CN109138480A - Historical building exterior wall granitic plaster painting metope does aging method - Google Patents

Historical building exterior wall granitic plaster painting metope does aging method Download PDF

Info

Publication number
CN109138480A
CN109138480A CN201811062346.9A CN201811062346A CN109138480A CN 109138480 A CN109138480 A CN 109138480A CN 201811062346 A CN201811062346 A CN 201811062346A CN 109138480 A CN109138480 A CN 109138480A
Authority
CN
China
Prior art keywords
colorant match
granitic plaster
color
exterior wall
metope
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201811062346.9A
Other languages
Chinese (zh)
Other versions
CN109138480B (en
Inventor
王辉平
连珍
陈莹
张斌
王利雄
刘淳
陈帅
朱辉
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shanghai Building Decoration Engineering Group Co Ltd
Original Assignee
Shanghai Building Decoration Engineering Group Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shanghai Building Decoration Engineering Group Co Ltd filed Critical Shanghai Building Decoration Engineering Group Co Ltd
Priority to CN201811062346.9A priority Critical patent/CN109138480B/en
Publication of CN109138480A publication Critical patent/CN109138480A/en
Application granted granted Critical
Publication of CN109138480B publication Critical patent/CN109138480B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

Aging method is done the present invention provides a kind of historical building exterior wall granitic plaster painting metope, in historical building exterior wall, through local reparative, granitic plaster painting metope after filling a vacancy is done in aging method, by being covered in through local reparative, the colorant match agent coating of the mortar bonding layer surface between granitic plaster painting metope after filling a vacancy, colorant match agent coating is formed by minerals colour system powder and inorganic siloxane solution mixed configuration, it is formed by acroleic acid polyurethane solution and inorganic siloxane solution mixed configuration, through local reparative, at the mortar stick portion of granitic plaster painting metope after filling a vacancy and the adjacent boundary without repairing mortar stick portion, it is provided with intermediate zone, the colorant match agent coating for having transition is also brushed in intermediate zone, the color of the colorant match agent coating of transition is to repair the original of target the reparation color and adjacent not repaired mortar stick portion of part Intermediate color between beginning color can achieve historical building exterior wall granitic plaster painting wall surface mortar adhesive layer and repair the old effect such as Gu.

Description

Historical building exterior wall granitic plaster painting metope does aging method
Technical field
Aging method is done the present invention relates to a kind of historical building exterior wall granitic plaster painting metope.
Background technique
The exterior wall of historical building experienced last 100 years natural erosion and artificial destruction, and many illnesss cannot be by simple Reparation can achieve the effect that restore history original state.
For the unified appearance and ornamental value of historical building, still advocate to repair old such as rule that is ancient, repairing old such as Gu.Repair it is old such as Gu, repairing ideally are the secondary uses by former exterior wall retained material or dismounting some materials itself.When nothing is stayed It deposits material or removes some materials when being unable to secondary use, it is necessary to find similar alternative materials and be repaired.Then this Under kind situation, the building " taking on an entirely new look " after reparation is difficult to restore with a long history, weather-beaten color and texture.In order to protect The appearance concordance and readability for holding historical building, it is outstanding based on aging method is done after the painting metope reparation of historical building exterior wall granitic plaster It is important.
Summary of the invention
Aging method is done the purpose of the present invention is to provide a kind of historical building exterior wall granitic plaster painting metope, is specially gone through History protection building, exterior wall granitic plaster paint metope through local reparative, fill a vacancy after do aging method, be able to solve original exterior wall water brush Mountain flour is whitewashed a wall after the local route repair of face, and new and old wall color is inconsistent, is unable to reach the problem of repairing the old effect such as Gu.
To solve the above problems, the present invention a kind of historical building exterior wall granitic plaster painting metope is provided do aging method, packet It includes:
The repairerment part and periphery of External Wall granitic plaster painting metope are cleaned, and it is substantially dry to repair adhesive mortar position Dry, moisture content is below 15%;
Determine the tinctorial pattern matching criterion of colorant match agent solvent, wherein the colorant match agent solvent is by minerals colour system powder and nothing Organic siloxane solution mixes, or is mixed by acroleic acid polyurethane solution and inorganic siloxane solution;
According to the color category and the tinctorial pattern matching criterion for repairing target mortar stick portion, determines and repair face than target The formula of the colorant match agent solvent of slightly deep one to two coloration of color, color shades become required odd colors after determining coating drying;
Before exterior wall granitic plaster painting metope repairs colorant match, the mortar for choosing the muti-piece granitic plaster painting metope on exterior wall is viscous Part is closed, is formulated obtained colorant match agent solvent with according to described, the mortar for the granitic plaster painting metope after filling a vacancy of learning from else's experience selected by brushing Stick portion surface, compare the mortar stick portion surface that colorant match agent has been brushed color and the target repair color whether one It causes, if inconsistent, the formula is adjusted according to comparison result;
External Wall granitic plaster painting metope is constructed on a large scale, comprising: is formulated or described adjusted is matched according to described Side, modulates the colorant match agent solvent of corresponding color;The table of each piece of mortar stick portion of metope is painted in exterior wall granitic plaster with writing brush The colorant match agent solvent of face brushing corresponding color;At the mortar stick portion boundary of granitic plaster painting metope, one or two are set Road intermediate zone chooses the middle transition of the target reparation color for repairing part and adjacent not repaired mortar bonding primitive color Color makees colorant match agent solvent, brushes to the intermediate zone;Before colorant match agent solvent final set, it is sticked to dry cloth wiped clean exposed Granitic plaster paints the colorant match agent solvent on metope.
Further, in the above-mentioned methods, the tinctorial pattern matching criterion of colorant match agent solvent is determined, comprising:
The weight percent of the colorant match agent solvent mineral colour system powder is 5-15%, and remaining weight percentage is nothing Organic siloxane solution.
Further, in the above-mentioned methods, the tinctorial pattern matching criterion of colorant match agent solvent is determined, comprising:
The weight percent of acroleic acid polyurethane solution is 10-15%, remaining weight percentage in the colorant match agent solvent For inorganic siloxane solution.
Further, in the above-mentioned methods, the minerals colour system powder, acroleic acid polyurethane solution and inorganic siloxanes Solution is hydrophobic material.
Further, in the above-mentioned methods, the material of the minerals colour system powder include iron oxide red, toluidine red, Iron oxide yellow, chrome yellow, chrome green, phthalocyanine green, ultramarine, chrome blue, phthalocyanine blue, iron oxide brown, iron oxide purple, iron oxide black, carbon black, manganese The combination of one or more of black and pine soot.
Further, in the above-mentioned methods, the sand with writing brush between each piece of granitic plaster of exterior wall granitic plaster painting metope Stick portion surface is starched to brush in the colorant match agent solvent of corresponding color,
The thickness that the surface of the granitic plaster painting wall surface mortar stick portion is formed by colorant match agent coating is less than 0.1mm。
Compared with prior art, the present invention repairs the mortar stick portion that granitic plaster paints metope by being covered in each piece The colorant match agent coating on surface, wherein the colorant match agent coating is mixed by minerals colour system powder and inorganic siloxane solution, Mixed by acroleic acid polyurethane solution and inorganic siloxane solution, through local reparative, fill a vacancy after granitic plaster paint wall At the boundary of the mortar stick portion in face and not repaired mortar stick portion, one or two intermediate zone, the mistake are set It crosses to take also to brush and has transition colorant match agent coating, the color of the transition colorant match agent coating is to repair the target reparation color of part With the intermediate chroma of the primitive color of adjacent not repaired mortar stick portion, repairing for historical building exterior wall requirement can achieve Old such as ancient effect.
Detailed description of the invention
Fig. 1 is the front signal for doing old structure of the historical building exterior wall granitic plaster painting metope of one embodiment of the invention Figure;
Fig. 2 is the side signal for doing old structure of the historical building exterior wall granitic plaster painting metope of one embodiment of the invention Figure;
Fig. 3 is that Fig. 1 of one embodiment of the invention is the historical building exterior wall granitic plaster painting metope of one embodiment of the invention The flow chart for doing aging method.
Specific embodiment
In order to make the foregoing objectives, features and advantages of the present invention clearer and more comprehensible, with reference to the accompanying drawing and specific real Applying mode, the present invention is described in further detail.
As shown in Fig. 1~2, what the present invention provided a kind of historical building exterior wall granitic plaster painting metope does old structure, comprising:
Local reparative, fill a vacancy after granitic plaster painting metope 1 mortar stick portion surface layer;
It is covered in the colorant match agent coating on the surface of the mortar stick portion, wherein the colorant match agent coating is by minerals Colour system powder and inorganic siloxane solution mix, and are mixed by acroleic acid polyurethane solution and inorganic siloxane solution, Through local reparative, fill a vacancy after granitic plaster painting metope mortar stick portion and the adjacent mortar bonding part without repairing Divide at 2 boundary, is additionally provided with one or two intermediate zone 2, also brushes the colorant match agent coating for having transition, institute in the intermediate zone The color for stating the colorant match agent coating of transition is the target reparation color for repairing part and the adjacent mortar stick portion without repairing Primitive color between intermediate color.
Here, the present invention is applied by being covered in the colorant match agent on the surface of the mortar stick portion of each piece of granitic plaster painting metope Layer, wherein the colorant match agent coating is mixed by minerals colour system powder and inorganic siloxane solution, by acroleic acid polyurethane Solution and inorganic siloxane solution mix, through local reparative, fill a vacancy after granitic plaster painting metope between mortar it is viscous It closes at part and the adjacent boundary without the mortar stick portion repaired, one or two intermediate zone, the intermediate zone is set On also brush and have a transition colorant match agent coating, the color of the transition colorant match agent coating be to repair the target reparation color and phase of part It is old as ancient to can achieve repairing for historical building exterior wall requirement without the intermediate color between the primitive color for the stick portion repaired by neighbour Effect.
Historical building exterior wall granitic plaster painting metope of the invention is done in one embodiment of old structure, the colorant match agent coating The weight percent of mineral colour system powder is 5-15%, and remaining weight percentage is inorganic siloxane solution, to be mixed Close uniform colorant match agent coating.
Historical building exterior wall granitic plaster painting metope of the invention is done in one embodiment of old structure, the colorant match agent coating The weight percent of middle acroleic acid polyurethane solution is 10-15%, and remaining weight percentage is inorganic siloxane solution, to obtain Uniformly mixed colorant match agent coating.
Historical building exterior wall granitic plaster painting metope of the invention is done in one embodiment of old structure, the minerals colour system Powder, acroleic acid polyurethane solution and inorganic siloxane solution are hydrophobic material.
Here, the minerals colour system powder, acroleic acid polyurethane solution and inorganic siloxane solution are hydrophobic material, Have fabulous alkali resistance, excellent water-sprinkling performance, excellent uvioresistant and weather resistance, is built with improving the history after repairing External wall waterproof effect is built, can not only prevent colorant match agent coating from being watered down by water, but also can prevent hydrone from infiltrating through exterior wall, is protected Hold the respirable elite clone of exterior wall.
Historical building exterior wall granitic plaster painting metope of the invention is done in one embodiment of old structure, the minerals colour system The material of powder includes iron oxide red, toluidine red, iron oxide yellow, chrome yellow, chrome green, phthalocyanine green, ultramarine, chrome blue, phthalocyanine blue, oxygen Change the combination of one or more of cologne earth, iron oxide purple, iron oxide black, carbon black, manganese black and pine soot, so that historical building exterior wall is wanted The effect for repairing old such as Gu asked is more preferable.
Here, the material table specific as follows of the minerals colour system powder:
Historical building exterior wall granitic plaster painting metope of the invention is done in one embodiment of old structure, the colorant match agent coating Thickness be less than 0.1mm.
Here, the thickness control of colorant match agent coating can be less than 0.1mm to avoid the metope repaired integrally blocked up. For example, the mass-tone system powder coating thickness is between 0.05mm~0.1mm.
As shown in figure 3, the present invention a kind of historical building exterior wall granitic plaster painting metope is provided do aging method, comprising:
The mortar stick portion of step S1, External Wall granitic plaster painting metope are cleaned, mortar stick portion after drying Moisture content is below 15%;
Here, needing to handle base: repair basal plane substantially dry, moisture content 15% hereinafter, basal plane defect, Such as: crack, seam crossing, junction no significant defect, before construction, base must be cleaned, without dirt, without waste, without the accumulation of salt in the surface soil, nothing Algae and moss etc.;
Step S2 determines the tinctorial pattern matching criterion of colorant match agent solvent, wherein the colorant match agent solvent is by minerals colour system powder Last and inorganic siloxane solution mixes, the colorant match agent coating or by acroleic acid polyurethane solution and inorganic siloxane solution It mixes;
Step S3 repairs color and the tinctorial pattern matching criterion according to the target of mortar stick portion, determines than the mesh Mark repairs the formula of the colorant match agent solvent of slightly deep one to two coloration of color;
Here, colorant match agent primary election: color phase can be selected according to tinctorial pattern matching criterion and the color for needing to repair wall The colorant match agent of close (slightly deep one to two coloration), makes color formulas;
Step S4 chooses the muti-piece on exterior wall granitic plaster painting metope before the painting metope colorant match construction of exterior wall granitic plaster Mortar stick portion brushes the table of selected muti-piece mortar stick portion with according to the colorant match agent solvent for being formulated and obtaining Face, whether the color and target reparation color on the surface for the mortar stick portion that comparing brushes painting is completed are consistent, if inconsistent, The formula is adjusted according to comparison result;
Here, colorant match agent determines: the repairing wall of muti-piece 0.5m*0.5m area can be chosen before metope is constructed on a large scale Metope is brushed with according to the obtained colorant match agent solvent that is formulated in face, and general thickness is less than 0.1mm, and the metope brushed is at end It should be protected from and drench with rain before solidifying, determine to do old color and the unified colorant match agent solvent of metope original appearance color;
Step S5, External Wall granitic plaster paint the construction of metope colorant match, comprising: according to the formula or described adjusted match Side, modulates the colorant match agent solvent of corresponding color;With mortar of the writing brush between each piece of granitic plaster of exterior wall granitic plaster painting metope The colorant match agent solvent of stick portion surface brushing corresponding color;Granitic plaster painting metope mortar stick portion and it is adjacent without At the boundary of the mortar stick portion of repairerment, be arranged one or two intermediate zone, choose repair part target repair color and The middle transition color of the adjacent mortar adhesive layer color without repairerment makees colorant match agent solvent, as transition colorant match agent solvent, to institute Intermediate zone is stated to be brushed;Before colorant match agent solvent final set, the spelling on granitic plaster painting metope is accidentally sticked to dry cloth wiped clean Toner solvent.
Here, the present invention is applied by being covered in the colorant match agent on the surface of the mortar stick portion of each piece of granitic plaster painting metope Layer, wherein the colorant match agent coating is mixed by minerals colour system powder and inorganic siloxane solution, by acroleic acid polyurethane Solution and inorganic siloxane solution mix, through local reparative, fill a vacancy after granitic plaster painting metope mortar bonding part Divide and one or two intermediate zone at the adjacent boundary without the mortar stick portion repaired, is set, is gone back in the intermediate zone Brushing has transition colorant match agent coating, and the color of the transition colorant match agent coating is to repair the target reparation color and adjacent nothing of part It is old as ancient to can achieve repairing for historical building exterior wall requirement for intermediate color between the primitive color for the mortar stick portion that need to be repaired Effect.
In addition, do it is old after the completion of, old effect can be done by visual inspection: stood with a distance from 1 meter of exterior wall, observation covering colorant match agent The metope of solvent and the adjacent original metope for not covering colorant match agent solvent then do old qualification without obvious boundary.
Historical building exterior wall granitic plaster painting metope of the invention is done in one embodiment of aging method, and step S2 is determined and spelled The tinctorial pattern matching criterion of toner solvent, comprising:
The weight percent of the colorant match agent solvent mineral colour system powder is 5-15%, and remaining weight percentage is nothing Organic siloxane solution, to obtain uniformly mixed colorant match agent solvent.
Historical building exterior wall granitic plaster painting metope of the invention is done in one embodiment of aging method, and step S2 is determined and spelled The tinctorial pattern matching criterion of toner solvent, comprising:
The weight percent of acroleic acid polyurethane solution is 10-15%, remaining weight percentage in the colorant match agent solvent For inorganic siloxane solution, to obtain uniformly mixed colorant match agent solvent.
Historical building exterior wall granitic plaster painting metope of the invention is done in one embodiment of aging method, the minerals colour system Powder, acroleic acid polyurethane solution and inorganic siloxane solution are hydrophobic material.
Here, the minerals colour system powder, acroleic acid polyurethane solution and inorganic siloxane solution are hydrophobic material, Have fabulous alkali resistance, excellent water-sprinkling performance, excellent uvioresistant and weather resistance, is built with improving the history after repairing External wall waterproof effect is built, can not only prevent colorant match agent coating from being watered down by water, but also can prevent water penetration from entering exterior wall.
Historical building exterior wall granitic plaster painting metope of the invention is done in one embodiment of aging method, the minerals colour system The material of powder includes iron oxide red, toluidine red, iron oxide yellow, chrome yellow, chrome green, phthalocyanine green, ultramarine, chrome blue, phthalocyanine blue, oxygen Change the combination of one or more of cologne earth, iron oxide purple, iron oxide black, carbon black, manganese black and pine soot, so that historical building exterior wall is wanted The effect for repairing old such as Gu asked is more preferable.
Here, the material table specific as follows of the minerals colour system powder:
Historical building exterior wall granitic plaster painting metope of the invention is done in one embodiment of aging method, with writing brush in exterior wall water Brush mountain flour whitewash a wall face each piece of granitic plaster between the surface of mortar stick portion (non-aqueous brush mountain flour whitewash a wall face part) brush pair It answers in the colorant match agent solvent of color,
The thickness that the surface of the mortar stick portion is formed by colorant match agent coating is less than 0.1mm.
Here, the thickness control of colorant match agent coating can be less than 0.1mm to avoid the metope repaired integrally blocked up. For example, the mass-tone system powder coating thickness is between 0.05mm~0.1mm.
Each embodiment in this specification is described in a progressive manner, the highlights of each of the examples are with other The difference of embodiment, the same or similar parts in each embodiment may refer to each other.
Obviously, those skilled in the art can carry out various modification and variations without departing from spirit of the invention to invention And range.If in this way, these modifications and changes of the present invention belong to the claims in the present invention and its equivalent technologies range it Interior, then the invention is also intended to include including these modification and variations.

Claims (6)

1. a kind of historical building exterior wall granitic plaster painting metope does aging method characterized by comprising
The repairerment part and periphery of External Wall granitic plaster painting metope are cleaned, and the mortar bond site after reparation is substantially dry Dry, moisture content is below 15%;
Determine the tinctorial pattern matching criterion of colorant match agent solvent, wherein the colorant match agent solvent is by minerals colour system powder and inorganic silicon Oxygen alkane solution mixes, or is mixed by acroleic acid polyurethane solution and inorganic siloxane solution;
According to the color category and the tinctorial pattern matching criterion for repairing target mortar stick portion, determine that repairing color than target omits The formula of the colorant match agent solvent of deep one to two coloration, color shades become required odd colors after determining coating drying;
Exterior wall granitic plaster painting metope construct on a large scale before, choose exterior wall granitic plaster paint metope on several pieces through local reparative, Mortar stick portion after filling a vacancy brushes selected mortar stick portion table with according to the colorant match agent solvent for being formulated and obtaining Face, erasing appear the colouring solvent on stone, and comparing brushes applies the face on the granitic plaster painting wall surface mortar stick portion surface completed Whether color and target reparation color are consistent, if inconsistent, adjust the formula according to comparison result;
External Wall granitic plaster painting metope is constructed on a large scale, according to the formula or the formula adjusted, modulation pair Answer the colorant match agent solvent of color;Corresponding face is brushed with the mortar bond site surface of the granitic plaster painting metope of writing brush after repair The colorant match agent solvent of color;The mortar stick portion and adjacent not repaired sand of granitic plaster painting metope after repairing, filling a vacancy It starches at bond site boundary, one or two intermediate zone is set, choose and repair the target of part and repair color and adjacent without repairing Intermediate chroma between the primitive color of multiple mortar stick portion makees colorant match agent solvent, as transition colorant match agent solvent to described Intermediate zone is brushed;Before colorant match agent solvent final set, the colorant match agent of granitic plaster painting metope is accidentally sticked to dry cloth wiped clean Solvent.
2. historical building exterior wall granitic plaster painting metope as described in claim 1 does aging method, which is characterized in that determine and spell The tinctorial pattern matching criterion of toner solvent, comprising:
The weight percent of the colorant match agent solvent mineral colour system powder is 5-15%, and remaining weight percentage is inorganic silicon Oxygen alkane solution.
3. historical building exterior wall granitic plaster painting metope as described in claim 1 does aging method, which is characterized in that determine and spell The tinctorial pattern matching criterion of toner solvent, comprising:
The weight percent of acroleic acid polyurethane solution is 10-15% in the colorant match agent solvent, and remaining weight percentage is nothing Organic siloxane solution.
4. historical building exterior wall granitic plaster painting metope as claimed in any one of claims 1 to 3 does aging method, feature exists In the minerals colour system powder, acroleic acid polyurethane solution and inorganic siloxane solution are hydrophobic material, guarantee that colorant match is molten Agent paints metope metope in granitic plaster, good can adhere to, block water and permeation functions.
5. historical building exterior wall granitic plaster painting metope as claimed in any one of claims 1 to 3 does aging method, feature exists In the material of the minerals colour system powder includes iron oxide red, toluidine red, iron oxide yellow, chrome yellow, chrome green, phthalocyanine green, group The combination of one or more of blueness, chrome blue, phthalocyanine blue, iron oxide brown, iron oxide purple, iron oxide black, carbon black, manganese black and pine soot.
6. historical building exterior wall granitic plaster painting metope as claimed in any one of claims 1 to 3 does aging method, feature exists In with the surface brushing corresponding color of mortar stick portion of the writing brush between each piece of granitic plaster of exterior wall granitic plaster painting metope Colorant match agent solvent in, the surface of the stick portion of the target reparation be formed by colorant match agent coating thickness be less than 0.1mm.
CN201811062346.9A 2018-09-12 2018-09-12 Antique-finishing method for wall surface painted by water-brushed stone on outer wall of historical building Active CN109138480B (en)