CN1090594C - 复合防火玻璃的干法合片方法 - Google Patents
复合防火玻璃的干法合片方法 Download PDFInfo
- Publication number
- CN1090594C CN1090594C CN97122388A CN97122388A CN1090594C CN 1090594 C CN1090594 C CN 1090594C CN 97122388 A CN97122388 A CN 97122388A CN 97122388 A CN97122388 A CN 97122388A CN 1090594 C CN1090594 C CN 1090594C
- Authority
- CN
- China
- Prior art keywords
- bag
- fireproof glass
- heating
- sheet
- poly
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本发明公开了一种利用玻璃单板生产复合防火玻璃的干法合片方法,它包括的主要工艺步骤是:①将两块防火玻璃单板的胶层面相扣合;②装入一接有真空泵的橡胶袋中抽真空:维持胶袋内气压100-950Pa,持续30-60分钟;③用50-100℃热空气于加热室内加热胶袋30-60分钟,同时继续保持袋内压力;④停止加热,维持袋内压力至加热室内温度降至40℃,关闭真空抽气系统;⑤降至室温,修边整理。用本方法合片防火玻璃生产操作方便,产品内外质量好。
Description
本发明涉及在两片玻璃之间夹置无机材料而制成复合防火玻璃的合片方法。
防火玻璃是一种玻璃深加工产品,具有防火、透光、透视等特点,广泛应用于高层建筑、展品陈列、防火隔断等方面。防火玻璃生产的一般工艺流程是:玻璃切割、浇注防火液、干燥得到防火玻璃单板,再合片、修边,而形成防火玻璃。其中的合片是一道关键工序,直接决定着产品的最终质量。现行的防火玻璃合片方法采用湿法合片,即在两块防火玻璃单板合片时,通过使用复合液使两玻璃板粘接在一起,形成防火玻璃。而湿法合片有以下弊端:
1、使胶合层中留有非常密集的微泡,影响视觉。
2、所使用的复合液受挤压后从两单板中间流出,污染防火玻璃外表面,形成难以擦净的白霜,影响成品的外观质量。
3、胶合层中水份含量过高,在以后的使用中易脱胶、起泡,缩短了产品的使用寿命。
4、因为复合液是滑腻的碱性油状物,湿法合片中玻璃的搬运等操作受到一定的影响,易出现滑脱现象。
本发明的目的在于针对上述现有湿法合片技术存在的问题,而提供一种复合防火玻璃的干法合片方法,从而避免湿法合片防火玻璃带来的缺陷。
为实现上述目的,本发明提供了一种复合防火玻璃的干法合片方法,它使用单面附置无机防火胶层的防火玻璃单板,该方法包括下述次序的工艺步骤:①将两块防火玻璃单板的胶层面相扣合,周边对齐;②装入一接有真空泵的橡胶袋中抽真空:维持胶袋内气压100-950Pa,持续30-60分钟;然后,③用50-100℃热空气干加热室内加热胶袋30-60分钟,同时继续保持袋内压力;④停止加热,维持袋内压力至加热室内温度降至40℃,关闭真空抽气系统;⑤降至室温,修边整理。
本合片方法抽真空时维持胶袋内气压的首选为100Pa,持续时间为30分钟。于加热室内加热胶袋的热空气温度首选值为95℃,持续时间为30分钟。
本发明与现有技术相比具有如下优点:
1、玻璃的非合片面没有污染,玻璃表面洁净。
2、消除了湿法合片所带来的微泡,提高了防火玻璃产品的质量。
3、避免了因使用复合液而造成的胶合层中含水份过高而引起的开胶这一缺陷。
4、因为没有滑腻的复合液,生产者操作更为方便。
5、在防火玻璃中夹丝、夹网更加方便,并且可减少破损率,提高成品率。
本复合防火玻璃的干法合片方法的具体实施步骤:①将干燥好的由单面附置无机防火胶层构成的防火玻璃单板的表面清洁干净;②将一块单板的合片面向上平置,将另一块与之配套合片的单板合片面向下扣在已放置好的单板上,调整好上下单板相对位置,使周边对齐并固定;③将已调整好的单板合片装入接有真空泵且置于加热室内的橡胶袋中,封闭袋口,启动真空泵进行抽真空:维持胶袋内气压100Pa,持续时间为30分钟;④用95℃热空气加热胶袋,持续30分钟,同时继续保持袋内压力;⑤停止加热,维持袋内压力至加热室内温度降至40℃,关闭真空抽气系统;⑥自然降至室温,打开胶袋,取出合好的防火玻璃,修边整理制得本发明复合防火玻璃。
Claims (3)
1、一种复合防火玻璃的干法合片方法,使用单面附置无机防火胶层的防火玻璃单板,其特征是:该方法包括下述次序的工艺步骤:
①将两块防火玻璃单板的胶层面相扣合,周边对齐;
②装入一接有真空泵的橡胶袋中抽真空:维持胶袋内气压100-950Pa,持续30-60分钟;然后,
③用50-100℃热空气于加热室内加热胶袋30-60分钟,同时继续保持袋内压力;
④停止加热,维持袋内压力至加热室内温度降至40℃,关闭真空抽气系统;
⑤降至室温,修边整理。
2、根据权利要求1所述的复合防火玻璃的干法合片方法,其特征是:抽真空时维持胶袋内气压100Pa,持续时间为30分钟。
3、根据权利要求1所述的复合防火玻璃的干法合片方法,其特征是:于加热室内加热胶袋的热空气为95℃,持续时间为30分钟。