CN108657581A - Inhibit the method for container inner wall fouling and can inhibit the container of fouling - Google Patents
Inhibit the method for container inner wall fouling and can inhibit the container of fouling Download PDFInfo
- Publication number
- CN108657581A CN108657581A CN201810709653.5A CN201810709653A CN108657581A CN 108657581 A CN108657581 A CN 108657581A CN 201810709653 A CN201810709653 A CN 201810709653A CN 108657581 A CN108657581 A CN 108657581A
- Authority
- CN
- China
- Prior art keywords
- flexible membrane
- container
- vessel
- wall
- fouling
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
A kind of method inhibiting container inner wall fouling and the container that can inhibit fouling, the method includes hanging to set one layer of flexible membrane in the inner wall of vessel, the flexible membrane is driven to shake using the surge impulse force of liquid, the crystal that liquid is precipitated is set to be not easy to be attached to the flexible membrane, to achieve the purpose that the crystal for inhibiting liquid to be precipitated in container inner wall fouling.The container that can inhibit fouling includes vessel and the flexible membrane that matches with the size of the vessel and shape, and the flexible membrane is hung on the inner wall of the vessel by the oral area that the upper end of the flexible membrane is fixed on the vessel.The present invention is to utilize the pre- good antiscale property of physics mode, will not corrosion failure container, and thinking is novel, simple in structure.
Description
Technical field
The present invention relates to liquid container more particularly to it is a kind of inhibit container inner wall fouling method and can inhibit fouling
Container.
Background technology
Chemical Solvents container inner wall is susceptible to crystal precipitation, forms fouling, container cavity is made to become smaller, and corrodes cavity, shadow
Working efficiency is rung, energy consumption is caused.
Existing solution is to go scale removal again after fouling is formed, and typically uses scale remover dissolving removal fouling, still
De-sludging effect unobvious.
Invention content
The object of the present invention is to provide a kind of method inhibiting container inner wall fouling and the containers that can inhibit fouling.
In order to achieve the above object, the technical solution adopted by the present invention is as follows:
A method of inhibiting container inner wall fouling, the method includes hanging to set one layer of flexibility in the inner wall of vessel
Film drives the flexible membrane to shake, the crystal that liquid is precipitated is made to be not easy to be attached to the flexible membrane using the surge impulse force of liquid,
To achieve the purpose that the crystal for inhibiting liquid to be precipitated in container inner wall fouling.
In a kind of scheme, the oral area Electrostatic Absorption of the upper end of the flexible membrane and the vessel, flexible membrane its
Remaining part point is in the state detached with the inner wall of vessel.
In another scheme, the upper end of the flexible membrane and the oral area hot melt of the vessel combine, flexible membrane
Rest part is in the state detached with the inner wall of vessel.
In also a kind of scheme, the upper end of the flexible membrane and the oral area of the vessel are bonded admittedly by glue or adhesive tape
Fixed, the rest part of flexible membrane is in the state detached with the inner wall of vessel.
Preferably, the flexible membrane is equipped with hole at the bottom close to container, and liquid enters the flexible membrane through the hole
Between chamber wall, make to maintain interval between flexible membrane and chamber wall.
A kind of container can inhibit fouling comprising vessel further includes size and shape with the vessel
The flexible membrane to match, the upper end of the flexible membrane be fixed on the vessel oral area the flexible membrane is hung on it is described
The inner wall of vessel.Preferably, the upper end Electrostatic Absorption of the flexible membrane is in the oral area of the vessel or described soft
Property film the upper end hot melt upper end of oral area or the flexible membrane that is fixed on the vessel be bonded and fixed at the container
The oral area of ontology.
The container can be kettle, food container or reagent container etc..Preferably, the flexible membrane is close to container
Hole is equipped at bottom.
Compared with prior art, the present invention at least has the advantages that:
The present invention sets what flexible membrane was precipitated the Disturbance Rejection liquid of flexible membrane using liquid by the way that the inner wall in container is outstanding
For crystal in container inner wall fouling, thinking is novel, simple in structure.
Compared to the mode for dissolving removal fouling with scale remover, the present invention is to utilize the pre- good antiscale property of physics mode, will not be corroded
Destroy container.
Description of the drawings
Fig. 1 is the position and combination schematic diagram of flexible membrane and vessel in some embodiments.
Specific implementation mode
The present invention will be further described with reference to the accompanying drawings and examples.
Fig. 1 is please referred to, the method for some embodiments inhibition container inner wall fouling includes:It hangs and sets in the inner wall of vessel 1
One layer of flexible membrane 2 drives the flexible membrane 2 to shake, the crystal that liquid is precipitated is made to be not easy to be attached to using the surge impulse force of liquid
The flexible membrane 2, to achieve the purpose that the crystal for inhibiting liquid to be precipitated in container inner wall fouling.
Power when the surge power of liquid can be liquid itself boiling, can also be pump, can also be external or interior
The external force of the generations such as the vibrator set.
Wherein, the upper end of the flexible membrane 2 and the oral area 4 of the vessel 1 are adhesively fixed by adhesive tape 3, flexible membrane 2
Rest part and the inner wall of vessel 1 be in the state detached.In addition it is also possible to which the upper end of flexible membrane 2 is bonded with glue
It is fixed on the oral area 4 of vessel 1.
As another embodiment, vessel uses plastic cement material, and the fusing point of fusing point and the flexible membrane is close, soft
Property film the oral area hot melt of upper end and the vessel combine, the rest part of flexible membrane and the inner wall of vessel are in point
From state.
In also a kind of embodiment, it is smooth minute surface that vessel, which uses glass or metal material, surface, passes through electrostatic
The upper end of flexible membrane is fixed on the oral area of vessel by suction type, at the rest part of flexible membrane and the inner wall of vessel
In the state of separation.
Flexible membrane described further is equipped with hole 5 at the bottom close to container, and liquid enters the flexible membrane through the hole 5
Between 2 and chamber wall, makes to maintain interval between flexible membrane 2 and chamber wall, chamber wall will not be pasted to, it is soft so as to ensure
The reliable shake of property film 2.
Fig. 1 is please referred to, the container that some embodiments can inhibit fouling includes:Vessel 1 further includes and the container sheet
The upper end of the flexible membrane 2 that the size and shape of body 1 match, the flexible membrane 2 is bonded and fixed at the container sheet by adhesive tape 3
The flexible membrane 2 is hung on the inner wall of the vessel 1 by the oral area 4 of body 1.
The container can be kettle, food container or reagent container etc..
2 preferred Kapton of flexible membrane, Kapton have high temperature resistant, tensile strength height, radiation hardness, nothing
The advantages that malicious, stable.Specifically, temperature -200 is used for a long time to 250 DEG C in 500 DEG C or so of decomposition temperature.Tensile strength exists
100Mpa or more, stupid type Kapton (kap ton) are 170Mpa or more, and biphenyl polyimides (Upi lexS) reaches
400Mpa.Film is 90% in 5x109rad block electron irradiation strength retentions.Insoluble in organic solvent, diluted acid is stablized, it is resistance to
Hydrolysis.The material is nontoxic, and stands thousands of disinfections.The material is self-extinguishing polymer, and smoke rate is low.According to practical application
Demand, flexible membrane can select other materials.
Above by specific embodiment, invention is explained in detail, these detailed description are only limited to help
Those skilled in the art understand that present disclosure, can not be interpreted as limiting the scope of the invention.Art technology
Personnel should be included in various retouchings, equivalent transformation etc. that said program carries out under present inventive concept the protection model of the present invention
In enclosing.
Claims (10)
1. a kind of method inhibiting container inner wall fouling, which is characterized in that the method includes hanging to set in the inner wall of vessel
One layer of flexible membrane drives the flexible membrane to shake, the crystal that liquid is precipitated is made to be not easy to be attached to institute using the surge impulse force of liquid
Flexible membrane is stated, to achieve the purpose that the crystal for inhibiting liquid to be precipitated in container inner wall fouling.
2. it is according to claim 1 inhibit container inner wall fouling method, which is characterized in that the upper end of the flexible membrane with
The oral area Electrostatic Absorption of the vessel, the rest part of flexible membrane are in the state detached with the inner wall of vessel.
3. it is according to claim 1 inhibit container inner wall fouling method, which is characterized in that the upper end of the flexible membrane with
The oral area hot melt of the vessel combines, and the rest part of flexible membrane is in the state detached with the inner wall of vessel.
4. it is according to claim 1 inhibit container inner wall fouling method, which is characterized in that the upper end of the flexible membrane with
The oral area of the vessel is adhesively fixed by glue or adhesive tape, and the rest part of flexible membrane and the inner wall of vessel are in and divide
From state.
5. the method as claimed in any of claims 1 to 4 for inhibiting container inner wall fouling, which is characterized in that described
Flexible membrane is equipped with hole at the bottom close to container, and liquid enters through the hole between the flexible membrane and chamber wall, makes flexibility
Interval is maintained between film and chamber wall.
6. a kind of container can inhibit fouling, including vessel, which is characterized in that further include the size with the vessel
And the flexible membrane that shape matches, the upper end of the flexible membrane are fixed on the oral area of the vessel and set the flexible membrane is outstanding
In the inner wall of the vessel.
7. the container according to claim 6 that can inhibit fouling, which is characterized in that the upper end Electrostatic Absorption of the flexible membrane
In the oral area of the vessel.
8. the container according to claim 6 that can inhibit fouling, which is characterized in that the upper end hot melt of the flexible membrane is fixed
In the oral area of the vessel.
9. the container according to claim 6 that can inhibit fouling, which is characterized in that the upper end of the flexible membrane is adhesively fixed
In the oral area of the vessel.
10. the container that can inhibit fouling according to any one of claim 6 to 9, which is characterized in that the container is
Kettle, food container or reagent container, the flexible membrane are equipped with hole at the bottom close to container.