CN109441078A - A kind of thermal-insulating type stone material or ceramic tile paste mosaic technology - Google Patents

A kind of thermal-insulating type stone material or ceramic tile paste mosaic technology Download PDF

Info

Publication number
CN109441078A
CN109441078A CN201811459860.6A CN201811459860A CN109441078A CN 109441078 A CN109441078 A CN 109441078A CN 201811459860 A CN201811459860 A CN 201811459860A CN 109441078 A CN109441078 A CN 109441078A
Authority
CN
China
Prior art keywords
ceramic tile
ash
wet
dry ash
dry
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201811459860.6A
Other languages
Chinese (zh)
Inventor
杨志朝
王金龙
季海峰
符海蓉
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Da Hong Point Commercial Decoration Engineering (shenzhen) Co Ltd
Original Assignee
Da Hong Point Commercial Decoration Engineering (shenzhen) Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Da Hong Point Commercial Decoration Engineering (shenzhen) Co Ltd filed Critical Da Hong Point Commercial Decoration Engineering (shenzhen) Co Ltd
Priority to CN201811459860.6A priority Critical patent/CN109441078A/en
Publication of CN109441078A publication Critical patent/CN109441078A/en
Pending legal-status Critical Current

Abstract

Mosaic technology is pasted the invention discloses a kind of thermal-insulating type stone material or ceramic tile, is related to technical field of building construction.The technique specifically includes that S1 land clearing;S2 is equipped with dry ash;S3 is equipped with wet ash;S4 soaks brick;S5 smears dry ash;S6 smears wet ash;S7 is laid with ceramic tile.The present invention has the following advantages and effects: when pasting ceramic tile, after dry ash being applied on wet ground, dry ash open up flat, then wet ash is applied on wet ceramic tile again, the ceramic tile for filling wet ash is placed on dry ash again, finally taps ceramic tile surface using rubber hammer.When dry ash and wet ash hardening, sticky wet ash will flow to ground along the gap of dry ash, and dry ash and ceramic tile are fixed on ground by the wet ash of high bond strength at this time, ceramic tile is avoided hollowing and obscission occur, has achieved the effect that improve cohesive force.

Description

A kind of thermal-insulating type stone material or ceramic tile paste mosaic technology
Technical field
The present invention relates to technical field of building construction, in particular to a kind of thermal-insulating type stone material or ceramic tile paste bed setter Skill.
Background technique
Ceramic tile is the metal oxide and half-metal oxide with fire resisting, via grinding, mixing, compacting, glazing, is sintered it Process, and the building or ornament materials of a kind of porcelain of the acid and alkali-resistance formed or stone matter, raw material are mostly by clay, quartz sand etc. Etc. mixing.
Ceramic tile is usually directly carried out stickup fixation using cement mortar in sticking construction by traditional stone material or ceramic tile, It is easy to appear hollowings and obscission for ceramic tile.By investigation, between ceramic tile and cement mortar or cement mortar and ground Cohesive force will directly affect whether it hollowing and obscission occurs, therefore, design a kind of applying for cohesive force improved between the two Work method is particularly important.
Summary of the invention
Mosaic technology is pasted the object of the present invention is to provide a kind of thermal-insulating type stone material or ceramic tile, has and improves cohesive force Effect.
Above-mentioned technical purpose of the invention has the technical scheme that a kind of thermal-insulating type stone material or ceramic tile Paste mosaic technology, it is characterised in that: include the following steps,
S1: the rubble on ground is cleared up in land clearing, and water spray moistens ground;
S2: with dry ash, after water, cement and fine sand are mixed, stirs evenly spare;
S3: with wet ash, after water and cement mixing, stirs evenly spare;
S4: ceramic tile is placed in water tank and impregnates by leaching brick;
S5: dry ash is smeared, dry ash is laid in ground, and flatten to dry ash;
S6: smearing wet ash, and wet ash is uniformly filled to the back side of ceramic tile;
S7: being laid with ceramic tile, ceramic tile be layed on dry ash, taps ceramic tile surface using rubber hammer.
By using above-mentioned technical proposal, when pasting ceramic tile, after dry ash being applied on wet ground, to dry ash into Row is opened up flat, then wet ash is applied on wet ceramic tile again, then the ceramic tile for filling wet ash is placed on dry ash, is finally utilized Rubber hammer taps ceramic tile surface.When dry ash and wet ash hardening, sticky wet ash will flow to ground along the gap of dry ash, this When dry ash and ceramic tile be fixed on by ground by the wet ash of high bond strength, avoid ceramic tile from hollowing and obscission occur, reach The effect for improving cohesive force is arrived.
The further setting of the present invention are as follows: S41 is provided between S4 and S5, S41 is as follows,
S41: ceramic tile is layed on dry ash by flatness detection, after tapping ceramic tile surface using rubber hammer, recycles horizontal ruler pair The flatness of ceramic tile surface is detected;If flatness is qualified, S5 is carried out;If flatness is unqualified, S41 is carried out again.
By using above-mentioned technical proposal, when being laid with ceramic tile, the flatness of ceramic tile surface, and root are measured using horizontal ruler After being adjusted according to the reading on horizontal ruler to dry ash surface, it is ensured that ceramic tile may be at horizontality after being laid with, then by wet ash The ceramic tile back side is smeared, and then guarantees to avoid repeatedly doing over again and cause the waste of dry ash and wet ash with one-pass molding when tile paste.
The further setting of the present invention are as follows: S11 is provided between S1 and S2, S11 is as follows,
S11:UV putty and UV priming paint even roll, first by the roller coating of UV putty on ground, after UV putty semi-solid preparation, the bottom direct roller coating UV Paint.
It, can because UV putty and UV priming paint can permeate in hole to the ground by using above-mentioned technical proposal To close to hole, the flatness on ground is improved, can also effectively improve the adhesion effect on dry ash and ground, is promoted dry The adhesive force of ash while improving cohesive force between the two, leads to porcelain after can also effectively avoiding dry ash that sinking phenomenon occurs There is hollowing or obscission in brick.
The further setting of the present invention are as follows: in S2, water, cement and fine sand carry out mixing outfit by the volume ratio of 1:1:5.
By using above-mentioned technical proposal, because the cement in dry ash can be caused because water is lacked if dry ash overdrying Cement cannot be sufficiently hardened, and the moisture in wet ash can quickly be absorbed by dry ash at this time, be easy to cause hollowing phenomenon.But dry ash mistake If wet, volume can slightly reduce after dry ash is stiff, it is also possible to will cause hollowing phenomenon.Therefore by aforementioned proportion by water, After cement and fine sand mixing, so that dry ash is in partial desiccation state, just dry ash just reaches overdrying and critical point overly moist Between, and then can effectively avoid ceramic tile from hollowing phenomenon occur, reach raising cohesive force effect.
The further setting of the present invention are as follows: in S3, water is carried out mixing outfit with cement by the volume ratio of 1:1.
It, will because a large amount of cement fragment will be contained in wet ash if wet ash overdrying by using above-mentioned technical proposal It will lead to wet ash and gage distortion phenomenon occur, after wet ash is dry, be easy to cause porcelain since the shrinkage stress of wet ash is inconsistent There is hollowing phenomenon in brick.But if wet ash is overly moist, it will cause the cohesive force between dry ash and ceramic tile to reduce, and work as wet ash After air-drying, wet ash will not play cementation, and then ceramic tile is caused break-off occur.And wet ash also takes a long time Can be stiff, extend the construction period.Therefore after being mixed water with cement by aforementioned proportion, so that wet ash is in thick State, and not cement fragment in wet ash, and then can effectively avoid ceramic tile from hollowing or obscission occur, reach raising Cohesive force effect, while the construction period can also be shortened.
The further setting of the present invention are as follows: in S4, ceramic tile is immersed in the water on the day before mentioning before stickup, and is pasted Preceding 1-2h, which is pulled out and stood up, to dry in the shade.
By using above-mentioned technical proposal, because in ceramic tile there is a large amount of hole first to soak ceramic tile before stickup Bubble, so that the hole in ceramic tile fully absorbs moisture.After absorbing sufficient moisture, then wet ash is spread, is just unlikely to blot porcelain Moisture in brick, thus can effectively avoid ceramic tile occur hollowing, fall off, crackle phenomena such as, and then reached raising cohesive force And the effect to prolong the service life.
The further setting of the present invention are as follows: it further include S8, S8 is as follows,
S8: jointing injects jointing agent in the gap between ceramic tile, then with flexible cloth by gap and the jointing agent of ceramic tile surface It cleans.
By using above-mentioned technical proposal, after jointing is handled, cohesive force, antiseepage, the cracking resistance between ceramic tile can be improved Function, and the service life of ceramic tile is influenced after can preventing hydrone from penetrating into the ceramic tile back side.And jointing agent is with certain soft Toughness, and then the slight shift of ceramic tile can be resisted, prevent ceramic tile from deforming or falling off, further extend ceramic tile uses the longevity Life.
The further setting of the present invention are as follows: S71 is provided between S7 and S8, S71 is as follows,
S71: joint filling injects the anti-knock agent being let down in the gap between ceramic tile.
By using above-mentioned technical proposal, because anti-knock agent can effectively fill the eyelet in dry ash and wet ash, resistance Below the ceramic tile with the circulation of the moisture of top, therefore when carrying out jointing processing to ceramic tile, first spray anti-knock agent to eyelet into Row filling, then carries out jointing processing again, and then position is filled up the defects of to eyelet, avoids what sinking occurred in jointing agent from showing As.
The further setting of the present invention are as follows: 6-7h is spaced between S71 and S8.
Anti-knock agent is allowed uniformly to penetrate into hole intraocular and right by standing 6-7h by using above-mentioned technical proposal Eyelet is thoroughly filled, so improve dry ash and it is wet ash between consolidation degree, effectively improve itself and jointing agent it Between cohesive force, avoid ceramic tile from hollowing and obscission occur.
In conclusion the invention has the following advantages:
1. sticky wet ash flow to ground along the hole between dry ash when dry ash and wet ash hardening, pass through high bonding at this time Dry ash and ceramic tile are fixed on ground by the wet ash of intensity, and ceramic tile is avoided hollowing and obscission occur, have reached raising bonding The effect of power;
2. improving the adhesion effect of dry ash and ground by roller coating UV putty and UV priming paint on ground again, promoting the attachment of dry ash Power improves cohesive force between the two, causes ceramic tile hollowing or obscission occur after avoiding dry ash that sinking phenomenon occurs;
3. by wet ash and dry ash that certain ratio is arranged, so that dry ash is between overdrying and critical point overly moist, together When make wet ash not cement fragment in viscous pasty state and wet ash, effectively avoid ceramic tile from hollowing or break-off occur, The construction period can also effectively be shortened simultaneously;
4. improving the cohesive force and seepage control and crack resistance function between ceramic tile after handling by setting jointing, that improves ceramic tile uses the longevity Life;
5. filling the eyelet in dry ash and wet ash by setting anti-knock agent, the circulation below ceramic tile with the moisture of top is obstructed, Avoid jointing agent that sinking phenomenon occurs.
Detailed description of the invention
Fig. 1 is the process schematic representation of embodiment.
Specific embodiment
Below in conjunction with attached drawing, invention is further described in detail.
As shown in Figure 1, a kind of thermal-insulating type stone material or ceramic tile paste mosaic technology, include the following steps,
S1: the rubble on ground is cleared up in land clearing, and water spray moistens ground.
S11:UV putty and UV priming paint even roll, first by the roller coating of UV putty on ground, after UV putty semi-solid preparation, direct roller coating UV priming paint.
S2: it is equipped with dry ash, after water, cement and fine sand are mixed by the volume ratio of 1:1:5, is stirred evenly spare.
S3: with wet ash, after water is mixed with cement by the volume ratio of 1:1, stirs evenly spare.
When dry ash overdrying, the cement in dry ash can cause cement that cannot be sufficiently hardened because water is lacked, at this time wet ash In moisture can quickly be absorbed by dry ash, be easy to cause hollowing phenomenon.When wet grey overdrying, a large amount of water will be contained in wet ash Mud fragment, it will cause wet ash gage distortion phenomenon occur, therefore after wet ash hardening, since the shrinkage stress of wet ash is different It causes, ceramic tile is also easy to cause hollowing phenomenon occur.
When dry ash is overly moist, volume can slightly reduce after dry ash is stiff, it is also possible to will cause hollowing phenomenon.When wet grey mistake If wet, it will cause the cohesive force between dry ash and ceramic tile to reduce, and after wet ash air-dries, wet ash will not play bonding and make With, and then ceramic tile is caused break-off occur.And wet overly moist also take a long time of ash could be stiff, extends construction work Phase.
Therefore water, cement and fine sand be equipped to by dry ash by the volume ratio of 1:1:5, by the volume of 1:1 by water and Cement is equipped to wet ash, so that dry ash is in partial desiccation state, wet ash is in viscous pasty state and internal not cement fragment, in turn It can effectively avoid ceramic tile from hollowing or obscission occur, while the construction period can also be shortened.
Because UV putty and UV priming paint can permeate in hole to the ground, the hole on ground can be sealed It closes, improves the flatness on ground, can also effectively improve the adhesion effect on dry ash and ground, promote the adhesive force of dry ash, mention While high cohesive force between the two, ceramic tile is caused hollowing or de- occur after can also effectively avoiding dry ash that sinking phenomenon occurs Fall phenomenon.
S4: ceramic tile is immersed in the water by leaching brick on the day before mentioning, and is pasted preceding 1-2h and pulled out and stand up and dry in the shade, so that ceramic tile In wet inside and dry outside state.
S41: ceramic tile is layed on dry ash by flatness detection, after tapping ceramic tile surface using rubber hammer, is recycled horizontal Ruler detects the flatness of ceramic tile surface;If flatness is qualified, S5 is carried out;If flatness is unqualified, S41 is carried out again.
S5: dry ash is smeared, dry ash is laid in ground, and flatten to dry ash.
S6: smearing wet ash, and wet ash is uniformly filled to the back side of ceramic tile.
S7: being laid with ceramic tile, ceramic tile be layed on dry ash, taps ceramic tile surface using rubber hammer.
By impregnating for a long time, so that the hole in ceramic tile fully absorbs moisture, after absorbing sufficient moisture, then smear Upper wet ash, is just unlikely to blot moisture in ceramic tile, thus can effectively avoid ceramic tile occur hollowing, fall off, crackle phenomena such as.
When pasting ceramic tile, after first dry ash is applied on wet ground, then dry ash open up flat, dry ash is compacted. Then ceramic tile is layed on dry ash, recycles the flatness of horizontal ruler measurement ceramic tile surface, and according to the reading on horizontal ruler After being adjusted to dry ash surface, until after ceramic tile surface is fully horizontal, then ceramic tile lightly removed spare.
Then wet ash is applied on wet ceramic tile again, the ceramic tile for filling wet ash is placed on dry ash, is finally utilized Rubber hammer taps ceramic tile surface, is fixed on dry ash so that ceramic tile is firm.When dry ash and wet ash hardening, sticky wet ash Gradually it will be flow to ground along the gap of dry ash, dry ash and ceramic tile are fixed on ground by the wet ash of high bond strength at this time Face, the stickup for completing ceramic tile are laid with.
S71: the anti-knock agent being let down is injected in the gap between ceramic tile, stands 6-7h by joint filling.
S8: jointing injects jointing agent in the gap between ceramic tile, then with flexible cloth by gap and the hook of ceramic tile surface Seam agent is cleaned.
Because anti-knock agent can effectively fill the eyelet in dry ash and wet ash, the moisture of barrier ceramic tile lower section and top Circulation, therefore when to ceramic tile carry out jointing processing when, first spray anti-knock agent eyelet is filled, then carry out at jointing again Reason avoids jointing agent from sagging phenomenon occur.
Again because jointing agent can effectively improve cohesive force and seepage control and crack resistance function between ceramic tile, and can prevent Hydrone penetrates into the service life of influence ceramic tile behind the ceramic tile back side.Jointing agent also has certain flexibility, and then can resist porcelain The slight shift of brick prevents ceramic tile from deforming or falling off.
Specific embodiment is only explanation of the invention, is not limitation of the present invention, those skilled in the art It can according to need the modification that not creative contribution is made to the present embodiment after reading this specification, but as long as in this hair All by the protection of Patent Law in bright scope of the claims.

Claims (9)

1. a kind of thermal-insulating type stone material or ceramic tile paste mosaic technology, it is characterised in that: include the following steps,
S1: the rubble on ground is cleared up in land clearing, and water spray moistens ground;
S2: with dry ash, after water, cement and fine sand are mixed, stirs evenly spare;
S3: with wet ash, after water and cement mixing, stirs evenly spare;
S4: ceramic tile is placed in water tank and impregnates by leaching brick;
S5: dry ash is smeared, dry ash is laid in ground, and flatten to dry ash;
S6: smearing wet ash, and wet ash is uniformly filled to the back side of ceramic tile;
S7: being laid with ceramic tile, ceramic tile be layed on dry ash, taps ceramic tile surface using rubber hammer.
2. a kind of thermal-insulating type stone material according to claim 1 or ceramic tile paste mosaic technology, it is characterised in that: S4 and S5 Between be provided with S41, S41 is as follows,
S41: ceramic tile is layed on dry ash by flatness detection, after tapping ceramic tile surface using rubber hammer, recycles horizontal ruler pair The flatness of ceramic tile surface is detected;If flatness is qualified, S5 is carried out;If flatness is unqualified, S41 is carried out again.
3. a kind of thermal-insulating type stone material according to claim 1 or ceramic tile paste mosaic technology, it is characterised in that: S1 and S2 Between be provided with S11, S11 is as follows,
S11:UV putty and UV priming paint even roll, first by the roller coating of UV putty on ground, after UV putty semi-solid preparation, the bottom direct roller coating UV Paint.
4. a kind of thermal-insulating type stone material according to claim 1 or ceramic tile paste mosaic technology, it is characterised in that: in S2, Water, cement and fine sand carry out mixing outfit by the volume ratio of 1:1:5.
5. a kind of thermal-insulating type stone material according to claim 4 or ceramic tile paste mosaic technology, it is characterised in that: in S3, Water is carried out mixing outfit with cement by the volume ratio of 1:1.
6. a kind of thermal-insulating type stone material according to claim 1 or ceramic tile paste mosaic technology, it is characterised in that: in S4, Ceramic tile is immersed in the water on the day before mentioning before stickup, and is pasted preceding 1-2h and pulled out and stand up and dry in the shade.
7. a kind of thermal-insulating type stone material according to claim 1 or ceramic tile paste mosaic technology, it is characterised in that: further include S8, S8 are as follows,
S8: jointing injects jointing agent in the gap between ceramic tile, then with flexible cloth by gap and the jointing agent of ceramic tile surface It cleans.
8. a kind of thermal-insulating type stone material according to claim 7 or ceramic tile paste mosaic technology, it is characterised in that: S7 and S8 Between be provided with S71, S71 is as follows,
S71: joint filling injects the anti-knock agent being let down in the gap between ceramic tile.
9. a kind of thermal-insulating type stone material according to claim 8 or ceramic tile paste mosaic technology, it is characterised in that: S71 with 6-7h is spaced between S8.
CN201811459860.6A 2018-11-30 2018-11-30 A kind of thermal-insulating type stone material or ceramic tile paste mosaic technology Pending CN109441078A (en)