CN109622425A - 一种筛选黑斑析锂风险电芯的方法 - Google Patents
一种筛选黑斑析锂风险电芯的方法 Download PDFInfo
- Publication number
- CN109622425A CN109622425A CN201811517760.4A CN201811517760A CN109622425A CN 109622425 A CN109622425 A CN 109622425A CN 201811517760 A CN201811517760 A CN 201811517760A CN 109622425 A CN109622425 A CN 109622425A
- Authority
- CN
- China
- Prior art keywords
- battery core
- capacity
- blackspot
- voltage
- constant
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种筛选黑斑析锂风险电芯的方法,方法步骤中包含:步骤S1:将电芯放电至设定电压;步骤S2:将电芯恒流充电至特定电压,并计算电芯恒流充电过程中的充电容量,记为CC容量;步骤S3:将电芯恒压充电至特定电流,并计算电芯恒压充电过程中的充电容量,记为CV容量;步骤S4:计算CC容量的CV容量的比值,比值越小,电芯黑斑析锂风险越高。本发明可以很好、很方便地筛选出存在黑斑析锂风险的电芯。
Description
技术领域
本发明涉及一种筛选黑斑析锂风险电芯的方法。
背景技术
目前,生产的个别电芯的NCM界面存在黑斑析锂风险,NCM界面出现黑斑析锂,影响电芯的电化学性能,但存在黑斑析锂风险的电芯不易筛选,甄别。
发明内容
本发明所要解决的技术问题是克服现有技术的缺陷,提供一种筛选黑斑析锂风险电芯的方法,它可以很好、很方便地筛选出存在黑斑析锂风险的电芯。
为了解决上述技术问题,本发明的技术方案是:一种筛选黑斑析锂风险电芯的方法,方法步骤中包含:
步骤S1:将电芯放电至设定电压;
步骤S2:将电芯恒流充电至特定电压,并计算电芯恒流充电过程中的充电容量,记为CC容量;
步骤S3:将电芯恒压充电至特定电流,并计算电芯恒压充电过程中的充电容量,记为CV容量;
步骤S4:计算CC容量的CV容量的比值,比值越小,电芯黑斑析锂风险越高。
进一步,步骤S1中,设定电压为2.8V;
步骤S2中,特定电压为4.3V;
步骤S3中,特定电流为0.05C。
进一步,在步骤S1和步骤S2之间,还包括静置电芯10s。
进一步为了消除极化影响,步骤S2中包含:
步骤S21:将电芯恒流充电至特定电压;
步骤S22:静置2min;
步骤S23:再将电芯恒流充电至特定电压;
步骤S24:计算电芯恒流充电过程中的充电容量,记为CC容量。
进一步,步骤S4之后,还包括:
步骤S5:将多个电芯的CC容量与CV容量的比值做散点分布图,根据散点分布图,筛选黑斑析锂风险电芯,CC容量与CV容量的比值在散点分布图中为偏低散点的电芯,为黑斑析锂风险电芯。
采用了上述技术方案后,电芯在充电过程中,如果界面出现黑斑析锂,恒流充电时,锂离子嵌入石墨极化大,达到特定电压时需要的充电容量较少,恒压充电过程中,充电电流较小,相对极化较小,达到特定电流可以充电的容量较高;相同设计的电芯,可以通过CC和CV容量的比值反应电芯极化大小,比值越小说明极化越大,黑斑析锂风险越高,本发明可以很好地筛选出存在黑斑析锂风险的电芯,方便快捷,进而保证电芯的电化学性能。
具体实施方式
为了使本发明的内容更容易被清楚地理解,下面根据具体实施例,对本发明作进一步详细的说明。
一种筛选黑斑析锂风险电芯的方法,方法步骤中包含:
步骤S1:将电芯放电至设定电压;
步骤S2:将电芯恒流充电至特定电压,并计算电芯恒流充电过程中的充电容量,记为CC容量;
步骤S3:将电芯恒压充电至特定电流,并计算电芯恒压充电过程中的充电容量,记为CV容量;
步骤S4:计算CC容量的CV容量的比值,比值越小,电芯黑斑析锂风险越高。
步骤S1中,设定电压为2.8V;
步骤S2中,特定电压为4.3V;
步骤S3中,特定电流为0.05C。
在步骤S1和步骤S2之间,还包括静置电芯10s。
为了消除极化影响,步骤S2中包含:
步骤S21:将电芯恒流充电至特定电压;
步骤S22:静置2min;
步骤S23:再将电芯恒流充电至特定电压;
步骤S24:计算电芯恒流充电过程中的充电容量,记为CC容量。
步骤S4之后,还包括:
步骤S5:将多个电芯的CC容量与CV容量的比值做散点分布图,根据散点分布图,筛选黑斑析锂风险电芯,CC容量与CV容量的比值在散点分布图中为偏低散点的电芯,为黑斑析锂风险电芯。
本发明的工作原理如下:
电芯在充电过程中,如果界面出现黑斑析锂,恒流充电时,锂离子嵌入石墨极化大,达到特定电压时需要的充电容量较少,恒压充电过程中,充电电流较小,相对极化较小,达到特定电流可以充电的容量较高;相同设计的电芯,可以通过CC和CV容量的比值反应电芯极化大小,比值越小说明极化越大,黑斑析锂风险越高,本发明可以很好地筛选出存在黑斑析锂风险的电芯,方便快捷,进而保证电芯的电化学性能。
以上所述的具体实施例,对本发明解决的技术问题、技术方案和有益效果进行了进一步详细说明,所应理解的是,以上所述仅为本发明的具体实施例而已,并不用于限制本发明,凡在本发明的精神和原则之内,所做的任何修改、等同替换、改进等,均应包含在本发明的保护范围之内。
Claims (5)
1.一种筛选黑斑析锂风险电芯的方法,其特征在于,方法步骤中包含:
步骤S1:将电芯放电至设定电压;
步骤S2:将电芯恒流充电至特定电压,并计算电芯恒流充电过程中的充电容量,记为CC容量;
步骤S3:将电芯恒压充电至特定电流,并计算电芯恒压充电过程中的充电容量,记为CV容量;
步骤S4:计算CC容量的CV容量的比值,比值越小,电芯黑斑析锂风险越高。
2.根据权利要求1所述的一种筛选黑斑析锂风险电芯的方法,其特征在于:
步骤S1中,设定电压为2.8V;
步骤S2中,特定电压为4.3V;
步骤S3中,特定电流为0.05C。
3.根据权利要求1所述的一种筛选黑斑析锂风险电芯的方法,其特征在于:
在步骤S1和步骤S2之间,还包括静置电芯10s。
4.根据权利要求1所述的一种筛选黑斑析锂风险电芯的方法,其特征在于:步骤S2中包含:
步骤S21:将电芯恒流充电至特定电压;
步骤S22:静置2min;
步骤S23:再将电芯恒流充电至特定电压;
步骤S24:计算电芯恒流充电过程中的充电容量,记为CC容量。
5.根据权利要求1所述的一种筛选黑斑析锂风险电芯的方法,其特征在于:步骤S4之后,还包括:
步骤S5:将多个电芯的CC容量与CV容量的比值做散点分布图,根据散点分布图,筛选黑斑析锂风险电芯,CC容量与CV容量的比值在散点分布图中为偏低散点的电芯,为黑斑析锂风险电芯。