CN107892854A - Formula of leather color inhibition synthesis resin and preparation method thereof - Google Patents

Formula of leather color inhibition synthesis resin and preparation method thereof Download PDF

Info

Publication number
CN107892854A
CN107892854A CN201711319279.XA CN201711319279A CN107892854A CN 107892854 A CN107892854 A CN 107892854A CN 201711319279 A CN201711319279 A CN 201711319279A CN 107892854 A CN107892854 A CN 107892854A
Authority
CN
China
Prior art keywords
parts
formula
color inhibition
leather
synthesis resin
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201711319279.XA
Other languages
Chinese (zh)
Inventor
马峰
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Guangzhou Mcgee Macromolecule Material Co Ltd
Original Assignee
Guangzhou Mcgee Macromolecule Material Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Guangzhou Mcgee Macromolecule Material Co Ltd filed Critical Guangzhou Mcgee Macromolecule Material Co Ltd
Priority to CN201711319279.XA priority Critical patent/CN107892854A/en
Publication of CN107892854A publication Critical patent/CN107892854A/en
Pending legal-status Critical Current

Abstract

A kind of formula of leather color inhibition synthesis resin, it is related to the resistance to yellow formula of leather, the component of the formula is color inhibition acrylic emulsion, paraffin wax emulsions, filler, thickener, hollow polymer spheroid, PH conditioning agents, defoamer, preservative and water;The parts by weight of the formula each component are 200 400 parts of 200 300 parts of color inhibition acrylic emulsion, 100 200 parts of paraffin wax emulsions, 80 160 parts of filler, 10 30 parts of thickener, 50 100 parts of hollow polymer spheroid, 10 30 parts of PH conditioning agents, 10 30 parts of defoamer, 50 100 parts of preservative and water.Glossiness, polish retention, non-plastic, the resistance to bent rich property of leather can additionally be increased, make the leather hand feeling after processing comfortable;And without the organic solvents such as APES class compound, safety and environmental protection in the formula.

Description

Formula of leather color inhibition synthesis resin and preparation method thereof
Technical field:
The present invention relates to the resistance to yellow formula of leather, and in particular to a kind of formula of leather color inhibition synthesis resin and its preparation side Method.
Background technology:
Color inhibition synthesis resin is can directly to add the product that pigment paste is covered with paint, lacquer, colour wash, etc., and the pulp layer allocated instead of skin factory worker can To save factory work intensity, operating efficiency is improved.Current most of synthesis resin is all unable to color inhibition, limits making for factory With in order to solve the above-mentioned technical problem, spy proposes a kind of new technical scheme.
The content of the invention:
In place of overcoming above-mentioned the shortcomings of the prior art, and provide a kind of leather color inhibition Formula of synthesis resin and preparation method thereof.
The technical solution adopted by the present invention is:A kind of formula of leather color inhibition synthesis resin, the component of the formula is resistance to Xanthochromia acrylic emulsion, paraffin wax emulsions, filler, thickener, hollow polymer spheroid, PH conditioning agents, defoamer, preservative and Water;The parts by weight of the formula each component are color inhibition acrylic emulsion 200-300 parts, paraffin wax emulsions 100-200 parts, filler 80-160 parts, thickener 10-30 parts, hollow polymer spheroid 50-100 parts, PH conditioning agent 10-30 parts, defoamer 10-30 parts, Preservative 50-100 parts and water 200-400 parts.
The parts by weight of the formula each component be color inhibition acrylic emulsion 250-260 parts, paraffin wax emulsions 150-160 parts, Filler 100-130 parts, thickener 15-20 parts, hollow polymer spheroid 70-80 parts, PH conditioning agent 20-26 parts, defoamer 15-20 Part, preservative 6-8 parts and water 250-300 parts.
Described color inhibition acrylic emulsion is by ethyl acrylate, acrylic acid, lauryl sodium sulfate and activated zinc oxide Composition;The parts by weight of the color inhibition acrylic emulsion each component are ethyl acrylate 50-100 parts, acrylic acid 20-50 parts, ten Sodium dialkyl sulfate 3-5 parts and activated zinc oxide 5-7 parts.
Described filler is made up of kaolin and cellulose;The filler each component parts by weight are kaolin 200-250 parts And cellulose 10-20 parts.
Described thickener is alkali swollen thickener.
Described preservative is made up of water lily fibrin, streptococcus lactis and Tea Polyphenols;The weight of the preservative each component It is water lily fibrin 1-3 parts, streptococcus lactis 2-5 parts and Tea Polyphenols 1-6 parts to measure number.
Described described defoamer is the fatty acid ester compounded thing of higher alcohols or polyoxyethylene polyoxy propyl alcohol amidogen ether.
This method comprises the following steps:
Step 1: by water, acrylic emulsion, polyaminoester emulsion, liquid wax emulsion, filler, pH value conditioning agent and preservative It is separately added into order in reactor, side adds, while stirring, mixing speed is 600~1600r/min;
Step 2: thickener is added slowly thereto, mixing liquid is set gradually slowly to thicken, to reach preferable denseness (4# Ford cups 50~120 seconds);
Step 3: the mixed system after thickening is filtered, detection, the synthesis resin of water-based color inhibition is obtained;
This method reaction condition is lower 5 DEG C~35 DEG C of normal temperature condition.
Beneficial effects of the present invention are:This formula has preferably embossing constancy, and film forming is soft, and covering is strong.This Glossiness, polish retention, non-plastic, the resistance to bent rich property of leather can also be increased outside, make the leather hand feeling after processing comfortable;And And without the organic solvents such as APES class compound, safety and environmental protection in the formula;The preparation method letter of the formula Single practical, consersion unit is not required to particularly customized, common mixer and the production of dispersion impeller can, and this method is prepared Leather finishing agent there is better stability, preparation method process stabilizing, be adapted to industrialized production.In addition, this method is prepared into The properties of product arrived are very outstanding, and use range is wide, reduce the probability using factory's compounding mistake, removed from office especially suitable for white, Color inhibition quality problems not up to standard and caused are avoided, can lift original Leather Properties, Leather Factory's also right and wrong when in use It is often convenient, it is simple to operate, it is cheap, factory's benefit can be lifted.
Embodiment:
The present invention is further described in conjunction with specific embodiments:
Embodiment one:
A kind of formula of leather color inhibition synthesis resin, the parts by weight of the formula each component are color inhibition acrylic emulsion 200 parts, 100 parts of paraffin wax emulsions, 80 parts of filler, 10 parts of thickener, 50 parts of hollow polymer spheroid, 10 parts of PH conditioning agents, defoaming 200 parts of 10 parts of agent, 50 parts of preservative and water.The parts by weight of the color inhibition acrylic emulsion each component are ethyl acrylate 50 Part, 20 parts of acrylic acid, 3 parts of lauryl sodium sulfate and 5 parts of activated zinc oxide.The filler each component parts by weight are kaolin 200 parts and 10 parts of cellulose.Described thickener is alkali swollen thickener.The parts by weight of the preservative each component are that water lily is fine 1 part of 1 part of fibrillarin, 2 parts of streptococcus lactis and Tea Polyphenols.Described described defoamer be the fatty acid ester compounded thing of higher alcohols or Polyoxyethylene polyoxy propyl alcohol amidogen ether.
Embodiment two:
A kind of formula of leather color inhibition synthesis resin, the parts by weight of the formula each component are color inhibition acrylic emulsion 150 parts, 150 parts of paraffin wax emulsions, 100 parts of filler, 20 parts of thickener, 90 parts of hollow polymer spheroid, 20 parts of PH conditioning agents, defoaming 300 parts of 20 parts of agent, 70 parts of preservative and water.The parts by weight of the color inhibition acrylic emulsion each component are ethyl acrylate 75 Part, 30 parts of acrylic acid, 4 parts of lauryl sodium sulfate and 6 parts of activated zinc oxide.The filler each component parts by weight are kaolin 220 parts and 15 parts of cellulose.Described thickener is alkali swollen thickener.The parts by weight of the preservative each component are that water lily is fine 5 parts of 2 parts of fibrillarin, 3 parts of streptococcus lactis and Tea Polyphenols.Described described defoamer be the fatty acid ester compounded thing of higher alcohols or Polyoxyethylene polyoxy propyl alcohol amidogen ether.
Embodiment three:
A kind of formula of leather color inhibition synthesis resin, the parts by weight of the formula each component are color inhibition acrylic emulsion 300 parts, 200 parts of paraffin wax emulsions, 160 parts of filler, 30 parts of thickener, 100 parts of hollow polymer spheroid, 30 parts of PH conditioning agents, disappear 400 parts of 30 parts of infusion, 100 parts of preservative and water.The parts by weight of the color inhibition acrylic emulsion each component are ethyl acrylate 7 parts of 100 parts, 50 parts of acrylic acid, 5 parts of lauryl sodium sulfate and activated zinc oxide.The filler each component parts by weight are kaolinite Native 250 parts and 20 parts of cellulose.Described thickener is alkali swollen thickener.The parts by weight of the preservative each component are water lily 6 parts of 3 parts of fibrin, 5 parts of streptococcus lactis and Tea Polyphenols.Described described defoamer is the fatty acid ester compounded thing of higher alcohols Or polyoxyethylene polyoxy propyl alcohol amidogen ether.
Three above embodiment is prepared using following preparation method:
This method comprises the following steps:
Step 1: by water, acrylic emulsion, polyaminoester emulsion, liquid wax emulsion, filler, defoamer and preservative by suitable Sequence is separately added into reactor, and side adds, while stirring, mixing speed is 600~1600r/min;
Step 2: thickener is added slowly thereto, mixing liquid is set gradually slowly to thicken, to reach preferable denseness (4# Ford cups 50~120 seconds);
Step 3: the mixed system after thickening is filtered, detection, the synthesis resin of water-based color inhibition is obtained.
Using effect is tested:
This research is examined the effect of the formula of leather color inhibition synthesis resin and preparation method thereof by 100 enterprises Examine, test event standards of grading are:Very satisfied 5 points, 4 points are satisfied with, general 3 points, is unsatisfied with 2 points, very dissatisfied 1 point.Its In common group be common leather color inhibition synthesis resin formula;
Test event Embodiment one Embodiment two Embodiment three Common group
The glossiness of leather 4.8 4.9 4.7 3.0
Polish retention 4.8 4.9 5.0 1.0
Non-plastic 4.7 4.9 4.8 3.0
Resistance to bent rich property 4.7 4.9 4.6 3.2
The feature of environmental protection 4.9 4.9 4.9 2.0
It is embossed constancy 4.7 4.9 4.8 3.0
Film flexibility 4.7 4.9 4.6 3.2
Covering 4.9 4.9 4.9 2.0
In summary, the present invention its not only can effectively solve the glossiness of leather, polish retention, non-plastic and resistance to The problem of bent rich property, and it is more healthy by human body with certain environmental-protecting performance.This formula has preferably embossing constancy, and Film forming is soft, and covering is strong.Glossiness, polish retention, non-plastic, the resistance to bent rich property of leather can additionally be increased, make place Leather hand feeling after reason is comfortable;And without the organic solvents such as APES class compound, safety collar in the formula Protect;The preparation method of the formula is simple and practical, and consersion unit is not required to particularly customized, common mixer and the life of dispersion impeller can Production, and the leather finishing agent that this method is prepared has better stability, preparation method process stabilizing, is adapted to industrial metaplasia Production.In addition, the properties of product that this method is prepared are very outstanding, use range is wide, reduces using the several of factory's compounding mistake Rate, removed from office especially suitable for white, avoid color inhibition quality problems not up to standard and caused, original Leather Properties can be lifted, Leather Factory be also when in use it is very convenient, it is simple to operate, it is cheap, factory's benefit can be lifted.
For those skilled in the art, it is various corresponding can be made according to above technical scheme and design for other Change and deformation, and all these change and deformation should all belong within the protection domain of the claims in the present invention.

Claims (9)

  1. A kind of 1. formula of leather color inhibition synthesis resin, it is characterised in that:The component of the formula be color inhibition acrylic emulsion, Paraffin wax emulsions, filler, thickener, hollow polymer spheroid, PH conditioning agents, defoamer, preservative and water;The formula each component Parts by weight are color inhibition acrylic emulsion 200-300 parts, paraffin wax emulsions 100-200 parts, filler 80-160 parts, thickener 10- 30 parts, hollow polymer spheroid 50-100 parts, PH conditioning agent 10-30 parts, defoamer 10-30 parts, preservative 50-100 parts and water 200-400 parts.
  2. 2. the formula of leather color inhibition synthesis resin according to claim 1, it is characterised in that:The weight of the formula each component Amount number is color inhibition acrylic emulsion 250-260 parts, paraffin wax emulsions 150-160 parts, filler 100-130 parts, thickener 15-20 Part, hollow polymer spheroid 70-80 parts, PH conditioning agent 20-26 parts, defoamer 15-20 parts, preservative 6-8 parts and water 250-300 Part.
  3. 3. the formula of leather color inhibition synthesis resin according to claim 1, it is characterised in that:Described color inhibition propylene Yogurt liquid is made up of ethyl acrylate, acrylic acid, lauryl sodium sulfate and activated zinc oxide;The color inhibition acrylic emulsion is each The parts by weight of component are ethyl acrylate 50-100 parts, acrylic acid 20-50 parts, lauryl sodium sulfate 3-5 parts and active oxygen Change zinc 5-7 parts.
  4. 4. the formula of leather color inhibition synthesis resin according to claim 1, it is characterised in that:Described filler is by kaolinite Soil and cellulose composition;The filler each component parts by weight are kaolin 200-250 parts and cellulose 10-20 parts.
  5. 5. the formula of leather color inhibition synthesis resin according to claim 1, it is characterised in that:Described thickener is alkali Swollen thickener.
  6. 6. the formula of leather color inhibition synthesis resin according to claim 1, it is characterised in that:Described preservative is by sleeping Lotus fibrin, streptococcus lactis and Tea Polyphenols composition;The parts by weight of the preservative each component are water lily fibrin 1-3 Part, streptococcus lactis 2-5 parts and Tea Polyphenols 1-6 parts.
  7. 7. the formula of leather color inhibition synthesis resin according to claim 1, it is characterised in that:Described described defoaming Agent is the fatty acid ester compounded thing of higher alcohols or polyoxyethylene polyoxy propyl alcohol amidogen ether.
  8. A kind of 8. preparation method of the formula of leather color inhibition synthesis resin, it is characterised in that:This method comprises the following steps:
    Step 1: by water, acrylic emulsion, polyaminoester emulsion, liquid wax emulsion, filler, pH value conditioning agent and preservative by suitable Sequence is separately added into reactor, and side adds, while stirring, mixing speed is 600~1600r/min;
    Step 2: thickener is added slowly thereto, mixing liquid is set gradually slowly to thicken, to reach preferable denseness (4# good fortune Special cup 50~120 seconds);
    Step 3: the mixed system after thickening is filtered, detection, the synthesis resin of water-based color inhibition is obtained;
  9. 9. the preparation method of the formula of leather color inhibition synthesis resin according to claim 8, it is characterised in that:This method Reaction condition is lower 5 DEG C~35 DEG C of normal temperature condition.
CN201711319279.XA 2017-12-12 2017-12-12 Formula of leather color inhibition synthesis resin and preparation method thereof Pending CN107892854A (en)