR PHYSICS; NUCLEAR ENGINEERING
- G21F—PROTECTION AGAINST X-RADIATION, GAMMA RADIATION, CORPUSCULAR RADIATION OR PARTICLE BOMBARDMENT; TREATING RADIOACTIVELY CONTAMINATED MATERIAL; DECONTAMINATION ARRANGEMENTS THEREFOR
- G21F9/00—Treating radioactively contaminated material; Decontamination arrangements therefor
- G21F9/28—Treating solids
- G21F9/30—Processing
Landscapes
- Physics & Mathematics (AREA)
- Engineering & Computer Science (AREA)
- General Engineering & Computer Science (AREA)
- High Energy & Nuclear Physics (AREA)
- Processing Of Solid Wastes (AREA)
Applications Claiming Priority (3)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2023-015014 | 2023-02-03 | ||
| JP2023015014 | 2023-02-03 | ||
| PCT/JP2023/034564 WO2024161698A1 (ja) | 2023-02-03 | 2023-09-22 | ガラス固化用ブリケット |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| CN119856233A true CN119856233A (zh) | 2025-04-18 |
Family
ID=92146059
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| CN202380065581.4A Pending CN119856233A (zh) | 2023-02-03 | 2023-09-22 | 玻璃凝固用团块 |
Country Status (3)
| Country | Link |
|---|---|
| JP (1) | JPWO2024161698A1 (https=) |
| CN (1) | CN119856233A (https=) |
| WO (1) | WO2024161698A1 (https=) |
Family Cites Families (6)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2536778B2 (ja) * | 1988-08-11 | 1996-09-18 | 動力炉・核燃料開発事業団 | 放射性廃液処理用カ―トリッジの製造法 |
| ES2530463T3 (es) * | 2008-11-10 | 2015-03-03 | Ald Vacuum Techn Gmbh | Material de matriz a base de grafito y aglutinantes inorgánicos adecuado para el almacenamiento definitivo de residuos radiactivos, procedimiento para su preparación, su elaboración y uso |
| JP6292854B2 (ja) * | 2012-12-25 | 2018-03-14 | セントラル硝子株式会社 | 放射性廃棄物のガラス固化体及びその形成方法 |
| CA3027528C (en) * | 2016-06-23 | 2023-11-28 | Nippon Chemical Industrial Co., Ltd. | Method for producing solidified radioactive waste |
| JP6430676B1 (ja) * | 2018-03-30 | 2018-11-28 | 日本無機株式会社 | 放射性廃液処理用カートリッジ |
| JP7458334B2 (ja) * | 2021-01-29 | 2024-03-29 | 株式会社東芝 | 放射性廃棄物固化方法、および、放射性廃棄物固化システム |
-
2023
- 2023-09-22 CN CN202380065581.4A patent/CN119856233A/zh active Pending
- 2023-09-22 JP JP2024574258A patent/JPWO2024161698A1/ja active Pending
- 2023-09-22 WO PCT/JP2023/034564 patent/WO2024161698A1/ja not_active Ceased
Also Published As
| Publication number | Publication date |
|---|---|
| JPWO2024161698A1 (https=) | 2024-08-08 |
| WO2024161698A1 (ja) | 2024-08-08 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| Kim et al. | Effect of Si/Al molar ratio and curing temperatures on the immobilization of radioactive borate waste in metakaolin-based geopolymer waste form | |
| JPS6046394B2 (ja) | 高レベル放射性廃液のガラスによる固化処理方法 | |
| Chaerun et al. | Retention mechanism of cesium in chabazite embedded into metakaolin-based alkali activated materials | |
| CN111056789B (zh) | 一种放射性废渣的固化方法 | |
| KR102228111B1 (ko) | 조립체, 그 제조 방법 및 유리 물품의 제조 방법 | |
| JPH0833493B2 (ja) | 硼珪酸ガラス内での核廃棄物の不動化方法 | |
| Shi et al. | Effect of PbO on the chemical durability of low-temperature PbO–B2O3–ZnO glass for cesium immobilization | |
| Han et al. | Comprehensive study of recycling municipal solid waste incineration fly ash in lightweight aggregate with bloating agent: Effects of water washing and bloating mechanism | |
| JPS6120839B2 (https=) | ||
| Vandevenne et al. | Alkali-activated materials for radionuclide immobilisation and the effect of precursor composition on Cs/Sr retention | |
| CN119856233A (zh) | 玻璃凝固用团块 | |
| Chen et al. | Cold reaction sintering of geopolymers for enhanced Cs+ immobilization: Synthesis, characterization, and leaching behavior | |
| CN105813993B (zh) | 用于低放射性废树脂玻璃化的玻璃组合物及利用其的低放射性废树脂的玻璃化方法 | |
| JP2001027694A (ja) | 放射性濃縮廃物質の固化体及び該固化体の製造方法 | |
| Mayzan et al. | Graphite immobilisation in iron phosphate glass composite materials produced by microwave and conventional sintering routes | |
| RU2766339C1 (ru) | Способ подготовки проб твердого минерального топлива к рентгенофлуоресцентному анализу | |
| Massoni et al. | Densification of non-radioactive porous siliceous particles loaded with cesium potassium copper hexacyanoferrate by spark plasma sintering | |
| KR20090080713A (ko) | 방사성 폐기물 과립화 방법 및 처리장치 | |
| US20020198431A1 (en) | Method for conditioning soda effluents in the form of nepheline | |
| Zhang et al. | Cold sintering of ammonium phosphomolybdate ((NH4) 3PMo12O40· xH2O) as soild-state matrices for cesium immobilization | |
| Luo et al. | Mechanical activation triggered in-situ crystallization of cordierite in ceramic prepared from ferrochrome slag | |
| AU2022201537B2 (en) | Process of obtaining powdered sodium silicate from sandy tailings originated from the iron ore concentration process, use of the sodium silicate, and sodium silicate | |
| JP4573174B2 (ja) | 放射性廃棄物の処理方法及びその焼結体 | |
| RU2800284C1 (ru) | Способ изготовления многокомпонентных образцов сравнения для рентгенофлуоресцентного анализа горных пород | |
| JP4787997B2 (ja) | リン酸二水素ナトリウムを含む放射性廃液の固化処理方法 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| PB01 | Publication | ||
| PB01 | Publication | ||
| SE01 | Entry into force of request for substantive examination | ||
| SE01 | Entry into force of request for substantive examination |