CN1196382A - Charcoal for roasting - Google Patents
Charcoal for roasting Download PDFInfo
- Publication number
- CN1196382A CN1196382A CN 98100500 CN98100500A CN1196382A CN 1196382 A CN1196382 A CN 1196382A CN 98100500 CN98100500 CN 98100500 CN 98100500 A CN98100500 A CN 98100500A CN 1196382 A CN1196382 A CN 1196382A
- Authority
- CN
- China
- Prior art keywords
- body layer
- layer
- component
- ignition
- water
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
A charcoal for cooking and roasting food is shaped fuel composed of main body layer and igniting layer. Said main body layer contains high-quality anthracite (65-68 Wt.%), rice husk char (10-13), starch (2-2.8), caustic soda (0.6-1.2) and water (16-19). Said igniting layer contains high-quality anthracite (22-25 Wt.%), barium nitrate (22-25), sodium nitrate (7-9), rice husk char (22-25), starch (2-2.8), caustic soda (0.6-1.2), water (16-19) and essence (0.02). The tickness ratio of igniting to main body layer is 1 : 4. Its advantages are quick ignition, no odour and easy application.
Description
The present invention relates to a kind of charcoal for roasting, belong to moulded coal fuel.
Present moulded coal fuel (as coal briquette, honeycomb briquette etc.) is used commonplace, need add the materials that ignite such as firewood when lighting a fire, and smoke pollution is big, and troublesome poeration is wasted time and energy, and peculiar smell is often all arranged, and uses inconvenient.
The objective of the invention is to overcome the deficiencies in the prior art, a kind of charcoal for roasting is provided, igniting is simple fast, and free from extraneous odour pollutes little, easy to use.
The object of the present invention is achieved like this: it is made up of body layer and an ignition layer, and body layer each component and weight percent thereof are high-quality anthracite 65-68, rice hull carbon 10-13, starch 2-2.8, caustic soda 0.6-1.2, water 16-19; An ignition layer each component and weight percent thereof are high-quality anthracite 22-25, nitrate of baryta 22-25, SODIUMNITRATE 7-9, rice hull carbon 22-25, starch 2-2.8, caustic soda 0.6-1.2, water 16-19, essence 0.02; Its making method is: the body layer each component is taken by weighing in proportion be rolled into the powder mixing, add water and stir standby; An ignition layer each component taken by weighing to roll with powder in proportion mix, add water and stir standby; Aforementioned body layer and an ignition layer raw material are respectively charged in two hoppers of molding coal machine, make the body layer raw material of the specified amount mould inner pressure system of bleeding earlier, an ignition layer raw material of specified amount is bled suppress on the body layer in the same mould, then the product that is pressed into is put into drying machine drying and got final product in 48 hours.
Compared with prior art, the invention has the advantages that igniting is time saving and energy saving, easy and simple to handle, free from extraneous odour, pollutes little, easy to use, especially suitable out on tours broil food.
Below in conjunction with embodiment in detail the present invention is described in detail.The present invention is made up of body layer and an ignition layer, and body layer each component and weight percent thereof are high-quality anthracite 65-68, rice hull carbon 10-13, starch 2-2.8, caustic soda 0.6-1.2, water 16-19; An ignition layer each component and weight percent thereof are high-quality anthracite 22-25, nitrate of baryta 22-25, SODIUMNITRATE 7-9, rice hull carbon 22-25, starch 2-2.8, caustic soda 0.6-1.2, water 16-19, essence 0.02: an ignition layer is positioned at body layer top, with the thickness ratio of body layer be 1: 4.The optimum weight per-cent of body layer each component is high-quality anthracite 66.8, rice hull carbon 11.8, starch 2.4, caustic soda 0.8, water 18.2; The optimum weight per-cent of an ignition layer each component is high-quality anthracite 23.6, nitrate of baryta 23.6, SODIUMNITRATE 7.8, rice hull carbon 23.6, starch 2.4, caustic soda 0.78, water 18.2, essence 0.02.Making method of the present invention is: the body layer each component is taken by weighing in proportion be rolled into the powder mixing, add water and stir standby; An ignition layer each component taken by weighing in proportion be rolled into powder and mix, add water and stir standby; Aforementioned body layer and igniting bed thickness material are respectively charged in two hoppers of molding coal machine, make the body layer raw material of the specified amount mould inner pressure system of bleeding earlier, an ignition layer raw material of specified amount is bled suppress on the body layer in the same mould, then the product that is pressed into is put into drying machine drying and got final product in 48 hours.
Embodiment:
To produce 1000kg is example, and the proportioning weight (kg) of each component sees the following form.
High-quality anthracite | Nitrate of baryta | SODIUMNITRATE | Rice hull carbon | Starch | Caustic soda | Water | Essence | ||
??1 | Body layer | ????657 | ??120 | ??25 | ??8 | ??190 | |||
An ignition layer | ????230 | ????240 | ????75 | ??230 | ??28 | ??9.8 | ??187 | ??0.2 | |
??2 | Body layer | ????670 | ??115 | ??27 | ??10 | ??178 | |||
An ignition layer | ????240 | ????230 | ????80 | ??235 | ??23 | ??7.8 | ??184 | ??0.2 | |
??3 | Body layer | ????660 | ??125 | ??26 | ??7 | ??182 | |||
An ignition layer | ????245 | ????234 | ????85 | ??220 | ??22 | ??6.8 | ??187 | ??0.2 | |
??4 | Body layer | ????668 | ??118 | ??24 | ??8 | ??182 | |||
An ignition layer | ????236 | ????236 | ????78 | ??236 | ??24 | ??7.8 | ??182 | ??0.2 | |
??5 | Body layer | ????680 | ??105 | ??20 | ??6 | ??189 | |||
An ignition layer | ????250 | ????235 | ????85 | ??223 | ??20 | ??6.8 | ??180 | ??0.2 |
The making method of each embodiment as described above.
Physical dimension length and width of the present invention, thickly can make 130mm * 100mm * 50mm main body bed thickness 40mm, igniting bed thickness 10mm also can make other various size as required, and be equipped with corresponding stove and accessory.During use,, just can ignite with the direct firing point fire bed of match.
Claims (4)
1, a kind of charcoal for roasting is characterized in that it is made up of body layer and an ignition layer, and body layer each component and weight percent thereof are high-quality anthracite 65-68, rice hull carbon 10-13, starch 2-2.8, caustic soda 0.6-1.2, water 16-19; An ignition layer each component and weight percent thereof are high-quality anthracite 22-25, nitrate of baryta 22-25, SODIUMNITRATE 7-9, rice hull carbon 22-25, starch 2-2.8, caustic soda 0.6-1.2, water 16-19, essence 0.02;
2, charcoal for roasting according to claim 1 is characterized in that an ignition layer is positioned at body layer top, with the thickness ratio of body layer be 1: 4.
3, charcoal for roasting according to claim 1, the optimum weight per-cent that it is characterized in that the body layer each component are high-quality anthracite 66.8, rice hull carbon 11.8, starch 2.4, caustic soda 0.8, water 18.2; The optimum weight per-cent of an ignition layer each component is high-quality anthracite 23.6, nitrate of baryta 23.6, SODIUMNITRATE 7.8, rice hull carbon 23.6, starch 2.4, caustic soda 0.78, water 18.2, essence 0.02.
4, the making method of charcoal for roasting as claimed in claim 1 is characterized in that:
A, the body layer each component taken by weighing in proportion be rolled into powder and mix, add water and stir standby;
6, an ignition layer each component is taken by weighing in proportion be rolled into powder and mix, add water and stir standby;
C, aforementioned body layer and an ignition layer raw material are respectively charged in two hoppers of molding coal machine, make the body layer raw material of the specified amount mould inner pressure system of bleeding earlier, an ignition layer raw material of specified amount is bled suppress on the body layer in the same mould, then the product that is pressed into is put into drying machine drying and got final product in 48 hours.