CN109703109A - A kind of processing method of highly intensified corrugated paper - Google Patents
A kind of processing method of highly intensified corrugated paper Download PDFInfo
- Publication number
- CN109703109A CN109703109A CN201910150341.XA CN201910150341A CN109703109A CN 109703109 A CN109703109 A CN 109703109A CN 201910150341 A CN201910150341 A CN 201910150341A CN 109703109 A CN109703109 A CN 109703109A
- Authority
- CN
- China
- Prior art keywords
- parts
- paper
- corrugated paper
- processing method
- highly intensified
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a kind of processing methods of highly intensified corrugated paper, comprising the following steps: Step 1: preparing body paper paper pulp;Step 2: reinforcing agent is added into body paper paper pulp;Step 3: being heat-treated to original paper;Step 4: the surface to original paper carries out gluing processing;Step 5: compound, obtained corrugated paper is carried out to original paper by Corrugating Machine;Step 6: cooling treatment after dry, obtains highly intensified corrugated paper.Which increase the burst index of corrugated paper and ring crush indexs, so that this corrugated paper has higher intensity, improve the service life of corrugated case, meet market use demand, be conducive to product promotion.
Description
Technical field
The invention belongs to corrugated paper processing technique fields, and in particular to a kind of processing method of highly intensified corrugated paper.
Background technique
Corrugated board is the adherend of a multilayer, it is at least made of one layer of waveform core paper interlayer and a layer paperboard.
Existing corrugated paper intensity is lower, it is difficult to satisfy the use demand.
Summary of the invention
The purpose of the present invention is to propose to a kind of processing method of highly intensified corrugated paper, overcome the prior art it is above-mentioned not
Foot, which increase the burst index of corrugated paper and ring crush indexs to improve corrugated paper so that this corrugated paper has higher intensity
The service life of case meets market use demand, is conducive to product promotion.
In order to reach above-mentioned purpose of design, The technical solution adopted by the invention is as follows:
A kind of processing method of highly intensified corrugated paper, comprising the following steps:
Step 1: preparing body paper paper pulp;
Step 2: reinforcing agent is added into body paper paper pulp;
Step 3: being heat-treated to original paper;
Step 4: the surface to original paper carries out gluing processing;
Step 5: compound, obtained corrugated paper is carried out to original paper by Corrugating Machine;
Step 6: cooling treatment after dry, obtains highly intensified corrugated paper.
The body paper paper pulp includes the various composition of following mass fraction: 8 parts of agricultural crop straw, 5 parts of Hickory, and white birch
8 parts of wood, 3 parts of pear wood, 2 parts of cassia siamea.
The reinforcing agent includes 8-10 parts of polyamidoimide, 2-4 parts of polyhydroxy chemical coupling agent, phosphorous acid by weight
3-5 parts of salt, 2-5 parts of ethylene copolymer, 5-10 parts of stabilizer.
In step 4, the binder that gluing processing uses includes following components by weight: 160 parts of starch, sodium bicarbonate
15 parts, 10 parts of strong catalyst, 2 parts of zinc borate, 6 parts of ethylene glycol amine, 10 parts of toluene di-isocyanate(TDI), 3 parts of alum, defoaming agent 5
Part, 30 parts of gelatine, 3 parts of benzoyl peroxide, 8 parts of polyalcohol, 20 parts of isopropanol, 9 parts of calcium stearate, 7 parts of aluminum aluminum sulfate, yin from
5 parts of sub- surfactant, 220 parts of water.
The binder production method the following steps are included:
Water is added in step 1 in a kettle, is heated to 80-90 DEG C, then plus starch stir 6 minutes, be gelatinized;
Step 2, by sodium bicarbonate, zinc borate, ethylene glycol amine, toluene di-isocyanate(TDI), alum, gelatine, benzoyl peroxide first
Acyl, calcium stearate, aluminum aluminum sulfate, anionic surfactant are dissolved by water, are added in reaction kettle and are stirred 25 minutes;
Polyalcohol, isopropanol, defoaming agent are dissolved in boiled water in addition reaction kettle by step 3, are stirred 6 minutes, are then allowed to stand
2 minutes;
Step 4 will stir evenly in strong catalyst addition reaction kettle, and the mixture stirred evenly is then poured into ultrasound
Wave dispersion machine carries out ultrasonic wave dispersion, ultrasonic power 120-150W, and jitter time is 30-50 minutes, and dispersion temperature is
150-160 DEG C, binder is obtained after dispersion.
The catalyst includes following components by weight: 3 parts of benzoyl peroxide, 3 parts of zinc borate, polyacrylamide
1.5 parts, 1 part of potassium cyanide and 12 parts of calcium stearate.
The defoaming agent includes following components by weight: 5 parts of nonylphenol polyoxyethylene ether, is gathered 3 parts of tributyl phosphate
1.5 parts of acid imide, 2 parts of diphenyl silanediol and 1 part of petroleum sodium sulfonate.
A kind of beneficial effect of the processing method of highly intensified corrugated paper of the present invention is: which increase the resistance to of corrugated paper
Broken index and ring crush index improve the service life of corrugated case, meet city so that this corrugated paper has higher intensity
Field use demand, is conducive to product promotion.
Specific embodiment
Preferred embodiment of the invention is described in further detail below.
In embodiment of the present invention, the processing method of the highly intensified corrugated paper, comprising the following steps:
Step 1: preparing body paper paper pulp;
Step 2: reinforcing agent is added into body paper paper pulp;
Step 3: being heat-treated to original paper;
Step 4: the surface to original paper carries out gluing processing;
Step 5: compound, obtained corrugated paper is carried out to original paper by Corrugating Machine;
Step 6: cooling treatment after dry, obtains highly intensified corrugated paper.
The body paper paper pulp includes the various composition of following mass fraction: 8 parts of agricultural crop straw, 5 parts of Hickory, and white birch
8 parts of wood, 3 parts of pear wood, 2 parts of cassia siamea.
The reinforcing agent includes 8-10 parts of polyamidoimide, 2-4 parts of polyhydroxy chemical coupling agent, phosphorous acid by weight
3-5 parts of salt, 2-5 parts of ethylene copolymer, 5-10 parts of stabilizer.
In step 4, the binder that gluing processing uses includes following components by weight: 160 parts of starch, sodium bicarbonate
15 parts, 10 parts of strong catalyst, 2 parts of zinc borate, 6 parts of ethylene glycol amine, 10 parts of toluene di-isocyanate(TDI), 3 parts of alum, defoaming agent 5
Part, 30 parts of gelatine, 3 parts of benzoyl peroxide, 8 parts of polyalcohol, 20 parts of isopropanol, 9 parts of calcium stearate, 7 parts of aluminum aluminum sulfate, yin from
5 parts of sub- surfactant, 220 parts of water.
The binder production method the following steps are included:
Water is added in step 1 in a kettle, is heated to 80-90 DEG C, then plus starch stir 6 minutes, be gelatinized;
Step 2, by sodium bicarbonate, zinc borate, ethylene glycol amine, toluene di-isocyanate(TDI), alum, gelatine, benzoyl peroxide first
Acyl, calcium stearate, aluminum aluminum sulfate, anionic surfactant are dissolved by water, are added in reaction kettle and are stirred 25 minutes;
Polyalcohol, isopropanol, defoaming agent are dissolved in boiled water in addition reaction kettle by step 3, are stirred 6 minutes, are then allowed to stand
2 minutes;
Step 4 will stir evenly in strong catalyst addition reaction kettle, and the mixture stirred evenly is then poured into ultrasound
Wave dispersion machine carries out ultrasonic wave dispersion, ultrasonic power 120-150W, and jitter time is 30-50 minutes, and dispersion temperature is
150-160 DEG C, binder is obtained after dispersion.
The catalyst includes following components by weight: 3 parts of benzoyl peroxide, 3 parts of zinc borate, polyacrylamide
1.5 parts, 1 part of potassium cyanide and 12 parts of calcium stearate.
The defoaming agent includes following components by weight: 5 parts of nonylphenol polyoxyethylene ether, is gathered 3 parts of tributyl phosphate
1.5 parts of acid imide, 2 parts of diphenyl silanediol and 1 part of petroleum sodium sulfonate.
The above content is the further descriptions for combining specific preferred embodiment to be the present invention, are convenient for the skill
The technical staff in art field can understand and apply the invention, and it cannot be said that specific implementation of the invention is only limited to these instructions.
For those of ordinary skill in the art to which the present invention belongs, it can also make without departing from the inventive concept of the premise
Several simple deduction or replace, without having to go through creative labor.Therefore, those skilled in the art are according to the present invention takes off
Show, the simple modifications made to the present invention all should be within protection scope of the present invention.
Claims (7)
1. a kind of processing method of highly intensified corrugated paper, it is characterised in that: the following steps are included:
Step 1: preparing body paper paper pulp;
Step 2: reinforcing agent is added into body paper paper pulp;
Step 3: being heat-treated to original paper;
Step 4: the surface to original paper carries out gluing processing;
Step 5: compound, obtained corrugated paper is carried out to original paper by Corrugating Machine;
Step 6: cooling treatment after dry, obtains highly intensified corrugated paper.
2. the processing method of highly intensified corrugated paper according to claim 1, it is characterised in that: the body paper paper pulp include with
The various composition of lower mass fraction: 8 parts of agricultural crop straw, 5 parts of Hickory, 8 parts of white birch wood, 3 parts of pear wood, 2 parts of cassia siamea.
3. the processing method of highly intensified corrugated paper according to claim 1, it is characterised in that: the reinforcing agent is by weight
Including 8-10 parts of polyamidoimide, 2-4 parts of polyhydroxy chemical coupling agent, 3-5 parts of phosphite, 2-5 parts of ethylene copolymer, steady
Determine 5-10 parts of agent.
4. the processing method of highly intensified corrugated paper according to claim 1, it is characterised in that: in step 4, gluing processing
The binder of use includes following components by weight: 160 parts of starch, 15 parts of sodium bicarbonate, and 10 parts of strong catalyst, zinc borate
2 parts, 6 parts of ethylene glycol amine, 10 parts of toluene di-isocyanate(TDI), 3 parts of alum, 5 parts of defoaming agent, 30 parts of gelatine, benzoyl peroxide 3
Part, 8 parts of polyalcohol, 20 parts of isopropanol, 9 parts of calcium stearate, 7 parts of aluminum aluminum sulfate, 5 parts of anionic surfactant, 220 parts of water.
5. the processing method of highly intensified corrugated paper according to claim 4, it is characterised in that: the binder production side
Method the following steps are included:
Water is added in step 1 in a kettle, is heated to 80-90 DEG C, then plus starch stir 6 minutes, be gelatinized;
Step 2, by sodium bicarbonate, zinc borate, ethylene glycol amine, toluene di-isocyanate(TDI), alum, gelatine, benzoyl peroxide, hard
Resin acid calcium, aluminum aluminum sulfate, anionic surfactant are dissolved by water, are added in reaction kettle and are stirred 25 minutes;
Polyalcohol, isopropanol, defoaming agent are dissolved in boiled water in addition reaction kettle by step 3, are stirred 6 minutes, are then allowed to stand 2 points
Clock;
Step 4 will stir evenly in strong catalyst addition reaction kettle, and the mixture stirred evenly is then poured into ultrasonic wavelength-division
It dissipates machine and carries out ultrasonic wave dispersion, ultrasonic power 120-150W, jitter time is 30-50 minutes, dispersion temperature 150-160
DEG C, binder is obtained after dispersion.
6. the processing method of highly intensified corrugated paper according to claim 5, it is characterised in that: the catalyst is by weight
Part includes following components: 3 parts of benzoyl peroxide, 3 parts of zinc borate, 1.5 parts of polyacrylamide, 1 part of potassium cyanide and calcium stearate
12 parts.
7. the processing method of highly intensified corrugated paper according to claim 6, it is characterised in that: the defoaming agent is by weight
Part includes following components: 5 parts of nonylphenol polyoxyethylene ether, 3 parts of tributyl phosphate, 1.5 parts of polyimides, diphenyl silanediol 2
Part and 1 part of petroleum sodium sulfonate.