CN107905551A - 墙体的加固结构施工方法 - Google Patents

墙体的加固结构施工方法 Download PDF

Info

Publication number
CN107905551A
CN107905551A CN201711245741.6A CN201711245741A CN107905551A CN 107905551 A CN107905551 A CN 107905551A CN 201711245741 A CN201711245741 A CN 201711245741A CN 107905551 A CN107905551 A CN 107905551A
Authority
CN
China
Prior art keywords
deformed bar
wall
reinforcing rib
grouting pipe
slurries
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201711245741.6A
Other languages
English (en)
Other versions
CN107905551B (zh
Inventor
朱奎
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Anhui Tianli Huaneng Construction Engineering Co ltd
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201711245741.6A priority Critical patent/CN107905551B/zh
Publication of CN107905551A publication Critical patent/CN107905551A/zh
Application granted granted Critical
Publication of CN107905551B publication Critical patent/CN107905551B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种墙体的加固结构施工方法,其特征是墙体加固施工步骤采用如下:(1)剥离粉刷层,预钻注浆管的埋设孔;(2)挂设预应力钢筋;(3)在预应力钢筋上面挂设加强筋;(4)对预应力钢筋进行预应力张拉;(5)预应力张拉完毕后用固定筋将预应力钢筋进行焊接锚定,将预应力钢筋与加强筋进行焊接固定;(6)埋设注浆管,注浆管与埋设孔的空隙采用结构胶进行封闭;(7)对墙体进行注浆。

Description

墙体的加固结构施工方法
技术领域
本发明涉及一种墙体施工方法,特别涉及一种墙体的加固结构施工方法。
背景技术
旧建筑物经长期使用后因各种原因会出现承载力下降的现象,主要表现在旧建筑物的墙体因沉降等原因出现裂缝,或者墙体承载力不能满足现有荷载的要求;旧建筑物的混凝土梁因混凝土碳化会出现承载力下降,或者因使用标准的提升而出现承载力不能达到要求。因此对于旧建筑物,要加强结构的整体承力效果,改善结构的力学性能。
发明内容
本发明是提供一种墙体的加固结构施工方法,解决墙体承载力的问题。
本发明针对墙体强度不够,采取以下加固结构:墙体剥离粉刷后在墙体表面布置一皮预应力钢筋,预应力钢筋直径为12~14mm,预应力钢筋间距为150~300mm,预应力钢筋上面再布置非预应力加强筋,预应力钢筋与加强筋进行焊接连接,加强筋直径为12~14mm,加强筋钢筋间距为150~300mm。预应力钢筋初布置方向与水平夹角为45度,加强筋布置方向与预应力钢筋初布置方向垂直。预应力钢筋张拉完毕后将预应力钢筋通过固定筋进行固定,固定筋与预应力钢筋进行焊接固定,固定筋直径为14~16mm。固定筋间距为150~300mm,每个张拉单元长度为150~300mm,在张拉单元的两个端头设置加强筋。预应力钢筋与非预应力加强筋形成的张拉单元内布置注浆管,注浆管间距为350~450mm,注浆管为直径10mm的不锈钢钢管,注浆管埋入墙体灰缝,埋入深度为60mm,用结构胶进行固定。注浆管与储浆罐之间设置三通阀门。
还可以采用下列加固结构:墙体剥离粉刷后在墙体表面布置一皮预应力钢筋,预应力钢筋直径为12~14mm,预应力钢筋间距为150~300mm,预应力钢筋上面再布置非预应力加强筋,预应力钢筋与加强筋进行焊接连接,加强筋直径为12~14mm,加强筋钢筋间距为150~300mm。预应力钢筋初布置方向为水平,加强筋布置方向为竖向布置。预应力钢筋张拉完毕后将预应力钢筋通过固定筋进行固定,固定筋与预应力钢筋进行焊接固定,固定筋直径为14~16mm。固定筋间距为300~600mm,每个张拉单元长度为300~600mm,在张拉单元的两个端头设置加强筋,在端头竖向加强筋和竖向固定筋之间布置一排加强筋。预应力钢筋与非预应力加强筋形成的张拉单元内布置注浆管,注浆管间距为350~450mm,注浆管为直径10mm的不锈钢钢管,注浆管埋入墙体灰缝,埋入深度为60mm,用结构胶进行固定。注浆管与储浆罐之间设置三通阀门。
墙体表面设置预应力钢筋后,墙体结构性能会有很大的提升,即使是结构的破坏形态也会很大的改善,会从塑性破坏过渡到弹性破坏,对结构安全会有显著的作用。
墙体加固施工步骤采用如下:
(1)剥离粉刷层,预钻注浆管的埋设孔,注浆管的埋设孔直径为12mm;预钻埋设孔使用电动旋转金刚石取芯钻,用水冷却钻头并带出砖屑;采用钢丝清理墙体表面的灰尘及浮渣或者松散部位并保持干燥;
(2)挂设预应力钢筋,通过U形铁扣将预应力钢筋固定在墙体,U形铁扣插入墙体灰缝;
(3)在预应力钢筋上面挂设加强筋,用钢丝将预应力钢筋与加强筋进行初步连接;
(4)对预应力钢筋进行预应力张拉,预应力钢筋张拉采用杠杆式夹紧工具,杠杆式夹紧工具的阻力臂与动力臂的比值为0.05~0.15。张拉工艺采用如下:将预应力钢筋初张拉张拉至10%的控制张拉应力,持荷3min建立初始应力,再张拉至控制张拉应力,持荷5min建立预应力。
(5)预应力张拉完毕后用固定筋将预应力钢筋进行焊接锚定,将预应力钢筋与加强筋进行焊接固定;
(6)埋设注浆管,注浆管与埋设孔的空隙采用结构胶进行封闭;
(7)对墙体进行注浆;用压力注浆机械浆液注入墙体,注浆从最下排位置开始,逐步向上和对称向两侧发展,在每一个注射点达到预期压力或者浆液在邻近注射点自由流出,注射方可终止,把注射孔堵塞。
如果浆液有渗漏,如找不到漏失通道,将浆液掺入速凝剂持续小量的注射使漏失通道逐渐沉淀堵塞。
浆液完全凝固后,拆除注浆管并进行封孔。
如果墙体有裂缝,在步骤(7)前要进行以下处理:
1)在裂缝中部埋设灌浆嘴,灌注点间距根据裂缝宽度和裂缝深度综合确定,间距为200~300mm;
2)封闭裂缝,灌浆嘴埋设后采用环氧胶泥封闭,形成一个密闭空间,预留浆液进出口,再用针筒将浆液压入缝隙,使其注满。
3)密封检查,沿裂缝涂一层肥皂,从灌浆嘴通入压缩空气,漏气部位予以修补密封至不漏为止。
4)灌浆,当裂缝宽度小于0.3mm时,采用环氧胶泥封闭裂缝后,再采用甲基丙烯酸脂类浆液灌注;当裂缝宽度大于或等于0.3mm且小于1mm时,采用环氧树脂类浆液灌注;当裂缝宽度大于或等于1mm时,采用水泥浆液灌注。
本发明结构性能好,安全可靠。
附图说明
图1为墙体加固结构示意图一,图2为墙体加固结构示意图二。
各附图中:1、预应力钢筋,2、加强筋,3、固定筋,4、注浆管,5、角钢,6、紧固螺杆,7、钢板,8、缀板。
具体实施方式
实施例一
本实施例针对墙体强度不够,采取以下加固结构:墙体剥离粉刷后在墙体表面布置一皮预应力钢筋1,预应力钢筋1直径为12mm,预应力钢筋1间距为200mm,预应力钢筋1上面再布置非预应力加强筋2,预应力钢筋1与加强筋2进行焊接连接,加强筋2直径为12mm,加强筋2钢筋间距为200mm。预应力钢筋1初布置方向与水平夹角为45度,加强筋2布置方向与预应力钢筋1初布置方向垂直,预应力钢筋1初布置为图1虚线位置,预应力钢筋1经张拉后变成实线位置。预应力钢筋1张拉完毕后将预应力钢筋1通过固定筋3进行固定,固定筋3与预应力钢筋1进行焊接固定,固定筋3直径为14mm。固定筋3间距为200mm,每个张拉单元长度为200mm,在张拉单元的两个端头设置加强筋2。预应力钢筋1与非预应力加强筋2形成的张拉单元内布置注浆管4,注浆管4间距为400mm,注浆管4为直径10mm的不锈钢钢管,注浆管4埋入墙体灰缝,埋入深度为60mm,用结构胶进行固定。注浆管4与储浆罐之间设置三通阀门。
还可以采用下列加固结构:墙体剥离粉刷后在墙体表面布置一皮预应力钢筋1,预应力钢筋1直径为12mm,预应力钢筋1间距为200mm,预应力钢筋1上面再布置非预应力加强筋2,预应力钢筋1与加强筋2进行焊接连接,加强筋2直径为12mm,加强筋2钢筋间距为200mm。预应力钢筋1初布置方向为水平,加强筋2布置方向为竖向布置,预应力钢筋1初布置为图2虚线位置,预应力钢筋1经张拉后变成实线位置。预应力钢筋1张拉完毕后将预应力钢筋1通过固定筋3进行固定,固定筋3与预应力钢筋1进行焊接固定,固定筋3直径为14~16mm。固定筋3间距为400mm,每个张拉单元长度为400mm,在张拉单元的两个端头设置加强筋2,在端头竖向加强筋2和竖向固定筋3之间布置一排加强筋2。预应力钢筋1与非预应力加强筋2形成的张拉单元内布置注浆管4,注浆管4间距为400mm,注浆管4为直径10mm的不锈钢钢管,注浆管4埋入墙体灰缝,埋入深度为60mm,用结构胶进行固定。注浆管4与储浆罐之间设置三通阀门。
墙体加固施工步骤采用如下:
(1)剥离粉刷层,预钻注浆管4的埋设孔,注浆管4的埋设孔直径为12mm;预钻埋设孔使用电动旋转金刚石取芯钻,用水冷却钻头并带出砖屑;采用钢丝清理墙体表面的灰尘及浮渣或者松散部位并保持干燥;
(2)挂设预应力钢筋1,通过U形铁扣将预应力钢筋1固定在墙体,U形铁扣插入墙体灰缝;
(3)在预应力钢筋1上面挂设加强筋2,用钢丝将预应力钢筋1与加强筋2进行初步连接;
(4)对预应力钢筋1进行预应力张拉,预应力钢筋1张拉采用杠杆式夹紧工具,杠杆式夹紧工具的阻力臂与动力臂的比值为0.05~0.15。张拉工艺采用如下:将预应力钢筋1初张拉张拉至10%的控制张拉应力,持荷3min建立初始应力,再张拉至控制张拉应力,持荷5min建立预应力。
(5)预应力张拉完毕后用固定筋3将预应力钢筋1进行焊接锚定,将预应力钢筋1与加强筋2进行焊接固定;
(6)埋设注浆管4,注浆管4与埋设孔的空隙采用结构胶进行封闭;
(7)对墙体进行注浆;用压力注浆机械浆液注入墙体,注浆从最下排位置开始,逐步向上和对称向两侧发展,在每一个注射点达到预期压力或者浆液在邻近注射点自由流出,注射方可终止,把注射孔堵塞。
如果浆液有渗漏,如找不到漏失通道,将浆液掺入速凝剂持续小量的注射使漏失通道逐渐沉淀堵塞。
浆液完全凝固后,拆除注浆管4并进行封孔。
如果墙体有裂缝,在步骤(7)前要进行以下处理:
1)在裂缝中部埋设灌浆嘴,灌注点间距根据裂缝宽度和裂缝深度综合确定,间距为200~300mm;
2)封闭裂缝,灌浆嘴埋设后采用环氧胶泥封闭,形成一个密闭空间,预留浆液进出口,再用针筒将浆液压入缝隙,使其注满。
3)密封检查,沿裂缝涂一层肥皂,从灌浆嘴通入压缩空气,漏气部位予以修补密封至不漏为止。
4)灌浆,当裂缝宽度小于0.3mm时,采用环氧胶泥封闭裂缝后,再采用甲基丙烯酸脂类浆液灌注;当裂缝宽度大于或等于0.3mm且小于1mm时,采用环氧树脂类浆液灌注;当裂缝宽度大于或等于1mm时,采用水泥浆液灌注。
实施例二
本实施例采用下列加固结构:墙体剥离粉刷后在墙体表面布置一皮预应力钢筋1,预应力钢筋1直径为12mm,预应力钢筋1间距为200mm,预应力钢筋1上面再布置非预应力加强筋2,预应力钢筋1与加强筋2进行焊接连接,加强筋2直径为12mm,加强筋2钢筋间距为200mm。预应力钢筋1初布置方向为水平,加强筋2布置方向为竖向布置,预应力钢筋1初布置为图2虚线位置,预应力钢筋1经张拉后变成实线位置。预应力钢筋1张拉完毕后将预应力钢筋1通过固定筋3进行固定,固定筋3与预应力钢筋1进行焊接固定,固定筋3直径为14~16mm。固定筋3间距为400mm,每个张拉单元长度为400mm,在张拉单元的两个端头设置加强筋2,在端头竖向加强筋2和竖向固定筋3之间布置一排加强筋2。预应力钢筋1与非预应力加强筋2形成的张拉单元内布置注浆管4,注浆管4间距为400mm,注浆管4为直径10mm的不锈钢钢管,注浆管4埋入墙体灰缝,埋入深度为60mm,用结构胶进行固定。注浆管4与储浆罐之间设置三通阀门。
墙体加固施工步骤采用如下:
(1)剥离粉刷层,预钻注浆管4的埋设孔,注浆管4的埋设孔直径为12mm;预钻埋设孔使用电动旋转金刚石取芯钻,用水冷却钻头并带出砖屑;采用钢丝清理墙体表面的灰尘及浮渣或者松散部位并保持干燥;
(2)挂设预应力钢筋1,通过U形铁扣将预应力钢筋1固定在墙体,U形铁扣插入墙体灰缝;
(3)在预应力钢筋1上面挂设加强筋2,用钢丝将预应力钢筋1与加强筋2进行初步连接;
(4)对预应力钢筋1进行预应力张拉,预应力钢筋1张拉采用杠杆式夹紧工具,杠杆式夹紧工具的阻力臂与动力臂的比值为0.05~0.15。张拉工艺采用如下:将预应力钢筋1初张拉张拉至10%的控制张拉应力,持荷3min建立初始应力,再张拉至控制张拉应力,持荷5min建立预应力。
(5)预应力张拉完毕后用固定筋3将预应力钢筋1进行焊接锚定,将预应力钢筋1与加强筋2进行焊接固定;
(6)埋设注浆管4,注浆管4与埋设孔的空隙采用结构胶进行封闭;
(7)对墙体进行注浆;用压力注浆机械浆液注入墙体,注浆从最下排位置开始,逐步向上和对称向两侧发展,在每一个注射点达到预期压力或者浆液在邻近注射点自由流出,注射方可终止,把注射孔堵塞。
如果浆液有渗漏,如找不到漏失通道,将浆液掺入速凝剂持续小量的注射使漏失通道逐渐沉淀堵塞。
浆液完全凝固后,拆除注浆管4并进行封孔。
如果墙体有裂缝,在步骤(7)前要进行以下处理:
1)在裂缝中部埋设灌浆嘴,灌注点间距根据裂缝宽度和裂缝深度综合确定,间距为200~300mm;
2)封闭裂缝,灌浆嘴埋设后采用环氧胶泥封闭,形成一个密闭空间,预留浆液进出口,再用针筒将浆液压入缝隙,使其注满。
3)密封检查,沿裂缝涂一层肥皂,从灌浆嘴通入压缩空气,漏气部位予以修补密封至不漏为止。
4)灌浆,当裂缝宽度小于0.3mm时,采用环氧胶泥封闭裂缝后,再采用甲基丙烯酸脂类浆液灌注;当裂缝宽度大于或等于0.3mm且小于1mm时,采用环氧树脂类浆液灌注;当裂缝宽度大于或等于1mm时,采用水泥浆液灌注。

Claims (1)

1.一种墙体的加固结构施工方法,其特征是墙体加固采取如下:墙体剥离粉刷后在墙体表面布置一皮预应力钢筋,预应力钢筋直径为12~14mm,预应力钢筋间距为150~300mm,预应力钢筋上面再布置非预应力加强筋,预应力钢筋与加强筋进行焊接连接,加强筋直径为12~14mm,加强筋钢筋间距为150~300mm;预应力钢筋张拉完毕后将预应力钢筋通过固定筋进行固定,固定筋与预应力钢筋进行焊接固定,固定筋直径为14~16mm;预应力钢筋与非预应力加强筋形成的张拉单元内布置注浆管,注浆管间距为350~450mm,注浆管为直径10mm的不锈钢钢管,注浆管埋入墙体灰缝,埋入深度为60mm,用结构胶进行固定;注浆管与储浆罐之间设置三通阀门;
预应力钢筋初布置方向与水平夹角为45度,加强筋布置方向与预应力钢筋初布置方向垂直;固定筋间距为150~300mm,每个张拉单元长度为150~300mm,在张拉单元的两个端头设置加强筋;
墙体加固施工步骤采用如下:
(1)剥离粉刷层,预钻注浆管的埋设孔,注浆管的埋设孔直径为12mm;预钻埋设孔使用电动旋转金刚石取芯钻,用水冷却钻头并带出砖屑;采用钢丝清理墙体表面的灰尘及浮渣或者松散部位并保持干燥;
(2)挂设预应力钢筋,通过U形铁扣将预应力钢筋固定在墙体,U形铁扣插入墙体灰缝;
(3)在预应力钢筋上面挂设加强筋,用钢丝将预应力钢筋与加强筋进行初步连接;
(4)对预应力钢筋进行预应力张拉,预应力钢筋张拉采用杠杆式夹紧工具,杠杆式夹紧工具的阻力臂与动力臂的比值为0.05~0.15;张拉工艺采用如下:将预应力钢筋初张拉张拉至10%的控制张拉应力,持荷3min建立初始应力,再张拉至控制张拉应力,持荷5min建立预应力;
(5)预应力张拉完毕后用固定筋将预应力钢筋进行焊接锚定,将预应力钢筋与加强筋进行焊接固定;
(6)埋设注浆管,注浆管与埋设孔的空隙采用结构胶进行封闭;
(7)对墙体进行注浆;用压力注浆机械浆液注入墙体,注浆从最下排位置开始,逐步向上和对称向两侧发展,在每一个注射点达到预期压力或者浆液在邻近注射点自由流出,注射方可终止,把注射孔堵塞;
如果浆液有渗漏,如找不到漏失通道,将浆液掺入速凝剂持续小量的注射使漏失通道逐渐沉淀堵塞;
浆液完全凝固后,拆除注浆管并进行封孔;
如果墙体有裂缝,在步骤(7)前要进行以下处理:
1)在裂缝中部埋设灌浆嘴,灌注点间距根据裂缝宽度和裂缝深度综合确定,间距为200~300mm;
2)封闭裂缝,灌浆嘴埋设后采用环氧胶泥封闭,形成一个密闭空间,预留浆液进出口,再用针筒将浆液压入缝隙,使其注满;
3)密封检查,沿裂缝涂一层肥皂,从灌浆嘴通入压缩空气,漏气部位予以修补密封至不漏为止;
4)灌浆,当裂缝宽度小于0.3mm时,采用环氧胶泥封闭裂缝后,再采用甲基丙烯酸脂类浆液灌注;当裂缝宽度大于或等于0.3mm且小于1mm时,采用环氧树脂类浆液灌注;当裂缝宽度大于或等于1mm时,采用水泥浆液灌注。
CN201711245741.6A 2016-05-21 2016-05-21 墙体的加固结构施工方法 Active CN107905551B (zh)