CN109705425A - Make the method for moulding agent constituent that disappears of environmental protection plastic products - Google Patents

Make the method for moulding agent constituent that disappears of environmental protection plastic products Download PDF

Info

Publication number
CN109705425A
CN109705425A CN201711020118.0A CN201711020118A CN109705425A CN 109705425 A CN109705425 A CN 109705425A CN 201711020118 A CN201711020118 A CN 201711020118A CN 109705425 A CN109705425 A CN 109705425A
Authority
CN
China
Prior art keywords
environmental protection
plastic products
protection plastic
agent
disappears
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Withdrawn
Application number
CN201711020118.0A
Other languages
Chinese (zh)
Inventor
陈金郎
Original Assignee
Guo Qiren
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Guo Qiren filed Critical Guo Qiren
Priority to CN201711020118.0A priority Critical patent/CN109705425A/en
Publication of CN109705425A publication Critical patent/CN109705425A/en
Withdrawn legal-status Critical Current

Abstract

The present invention relates to a kind of methods for moulding agent constituent that disappears for making environmental protection plastic products.This disappear mould agent constituent include: recycling and reusing vinyon grain, the first additive, Second addition and micro lubricating agent, through mixing, kneading and again through melting, extruding, cooling, cutting granulating, and it is made and moulds agent for disappearing for environmental protection plastic products of production.Provided by the present invention disappear moulds agent constituent, and made environmental protection plastic products can be suitable for burying extensively, incinerate resolution process;Made environmental protection plastic products have the air permeability effect such as paper products;Made environmental protection plastic products fuel value is low, and low cigarette when burning, does not agglomerate after incineration, can become powder after ashing completely.

Description

Make the method for moulding agent constituent that disappears of environmental protection plastic products
Technical field
The vinyon grain that the present invention relates to a kind of with recycling and reusing mixes the first additive, Second addition and micro- Lubricant is measured, through mixing, kneading and again through melting, extruding, cooling, cutting granulating, and is made for making environmental protection plastic products The method for moulding agent constituent that disappears.
Background technique
Known correlation scrapped plastic products (such as large polybag used) by incineration, bury or in a manner of piling up Reason, such as photodegradation polybag are to allow polybag to carry out oxidation and pyrolysis automatically and reach using light, oxygen and heat factor Crack polybag, but photodegradation polybag when being buried if can not crack;Or such as biological decomposition bag is handled in a manner of burial, But need huge burial place;When incineration, then flame temperature is high, thickness and can generate the toxic gases such as dioxin, seriously It is detrimental to health and environmental pollution.
Summary of the invention
In view of this, can make disappearing for environmental protection plastic products the purpose of the present invention is to provide one kind moulds the side of agent constituent Method.
In order to reach above-mentioned purpose, the present invention, which provides, a kind of to be made disappearing for environmental protection plastic products and moulds the side of agent constituent Method, the constituent include: the recycle polyethylene plastic pellet of 20 ~ 80wt%, the first additive of 10 ~ 40wt%, 10 ~ 40wt% Two additives and micro lubricating agent through mixing, kneading and again through melting, extruding, cooling, cutting granulating, and are made for production Agent is moulded in disappearing for environmental protection plastic products;
First additive with recycle polyethylene particle, 65 ~ 80wt% and the partial size of 17 ~ 32wt% be 3 ~ 5 μm thick filler and 1 ~ Lubricant, dispersing agent and the mix polyethylene plastic pellet of 5wt% through mixing, kneading, melting, extruding, cooling, is pelletized;
Second addition with recycle polyethylene particle, 65 ~ 80wt% and the partial size of 17 ~ 32wt% be 1 ~ 2 μm thin filler and 1 ~ Lubricant, dispersing agent and the mix polyethylene plastic pellet of 5wt% through mixing, kneading, melting, extruding, cooling, is pelletized;
Above-mentioned thick filler includes the mineral powders of 50 ~ 70wt%, the corn flour of 10 ~ 20wt%, the starch of 15 ~ 25wt%, 10 It is formed mixed by the bran powder of ~ 20wt% and the leaf powder of 10 ~ 20wt%;
Above-mentioned thin filler includes the mineral powders of 50 ~ 70wt%, the corn flour of 10 ~ 20wt%, the starch of 15 ~ 25wt%, 10 It is formed mixed by the rice bran powder of ~ 20wt% and the leaf powder of 10 ~ 20wt%.
Further, wherein the lubricant is fatty acid amide or stearate, or is oleamide, erucic amide, tristearin Sour zinc or calcium stearate.
Further, wherein the mixing is mediated 20 ~ 30 minutes under 120 ~ 180 degree Celsius with kneader.
Further, the wherein high density polyethylene (HDPE) and 25 ~ 40wt% of the vinyon grain of the recycling including 60 ~ 75wt% Linear low density polyethylene (LLDPE).
Further, wherein the mineral powders be 2 ~ 3 μm of partial sizes calcium carbonate, marble, mica, gypsum or hydroxide Aluminium.
The invention has the following advantages:
Provided by the present invention disappear moulds agent constituent, and made environmental protection plastic products can be suitable for burying extensively, incinerate and decompose Processing;
Provided by the present invention disappear moulds agent constituent, and made environmental protection plastic products have the air permeability effect such as paper products;
Provided by the present invention disappear moulds agent constituent, and made environmental protection plastic products fuel value is low, and low cigarette when burning, incinerates It does not agglomerate afterwards, powder can be become after ashing completely.
Provided by the present invention disappear moulds agent constituent, and made environmental protection plastic products are recyclable to be recycled.
Specific embodiment
The following example will be further illustrated the embodiments such as other features and advantages of the present invention, but this it is merely illustrative and With not limitation of the present invention.
The present invention provides a kind of methods for moulding agent constituent that disappears for making environmental protection plastic products, disappear and mould agent constituent packet Include: vinyon grain, the first additive, Second addition and the micro lubricating agent of recycling and reusing, preparation method is by above-mentioned time Vinyon grain, the first additive, Second addition and the micro lubricating agent recycled is received, through mixing, is mediated and again through melting Molten, extruding, cooling, cutting, and be made and mould agent for disappearing for environmental protection plastic products of production.
The vinyon grain of the recycling and reusing can include the materials such as polybag, plastic foil by the plastic products recycled Expect, coarse crushing, fine crushing are carried out in crusher of making a gift to someone, small plastic tab heating stirs melting into the poly- second of liquid state by treated Alkene, and liquid state polyethylene cools the threadiness extruded into solid through extruder, then by the polyethylene of solid threadiness through cutting Grain machine-cut is cut into cooling in granular and cooling water of making a gift to someone, and gives dried recovered again after cooling.The polyethylene particles of the recycling include The high density polyethylene (HDPE) of 60 ~ 75wt% and the linear low density polyethylene (LLDPE) of 25 ~ 40wt%.
First additive is taken the photograph with the thick filler of the recycle polyethylene plastic pellet of 17 ~ 32wt% and 65 ~ 80wt% through kneading machine After the mixing of 120 ~ 180 degree of family name stirs 20 ~ 30 minutes uniformly, then be sequentially put into 1 ~ 5wt% lubricant, dispersing agent and mixing it is poly- Vinyl plastics grain, and after carrying out kneading 20 ~ 30 minutes in kneader of making a gift to someone, extrudes to pelletize and simultaneously filter, then cooling collects to produce First additive;Wherein the thick filler includes the mineral powders of 50 ~ 70wt%, the corn flour of 10 ~ 20wt%, 15 ~ 25wt% It forms mixed by the leaf powder of starch, the bran powder of 10 ~ 20wt% and 10 ~ 20wt%, can be kneaded in mixing to partial size 3 ~ 5 μm granular.Above-mentioned mineral powders can be calcium carbonate (talcum), marble, mica, gypsum or the hydrogen-oxygen of 2 ~ 3 μm of partial sizes Change aluminium.Above-mentioned lubricant can be fatty acid amide or stearate, also can be oleamide, erucic amide, zinc stearate or tristearin Sour calcium.And the first additive is made to generate aqueous vapor through resurgence process.
Second addition is taken the photograph with the thin filler of the recycle polyethylene plastic pellet of 17 ~ 32wt% and 65 ~ 80wt% through kneading machine After the mixing of 120 ~ 180 degree of family name stirs 20 ~ 30 minutes uniformly, then be sequentially put into 1 ~ 5wt% lubricant, dispersing agent and mixing it is poly- Vinyl plastics grain, and after carrying out kneading 20 ~ 30 minutes in kneader of making a gift to someone, extrudes to pelletize and simultaneously filter, then cooling collects to produce Second addition;Wherein the thin filler includes the mineral powders of 50 ~ 70wt%, the corn flour of 10 ~ 20wt%, 15 ~ 25wt% It forms mixed by the leaf powder of starch, the rice bran powder of 10 ~ 20wt% and 10 ~ 20wt%, can be kneaded in mixing to grain 1 ~ 2 μm of diameter granular.Above-mentioned mineral powders can for the calcium carbonate (talcum) of 2 ~ 3 μm of partial sizes, marble, mica, gypsum or Aluminium hydroxide.Above-mentioned lubricant can be fatty acid amide or stearate, also can for oleamide, erucic amide, zinc stearate or Calcium stearate.
By the recycle polyethylene plastic pellet of 20 ~ 80wt%, the first additive (through resurgence process) of 10 ~ 40wt%, 10 ~ The Second addition of 40wt% and micro lubricating agent, through mixing, kneading, melting, extruding, cooling and cutting granulating, and being made can make Make disappearing for environmental protection plastic products and moulds agent.
Disappeared by this and mould environmental protection plastic products made by agent, that is, including can be suitable for burying extensively, incinerate at decomposition Reason, manufactured plastic products have the air permeability effect such as paper products, low combustion value, and low cigarette when burning, do not agglomerate after incineration, ash It can become powder and other effects after change completely.
In conclusion the foregoing is merely presently preferred embodiments of the present invention, not thereby limits patent of the invention and protect Shield range, therefore made equivalence changes of description of the invention etc. such as, should all be included in protection scope of the present invention.

Claims (5)

1. a kind of method for moulding agent constituent that disappears for making environmental protection plastic products, which includes: that the recycling of 20 ~ 80wt% is poly- Vinyl plastics grain, the first additive of 10 ~ 40 wt%, the Second addition of 10 ~ 40wt% and micro lubricating agent, are kneaded, are mediated And again through melting, extruding, cooling, cutting granulating, and it is made and moulds agent for disappearing for environmental protection plastic products of production;It is characterized by: The thick filler and 1 ~ 5wt% that first additive is 3 ~ 5 μm with recycle polyethylene particle, 65 ~ 80wt% and the partial size of 17 ~ 32wt% Lubricant, dispersing agent and mix polyethylene plastic pellet, through mixing, kneading, melting, extruding, cooling, pelletize;
Second addition with recycle polyethylene particle, 65 ~ 80wt% and the partial size of 17 ~ 32wt% be 1 ~ 2 μm thin filler and 1 ~ Lubricant, dispersing agent and the mix polyethylene plastic pellet of 5wt% through mixing, kneading, melting, extruding, cooling, is pelletized;
Above-mentioned thick filler includes the mineral powders of 50 ~ 70wt%, the corn flour of 10 ~ 20wt%, the starch of 15 ~ 25wt%, 10 It is formed mixed by the bran powder of ~ 20wt% and the leaf powder of 10 ~ 20wt%;Above-mentioned thin filler includes the mineral of 50 ~ 70wt% Matter powder, the corn flour of 10 ~ 20wt%, the starch of 15 ~ 25wt%, the rice bran powder of 10 ~ 20wt% and 10 ~ 20wt% leaf powder It is mixed to form.
2. the method for moulding agent constituent that disappears of production environmental protection plastic products as described in claim 1, it is characterised in that: the lubrication Agent is fatty acid amide or stearate, or is oleamide, erucic amide, zinc stearate or calcium stearate.
3. the method for moulding agent constituent that disappears of production environmental protection plastic products as described in claim 1, it is characterised in that: the mixing It is mediated 20 ~ 30 minutes under 120 ~ 180 degree Celsius with kneader.
4. the method for moulding agent constituent that disappears of production environmental protection plastic products as described in claim 1, it is characterised in that: the recycling Vinyon grain including 60 ~ 75wt% high density polyethylene (HDPE) and 25 ~ 40wt% linear low density polyethylene (LLDPE).
5. the method for moulding agent constituent that disappears of production environmental protection plastic products as described in claim 1, it is characterised in that: the mineral Matter powder is calcium carbonate, marble, mica, gypsum or the aluminium hydroxide of 2 ~ 3 μm of partial sizes.
CN201711020118.0A 2017-10-26 2017-10-26 Make the method for moulding agent constituent that disappears of environmental protection plastic products Withdrawn CN109705425A (en)