CN109352982A - A kind of tow sides applique process - Google Patents

A kind of tow sides applique process Download PDF

Info

Publication number
CN109352982A
CN109352982A CN201811403923.6A CN201811403923A CN109352982A CN 109352982 A CN109352982 A CN 109352982A CN 201811403923 A CN201811403923 A CN 201811403923A CN 109352982 A CN109352982 A CN 109352982A
Authority
CN
China
Prior art keywords
mold
applique
bowl
former
formpiston
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201811403923.6A
Other languages
Chinese (zh)
Inventor
张万龙
吕少飞
张高桢
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Hezhou Baoxing New Materials Co Ltd
Original Assignee
Hezhou Baoxing New Materials Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Hezhou Baoxing New Materials Co Ltd filed Critical Hezhou Baoxing New Materials Co Ltd
Priority to CN201811403923.6A priority Critical patent/CN109352982A/en
Publication of CN109352982A publication Critical patent/CN109352982A/en
Pending legal-status Critical Current

Abstract

The invention discloses a kind of tow sides applique processes, technical points include the first mold and the second mold for being equipped with former and formpiston, the formpiston of the former of first mold and the second mold is arranged in the same lower die, the former of the formpiston of first mold and the second mold is arranged in the same upper mold, its applique process uses following steps: S1, sprinkling light powder in the former of the first mold and sticks marble paper, then the bowl tool of non-applique is put into the first mold;S2, the bowl tool of non-applique is put on the formpiston of the second mold, sticks marble paper on bowl tool surface and is sprinkled with light powder;S3, molding temperature-pressure form the semi-finished product of a wherein face applique;S4, the semi-finished product location swap in the first mold and the second mold, repeat step S1 and S2 to the another side that bowl has;S5, molding temperature-pressure forms the finished product of the equal applique in two sides again.The present invention can carry out applique to two or more bowl tools simultaneously, improve the efficiency of batch production.

Description

A kind of tow sides applique process
Technical field
The present invention relates to a kind of applique processes, more specifically to a kind of tow sides applique process.
Background technique
Currently, in order to make bowl tool used in daily life be not easy to break into pieces, and can be more beautiful, now with melamine system Make bowl tool, and applique is carried out to its surface, can have surface in bowl in this way and form protective film, melamine bowl tool can not also be allowed straight It connects and is contacted with food.But existing applique process is wherein to stick marble paper on one side to what bowl had while melamine molding, Another side needs bowl tool to suck up puts marble paper on mold again, this, which will have bowl, singly processes, and especially two There is apparent indent in face, is otherwise easy to make marble paper to be attached on mold on bowl tool, therefore production efficiency is low, cannot be to more A bowl of tool simultaneous processing production.
Summary of the invention
The present invention provides a kind of tow sides appliquers that can quickly carry out multiple bowls of two sides applique, energy tool simultaneous processings Skill.
To achieve the above object, a kind of tow sides applique process provided by the invention, including it is equipped with former and formpiston The first mold and the second mold, the formpiston of the former of the first mold and the second mold is arranged in the same lower die, the first mould The former of the formpiston of tool and the second mold is arranged in the same upper mold, and applique process uses following steps:
S1, light powder is sprinkled in the former of the first mold and sticks marble paper, then the bowl tool of non-applique is put into the first mold In;
S2, the bowl tool of non-applique is put on the formpiston of the second mold, sticks marble paper on bowl tool surface and is sprinkled with light powder;
S3, molding temperature-pressure form the semi-finished product of a wherein face applique;
S4, the semi-finished product location swap in the first mold and the second mold, to the another side that bowl has repeat step S1 and S2;
S5, molding temperature-pressure forms the finished product of the equal applique in two sides again.
It further, further include preparation process S0 before step S1, specifically:
S01, the first mold and the second mold are preheated to 150 DEG C~180 DEG C;
S02, appropriate melamine is placed on the bowl that the non-applique of temperature-pressure formation is molded in the first mold and the second mold Tool;
S03, to have size size that decal paper is cut into needs according to bowl spare.
Further, in step S02, melamine powder raw material is put into before mold, to melamine raw material preheating to 40 DEG C~ 50 DEG C, the time is 30~40s.
Further, in step S3, S5 and S02, molding is heated up to 160 DEG C~190 DEG C.
Further, in step S3, S5 and S02, molding is forced into 100MPa~200MPa.
Further, in step S3 and S5, the time for molding temperature-pressure is 0.5~3s.
Further, in step S02, the time for molding temperature-pressure is 15~40s.
Beneficial effect
Compared with prior art, the invention has the following advantages that
1, the present invention is the process for having two-sided applique to melamine bowl, can efficiently complete the Double-face adhesive of bowl tool Flower, and multiple bowls of tools can be processed together simultaneously, it avoids the issuable marble paper of the prior art and bowl from having surface and is detached from, especially It is that bowl tool two sides has apparent indent, this method can more ideally be such that marble paper is bonded with bowl tool surface;
2, applique process directly can carry out step of the invention on the molding bowl tool of melamine, without preheating again, benefit Marble paper can be preferably set to be bonded with its surface with the residual temperature of molding bowl tool;
3, it when carrying out melamine molding, needs to avoid mold and material preheater unexpected temperature-pressure and make bowl Tool cracks, and leads to defect ware occur.
Detailed description of the invention
Fig. 1 is mold sections schematic diagram of the invention.
In figure: 1, the first mold;2, the second mold.
Specific embodiment
With reference to the accompanying drawing, specific embodiments of the present invention will be described in detail, it is to be understood that guarantor of the invention Shield range is not limited by the specific implementation.
Embodiment 1
The embodiment of the present invention is such that as shown in Figure 1, a kind of tow sides applique process, including is equipped with former With the first mold 1 and the second mold 2 of formpiston, the formpiston of the former of the first mold 1 and the second mold 2 is arranged in the same lower die On, the former of the formpiston of the first mold 1 and the second mold 2 is arranged in the same upper mold, and applique process uses following steps:
S1, the former in the first mold 1 sprinkle light powder and stick marble paper, then the bowl tool of non-applique is put into the first mold In 1;
S2, the bowl tool of non-applique is put on the formpiston of the second mold 2, sticks marble paper on bowl tool surface and is sprinkled with light powder;
S3, molding temperature-pressure form the semi-finished product of a wherein face applique;
S4, the semi-finished product location swap in the first mold 1 and the second mold 2, repeat step S1 to the another side that bowl has And S2;
S5, molding temperature-pressure forms the finished product of the equal applique in two sides again.
The present invention is the process for having two-sided applique to melamine bowl, can efficiently complete the two-sided applique of bowl tool, And multiple bowls of tools can be processed together simultaneously, it avoids the issuable marble paper of the prior art and bowl from having surface and is detached from, especially There is apparent indent on bowl tool two sides, by the way that marble paper is directly attached to surface, marble paper and bowl can more ideally be made to have surface patch It closes.
It in the present embodiment, further include preparation process S0 before step S1, specifically:
S01, the first mold 1 and the second mold 2 are preheated to 150 DEG C~180 DEG C;
S02, appropriate melamine is placed on the non-applique of molding temperature-pressure formation in the first mold 1 and the second mold 2 Bowl tool;
S03, to have size size that decal paper is cut into needs according to bowl spare.
Above-mentioned preparation process S0 is carried out before applique, so that melamine is shaped to bowl tool model, then the step of applique S1~S5 can be carried out directly on also uncooled mold, without preheating again to mold, procedure of processing be reduced, into one Step improves efficiency.And in preparation process, marble paper size is prepared according to molded bowl tool, avoids size from not corresponding to, phase Than the applique simultaneously in form in the prior art with melamine the step of, it is avoided that a bowl tool size is reduced and makes marble paper when molding Size is not suitable for, especially for recess.
In step S02, melamine powder raw material is put into before mold, to melamine raw material preheating to 40 DEG C~50 DEG C, the time For 30~40s.When carrying out melamine molding, need to avoid mold and material preheater unexpected temperature-pressure and make bowl Tool cracks, and leads to defect ware occur.
In the present embodiment, in step S3, S5 and S02, molding is heated up to 160 DEG C~190 DEG C, and molding is forced into 100MPa~200MPa.In step S3 and S5, the time for molding temperature-pressure is 0.5~3s.In step S02, molding adds The time of temperature pressurization is 15~40s.10 DEG C or so of temperature when practical heating is higher than preheating, the temperature of promotion can preferably make bowl Tool forms and sticks marble paper, and pressurization cannot be excessive, and the time can not be too long, avoids marble paper cracked, and when bowl tool molding The temperature-pressure time can be relatively long, be further divided into two to completing three times, reinforce melamine further.
The above is only the preferred embodiment of the present invention, it should be pointed out that for those skilled in the art, is not taking off Under the premise of from structure of the invention, also in advance to make several modifications and improvements, these all will not influence the effect that the present invention is implemented And patent practicability.

Claims (7)

1. a kind of tow sides applique process, which is characterized in that the first mold (1) and second including being equipped with former and formpiston Mold (2), the former of the first mold (1) and the formpiston of the second mold (2) are arranged in the same lower die, the first mold (1) The former of formpiston and the second mold (2) is arranged in the same upper mold, and applique process uses following steps:
S1, light powder is sprinkled in the former of the first mold (1) and sticks marble paper, then the bowl tool of non-applique is put into the first mold (1) in;
S2, the bowl tool of non-applique is put on the formpiston of the second mold (2), sticks marble paper on bowl tool surface and is sprinkled with light powder;
S3, molding temperature-pressure form the semi-finished product of a wherein face applique;
S4, the semi-finished product location swap in the first mold (1) and the second mold (2), repeat step S1 to the another side that bowl has And S2;
S5, molding temperature-pressure forms the finished product of the equal applique in two sides again.
2. a kind of tow sides applique process according to claim 1, which is characterized in that further include standard before step S1 Standby step S0, specifically:
S01, the first mold (1) and the second mold (2) are preheated to 150 DEG C~180 DEG C;
S02, appropriate melamine is placed on the non-applique of molding temperature-pressure formation in the first mold (1) and the second mold (2) Bowl tool;
S03, to have size size that decal paper is cut into needs according to bowl spare.
3. a kind of tow sides applique process according to claim 2, which is characterized in that in step S02, melamine is former Material is put into before mold, and to melamine raw material preheating to 40 DEG C~50 DEG C, the time is 30~40s.
4. a kind of tow sides applique process according to claim 2, which is characterized in that in step S3, S5 and S02, Molding is heated up to 160 DEG C~190 DEG C.
5. a kind of tow sides applique process according to claim 4, which is characterized in that in step S3, S5 and S02, Molding is forced into 100MPa~200MPa.
6. a kind of tow sides applique process according to claim 5, which is characterized in that in step S3 and S5, molding The time of temperature-pressure is 0.5~3s.
7. a kind of tow sides applique process according to claim 5, which is characterized in that in step S02, molding heating The time of pressurization is 15~40s.
CN201811403923.6A 2018-11-23 2018-11-23 A kind of tow sides applique process Pending CN109352982A (en)