CN110001039A - A kind of polarisation sheet method for straightening warp - Google Patents

A kind of polarisation sheet method for straightening warp Download PDF

Info

Publication number
CN110001039A
CN110001039A CN201910364632.9A CN201910364632A CN110001039A CN 110001039 A CN110001039 A CN 110001039A CN 201910364632 A CN201910364632 A CN 201910364632A CN 110001039 A CN110001039 A CN 110001039A
Authority
CN
China
Prior art keywords
polarisation sheet
polarisation
warpage
environment
correction
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201910364632.9A
Other languages
Chinese (zh)
Other versions
CN110001039B (en
Inventor
张宾
廖志超
侯廷基
迟轶男
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SHENZHEN SAPO PHOTOELECTRIC CO Ltd
Original Assignee
SHENZHEN SAPO PHOTOELECTRIC CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SHENZHEN SAPO PHOTOELECTRIC CO Ltd filed Critical SHENZHEN SAPO PHOTOELECTRIC CO Ltd
Priority to CN201910364632.9A priority Critical patent/CN110001039B/en
Publication of CN110001039A publication Critical patent/CN110001039A/en
Application granted granted Critical
Publication of CN110001039B publication Critical patent/CN110001039B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The present invention provides a kind of polarisation sheet method for straightening warp, polarisation sheet is placed in cylinder by this method, then is placed under the conditions of suitable environment temperature, temperature together, certain time is corrected, to corrected the product of warpage NG again as qualified products.The present invention overcomes the places of prior art, device requirement constraint;It is with the obvious advantage in terms of cost, specific aim correction is done to the finished product of warpage NG, reduces the waste of cost;Correction tool structure is simple, not high to environmental requirement precision, and batch may be implemented and correct.

Description

A kind of polarisation sheet method for straightening warp
Technical field
The present invention relates to the post-processing field of finished product polarizer, especially a kind of polarisation sheet method for straightening warp.
Background technique
When coiled material polaroid finds there are warpage issues when cutting, generally use to the polarisation coiled sheet for being not processed into sheet material Material carries out the exchange cards containing all personal details and become sworn brothers mode of protective film of heavy industry and calibrates warpage;The product for having cut into sheet material warpage NG then can only be reported all Useless processing;To because visitor caused by warpage NG moves back warpage NG product caused by product or lengthy warehousing and also can only all scrap place Reason.
The above-mentioned processing mode to sheet material warpage, there is defects below:
(1) it examines anti-operation and needs equipment, material, human cost investment, and have certain loss;
(2) correction warpage cannot be completely secured in polaroid re-posted protective film (examining anti-operation), there is certain probability of failure;
It (3) is to scrap processing, cost of idleness to the product of warpage NG at present without antidote.
Summary of the invention
In view of the problems of the existing technology, the present invention provides a kind of polarisation sheet method for straightening warp, mainly for It because of the sheet material of warpage NG, is corrected under particular circumstances, meets customer specifications, scrap is become into non-defective unit.
The principle of warpage is: polarisation sheet is multilayered structure, and each layer is bonded with glue.In polarisation sheet Membrane material can be drawn high with compared with hightension in manufacturing process, membrane material can bounce back after pulling force disappears.Glue can be shunk in the drying process, film Material can also bounce back in the drying process.Since there are two retraction process, different membrane material retraction degree is different, will be in polarisation The formation internal stress between layers of sheet, if internal stress balances warpage with regard to OK, if internal stress is uneven between each other Warpage issues (just stick up and bear and stick up NG) will be generated.
The principle of correction is: the one of the inside warpage of polarisation sheet being placed in cylinder down, in certain environment Under the conditions of equably discharge the unbalanced internal stress of polarisation sheet in certain time, correct polarisation sheet warpage, Meet customer specifications.
Technical scheme is as follows:
A kind of polarisation sheet method for straightening warp, comprising the following steps:
S1 down by the one of the inside warpage of polarisation sheet is put into corresponding cylinder, the size of polarisation sheet With the relationship of corresponding circular cylinder radius are as follows:
Cylinder is placed on 30~80 DEG C of temperature together with polarisation sheet by S2, in the environment of humidity 20~90%, correction 1~48hr of time, product warpage are corrected.
As a further improvement of the present invention, the warpage degree of polarisation sheet is higher, thickness is bigger, then the environment corrected Temperature it is higher, the improvement time is longer;Environment temperature is 40-60 DEG C, and the improvement time is 12~r for 24 hours.
As a further improvement of the present invention, the moisture content of polarisation sheet is higher, then the humidity of the environment selected is higher; The moisture content of polarisation sheet material is below 0.1%, and the humidity of environment is 20-50%;The moisture content of polarisation sheet material 0.1% and with On, the humidity of environment is 60-90%.
As a further improvement of the present invention, further include S3, correct endpoint: after choosing correction condition, first lacking The correction test of warp products is measured, timing takes out whether measurement warp products meet customer specifications, if meeting customer specifications, It may determine that correct terminal, record correction condition, carry out scale is high-volume corrected;Ideal correction terminal is that quadrangle and four sides are stuck up Song is zero.
Compared with prior art, the invention has the benefit that
(1) new technology overcomes the place of prior art, device requirement constraint;
(2) with the obvious advantage in terms of cost, specific aim correction is done to the finished product of warpage NG, reduces the wave of cost Take.
(3) correction tool structure is simple, not high to environmental requirement precision, and batch may be implemented and correct.
Detailed description of the invention
Fig. 1 is the polarizer sheet structure figure of warpage NG of the invention a kind of.
Fig. 2 is the polarisation sheet in being corrected using antidote of the invention.
Fig. 3 is to have arrived at the polarisation sheet of correction terminal using antidote of the invention.
Specific embodiment
In order to illustrate the technical solutions in the embodiments of the present application or in the prior art more clearly, with reference to the accompanying drawing and specifically The present invention is further described for embodiment.
Embodiment 1
It corrects endpoint: after choosing correction condition, first doing the correction test of a small amount of warp products, measurement is taken out in timing Whether warp products meet customer specifications, if meeting customer specifications, may determine that correct terminal, record correction item Part, carry out scale are high-volume corrected;Ideal correction terminal is quadrangle and four side warpages are zero.
The polarisation sheet of warpage NG is put into cylinder, as shown in Figure 1-3, correction condition such as table 1, correction result such as table 2。
Table 1 corrects condition list
Correction condition Temperature Humidity Cylinder Sheet thickness Sheets of sizes Improvement time
Parameter 40℃ 40% 12 cun 306μm 19 cun 24hr
2 correction result of table measures table
Embodiment 1 the results show that antidote of the invention overcomes the place of prior art, device requirement condition Constraint;It is with the obvious advantage in terms of cost, specific aim correction is done to the finished product of warpage NG, reduces the waste of cost;Correction Tool construction is simple, not high to environmental requirement precision, and batch may be implemented and correct.
The foregoing is merely illustrative of the preferred embodiments of the present invention, is not intended to limit the invention, all in essence of the invention Made any modifications, equivalent replacements, and improvements etc., should all be included in the protection scope of the present invention within mind and principle.

Claims (4)

1. a kind of polarisation sheet method for straightening warp, which comprises the following steps:
S1 down by the one of the inside warpage of polarisation sheet is put into corresponding cylinder, size and the phase of polarisation sheet The relationship of corresponding circular cylinder radius are as follows:
Cylinder is placed on 30~80 DEG C of temperature together with polarisation sheet by S2, in the environment of humidity 20~90%,
1~48hr of improvement time, product warpage are corrected.
2. a kind of polarisation sheet method for straightening warp according to claim 1, which is characterized in that polarisation sheet is stuck up Qu Chengdu is higher, thickness is bigger, then the temperature for the environment corrected is higher, and the improvement time is longer;Environment temperature is 40-60 DEG C, is rectified The positive time is 12~r for 24 hours.
3. a kind of polarisation sheet method for straightening warp according to claim 1, which is characterized in that polarisation sheet contains Water rate is higher, then the humidity of the environment selected is higher;The moisture content of polarisation sheet material is below 0.1%, and the humidity of environment is 20- 50%;For the moisture content of polarisation sheet material 0.1% or more, the humidity of environment is 60-90%.
4. a kind of polarisation sheet method for straightening warp according to claim 1-3, which is characterized in that further include S3 corrects endpoint: after choosing correction condition, first doing the correction test of a small amount of warp products, measurement warpage is taken out in timing Whether product meets customer specifications, if meeting customer specifications, may determine that correct terminal, records correction condition, into Professional etiquette mould is high-volume corrected;Ideal correction terminal is quadrangle and four side warpages are zero.
CN201910364632.9A 2019-04-30 2019-04-30 Method for correcting warping of polarizing plate sheet Active CN110001039B (en)