CN110326860A - A method of optimization pearl freshwater mussel shell plate color - Google Patents

A method of optimization pearl freshwater mussel shell plate color Download PDF

Info

Publication number
CN110326860A
CN110326860A CN201910584304.XA CN201910584304A CN110326860A CN 110326860 A CN110326860 A CN 110326860A CN 201910584304 A CN201910584304 A CN 201910584304A CN 110326860 A CN110326860 A CN 110326860A
Authority
CN
China
Prior art keywords
shell plate
color
freshwater mussel
effect
pearl freshwater
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201910584304.XA
Other languages
Chinese (zh)
Inventor
童银洪
刘永
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Guangdong Ocean University
Original Assignee
Guangdong Ocean University
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Guangdong Ocean University filed Critical Guangdong Ocean University
Priority to CN201910584304.XA priority Critical patent/CN110326860A/en
Publication of CN110326860A publication Critical patent/CN110326860A/en
Pending legal-status Critical Current

Abstract

The invention discloses a kind of methods for optimizing pearl freshwater mussel shell plate color, pearl freshwater mussel shell plate is sent into -60 gamma irradiation device of cobalt of loading of source amount 1000k~2000k Curie and is irradiated 12~24 hours, take out pearl freshwater mussel shell plate, observe shell plate color, if shell plate color reaches required color effect, radiation treatment is completed;If shell plate is of light color, rainbow effect is unobvious, it is sent into irradiation devices irradiates 6~12 hours again, until shell plate color reaches required color effect.The present invention has the advantage that 1. optimizing the significant effect of color, plate color can occur irreversible transformation, while enhance rainbow effect from canescence, pink to Dark grey, grey black, bluish violet, and shell is made to produce multicoloured effect.2. processing process is simple, processed shell plate safety, radiationless residual.3. irradiation processing mechanism is more and radiation treatment is low-cost.

Description

A method of optimization pearl freshwater mussel shell plate color
Technical field
It is especially a kind of that pearl freshwater mussel shell plate color is optimized using irradiation technique the present invention relates to pearl manufacture field Method.
Background technique
The traditional advantage industry that pearl is China is cultivated using fresh water pearl freshwater mussel, therefore, it is precious that China possesses fresh water abundant Pearl oyster shell resource.The mainly CaCO of fresh water pearl freshwater mussel shell3Aragonite and a small amount of organic matter (including Chitosan-alginate microcapsules, pigment have Machine matter etc.) it interacts and accumulates.In addition, rich in metallic elements such as Mn, Fe and Cr in fresh water pearl freshwater mussel shell.
Fresh water pearl freshwater mussel shell while with charming pearly luster, also there is composition crystal grain be tiny, compact structure, Therefore the characteristics such as compression strength is high, nontoxic and pollution-free and machining property is good have using the production of fresh water pearl freshwater mussel shell The plate of regular geometric shape can be used for producing house decorative material and craftwork, has very high ornamental value and uses valence Value.With the fast development of China's economy and real estate, high-quality, multi-functional craftwork and ornament materials demand persistently increase It is long, the wide market of pearl freshwater mussel shell plate.
Color and gloss (i.e. color) are an important factor for influencing pearl freshwater mussel shell plate quality and price.Currently, China Fresh water pearl freshwater mussel shell plate color is relatively simple based on white, canescence and pink, therefore, to pearl freshwater mussel shell plate Material carries out color optimization and gloss finish, can enrich pearl freshwater mussel shell plate designs and varieties, improves ornamental value and using effect.
Summary of the invention
The purpose of the present invention is to provide a kind of methods for optimizing pearl freshwater mussel shell plate color, enrich pearl freshwater mussel shell plate The color of material, the gloss for enhancing pearl freshwater mussel shell plate improve the value of pearl freshwater mussel shellwork.
The technical solution adopted by the present invention is that: a method of optimization pearl freshwater mussel shell plate color, it is characterised in that: will Pearl freshwater mussel shell plate is sent into -60 gamma irradiation device of cobalt of loading of source amount 1000k~2000k Curie and irradiates 12~24 hours, Pearl freshwater mussel shell plate is taken out, shell plate color is observed, if shell plate color reaches required color effect, completing should The color of shell plate optimizes;If shell plate is of light color, rainbow effect is unobvious, it is sent into irradiation devices irradiates 6 again ~12 hours, until shell plate color reaches required color effect.
The beneficial effects of the present invention are: the present invention is by using -60 radiated by gamma-ray pearl freshwater mussel shell plate of cobalt, it can So that the bivalent manganese in shell plate is converted into coloured value Mn, while certain organic matter conformations in shell plate occur Change and color is presented, darken, rainbow effect enhancing achievees the effect that optimize pearl freshwater mussel shell plate color.
Method of the invention have the advantages that 1. optimize color significant effect, can make pearl freshwater mussel shell plate face by To Dark grey, grey black, bluish violet etc. irreversible transformation occurs for canescence, pink, while enhancing rainbow effect, makes Shell plate produces multicoloured effect.2. processing process is simple, processed shell plate safety, radiationless Residual.3. irradiation processing mechanism facilitates the radiation treatment of shell plate, and radiation treatment throughout China fresh water pearl producing region It is low-cost.
Detailed description of the invention
Fig. 1 is to be compared using the method for the present invention the color variation before and after pearl freshwater mussel shell plate radiation treatment.
Specific embodiment
A kind of method for optimizing pearl freshwater mussel shell plate color of the present invention, using following technical process: by pearl freshwater mussel shell Plate is sent into -60 gamma irradiation device of cobalt of loading of source amount 1000k~2000k Curie and irradiates 12~24 hours, takes out pearl freshwater mussel Shell plate observes shell plate color if shell plate color reaches required color effect and completes the shell plate Color optimization;If shell plate is of light color, rainbow effect is unobvious, it is sent into irradiation devices irradiates 6~12 hours again, directly Reach required color effect to shell plate color.
It is illustrated below by specific embodiment operation.
Embodiment 1
A method of optimization pearl freshwater mussel shell plate color, by following process implementing:
White pearl freshwater mussel shell plate is sent into -60 gamma irradiation device of cobalt of loading of source amount 1000k Curie and is irradiated 12 hours;It takes Sample observation, product is in light grey or grey;Plate is sent into above-mentioned irradiation devices again and is irradiated 10 hours;Sampling observation, produces Product are in grey black or bluish violet, and rainbow effect enhancing reaches required color effect, completes radiation treatment.
Embodiment 2
A method of optimization pearl freshwater mussel shell plate color, by following process implementing:
Pink pearl freshwater mussel shell plate is sent into -60 gamma irradiation device of cobalt of loading of source amount 1000k Curie and is irradiated 16 hours; Sampling observation, product gray;Plate is sent into above-mentioned irradiation devices again and is irradiated 6 hours;Product is in grey black, rainbow effect It should enhance, reach required color effect, complete radiation treatment.
Embodiment 3
A method of optimization pearl freshwater mussel shell plate color, by following process implementing:
Pink pearl freshwater mussel shell plate is sent into -60 gamma irradiation device of cobalt of loading of source amount 2000k Curie and is irradiated 12 hours; Sampling observation, product are in grey black;Plate is sent into above-mentioned irradiation devices again and is irradiated 8 hours;Product is in bluish violet, rainbow Effect enhancing, reaches required color effect, completes radiation treatment.
Finally it should be noted that the above content is merely illustrative of the technical solution of the present invention, rather than the present invention is protected The limitation of range, the simple modification or equivalent replacement that those skilled in the art carry out technical solution of the present invention, All without departing from the spirit and scope of technical solution of the present invention.

Claims (1)

1. a kind of method for optimizing pearl freshwater mussel shell plate color, it is characterised in that: pearl freshwater mussel shell plate is sent into loading of source amount It is irradiated 12~24 hours in -60 gamma irradiation device of cobalt of 1000k~2000k Curie, takes out pearl freshwater mussel shell plate, observe shellfish Coverboard material color completes radiation treatment if shell plate color reaches required color effect;If shell plate is of light color, Rainbow effect is unobvious, then is sent into irradiation devices and irradiates 6~12 hours again, until shell plate color reaches required color Damp effect.
CN201910584304.XA 2019-07-01 2019-07-01 A method of optimization pearl freshwater mussel shell plate color Pending CN110326860A (en)