CN108544626A - English walnut wood gas grinding process - Google Patents

English walnut wood gas grinding process Download PDF

Info

Publication number
CN108544626A
CN108544626A CN201810294902.9A CN201810294902A CN108544626A CN 108544626 A CN108544626 A CN 108544626A CN 201810294902 A CN201810294902 A CN 201810294902A CN 108544626 A CN108544626 A CN 108544626A
Authority
CN
China
Prior art keywords
wood
wax
wood surface
gas
grinding process
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201810294902.9A
Other languages
Chinese (zh)
Inventor
邱红霞
曾祥华
陈丽嘉
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Dongguan Noah Family Furniture Co Ltd
Original Assignee
Dongguan Noah Family Furniture Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Dongguan Noah Family Furniture Co Ltd filed Critical Dongguan Noah Family Furniture Co Ltd
Priority to CN201810294902.9A priority Critical patent/CN108544626A/en
Publication of CN108544626A publication Critical patent/CN108544626A/en
Pending legal-status Critical Current

Abstract

The present invention relates to field of furniture, and in particular to English walnut wood gas grinding process;English walnut wood gas grinding process includes the following steps, a, pre-treatment:Polishing and dedusting are carried out to the smooth no particle of wood surface to wood surface, b, it is coated with one layer of wood wax oil in wood surface, c, wood surface is polished with gas mill polish brush, to wood surface haze tallow oil reservoir without impression of the hand, d, second polishing to wood surface is carried out to the timber after gas grinding and polishing light to be smooth to the touch, e, repeat step b, c, d at least once with sand paper more than 1200 mesh.Production efficiency of the present invention is high, wood wax oil energy Quick uniform infiltrates through that wood internal, wood surface gloss are uniform and stable, specious and protective effect is good.

Description

English walnut wood gas grinding process
Technical field
The present invention relates to field of furniture, more particularly to English walnut wood gas grinding process.
Background technology
Furniture refers to that the mankind maintain normal life, are engaged in production practices and carry out the essential utensil facility of social activities Major class.Furniture also follows the step in epoch to continue to develop innovation, and of a great variety by now, materials are different, great variety of goods, and purposes is not One.It is the important foundation for establishing Working Life space.Furniture is made of material, structure, appearance forrns and function four factors, Wherein function is guide, is the power for pushing furniture development;Structure is trunk, is the basis for realizing function.These four factors are mutual It is associated, and conditions each other.
For English walnut wooden furniture, after the completion of production, need to coat one layer of wood wax oil on surface, wood wax oil is natural The green environmental friendly coatings that vegetable oil wax is process through special process, it, which can be protected, wooden plays the role of cracking resistance.Wood wax oil applies It after the completion of covering, often needs to stand a period of time, generally need 6 hours or more, allow wood wax oil uniformly penetrating into wood internal.But it is this Method has the following deficiencies, on the one hand, time of repose is long, influences whole production efficiency, second aspect, wood wax oil can not be equal It is even to infiltrate through wood internal, cause wood surface glossiness to differ.The third aspect, traditional wood wax oil and timber combination force difference, It is to be improved to the protective effect of timber.
Invention content
To solve the above problems, a kind of production efficiency of present invention offer is high, wood wax oil energy Quick uniform infiltrates through in timber Portion, the English walnut wood gas grinding process that wood surface gloss is uniform and stable, specious and protective effect is good.
The technical solution adopted in the present invention is:English walnut wood gas grinding process, includes the following steps, a, pre-treatment:To timber Surface carries out polishing and dedusting to the smooth no particle of wood surface, b, is coated with one layer of wood wax oil in wood surface, c, with gas grinding and polishing Light brush is polished wood surface, until d, the haze tallow oil reservoir of wood surface grinds gas with sand paper more than 1200 mesh without impression of the hand Timber after polishing carries out second polishing to wood surface and is smooth to the touch, and e, repeats step b, c, d at least once.
To being further improved as in step b, when applying wood wax oil, in room temperature and draughty ring for above-mentioned technical proposal It is carried out under border, and by the grain direction brushing wood wax oil of timber.
To above-mentioned technical proposal be further improved for, in step b, wood wax oil is counted in parts by weight, and component includes, 60% vegetable oil, 12% linseed wax, 2% Brazil wax, 25% D40 solvent naphthas, 0.2% ultraviolet radiation absorption Agent, 0.3% antifoaming agent, 0.5% drier.
To above-mentioned technical proposal be further improved for, in step b, linseed wax be extraction linseed outer layer wax and The mixture of internal layer wax, and the mass ratio of linseed outer layer wax and internal layer wax is 3:2.
To being further improved as in step c, the spray gun pressure that gas grinds polish brush is 0.5kPa- for above-mentioned technical proposal 1.2kPa。
Beneficial effects of the present invention are:
1, on the one hand, in the present invention, relative to the method for traditional timber standing and drying for being coated with wood wax oil, pass through Gas grinding and polishing light, which brushes, wipes wood surface, accelerates the flowing of wood surface air so that and wood wax oil energy rapid osmotic enters wood internal, and Rate of drying is fast, and it is uniform and stable, outer that production efficiency is high, wood wax oil energy Quick uniform infiltrates through wood internal, wood surface gloss Table is beautiful.Second aspect, using gas mill polish brush timber is handled after, using sand paper more than 1200 mesh to timber into Row second polishing so that wood surface is smooth and glossiness is good, further improves timber surface aesthetics.The third aspect, weight Multiple gas grinding and polishing light and sand paper polishing step are twice so that the haze tallow oil reservoir of wood surface has certain thickness, high mechanical strength, energy Preferably protection timber.
2, it in step b, when applying wood wax oil, is carried out in the environment of room temperature and well-ventilated, accelerates the sky of haze tallow oil meter face Flow of air improves wood wax oil drying efficiency, by the grain direction brushing wood wax oil of timber so that wood wax oil can be infiltrated through preferably Wood internal, to preferably be protected to timber.
3, in step b, wood wax oil is counted in parts by weight, and component includes, 60% vegetable oil, 12% linseed wax, 2% Brazil wax, 25% D40 solvent naphthas, 0.2% ultra-violet absorber, 0.3% antifoaming agent, 0.5% urge it is dry Agent.The component safety and environmental protection of wood wax oil, and rate of drying is fast, the haze tallow oil reservoir of formation has certain intensity, and glossiness is good, appearance Beauty, and protective value is good.
4, in step b, linseed wax is the mixture of the linseed outer layer wax and internal layer wax of extraction, and outside linseed The mass ratio of layer wax and internal layer wax is 3:2.Using the compatibility of internal layer wax and wood raw material, wood internal can be goed deep into, Timber duct is soaked, the conjugation of timber and wood wax oil is improved.
5, in step c, the spray gun pressure that gas grinds polish brush is 0.5kPa-1.2kPa, and spray gun pressure is big, can damage timber table The haze tallow oil reservoir in face, spray gun pressure is small, and gas grinding and polishing light action can be caused poor, when the spray gun pressure that gas grinds polish brush is 0.8kPa When, the light effect of gas grinding and polishing at this time is good, and the paraffin oil rate of drying of wood surface is fast, and paint film is completely uniform, is conducive to improve life Produce the aesthetics of efficiency and wood surface.
Specific implementation mode
Below in conjunction with embodiment, the present invention is further illustrated.
English walnut wood gas grinding process, includes the following steps, a, pre-treatment:Polishing and dedusting are carried out to timber table to wood surface B, the smooth no particle in face is coated with one layer of wood wax oil in wood surface, c, is polished to wood surface with gas mill polish brush, until wood D, the haze tallow oil reservoir on material surface carries out second polishing to wood with sand paper more than 1200 mesh without impression of the hand to the timber after gas grinding and polishing light Material Surface feel is smooth, e, repeats step b, c, d at least once.
It in step b, when applying wood wax oil, is carried out in the environment of room temperature and well-ventilated, accelerates the air of haze tallow oil meter face Flowing improves wood wax oil drying efficiency, by the grain direction brushing wood wax oil of timber so that wood wax oil can preferably infiltrate through wood Inside material, to preferably be protected to timber.
In step b, wood wax oil is counted in parts by weight, and component includes, 60% vegetable oil, 12% linseed wax, 2% Brazil wax, 25% D40 solvent naphthas, 0.2% ultra-violet absorber, 0.3% antifoaming agent, 0.5% drier. The component safety and environmental protection of wood wax oil, and rate of drying is fast, the haze tallow oil reservoir of formation has certain intensity, and glossiness is good, physical beauty It sees, and protective value is good.
In step b, linseed wax is the mixture of the linseed outer layer wax and internal layer wax of extraction, and linseed outer layer The mass ratio of wax and internal layer wax is 3:2.Using the compatibility of internal layer wax and wood raw material, wood internal can be goed deep into, moistened The conjugation of timber and wood wax oil is improved in unseasoned lumber duct.
In step c, the spray gun pressure that gas grinds polish brush is 0.5kPa-1.2kPa, and spray gun pressure is big, can damage wood surface Haze tallow oil reservoir, spray gun pressure is small, and gas grinding and polishing light action can be caused poor, when gas grind polish brush spray gun pressure be 0.8kPa when, The light effect of gas grinding and polishing at this time is good, and the paraffin oil rate of drying of wood surface is fast, and paint film is completely uniform, is conducive to improve production effect The aesthetics of rate and wood surface.
On the one hand, in the present invention, relative to the method for traditional timber standing and drying for being coated with wood wax oil, pass through gas Grinding and polishing light, which brushes, wipes wood surface, accelerates the flowing of wood surface air so that wood wax oil energy rapid osmotic enters wood internal, and dry Dry speed is fast, and production efficiency is high, wood wax oil energy Quick uniform infiltrates through that wood internal, wood surface gloss is uniform and stable, appearance It is beautiful.Second aspect carries out timber using sand paper more than 1200 mesh after being handled timber using gas mill polish brush Second polishing so that wood surface is smooth and glossiness is good, further improves timber surface aesthetics.The third aspect repeats Gas grinding and polishing light and sand paper polishing step are twice so that the haze tallow oil reservoir of wood surface has certain thickness, and high mechanical strength can be more Good protection timber.
Several embodiments of the invention above described embodiment only expresses, the description thereof is more specific and detailed, but simultaneously Cannot the limitation to the scope of the claims of the present invention therefore be interpreted as.It should be pointed out that for those of ordinary skill in the art For, without departing from the inventive concept of the premise, various modifications and improvements can be made, these belong to the guarantor of the present invention Protect range.Therefore, the protection domain of patent of the present invention should be determined by the appended claims.

Claims (5)

1. English walnut wood gas grinding process, it is characterised in that:Include the following steps, a, pre-treatment:It is polished wood surface and is removed B, dirt is coated with one layer of wood wax oil to wood surface smooth no particle in wood surface, c, ground with gas polish brush to wood surface into Row polishing, until d, the haze tallow oil reservoir of wood surface carries out the timber after gas grinding and polishing light with sand paper more than 1200 mesh without impression of the hand Second polishing to wood surface is smooth to the touch, and e, repeats step b, c, d at least once.
2. English walnut wood gas grinding process according to claim 1, it is characterised in that:In step b, when applying wood wax oil, in room temperature And carried out in the environment of well-ventilated, and by the grain direction brushing wood wax oil of timber.
3. English walnut wood gas grinding process according to claim 2, it is characterised in that:In step b, wood wax oil is in parts by weight Meter, component includes, 60% vegetable oil, 12% linseed wax, 2% Brazil wax, 25% D40 solvent naphthas, 0.2% ultra-violet absorber, 0.3% antifoaming agent, 0.5% drier.
4. English walnut wood gas grinding process according to claim 3, it is characterised in that:In step b, linseed wax is the Asia of extraction The mixture of numb seed outer layer wax and internal layer wax, and the mass ratio of linseed outer layer wax and internal layer wax is 3:2.
5. English walnut wood gas grinding process according to claim 4, it is characterised in that:In step c, gas grinds the spray gun pressure of polish brush Power is 0.5kPa-1.2kPa.
CN201810294902.9A 2018-03-30 2018-03-30 English walnut wood gas grinding process Pending CN108544626A (en)