Prior art keywords
solution
tile carving
shade
finished product
color
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201810330600.2A
Other languages
English (en)
Inventor
吴正辉
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201810330600.2A priority Critical patent/CN110385937A/zh
Publication of CN110385937A publication Critical patent/CN110385937A/zh
Pending legal-status Critical Current

Links

Classifications

    • BPERFORMING OPERATIONS; TRANSPORTING
    • B44DECORATIVE ARTS
    • B44FSPECIAL DESIGNS OR PICTURES
    • B44F9/00Designs imitating natural patterns

Landscapes

  • Printing Methods (AREA)

Abstract

本发明公开了一种砖雕仿古的方法,具体步骤如下:步骤一,将修复好的砖雕在常温下阴干,将整块砖雕用第一溶液刷一遍;步骤二,涂刷过第一溶液的砖雕自然阴干后,将第二溶液涂刷在砖雕上;步骤三,涂刷过第二溶液的砖雕自然阴干后,将第三溶液喷洒在砖雕上,自然风干后再次喷洒一遍,一共喷洒三遍,每次喷洒的第三溶液质量相同,得到半成品;步骤四,半成品阴干后继续观察半成品的颜色,发现新色和老色差别较大的地方继续用第二溶液刷涂一遍,直至完全接近老色,得到成品。本发明的方法要观察其老色,进行待别调色,采用墨汁与高锰酸钾两种分别调配并且多次调配,直到颜色统一,可以达到仿古的效果,整体美观性好。

Description

一种砖雕仿古的方法
技术领域
本发明涉及砖雕领域,具体是一种砖雕仿古的方法。
背景技术
我国古代有许多遗留下来的瑰宝,文物中的砖雕就是其中一种。砖雕指在青砖上雕出山水、花卉、人物等图案,是古建筑雕刻中很重要的一种艺术形式,制作工艺与核心点是在于用金砖等级的成品青砖进行表面深度雕刻,这是我国几百年来传统意义上真正的砖雕,传统砖雕精致细腻、气韵生动、极富书卷气等特点。
古代的砖雕经过风雨的侵蚀会造成破损,人们对破损的部分进行修复并且进行仿古处理,但是仿古处理时砖雕在新砖和老砖的接缝处很难达到颜色统一,这就影响了整体的视觉。
发明内容
本发明的目的在于提供一种砖雕仿古的方法,以解决上述背景技术中提出的问题。
为实现上述目的,本发明提供如下技术方案:
一种砖雕仿古的方法,具体步骤如下:
步骤一,将修复好的砖雕在常温下阴干,将红泥和水按照质量比3∶7混合并且搅拌均匀,得到第一溶液,将整块砖雕用第一溶液刷一遍;
步骤二,涂刷过第一溶液的砖雕自然阴干后,将第二溶液涂刷在砖雕上,第二溶液为墨汁和水按照质量比为1∶10混合均匀得到;
步骤三,涂刷过第二溶液的砖雕自然阴干后,将第三溶液喷洒在砖雕上,自然风干后再次喷洒一遍,一共喷洒三遍,每次喷洒的第三溶液质量相同,得到半成品,第三溶液为高锰酸钾和水按照质量比为1∶250混合均匀得到,一块30*38厘米的砖一共需要喷洒753g第三溶液;
步骤四,半成品阴干后继续观察半成品的颜色,发现新色和老色差别较大的地方继续用第二溶液刷涂一遍,直至完全接近老色,得到成品。
作为本发明进一步的方案:红泥采用老红泥,墨汁采用淡墨汁。
作为本发明进一步的方案:刷涂第一溶液、第二溶液和第三溶液时用细毛刷顺着一个方向刷涂,刷涂速度必须匀速。
作为本发明进一步的方案:阴干的温度为15-30摄氏度。
与现有技术相比,本发明的有益效果是:本发明的方法要观察其老色,进行待别调色,采用墨汁与高锰酸钾两种分别调配并且多次调配,直到颜色统一,可以达到仿古的效果,整体美观性好。
附图说明
图1为砖雕仿古的方法中一种实施例在实施前的图。
图2为砖雕仿古的方法中一种实施例在实施后的效果图。
图3为砖雕仿古的方法中另一种实施例在实施前的图。
图4为砖雕仿古的方法中另一种实施例在实施后的效果图。
具体实施方式
下面结合具体实施方式对本专利的技术方案作进一步详细地说明。
请参阅图1-4,一种砖雕仿古的方法,具体步骤如下:
步骤一,将修复好的砖雕在常温下阴干,将红泥和水按照质量比3∶7混合并且搅拌均匀,得到第一溶液,将整块砖雕用第一溶液刷一遍;
步骤二,涂刷过第一溶液的砖雕自然阴干后,将第二溶液涂刷在砖雕上,第二溶液为墨汁和水按照质量比为1∶10混合均匀得到;
步骤三,涂刷过第二溶液的砖雕自然阴干后,将第三溶液喷洒在砖雕上,自然风干后再次喷洒一遍,一共喷洒三遍,每次喷洒的第三溶液质量相同,得到半成品,第三溶液为高锰酸钾和水按照质量比为1∶250混合均匀得到,一块30*38厘米的砖一共需要喷洒753g第三溶液;
步骤四,半成品阴干后继续观察半成品的颜色,发现新色和老色差别较大的地方继续用第二溶液刷涂一遍,直至完全接近老色,得到成品。
红泥采用老红泥,墨汁采用淡墨汁。刷涂第一溶液、第二溶液和第三溶液时用细毛刷顺着一个方向刷涂,刷涂速度必须匀速,不能太快,也不能太慢。阴干的温度为15-30摄氏度。高锰酸钾要严格安上述面积和比例调配,少了颜色变谈,多了颜色变深。在调水和墨汁时要调均匀。要观察其老色,进行待别调色,需墨汁与高锰酸钾两种分别调配并且多次调配,直到颜色统一。要对老砖雕包浆有一定了解。刷涂后要阴干,不能日晒。
对于本领域技术人员而言,显然本发明不限于上述示范性实施例的细节,而且在不背离本发明的精神或基本特征的情况下,能够以其他的具体形式实现本发明。因此,无论从哪一点来看,均应将实施例看作是示范性的,而且是非限制性的,本发明的范围由所附权利要求而不是上述说明限定,因此旨在将落在权利要求的等同要件的含义和范围内的所有变化囊括在本发明内。不应将权利要求中的任何附图标记视为限制所涉及的权利要求。
此外,应当理解,虽然本说明书按照实施方式加以描述,但并非每个实施方式仅包含一个独立的技术方案,说明书的这种叙述方式仅仅是为清楚起见,本领域技术人员应当将说明书作为一个整体,各实施例中的技术方案也可以经适当组合,形成本领域技术人员可以理解的其他实施方式。

Claims (4)

1.一种砖雕仿古的方法,其特征在于,具体步骤如下:
步骤一,将修复好的砖雕在常温下阴干,将红泥和水按照质量比3∶7混合并且搅拌均匀,得到第一溶液,将整块砖雕用第一溶液刷一遍;
步骤二,涂刷过第一溶液的砖雕自然阴干后,将第二溶液涂刷在砖雕上,第二溶液为墨汁和水按照质量比为1∶10混合均匀得到;
步骤三,涂刷过第二溶液的砖雕自然阴干后,将第三溶液喷洒在砖雕上,自然风干后再次喷洒一遍,一共喷洒三遍,每次喷洒的第三溶液质量相同,得到半成品,第三溶液为高锰酸钾和水按照质量比为1∶250混合均匀得到,一块30*38厘米的砖一共需要喷洒753g第三溶液;
步骤四,半成品阴干后继续观察半成品的颜色,发现新色和老色差别较大的地方继续用第二溶液刷涂一遍,直至完全接近老色,得到成品。
2.根据权利要求1所述的砖雕仿古的方法,其特征在于,所述红泥采用老红泥,墨汁采用淡墨汁。
3.根据权利要求1所述的砖雕仿古的方法,其特征在于,所述刷涂第一溶液、第二溶液和第三溶液时用细毛刷顺着一个方向刷涂,刷涂速度必须匀速。
4.根据权利要求1所述的砖雕仿古的方法,其特征在于,所述阴干的温度为15-30摄氏度。
CN201810330600.2A 2018-04-16 2018-04-16 一种砖雕仿古的方法 Pending CN110385937A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201810330600.2A CN110385937A (zh) 2018-04-16 2018-04-16 一种砖雕仿古的方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201810330600.2A CN110385937A (zh) 2018-04-16 2018-04-16 一种砖雕仿古的方法

Publications (1)

Publication Number Publication Date
CN110385937A true CN110385937A (zh) 2019-10-29

Family

ID=68282533

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201810330600.2A Pending CN110385937A (zh) 2018-04-16 2018-04-16 一种砖雕仿古的方法

Country Status (1)

Country Link
CN (1) CN110385937A (zh)

Citations (6)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US5244744A (en) * 1991-08-20 1993-09-14 Rush Victoria L Article with antique appearance and method of making same
CN101108571A (zh) * 2006-07-20 2008-01-23 潮州市威成瓷艺有限公司 一种仿古陈设艺术陶器的制作方法
CN101172373A (zh) * 2006-11-03 2008-05-07 王卿芳 石材仿古工艺方法
CN104438027A (zh) * 2014-10-09 2015-03-25 安徽省孟府家工艺品有限公司 一种仿古家具的做旧处理方法
US20170190210A1 (en) * 2015-01-21 2017-07-06 Desong Ma Method for processing ink, stone and oil painting
CN106977143A (zh) * 2017-04-07 2017-07-25 广西汇益企业管理有限公司 一种高强度仿古青砖的配方

Patent Citations (6)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US5244744A (en) * 1991-08-20 1993-09-14 Rush Victoria L Article with antique appearance and method of making same
CN101108571A (zh) * 2006-07-20 2008-01-23 潮州市威成瓷艺有限公司 一种仿古陈设艺术陶器的制作方法
CN101172373A (zh) * 2006-11-03 2008-05-07 王卿芳 石材仿古工艺方法
CN104438027A (zh) * 2014-10-09 2015-03-25 安徽省孟府家工艺品有限公司 一种仿古家具的做旧处理方法
US20170190210A1 (en) * 2015-01-21 2017-07-06 Desong Ma Method for processing ink, stone and oil painting
CN106977143A (zh) * 2017-04-07 2017-07-25 广西汇益企业管理有限公司 一种高强度仿古青砖的配方

Non-Patent Citations (2)

* Cited by examiner, † Cited by third party
Title
刘树林: "《历代文物艺术品收藏保养知识手册》", 31 August 2012, 北京:中国书店 *
钟仰智: "《装饰镶贴工》", 31 December 2002, 北京:蓝天出版社 *

Similar Documents

Publication Publication Date Title
CN103483010B (zh) 一种立体釉下五彩陶瓷制作工艺
CN104473392A (zh) 一种银胎画珐琅的制造工艺
CN103613409B (zh) 一种泥釉及其红壤陶制品的制造方法
CN101879834B (zh) 一种在陶瓷青坯上形成凸起画面的装饰方法
CN103963547B (zh) 一种陶瓷没骨画及其制作技法
CN104387120B (zh) 一种陶瓷釉下五彩丝网移印方法
CN104478494A (zh) 釉下泼彩陶瓷的制作方法
CN113773118A (zh) 一种钧瓷釉上彩绘制工艺
CN109304039A (zh) 一种搪胶玩具的制作方法
CN110385937A (zh) 一种砖雕仿古的方法
CN105330147B (zh) 一种骨质瓷用硅酸锌结晶釉料的制备方法
CN104418505A (zh) 彩绘琉璃的制备工艺
CN103522827A (zh) 一种雕漆工艺品的制造方法
CN105711323B (zh) 一种制作点缀形珍珠地的且明暗刻花的装饰工艺品的工艺方法
CN103692845A (zh) 彩墨水画的绘制方法
CN106401094B (zh) 一种仿古明城墙墙面处理方法
CN105130367B (zh) 一种砂壁状建筑仿石涂料
CN111348938B (zh) 一种墨玉彩彩绘颜料及其制备方法和应用
CN101941352B (zh) 一种制作具有奇幻图案漆画的方法
CN105150751A (zh) 一种水木类漆画的制作方法
CN101314306B (zh) 一种带有植物纤维画的红瓷工艺品的制作方法
CN107965261A (zh) 一种电动竹帘
CN109400216A (zh) 一种陶瓷釉上绘画色浆及陶瓷釉上绘画方法和应用
CN106738238A (zh) 一种青花陶瓷的制备方法
CN103144184B (zh) 一种陶瓷釉下绘画方法

Legal Events

Date Code Title Description
PB01 Publication
PB01 Publication
SE01 Entry into force of request for substantive examination
SE01 Entry into force of request for substantive examination
RJ01 Rejection of invention patent application after publication

Application publication date: 20191029

RJ01 Rejection of invention patent application after publication