CN108165833A - 一种阻隔防爆材料 - Google Patents

一种阻隔防爆材料 Download PDF

Info

Publication number
CN108165833A
CN108165833A CN201711429415.0A CN201711429415A CN108165833A CN 108165833 A CN108165833 A CN 108165833A CN 201711429415 A CN201711429415 A CN 201711429415A CN 108165833 A CN108165833 A CN 108165833A
Authority
CN
China
Prior art keywords
explosion
component
proof
present
block blast
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201711429415.0A
Other languages
English (en)
Inventor
李蓓
韩建乐
张玲
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Luoyang Mingli Science and Technology Development Co Ltd
Original Assignee
Luoyang Mingli Science and Technology Development Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Luoyang Mingli Science and Technology Development Co Ltd filed Critical Luoyang Mingli Science and Technology Development Co Ltd
Priority to CN201711429415.0A priority Critical patent/CN108165833A/zh
Publication of CN108165833A publication Critical patent/CN108165833A/zh
Pending legal-status Critical Current

Abstract

一种阻隔防爆材料,其组分及各组分的质量百分含量为:Mg 0.05‑0.07%,Cu 0.4‑0.8%,Si 0.4‑0.8%,Pd 0.4‑0.8%,Ba 0.4‑0.8%,Bi 0.4‑0.8%,Fe 0.5‑1.0%,Mn 1.0‑2.0%,Ti 0.1‑0.3%,Cr 0.03‑0.06%,余量为Al。借由上述技术方案,本发明提出的防爆材料添加一定量的镁、钛和铬,并通过其他金属元素的合理配比有效提高材料的耐腐蚀性能、屈服强度和抗拉前度,制造成本低廉同时具有更好的耐腐蚀性能、防爆性能,使用更安全、可靠。

Description

一种阻隔防爆材料
技术领域
本发明属于金属材料领域,特别是涉及一种阻隔防爆材料。
背景技术
阻隔防爆材料可以有效地防止液态易燃易爆物品在储存、运输等过程中发生爆炸。阻隔防爆材料主要是由金属箔通过剪切、拉伸形成网状结构后填充进容器、储罐中实现防爆。因此决定防爆储罐的性能的因素主要有防爆材料的化学性能及填充的效果,填充效果不仅可以依靠填充材料的结构来改善,还可以通过化学方法改变防爆材料的物理性能,提高防爆材料的强度、韧性来实现。目前现有的防爆材料在强度、韧性及耐腐蚀性能方面均有待提高。
发明内容
本发明的目的在于,克服现有防爆材料的缺陷,而提出一种具有更高的强度、韧性的成本低廉的防爆材料,从而更加适于实用。
本发明的目的及解决其技术问题是采用以下技术方案来实现。依据本发明提出的一种防爆材料,其组分及各组分的质量百分含量为Mg 0.05-0.07%,Cu 0.4-0.8%,Si0.4-0.8%,Pd 0.4-0.8%,Ba 0.4-0.8%,Bi 0.4-0.8%,Fe 0.5-1.0%,Mn 1.0-2.0%,Ti0.1-0.3%,Cr 0.03-0.06%,余量为Al。
本发明的目的及解决其技术问题还采用以下技术措施来进一步实现。
前述的防爆材料,其组分及各组分的质量百分含量为Mg 0.06-0.07%,Cu 0.6-0.8%,Si 0.6-0.8%,Pd 0.6-0.8%,Ba 0.6-0.8%,Bi 0.6-0.8%,Fe 0.6-1.0%,Mn1.2-2.0%,Ti 0.2-0.3%,Cr 0.05-0.06%,余量为Al。
借由上述技术方案,本发明提出的防爆材料添加一定量的镁、钛和铬,并通过其他金属元素的合理配比有效提高材料的耐腐蚀性能、屈服强度和抗拉前度,制造成本低廉同时具有更好的耐腐蚀性能、防爆性能,使用更安全、可靠。
上述说明仅是本发明技术方案的概述,为了能够更清楚了解本发明的技术手段,而可依照说明书的内容予以实施,并且为了让本发明的上述和其他目的、特征和优点能够更明显易懂,以下特举较佳实施例详细说明。
具体实施方式
实施例1
本发明一种成本低廉的防爆材料,其组分及各组分的质量百分含量为Mg 0.06%,Cu 0.6%,Si 0.6%,Pd 0.6%,Ba 0.6%,Bi 0.6%,Fe 0.6%,Mn 1.4%,Ti 0.2%,Cr0.05%,余量为Al。
实施例2
本发明一种成本低廉的防爆材料,其组分及各组分的质量百分含量为Mg 0.07%,Cu 0.8%,Si 0.8%,Pd 0.8%,Ba 0.8%,Bi 0.8%,Fe 1.0%,Mn 2.0%,Ti0.3%,Cr0.06%,余量为Al。
实施例3
本发明一种成本低廉的防爆材料,其组分及各组分的质量百分含量为Mg 0.05%,Cu 0.4%,Si 0.4%,Pd 0.4%,Ba 0.4%,Bi 0.4%,Fe 0.5%,Mn 1.0%,Ti 0.1%,Cr0.03%,余量为Al。
以上所述,仅是本发明的较佳实施例而已,并非对本发明做任何形式上的限制,虽然本发明已以较佳实施例揭露如上,然而并非用以限定本发明,任何熟悉本专业的技术人员,在不脱离本发明技术方案范围内,当可利用上述揭示的技术内容做出些许更动或修饰为等同变化的等效实施例,但凡是未脱离本发明技术方案的内容,依据本发明的技术实质对以上实施例所做的任何简单修改、等同变化与修饰,均仍属于本发明技术方案的范围内。

Claims (2)

1.一种阻隔防爆材料,其特征在于:其组分及各组分的质量百分含量为:Mg 0.05-0.07%,Cu 0.4-0.8%,Si 0.4-0.8%,Pd 0.4-0.8%,Ba 0.4-0.8%,Bi 0.4-0.8%,Fe0.5-1.0%,Mn 1.0-2.0%,Ti 0.1-0.3%,Cr 0.03-0.06%,余量为Al。
2.根据权利要求1所述的阻隔防爆材料,其特征在于:其组分及各组分的质量百分含量为:Mg 0.06-0.07%,Cu 0.6-0.8%,Si 0.6-0.8%,Pd 0.6-0.8%,Ba 0.6-0.8%,Bi 0.6-0.8%,Fe 0.6-1.0%,Mn 1.2-2.0%,Ti 0.2-0.3%,Cr 0.05-0.06%,余量为Al。
CN201711429415.0A 2017-12-26 2017-12-26 一种阻隔防爆材料 Pending CN108165833A (zh)