CN108688365A - A kind of novel anti-wear-resisting printing technology of deinking - Google Patents

A kind of novel anti-wear-resisting printing technology of deinking Download PDF

Info

Publication number
CN108688365A
CN108688365A CN201810507592.4A CN201810507592A CN108688365A CN 108688365 A CN108688365 A CN 108688365A CN 201810507592 A CN201810507592 A CN 201810507592A CN 108688365 A CN108688365 A CN 108688365A
Authority
CN
China
Prior art keywords
ink
printing
packaging box
wear
deinking
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201810507592.4A
Other languages
Chinese (zh)
Inventor
龚佳佳
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Dragon Lede Intelligent Polytron Technologies Inc
Original Assignee
Dragon Lede Intelligent Polytron Technologies Inc
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Dragon Lede Intelligent Polytron Technologies Inc filed Critical Dragon Lede Intelligent Polytron Technologies Inc
Priority to CN201810507592.4A priority Critical patent/CN108688365A/en
Publication of CN108688365A publication Critical patent/CN108688365A/en
Pending legal-status Critical Current

Abstract

The invention discloses a kind of novel anti-wear-resisting printing technologies of deinking, include the following steps:S1, printing ink is produced, anti-wear agent and toner is added into ink, is then mixed evenly, it is spare, while preparing the Packaging Box for needing to print, it is spare;S2, by the ink stirred evenly be placed on heating interior preheat, bleeding agent is added thereto, stirs evenly, at the same also by Packaging Box be placed on heating interior preheat;S5, Packaging Box is printed, so that the printing ink solvent of Packaging Box surface printing is volatilized using hot-air oven or infrared-ray oven after printing, then passes through ultraviolet curing again;S6, UV glazings will be carried out to its printing surface using oil polish via step S5 treated Packaging Box.Through UV glazing process treated printed matter, color is obviously bright-coloured compared with other processing methods beautiful, and the coating after curing is wear-resisting, has more resistance to chemical reagents and chemical resistance, stability is good.

Description

A kind of novel anti-wear-resisting printing technology of deinking
Technical field
The invention belongs to printing technologies, more specifically, more particularly to a kind of novel anti-wear-resisting printing technology of deinking.
Background technology
By comprehensive investigation to market, decides through discussion design by further investigation and develop, the novel anti-wear-resisting print of deinking Dataller's skill, at abroad, books and periodicals, magazine, cover are widely used in terms of the gloss processing of the printed matters such as tape big envelope; The defect that existing plastic film coated technique often occurs, such as phenomena such as alice blistering corrugation delamination, the plastic film coated technique is not only It is expensive, and technique is multiple, and working efficiency is low.
Invention content
The purpose of the present invention is to solve disadvantages existing in the prior art, and the novel anti-deinking of one kind proposed is wear-resisting Printing technology.
To achieve the above object, the present invention provides the following technical solutions:
A kind of novel anti-wear-resisting printing technology of deinking, includes the following steps:
S1, printing ink is produced, anti-wear agent and toner is added into ink, is then mixed evenly, it is spare, prepare simultaneously The Packaging Box printed is needed, it is spare;
S2, by the ink stirred evenly be placed on heating interior preheat, bleeding agent is added thereto, stirs evenly, simultaneously Also Packaging Box heating interior is placed on to preheat;
S3, treated in step s 2 ink and Packaging Box are individually positioned in the ink containment tank on printing machine Nei and print On delivery platform;
S4, the ink in ink containment tank is heated again, allows and generates chemical reaction between its layers of material, it in this way can be with Vapor away the moisture of the ink of a part;
S5, Packaging Box is printed, Packaging Box surface printing is made using hot-air oven or infrared-ray oven after printing Printing ink solvent volatilizees, and then passes through ultraviolet curing again;
S6, UV glazings will be carried out to its printing surface using oil polish via step S5 treated Packaging Box.
Preheating temperature in the step S2 is 30~35 degrees Celsius.
Oil polish in the step S5, oil polish by volume: dumb paint=12: 1~50: 1 ratio is prepared.
Ink in the step S4 in ink containment tank is heated again, and heating temperature is 35~38 degrees Celsius.
The technique effect and advantage of the present invention:The novel anti-wear-resisting printing technology of deinking of one kind provided by the invention, oil polish It is practically free of solvent, organic volatile discharge capacity is few, therefore reduces air pollution, improves working environment, decreases The danger of fire occurs;
Oil polish is free of solvent, and when solidification does not need thermal energy, and the energy consumption needed for solidification only has infrared curing type ink and infrared 20% or so of curing type oil polish.In addition, this oil polish is strong to ink affinity, adhesion-tight, 80 --- 120W/CM The lower curing rate of ultraviolet radiator irradiation is up to 100 --- 300M/MIN;
Through UV glazing process treated printed matter, color is obviously bright-coloured compared with other processing methods beautiful, and the painting after curing Layer is wear-resisting, has more resistance to chemical reagents and chemical resistance, and stability is good, and water and ethyl alcohol can be used to clean;
Oil polish active ingredient is high, and volatilization is few, so low-consuming.The oil polish coating weight of general art paper is only 4g/m2 or so, Cost is about overlay film cost 60% or so;
The defect that can often occur to avoid plastic film coated technique, such as phenomena such as alice blistering corrugation delamination, UV glazings product is not Adhesion can be stacked after solidification and is placed with conducive to the rear process processing operation such as bookbinding;
It can recycle.Solve the compound paper substrate of plastics cannot recycle and the problem of environmental pollution that is formed.
The duplicate surface for completing picture and text printing, prints oil polish once or twice with printing plate on the spot or picture and text printing plate, makes again Printed matter surface obtains light VU film layers.Printing coating can enhance the light fastness of ink, increase ink layer solar heat protection, moisture-proof Ability.Play the role of that trace beautify product is protected to substitute overlay film.Printing coating is compared with overlay film etc., not only cheap Simple process, and both can be with full version glazing, it can also local glazing.
Specific implementation mode
In order to make the purpose , technical scheme and advantage of the present invention be clearer, below in conjunction with specific embodiment, to this Invention is further elaborated.It should be appreciated that the specific embodiments described herein are merely illustrative of the present invention, not For limiting the present invention.Based on the embodiments of the present invention, those of ordinary skill in the art are not before making creative work The every other embodiment obtained is put, shall fall within the protection scope of the present invention.
A kind of novel anti-wear-resisting printing technology of deinking, includes the following steps:
S1, printing ink is produced, anti-wear agent and toner is added into ink, is then mixed evenly, it is spare, prepare simultaneously The Packaging Box printed is needed, it is spare;
S2, by the ink stirred evenly be placed on heating interior preheat, bleeding agent is added thereto, stirs evenly, simultaneously Also Packaging Box heating interior is placed on to preheat;
S3, treated in step s 2 ink and Packaging Box are individually positioned in the ink containment tank on printing machine Nei and print On delivery platform;
S4, the ink in ink containment tank is heated again, allows and generates chemical reaction between its layers of material, it in this way can be with Vapor away the moisture of the ink of a part;
S5, Packaging Box is printed, Packaging Box surface printing is made using hot-air oven or infrared-ray oven after printing Printing ink solvent volatilizees, and then passes through ultraviolet curing again;
S6, UV glazings will be carried out to its printing surface using oil polish via step S5 treated Packaging Box.
Preheating temperature in the step S2 is 30 degrees Celsius.
Oil polish in the step S5, oil polish by volume: dumb paint=40: 1 ratio is prepared.
Ink in the step S4 in ink containment tank is heated again, and heating temperature is 35 degrees Celsius.
The flowing of ink roller curing ink is uneven, some local non-sticking ink, especially metal rolls are even more serious, often printing plate are made to go out Existing clear area, that is, ink is difficult to pass on ink foundation roller in the ink fountain of offset press.Appearance deinking one, which is ink, fountain solution It is sensitive(Hydrophilic emulsification)Property;Second is that the yield value of ink is big, thixotropic coefficient is high, and cohesive force is very strong, and ink stickiness is small, but Consistency is big.Ink viscosity problem is to cause one of the maximum reason of void.
Ink viscosity height can slow down the drying property of ink, when ink does not have rapid draing to be easy for generating void.Institute It is the method for overcoming deinking best to reduce ink viscosity.Color generates deviation after being reduced such as viscosity, can improve the color of ink Powder content, to ensure the correctness and stability of ink colors.
The followed by wearability of ink.The wearability of ink is mainly reflected in the cohesiveness and adhesive force of ink, works as ink The wearability of ink is deteriorated after cohesiveness and adhesive force reduce, this and ink itself are closely bound up.Ink after such as printing It has been dried that, have serious void with hand or paper wiping ink, that just illustrates that ink abrasion resistance is poor, this just needs to increase wear-resisting Agent is black from brand-new.
Paper water imbibition is low, then the water imbibition of ink also reduces naturally, ink, which floats on paper surface and is easy to generate, to be taken off Ink.If it is known that paper water imbibition is poor, then will improve since on watt line.The received heat for improving facial tissue first, by carrying High paper heat failure mechanics paper fiber and paper sizing layer to improve the absorbency of paper, and improve ink in printing The usage amount of bleeding agent thus can more preferably prevent the generation of printing void.
Deinking is common, each deinking reason is also different, only finds true cause and seeks suitable side again Method is improved, and effect just can be more preferable.
Oil polish is practically free of solvent, and organic volatile discharge capacity is few, therefore reduces air pollution, improves work Environment decreases the danger that fire occurs;
Oil polish is free of solvent, and when solidification does not need thermal energy, and the energy consumption needed for solidification only has infrared curing type ink and infrared 20% or so of curing type oil polish.In addition, this oil polish is strong to ink affinity, adhesion-tight, 80 --- 120W/CM The lower curing rate of ultraviolet radiator irradiation is up to 100 --- 300M/MIN;
Through UV glazing process treated printed matter, color is obviously bright-coloured compared with other processing methods beautiful, and the painting after curing Layer is wear-resisting, has more resistance to chemical reagents and chemical resistance, and stability is good, and water and ethyl alcohol can be used to clean;
Oil polish active ingredient is high, and volatilization is few, so low-consuming.The oil polish coating weight of general art paper is only 4g/m2 or so, Cost is about overlay film cost 60% or so;
The defect that can often occur to avoid plastic film coated technique, such as phenomena such as alice blistering corrugation delamination, UV glazings product is not Adhesion can be stacked after solidification and is placed with conducive to the rear process processing operation such as bookbinding;
It can recycle.Solve the compound paper substrate of plastics cannot recycle and the problem of environmental pollution that is formed.
The duplicate surface for completing picture and text printing, prints oil polish once or twice with printing plate on the spot or picture and text printing plate, makes again Printed matter surface obtains light VU film layers.Printing coating can enhance the light fastness of ink, increase ink layer solar heat protection, moisture-proof Ability.Play the role of that trace beautify product is protected to substitute overlay film.Printing coating is not only cheap compared with overlay film etc.. Simple process, and both can be with full version glazing, it can also local glazing.
Finally it should be noted that:The foregoing is only a preferred embodiment of the present invention, is not intended to restrict the invention, Although the present invention is described in detail referring to the foregoing embodiments, for those skilled in the art, still may be used With technical scheme described in the above embodiments is modified or equivalent replacement of some of the technical features, All within the spirits and principles of the present invention, any modification, equivalent replacement, improvement and so on should be included in the present invention's Within protection domain.

Claims (4)

1. a kind of novel anti-wear-resisting printing technology of deinking, it is characterised in that:Include the following steps:
S1, printing ink is produced, anti-wear agent and toner is added into ink, is then mixed evenly, it is spare, prepare simultaneously The Packaging Box printed is needed, it is spare;
S2, by the ink stirred evenly be placed on heating interior preheat, bleeding agent is added thereto, stirs evenly, simultaneously Also Packaging Box heating interior is placed on to preheat;
S3, treated in step s 2 ink and Packaging Box are individually positioned in the ink containment tank on printing machine Nei and print On delivery platform;
S4, the ink in ink containment tank is heated again, allows and generates chemical reaction between its layers of material, it in this way can be with Vapor away the moisture of the ink of a part;
S5, Packaging Box is printed, Packaging Box surface printing is made using hot-air oven or infrared-ray oven after printing Printing ink solvent volatilizees, and then passes through ultraviolet curing again;
S6, UV glazings will be carried out to its printing surface using oil polish via step S5 treated Packaging Box.
2. the novel anti-wear-resisting printing technology of deinking of one kind described in claim 1, it is characterised in that:Preheating in the step S2 Temperature is 30~35 degrees Celsius.
3. the novel anti-wear-resisting printing technology of deinking of one kind described in claim 1, it is characterised in that:Glazing in the step S5 Oil, oil polish by volume: dumb paint=12: 1~50: 1 ratio is prepared.
4. the novel anti-wear-resisting printing technology of deinking of one kind described in claim 1, it is characterised in that:Ink stores up in the step S4 The ink deposited in tank is heated again, and heating temperature is 35~38 degrees Celsius.
CN201810507592.4A 2018-05-24 2018-05-24 A kind of novel anti-wear-resisting printing technology of deinking Pending CN108688365A (en)