CN108554629A - 铁精粉提质降硅选矿工艺 - Google Patents
铁精粉提质降硅选矿工艺 Download PDFInfo
- Publication number
- CN108554629A CN108554629A CN201810276053.4A CN201810276053A CN108554629A CN 108554629 A CN108554629 A CN 108554629A CN 201810276053 A CN201810276053 A CN 201810276053A CN 108554629 A CN108554629 A CN 108554629A
- Authority
- CN
- China
- Prior art keywords
- concentrate
- tailing
- ore
- sections
- carried out
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
铁精粉提质降硅选矿工艺,采用预选抛尾—三段磨矿—磁选提铁降硅工艺,一段:‑0.076mm 45%,二段:‑0.076mm 80%,三段:‑0.076mm95%。对于6~0mm和3~0mm可获得铁品位大于68%、SiO2含量小于4%的指标;在实现精矿铁品位大于68%、SiO2含量小于4%的目标下,研究尽可能多抛粗粒尾矿及从一段磁选尾矿中提取+0.3mm粗粒尾砂。
Description
技术领域
本发明涉及一种选矿工艺,具体涉及一种铁精粉提质降硅选矿 工艺。
背景技术
选矿设计流程为原矿-预选(包括中碎产品干式预选和辊压产品 湿式预选)-阶段磨矿-阶段弱磁选流程,其中一段磨矿细度为 -0.076mm 50%,二段磨矿细度为-0.076mm85%。在实际生产当中, 为了尽可能降低铁精矿硅含量,将一段和二段磨矿细度分别提高到 -0.076mm 60%和-0.076mm 90%左右,尽管精矿铁品位达到了 66.36%,但精矿SiO2含量仍高达7.32%。此外,生产中细粒尾矿量 大,粗粒尾砂量少,而井下空区有限,难以实现采充平衡。
发明内容
本发明所要解决的技术问题在于克服现有技术的缺陷,提供一 种铁精粉提质降硅选矿工艺。
本发明所要解决的技术问题采用以下技术方案来实现。
铁精粉提质降硅选矿工艺,其特征在于:具体为
将原矿样品混匀、缩分后、破碎;
将破碎后的原矿进行4000Oe的磁场强度粗选,所得精矿一与尾 矿,精矿一进行一段磨矿,一段磨矿细度为-0.076mm 45%;尾矿经过 0.3mm筛分,得到粗尾矿和细尾矿;
再将经过一段磨矿后的精矿一进行2000Oe的磁场强度粗选,得 到精矿二与尾矿,精矿二进行二段磨矿,二段磨矿细度为-0.076mm 80%;尾矿经过0.3mm筛分,得到粗尾矿和细尾矿;
再将经过二段磨矿后的精矿二进行1600Oe的磁场强度粗选,得 到精矿三与尾矿;
再将精矿三进行三段磨矿三段磨矿细度为-0.076mm 95%;
再将经过三段磨矿后的精矿三进行2000Oe的磁场强度粗选,得 到精矿四与尾矿;
再将精矿四进行1600Oe的磁场强度粗选,得到精矿五与尾矿。
有益效果:采用预选抛尾—三段磨矿—磁选提铁降硅工艺(一 段:-0.076mm45%,二段:-0.076mm 80%,三段:-0.076mm95%), 对于6~0mm和3~0mm可获得铁品位大于68%、SiO2含量小于4%的 指标;(2)在实现精矿铁品位大于68%、SiO2含量小于4%的目标 下,研究尽可能多抛粗粒尾矿及从一段磁选尾矿中提取+0.3mm粗粒 尾砂。
具体实施方式
对本发明实施例中的技术方案进行清楚、完整地描述,显然, 所描述的实施例仅仅是本发明的部分实施例,而不是全部的实施例。
铁精粉提质降硅选矿工艺,具体为
将原矿样品混匀、缩分后、破碎;
将破碎后的原矿进行4000Oe的磁场强度粗选,所得精矿一与尾 矿,精矿一进行一段磨矿,一段磨矿细度为-0.076mm 45%;尾矿经过 0.3mm筛分,得到粗尾矿和细尾矿;
再将经过一段磨矿后的精矿一进行2000Oe的磁场强度粗选,得 到精矿二与尾矿,精矿二进行二段磨矿,二段磨矿细度为-0.076mm 80%;尾矿经过0.3mm筛分,得到粗尾矿和细尾矿;
再将经过二段磨矿后的精矿二进行1600Oe的磁场强度粗选,得 到精矿三与尾矿;
再将精矿三进行三段磨矿三段磨矿细度为-0.076mm 95%;
再将经过三段磨矿后的精矿三进行2000Oe的磁场强度粗选,得 到精矿四与尾矿;
再将精矿四进行1600Oe的磁场强度粗选,得到精矿五与尾矿。
将原矿样品(现场高压辊磨排矿)混匀、缩分、取样后,将原 矿样品破碎至6~0mm、3~0mm、2~0mm三个不同粒级的样品进行后续 试验。
不同给矿粒度及不同磁场强度湿式粗粒磁选试验结果(%)
6~0mm和3~0mm样品提铁降硅试验结果(%)
6~0mm样品尾矿总砂量计算结果(%)
3~0mm样品尾矿总砂量计算结果(%)
试验结果表明:(1)采用预选抛尾—三段磨矿—磁选提铁降硅 工艺(一段:-0.076mm 45%,二段:-0.076mm 80%,三段:-0.076mm95%), 对于6~0mm和3~0mm样品均可获得铁品位大于68%、SiO2含量小 于4%的指标;(2)通过改变入选粒度、降低磁场强度或放粗一段磨 矿细度,尾矿中+0.3mm粗粒尾砂量虽有所提高。
以上所述,仅为本发明较佳的具体实施方式,但本发明的保护范 围并不局限于此,任何熟悉本技术领域的技术人员在本发明揭露的技 术范围内,根据本发明的技术方案及其发明构思加以等同替换或改 变,都应涵盖在本发明的保护范围之内。
Claims (1)
1.铁精粉提质降硅选矿工艺,具体为
将原矿样品混匀、缩分后、破碎;
将破碎后的原矿进行4000Oe的磁场强度粗选,所得精矿一与尾矿,精矿一进行一段磨矿,一段磨矿细度为-0.076mm 45%;尾矿经过0.3mm筛分,得到粗尾矿和细尾矿;
再将经过一段磨矿后的精矿一进行2000Oe的磁场强度粗选,得到精矿二与尾矿,精矿二进行二段磨矿,二段磨矿细度为-0.076mm 80%;尾矿经过0.3mm筛分,得到粗尾矿和细尾矿;
再将经过二段磨矿后的精矿二进行1600Oe的磁场强度粗选,得到精矿三与尾矿;
再将精矿三进行三段磨矿三段磨矿细度为-0.076mm 95%;
再将经过三段磨矿后的精矿三进行2000Oe的磁场强度粗选,得到精矿四与尾矿;
再将精矿四进行1600Oe的磁场强度粗选,得到精矿五与尾矿。